Search NASA⌕ Search

SEARCH · Search NASA

Results for “Capacity fade”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Life Prediction Model for Grid-Connected Li-ion Battery Energy Storage System

Lithium-ion (Li-ion) batteries are being deployed on the electrical grid for a variety of purposes, such as to smooth fluctuations in solar renewable power generation. The lifetime of these batteries will vary depending on their thermal environment and how they are charged and discharged. To optimal utilization of a battery over its lifetime requires characterization of its performance degradation under different storage and cycling conditions. Aging tests were conducted on commercial graphite/nickel-manganese-cobalt (NMC) Li-ion cells. A general lifetime prognostic model framework is applied to model changes in capacity and resistance as the battery degrades. Across 9 aging test conditions from 0oC to 55oC, the model predicts capacity fade with 1.4% RMS error and resistance growth with 15% RMS error. The model, recast in state variable form with 8 states representing separate fade mechanisms, is used to extrapolate lifetime for example applications of the energy storage system integrated with renewable photovoltaic (PV) power generation.

25 ENERGY STORAGE↗

Density impact on performance of composite Si/graphite electrodes

The ability of alkali-substituted binders for composite Si and graphite negative electrodes to minimize capacity fade for lithium ion batteries is investigated. Polymer films and electrodes are described and characterized by FTIR following immersion in electrolyte (1:2 EC:DMC) for 24 h. FTIR analysis following electrode formation displayed similar alkali-ion dependent shifts in peak location suggesting that changes in the vibrational structure of the binder are maintained after electrode formation. The Si and graphite composite electrodes prepared using the alkali-substituted polyacrylates were also exposed to electrochemical cycling and it has been found that the performance of the Na-substituted binder is superior to a comparable density K-substituted system. However, in comparing performance across many different electrode densities attention needs to be placed on making comparisons at similar densities, as low density electrodes tend to exhibit lower capacity fade over cycling. This is highlighted by a 6% difference between a low density K-substituted electrode and a high density Na-substituted sample. As a result, this low variance between the two systems makes it difficult to quickly make a direct evaluation of binder performance unless electrode density is tightly controlled.

25 ENERGY STORAGE↗

Probing how Ti- and Nb-substitution affect the stability and improve the electrochemical performance of β- and ε-LiVOPO 4

LiVOPO 4 is a promising next-generation multi-electron cathode material, boasting a theoretical capacity of 305 mA h g -1 , significantly higher than any commercially used Li-ion battery cathode material. However, the material still faces several limitations, including the difficulty in attaining the full theoretical capacity at higher rates and capacity fade over several cycles. Here, in this paper, we show that Ti- and Nb-substitution can be used to improve the thermal stability and electrochemical performance of LiVOPO 4 . We show through in situ heating with XRD and a novel gradient heating technique that both Ti- and Nb-substitution cause β-LiVOPO 4 to be stabilized relative to ε-LiVOPO 4 . This is due to transition-metal substitution, which increases the O-vacancy formation energies, pushing the β → ε transition to higher temperatures. We show that it is still possible to synthesize pure-phase ε-LiVOPO 4 through the use of high temperatures to generate these O-vacancies. We show that even 1% of Ti- or Nb-substitution can improve the initial capacity and long term cycling capability of LiVOPO 4 by improving the high-voltage capacity and reducing the capacity fade in both the high- and low-voltage regions. This is due to the overall improved Li + ion diffusion which is caused by an improved charge-transfer resistance during cycling.

25 ENERGY STORAGE↗

Modeling Stationary Lithium-Ion Batteries for Optimization and Predictive Control

Accurately modeling stationary battery storage behavior is crucial to understand and predict its limitations in demand-side management scenarios. In this paper, a lithium-ion battery model was derived to estimate lifetime and state-of-charge for building-integrated use cases. The proposed battery model aims to balance speed and accuracy when modeling battery behavior for real-time predictive control and optimization. In order to achieve these goals, a mixed modeling approach was taken, which incorporates regression fits to experimental data and an equivalent circuit to model battery behavior. A comparison of the proposed battery model output to actual data from the manufacturer validates the modeling approach taken in the paper. Additionally, a dynamic test case demonstrates the effects of using regression models to represent internal resistance and capacity fading.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

