Reaction diffusion in the nickel-chromium-aluminum and cobalt-chromium-aluminum systems

The effects of MCrAl coating-substrate interdiffusion on oxidation life and the general mutliphase, multicomponent diffusion problem were examined. Semi-infinite diffusion couples that had sources representing coatings and sinks representing gas turbine alloys were annealed at 1,000, 1,095, 1,150, or 1,205 C for as long as 500 hours. The source and sink aluminum and chromium contents and the base metal (cobalt or nickel) determined the parabolic diffusion rate constants of the couples and predicted finite coating lives. The beta source strength concept provided a method (1) for correlating beta recession rate constants with composition; (2) for determining reliable average total, diffusion, and constitutional activation energies; and (3) for calculating interdiffusion coefficients.

Levine, S. R.↗

Hot corrosion of S-57, 1 cobalt-base alloy

A cobalt base alloy, S-57, was hot corrosion tested in Mach 0.3 burner rig combustion gases at maximum alloy temperatures of 900 and 1000 C. Various salt concentrations were injected into the burner: 0.5, 2, 5, and 10 ppm synthetic sea salt and 4 ppm sodium sulfate (Na2SO4). S-57 underwent accelerated corrosion only under the most severe test conditions, for example, 4 ppm Na2SO4 at 900 C. The process of the accelerated corrosion was primarily sulfidation.

Santoro, G. J.↗

Formation of amino acids by cobalt-60 irradiation of hydrogen cyanide solutions

Experiments were conducted to study the pathway for the prebiotic origin of amino acids from hydrogen cyanide (HCN) under the action of ionizing radiation considered as an effective source of energy on the primitive earth. The irradiations were performed in a cobalt-60 source with a dose rate of 200,000 rad/hr. Seven naturally occurring amino acids are identified among the products formed by the hydrolysis of gamma-irradiated solutions of HCN: glycine, alanine, valine, serine, threonine, aspartic acid, and glutamic acid. The identity of these amino acids is established by gas chromatography and mass spectrometry. Control experiments provided evidence that the amino acids are not the result of contamination.

Sweeney, M. A.↗

Static and dynamic cyclic oxidation of 12 nickel-, cobalt-, and iron-base high-temperature alloys

Twelve typical high-temperature nickel-, cobalt-, and iron-base alloys were tested by 1 hr cyclic exposures at 1038, 1093, and 1149 C and 0.05 hr exposures at 1093 C. The alloys were tested in both a dynamic burner rig at Mach 0.3 gas flow and in static air furnace for times up to 100 hr. The alloys were evaluated in terms of specific weight loss as a function of time, and X-ray diffraction analysis and metallographic examination of the posttest specimens. A method previously developed was used to estimate specific metal weight loss from the specific weight change of the sample. The alloys were then ranked on this basis. The burner-rig test was more severe than a comparable furnace test and resulted in an increased tendency for oxide spalling due to volatility of Cr in the protective scale and the more drastic cooling due to the air-blast quench of the samples. Increased cycle frequency also increased the tendency to spall for a given test exposure. The behavior of the alloys in both types of tests was related to their composition and their tendency to form scales. The alloys with the best overall behavior formed alpha-Al2O3 aluminate spinels.

Barrett, C. A.↗

The critical points of alloys of iron and cobalt during rapid heating

The influence of the rate of heating on the position of the critical points of iron-cobalt alloys was studied. It is shown that when an alloy with 8% Co by weight is heated at the rate of 7000 deg/sec, a shift in the temperature of phase conversion of almost 30 deg occurs. When an alloy with 15% Co by weight is heated at the same rate, the conversion temperature is shifted by approximately 20 deg. For an alloy with 15% Co by weight, for which under ordinary conditions of heating the points of phase conversion and magnetic randomization (the Curie point) coincide, it was possible to show that for high rates of heating, a separation with respect to temperature occurs which clearly confirms the fact of the shift in the critical points of phase conversion.

Gridnev, V. N.↗

Ultimate intrinsic-coercivity samarium-cobalt magnet: An Earth-based feasibility study for space-shuttle missions

Techniques for containerless melting and solidification of the samarium-cobalt alloy without excessive oxidation were developed. The rationale for extending these experiments in a weightless environment is also discussed. The effect of oxygen content from 0.15 to 0.63 weight percent and grain size in the range of 2 to 10 micrometers has been examined on arc-plasma-sprayed SmCo5 magnets. Contrary to expectations, the larger grain sizes tended to improve the coercivities. This was attributed to an increase in homogeneity resulting from higher temperature treatments used to produce larger grain size. No significant differences in coercivity were observed on the basis of oxygen content in the range examined. It is expected that more meaningful data on the relationship between oxygen content and coercivity will be seen when the oxygen content can be lowered to less than 0.1 weight percent.