LiNi0.8Mn0.1Co0.1O2 Thin Films Prepared by Polymer-Assisted Deposition for the Study of Cathode-Electrolyte Interphases in Lithium-Ion Batteries

High-nickel layered oxide cathodes such as LiNi0.8Mn0.1Co0.1O2 (NMC811) are critical for next-generation lithium-ion batteries (LIBs) due to their superior energy density and reduced reliance on cobalt. However, many Ni-rich cathodes suffer from rapid capacity fade and structural instability originating from complex interfacial reactions at the cathode-electrolyte interface. Traditional composite electrodes exhibit degradation mechanisms that are challenging to quantitatively understand due to additives, including binders and carbon black. In this study, we demonstrate a new synthesis approach for binder- and additive-free NMC811 thin films using polymer-assisted deposition (PAD). PAD-NMC811 are model thin-film cathodes for investigating interfacial phenomena that can be obscured in composite cathodes. Structural and chemical characterization by X-ray diffraction, soft X-ray absorption spectroscopy, and atomic force microscopy show that PAD-NMC811 films possess high phase purity, crystallinity, chemical homogeneity, and morphological uniformity. Electrochemical analyses using cyclic voltammetry and galvanostatic cycling revealed electrochemical behavior consistent with that of composite electrodes, along with a moderate capacity fade indicative of cathode-electrolyte interphase (CEI) formation. Our findings illustrate the effectiveness of PAD synthesis of thin films tailored for detailed mechanistic studies, which offer critical insights into CEI evolution and cathode degradation pathways.

25 ENERGY STORAGE↗

Freestanding three-dimensional core–shell nanoarrays for lithium-ion battery anodes

Here, structural degradation and low conductivity of transition-metal oxides lead to severe capacity fading in lithium-ion batteries. Recent efforts to solve this issue have mainly focused on using nanocomposites or hybrids by integrating nanosized metal oxides with conducting additives. Here we design specific hierarchical structures and demonstrate their use in flexible, large-area anode assemblies. Fabrication of these anodes is achieved via oxidative growth of copper oxide nanowires onto copper substrates followed by radio-frequency sputtering of carbon-nitride films, forming freestanding three-dimensional arrays with core–shell nano-architecture. Cable-like copper oxide/carbon-nitride core–shell nanostructures accommodate the volume change during lithiation-delithiation processes, the three-dimensional arrays provide abundant electroactive zones and electron/ion transport paths, and the monolithic sandwich-type configuration without additional binders or conductive agents improves energy/power densities of the whole electrode.

25 ENERGY STORAGE↗

In Situ ATR-FTIR Study of the Cathode–Electrolyte Interphase: Electrolyte Solution Structure, Transition Metal Redox, and Surface Layer Evolution

We present a study of the lithium nickel manganese cobalt oxide (LiNi 0.6 Mn 0.2 Co 0.2 O 2 , NMC622) cathode-electrolyte interphase (CEI) during galvanostatic charging and discharging using in situ attenuated total reflectance Fourier transform infrared (ATR-FTIR) methods to investigate the voltage dependent electrolyte solution structure changes at the interface, transition metal (TM) redox chemistry, and cathode/electrolyte interfacial layer evolution. Furthermore, our in situ cell design provides both reliable electrochemical device testing and strong FTIR vibrational absorption signals near the cathode surface. Specifically, advanced spectral analysis elucidates changes of near-surface Li+ ion (de)solvation by solvent molecules during galvanostatic cycling. Moreover, cathode metal-oxygen vibrational absorptions, sensitive to TM redox behaviors and subsequent local structural variations, were correlated to cathode de-lithiation (and lithiation) and electrolyte solution structure changes. In addition, we have detected the formation and evolution of a CEI surface layer on the NMC622 cathode that contributes to the cell's capacity fade.