Das, D. K.↗

Certain physical properties of cobalt and nickel borides

The temperature dependence of the electrical resistivity, the thermal conductivity, and the thermal emf of cobalt and nickel borides were studied. In the case of the nickel borides the magnetic susceptibility and the Hall coefficient were determined at room temperature. The results are discussed with allowance for the current carrier concentration, the effect of various mechanisms of current-carrier scattering and the location of the Fermi level in relation to the 3d band.

Kostetskiy, I. I.↗

The influence of cobalt on the microstructure of the nickel-base superalloy MAR-M247

Nickel was substituted for Co to produce 0, 5, and the standard 10% versions of MAR-M247, a cast nickel-base superalloy. The microstructures of the alloys were examined in as-cast, heat treated, aged, and stress-rupture tested conditions using a variety of metallographic techniques and differential thermal analysis. As cobalt concentration was reduced from 10 to 0 wt %, the gamma-prime weight fraction decreased from 59 to 41%; W and Ti concentrations in the gamma-prime phase increased from 5 to 8 and 2 to 3 at.%, respectively; the mean gamma-prime particle size increased from 0.6 to 0.8 micron; Cr and Al concentrations in the gamma matrix decreased from 17 to 13 and 15 to 12 at.%, respectively; and the weight fraction of carbides increased by approximately 1%.

Nathal, M. V.↗

Catalytic recombination of nitrogen and oxygen on iron-cobalt-chromia spinel

The energy-transfer catalytic recombination coefficient for nitrogen and oxygen recombination on iron-cobalt-chromia spinel is inferred from stagnation-point heat flux measurements in dissociated arc-jet flow. This material was coated on several Space Shuttle Orbiter thermal protection tiles. The resulting coefficients are correlated with an Arrhenius model for convenience, and these expressions may be used to account for catalytic recombination in predictions of the heat flux on the spinel-coated tiles flown on several Space Shuttle Orbiter flights. The results are compared with those inferred by Rakich, Stewart, and Lanfranco from an Orbiter flight and arc-jet experiments. Good agreement is obtained for oxygen recombination, but agreement for nitrogen is poor.

Scott, C. D.↗

Analysis of thermoelectric properties of high-temperature complex alloys of nickel-base, iron-base and cobalt-base groups

The thermoelectric properties alloys of the nickel-base, iron-base, and cobalt-base groups containing from 1% to 25% 106 chromium were compared and correlated with the following material characteristics: atomic percent of the principle alloy constituent; ratio of concentration of two constituents; alloy physical property (electrical resistivity); alloy phase structure (percent precipitate or percent hardener content); alloy electronic structure (electron concentration). For solid-solution-type alloys the most consistent correlation was obtained with electron concentration, for precipitation-hardenable alloys of the nickel-base superalloy group, the thermoelectric potential correlated with hardener content in the alloy structure. For solid-solution-type alloys, no problems were found with thermoelectric stability to 1000; for precipitation-hardenable alloys, thermoelectric stability was dependent on phase stability. The effects of the compositional range of alloy constituents on temperature measurement uncertainty are discussed.

Holanda, R.↗

Effects of cobalt, boron, and zirconium on the microstructure of Udimet 738

A structural study was carried out on Co modified Udimet 738 alloys containing 0.04, 0.10, and 0.20 wt % Zr at 0.01 and 0.03 wt % B levels. Samples in the as-cast and solution-treated conditions were exposed at 843 C to study structural stability. The structures produced by the interactions of Co, Zr, and B were studied by SEM, X-ray diffraction, and dispersive analysis techniques. The additions of large amounts of Zr and B were found to increase the solidification range of the U-738. Structural changes involved eutectic gamma prime islands, formation of low melting point compounds, and precipitation of borides and Zr rich phases. Boron and zirconium additions did not show substantial changes in mechanical properties. Removal of Co from the alloys resulted in reduction of the matrix solubility for carbon and increase in the gamma prime solvus. Structural instabilities found were continuous grain boundary M23C6 films, MC breakdown, and plate-like phases. Removal of cobalt resulted in a slight decrease in tensile and stress rupture properties. Detailed structural results presented.

Nakanishi, T. G.↗

Low-Cobalt Powder-Metallurgy Superalloy

Highly-stressed jet-engine parts made with less cobalt. Udimet 700* (or equivalent) is common nickel-based superalloy used in hot sections of jet engines for many years. This alloy, while normally used in wrought condition, also gas-atomized into prealloyed powder-metallurgy (PM) product. Product can be consolidated by hot isostatically pressing (HIPPM condition) and formed into parts such as turbine disk. Such jet-engine disks "see" both high stresses and temperatures to 1,400 degrees F (760 degrees C).