25 ENERGY STORAGE↗

A comparison of battery testing protocols: Those used by the U.S. advanced battery consortium and those used in China

Two testing protocols, QC/T 743 and those used by the U.S. Advanced Battery Consortium (USABC), were compared using cells based on LiFePO4/graphite chemistry. Differences in the protocols directly affected the data and the performance decline mechanisms deduced from the data. In all cases, the rate of capacity fade was linear with time. Overall, the testing protocols produced very similar data when the testing conditions and metrics used to define performance were similar. The choice of depth of discharge and pulse width had a direct effect on the apparent rate of resistance increased and estimated cell life. At greater percent depth of discharge (%DOD) and pulse width, the estimated life was shorter that at lower %DOD and shorter pulse width. This indicates that cells which were at the end of life based on the USABC protocol were not at end of life based on the QC/T 743 protocol by a large margin. (C) 2016 ELSEVIER B.V. All rights reserved.

battery testing↗

Surface degradation of Li{sub 1–x}Ni{sub 0.80}Co{sub 0.15}Al{sub 0.05}O{sub 2} cathodes: Correlating charge transfer impedance with surface phase transformations

The pronounced capacity fade in Ni-rich layered oxide lithium ion battery cathodes observed when cycling above 4.1 V (versus Li/Li{sup +}) is associated with a rise in impedance, which is thought to be due to either bulk structural fatigue or surface reactions with the electrolyte (or combination of both). Here, we examine the surface reactions at electrochemically stressed Li{sub 1–x}Ni{sub 0.8}Co{sub 0.15}Al{sub 0.05}O{sub 2} binder-free powder electrodes with a combination of electrochemical impedance spectroscopy, spatially resolving electron microscopy, and spatially averaging X-ray spectroscopy techniques. We circumvent issues associated with cycling by holding our electrodes at high states of charge (4.1 V, 4.5 V, and 4.75 V) for extended periods and correlate charge-transfer impedance rises observed at high voltages with surface modifications retained in the discharged state (2.7 V). The surface modifications involve significant cation migration (and disorder) along with Ni and Co reduction, and can occur even in the absence of significant Li{sub 2}CO{sub 3} and LiF. These data provide evidence that surface oxygen loss at the highest levels of Li{sup +} extraction is driving the rise in impedance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Mechanism of Zn Insertion into Nanostructured δ-MnO 2 : A Nonaqueous Rechargeable Zn Metal Battery

Unlike the more established lithium-ion based energy storage chemistries, the complex intercalation chemistry of multivalent cations in a host lattice is not well understood, especially the relationship between the intercalating species solution chemistry and the prevalence and type of side reactions. Among multivalent metals, a promising model system can be based on nonaqueous Zn2+ ion chemistry. Several examples of these systems support the use of a Zn metal anode, and reversible intercalation cathodes have been reported. This study utilizes a combination of analytical tools to probe the chemistry of a nanostructured delta-MnO2 cathode in association with a nonaqueous acetonitrile-Zn(TFSI)(2) electrolyte and a Zn metal anode. As many of the issues related to understanding a multivalent battery relate to the electrolyte electrode interface, the high surface area of a nanostructured cathode provides a significant interface between the electrolyte and cathode host that maximizes the spectroscopic signal of any side reactions or minor mechanistic pathways. Numerous factors affecting capacity fade and issues associated with the second phase formation including Mn dissolution in heavily cycled Zn/delta-MnO2 cells are presented including dramatic mechanistic differences in the storage mechanism of this couple when compared to similar aqueous electrolytes are noted.

25 ENERGY STORAGE↗

Electrochemical properties and structural evolution of O3-type layered sodium mixed transition metal oxides with trivalent nickel

The electrochemical properties of NaNi 0.5 Co 0.5 O 2 and NaNi 0.5 Fe 0.5 O 2 and their structural transitions as a function of Na extraction associated with redox reactions are investigated. Synthesized in the O3-type layered structure, both materials show reasonable electrochemical activities at room temperature, delivering approximately 0.5 Na per formula unit at C/10 discharge. More Na can be reversibly cycled in NaNi 0.5 Co 0.5 O 2 at elevated temperature and/or in an extended voltage window, while NaNi 0.5 Fe 0.5 O 2 shows significant capacity fading at a high voltage cutoff which is likely due to Fe 4+ migration. In situ X-ray diffraction shows that the structural changes in the two materials upon desodiation are very different. NaNi 0.5 Co 0.5 O 2 goes through many different two-phase reactions including three different O3-type and three different P3-type structures during cycling, producing a voltage profile with multiple plateau-like features. In contrast, NaNi 0.5 Fe 0.5 O 2 has a smooth voltage profile and shows the typical O3–P3 phase transition without lattice distortion seen in other materials. Finally, this different structural evolution upon desodiation and re-sodiation can be explained by the electronic structure of the mixed transition metals and how it perturbs the ordering between Na ions differently.

36 MATERIALS SCIENCE↗

In Situ Chemical Imaging of Solid-Electrolyte Interphase Layer Evolution in Li–S Batteries

Parasitic reactions of electrolyte and polysulfide with the Li-anode in lithium sulfur (Li-S) batteries lead to the for-mation of solid electrolyte interphase (SEI) layers, which are the major reason behind severe capacity fading in these systems. Despite numerous studies, the evolution mechanism of the SEI layer and specific roles of polysulfides and oth-er electrolyte components are still unclear. We report an in-situ X-ray photoelectron spectroscopy (XPS) and chemical imaging analysis combined with ab initio molecular dynamics (AIMD) computational modeling to gain fundamental understanding regarding the evolution of SEI layers on Li-anodes within Li-S batteries. A multi-modal approach in-volving AIMD modeling and in-situ XPS characterization uniquely reveals the chemical identity and distribution of active participants in parasitic reactions as well as the SEI layer evolution mechanism. The SEI layer evolution has three major stages: the formation of a primary composite mixture phase involving stable lithium compounds (Li2S, LiF, Li2O etc); and formation of a secondary matrix type phase due to cross interaction between reaction products and elec-trolyte components, which is followed by a highly dynamic mono-anionic polysulfide (i.e. LiS5) fouling process. These new molecular-level insights into the SEI layer evolution on Li- anodes are crucial for delineating effective strategies for the development of Li–S batteries.

25 ENERGY STORAGE↗

Investigating the Chemical Reactivity of Lithium Silicate Model SEI Layers

Silicon anodes suffer from an unstable solid electrolyte interphase (SEI) layer that contributes to undesirable capacity fade with cycling. A key part to addressing this unstable SEI formation is to examine how certain components of the SEI react with the electrolyte over time. One SEI component that has not been thoroughly studied in the context of the chemical reactivity against the electrolyte is lithiated silicate. Four model silicate thin films with increasing lithium content were deposited by radio frequency (RF) magnetron sputtering to study how the lithiation of the native oxide on a silicon anode affects the chemical stability of the anode surface. SiO2, Li2Si2O5, Li2SiO3, and Li3SiOx films were exposed to 1.2 M LiPF6 in the 3:7 wt% ethylene carbonate/ethyl methyl carbonate (EC/EMC) electrolyte for periods of time that are representative of the amount of time it takes to undergo cell formations. Soaked samples were rinsed, dried, and characterized by a combination of attenuated total reflectance-infrared spectroscopy (ATR-IR), focused ion beam-secondary electron microscopy (FIB-SEM), and X-ray photoelectron spectroscopy (XPS) depth profiling. It was found that the rate of the decrease in film thickness of the silicates exposed to the electrolyte over time increases as a function of the lithium content in the thin film. This reaction involves HF etching and LiPF6 salt degradation leading to silicate loss and fluorination throughout the bulk. Understanding this chemical instability is critical to determining the overall mechanism of SEI degradation over time.

ADVANCED PROPULSION SYSTEMS,ENERGY STORAGE↗

First-Principles Analysis of Defect Thermodynamics and Ion Transport in Inorganic SEI Compounds: LiF and NaF