Harf, F. H.↗

The influence of cobalt, tantalum, and tungsten on the elevated temperature mechanical properties of single crystal nickel-base superalloys

The influence of composition on the tensile and creep strength of 001-line oriented nickel-base superalloy single crystals at temperatures near 1000 C was investigated. Cobalt, tantalum, and tungsten concentrations were varied according to a matrix of compositions based on the single crystal version of MAR-M247. For alloys with the baseline refractory metal level of 3 wt pct Ta and 10 wt pct W, decreases in Co level from 10 to 0 wt pct resulted in increased tensile and creep strength. Substitution of 2 wt pct W for 3 wt pct Ta resulted in decreased creep life at high stresses, but improved life at low stresses. Substitution of Ni for Ta caused large reductions in tensile strength and creep resistance, and corresponding increases in ductility. For these alloys with low Ta-plus-W totals, strength was independent of Co level. The effects of composition on properties were related to the microstructural features of the alloys. In general, high creep strength was associated with high levels of gamma-prime volume fraction, gamma-gamma-prime lattice mismatch, and solid solution hardening.

Nathal, M. V.↗

Investigation of the effects of cobalt ions on epoxy properties

The effects of Co(acac)sub x complexes on MY-720 epoxy properties have been investigated. It appears that Co2(+) ions form antibonding or nonbonding orbitals which increase the free volume and also reduce the cohesiveness of the host epoxy. The effects of Co2(+) ions, on the other hand, seem to result in increased Cohesiveness of the epoxy. The experimental values of magnetic moments of both types of ions in MY-720 suggest that the orbital momentum contributions of the (3d) electrons are partially conserved, though the effect is more pronounced for Co2(+) ions. The coordination environment of the cobalt ions in the host epoxy does not appear to be uniquely defined. These results indicate that the effects of metal ions on resin properties cannot be easily predicted on the basis of ligand field theory argument alone. Complex interactions between metal ions and host epoxy molecular structure suggest the desirability of parallel experimental investigations of electronic, magnetic, and mechanical properties of metal ion-containing epoxy samples for comparison with theory.

Singh, J. J.↗

The formation of volatile corrosion products during the mixed oxidation-chlorination of cobalt at 650 C

The reaction of cobalt with 1 pct Cl2 in 1, 10, and 50 pct O2/Ar atmospheres has been studied at 650 C with thermogravimetry and mass spectrometry. The principal vapor species appear to be CoCl2 and CoCl3. In all cases, CoCl2(s) forms at the oxide/metal interface and equilibration of the volatile chlorides with Co3O4 does not occur in the early stages of the reaction. In the 1 pct Cl2 1 pct O2-Ar case, continuous volatilization occurs. In the 1 pct Cl2-10 pct O2-Ar and 1 pct CL2-50 pct O2-Ar cases, volatilization occurs only in the first few minutes of reaction. Afterwards, the reaction is predominantly oxidation.

Jacobson, N. S.↗

Gas atomization of cobalt ferrite-phosphate melts

XRD, Moessbauer spectroscopy, and EDXS have been used to characterize a rapidly-solidified (Co,Fe)3O4 spinel generated in a cobalt-iron-phosphate glass matrix by gas atomization of melts. Of the two compositions tested, that containing 20 mol pct P2O5 exhibited randomly-oriented ferrite crystallization whose growth appears to have been diffusion-controlled. Unlike the ferrite, in which the iron has both tetrahedral and octahedral coordination, the iron in the glassy matrix was primarily of distorted-octahedral coordination. Calculations indicate that the cooling rates obtained with oxide melts vary strongly with droplet size, but less strongly with melt temperature.

De Guire, Mark R.↗

Gamma rays, X-rays, and optical light from the cobalt and the neutron star in SN 1987A

Recent developments in modeling the X-ray and gamma-ray emission from SN 1987A are discussed by taking into account both the decaying cobalt and the buried neutron star. The light curve and the spectra evolution of X-rays and gamma-rays are well modeled up to day of about 300 if mixing of Co-56 into hydrogen-rich envelope is assumed. However, the 16-28 keV flux observed by Ginga declines very slowly, whereas the spherical mixing model predicts that the flux should have decreased by a large factor at t greater than 300d. It is shown that this problem can be solved if the photoelectric absorption of X-rays is effectively reduced as a result of the formation of chemically inhomogeneous clumps. Based on the adopted hydrodynamical model and the abundance distribution, predictions are offered for future optical, X-ray, and gamma-ray light curves by taking into account other radioactive sources and various types of the central source, e.g., a buried neutron star accreting the reinfalling material or an isolated pulsar.

Kumagai, Shiomi↗

The 23 to 300 C demagnetization resistance of samarium-cobalt permanent magnets

The influence of temperature on knee point and squareness of the M-H demagnetization characteristic of permanent magnets is important information for the full utilization of the capabilities of samarium-cobalt magnets at high temperature in demagnetization resistent permanent magnet devices. Composite plots of the knee field and the demagnetizing field required to produce a given magnetic induction swing below remanence were obtained for several commercial Sm2Co17 type magnet samples in the temperature range of 23 to 300 C. Using the knee point to define the limits of operation safe against irreversible demagnetization, such plots are shown to provide an effective overview of the useable regions in the space of temperature-induction swing parameters. The observed second quadrant M-H characteristic squareness is shown, by two measures, to increase gradually with temperature, reaching a peak in the interval 200 to 300 C.

Niedra, Janis M.↗