The formation mechanism and composition of the solid electrolyte interphase (SEI) in lithium ion batteries has been widely explored. However, relatively little is known about the function of the SEI as a transport medium. Such critical information is directly relevant to battery rate performance, power loss, and capacity fading. To partially bridge this gap in the case of inorganic SEI compounds, we report herein the results of first-principles calculations on the defect thermodynamics, the dominant diffusion carriers, and the diffusion pathways associated with crystalline LiF and NaF, which are stable components of the SEI in Li-ion and Na-ion batteries, respectively. The thermodynamics of common point defects are computed, and the dominant diffusion carriers are determined over a voltage range of 0-4 V, corresponding to conditions relevant to both anode and cathode SEI's. Our analyses reveal that for both compounds, vacancy defects are energetically more favorable, therefore form more readily than interstitials, due to the close-packed nature of the crystal structures. However, the vacancy concentrations are very small for the diffusion processes facilitated by defects. Ionic conductivities are calculated as a function of voltage, considering the diffusion carrier concentration and the diffusion barriers as determined by nudged elastic band calculations. These conductivities are more than ten orders of magnitude smaller in NaF than in LiF. As compared to the diffusivity of Li in other common inorganic SEI compounds, such as Li2CO3 and Li2O,the cation diffusivity in LiF and NaF is quite low, with at least three orders of magnitude lower ionic conductivities. The results quantify the extent to which fluorides pose rate limitations in Li and Na batteries.

Yildirim, Handan↗

Surpassing the Organic Cathode Performance for Lithium-Ion Batteries with Robust Fluorinated Covalent Quinazoline Networks

Organic electrode materials have promising application prospects in energy storage, but issues including rapid capacity fading and poor power capacity restrict their practical applications. In this study, nanoporous fluorinated covalent quinazoline networks (F-CQNs) were constructed by condensation of fluorinated aromatic aminonitrile precursors via an ionothermal pathway. Precise control of the reaction parameters afforded F-CQN-1-600 material featuring high surface area, permanent porosity, high nitrogen content (23.49 wt %), extended π-conjugated architecture, layered structure, and bipolar combination of benzene and tricycloquinazoline. Synergy among these unique properties leads to a good performance as a cathode source for lithium-ion batteries (LIBs) in terms of high capacity (250 mA h g –1 at 0.1 A g –1 ), high rate capability (105 mA h g –1 at 5.0 A g –1 ), and impressive cycling stability (95.8% retention rate after 2000 cycles at 2.0 A g –1 together with a high Coulombic efficiency of 99.95%), surpassing most of the previous organic cathode counterparts.

25 ENERGY STORAGE↗

High damage tolerance of electrochemically lithiated silicon

Mechanical degradation and resultant capacity fade in high-capacity electrode materials critically hinder their use in high-performance rechargeable batteries. Despite tremendous efforts devoted to the study of the electro–chemo–mechanical behaviours of high-capacity electrode materials, their fracture properties and mechanisms remain largely unknown. In this paper, we report a nanomechanical study on the damage tolerance of electrochemically lithiated silicon. Our in situ transmission electron microscopy experiments reveal a striking contrast of brittle fracture in pristine silicon versus ductile tensile deformation in fully lithiated silicon. Quantitative fracture toughness measurements by nanoindentation show a rapid brittle-to-ductile transition of fracture as the lithium-to-silicon molar ratio is increased to above 1.5. Molecular dynamics simulations elucidate the mechanistic underpinnings of the brittle-to-ductile transition governed by atomic bonding and lithiation-induced toughening. Finally, our results reveal the high damage tolerance in amorphous lithium-rich silicon alloys and have important implications for the development of durable rechargeable batteries.

25 ENERGY STORAGE↗

Tailoring the surface properties of LiNi 0.4 Mn 0.4 Co 0.2 O₂ by titanium substitution for improved high voltage cycling performance

The present research aims to provide insights into the behavior of LiNi0.4Mn0.4Co0.2O2 (NMC442) and LiNi 0.4 Mn 0.4 Co 0.2 O₂ (NMC442-Ti02) cathode materials under galvanostatic cycling to high potentials, in the context of previous work which predicted that Ti-substituted variants should deliver higher capacities and exhibit better cycling stability than the unsubstituted compounds. It is found that NMC cathodes containing Ti show equivalent capacity fading but greater specific capacity than those without Ti in the same potential range. When repeatedly charged to the same degree of delithiation, NMC cathodes containing Ti showed better capacity retention. Soft x-ray absorption spectroscopy (XAS) spectra for Mn and Co indicated increased reduction in these elements for NMC cathodes without Ti, indicating that the substitution of Ti for Co acts to suppress the formation of a high impedance rock salt phase at the surface of NMC cathode particles. The results of this study validate the adoption of a facile change to existing NMC chemistries to improve cathode capacity retention under high voltage cycling conditions.

36 MATERIALS SCIENCE↗