Electrolyte–Electrocatalyst Interfacial Effects of Polymeric Materials for Tandem CO 2 Capture and Conversion Elucidated Using In Situ Electrochemical AFM

Integrating CO 2 capture and electrochemical conversion has been proposed as a strategy to reduce the net energy required for CO 2 regeneration in traditional CO 2 capture and conversion schemes and can be coupled with carbon-free renewable electricity. Polyethylenimine (PEI)-based materials have been previously studied as CO 2 capture materials and can be integrated in these reactive capture processes. PEI-based electrolytes have been found to significantly increase the CO 2 loading, and impact selectivity and rate of product formation when compared to the conventional aqueous electrolytes. However, the influence of these materials at the catalyst–electrode interface is currently not well understood. In this study, PEI-based electrolytes were prepared and their impact on the morphology of a silver electrode performing electrochemical CO 2 reduction (CO 2 R) was studied using in situ electrochemical atomic force microscopy (EC-AFM). The presence of PEI on the electrode surface could be distinguished based on nanomechanical properties (DMT modulus), and changes were observed as negative polarization was applied, revealing a reorganization of the PEI chains due to electrostatic interactions. These changes were impacted by the electrolyte composition, including the addition of supporting electrolyte KHCO 3 salt, as well as CO 2 captured by the PEI-based electrolyte, which minimized the change in surface mechanical properties and degree of PEI alignment on the electrode surface. The changes in surface mechanical properties were also dependent on the PEI polymer length, with higher molecular weight PEI showing different reconfiguration than the shorter polymer brushes. The study highlights that the choice of polymer material, the electrolyte composition, and CO 2 captured impact the nearelectrode environment, which has implications for CO 2 R, and presents EC-AFM as a new tool that can be used to probe the dynamic behavior of these interfaces during electrocatalysis.

36 MATERIALS SCIENCE↗

Effect of Diphenyl Content on Viscoelasticity of Poly(dimethyl- co -diphenyl)siloxane Melt and Network

Polydimethylsiloxane (PDMS) is one of the most widely used polymeric materials for sealants, adhesives, lubricants, and thermal as well as electrical insulation. At low temperatures, however, PDMS is subject to crystallization that can cause deterioration in mechanical function. A common way to suppress such crystallization is through the incorporation of phenylsiloxane into the backbone of polysiloxane. Nevertheless, the introduction of phenyl components, even in small quantities, could potentially change the properties of the siloxane in a significant way. In this work, a series of mechanical tests and finite element simulations were performed to study the macroscale viscoelasticity of two poly(dimethyl-co-diphenyl)siloxane formulations in order to understand the effects of a few percent diphenyl contents on the viscoelasticity of the polysiloxane material. Here, we utilized the small-angle X-ray scattering to investigate the microscopic structures of the copolymers and broadband dielectric spectroscopy and rheology to probe the chain dynamics at the microscale. The results of these characterizations were used to inform the finite element simulations. We found that the degree of cross-linking does not significantly alter the microstructure but can profoundly affect the viscoelastic response of the copolymer networks. The corresponding hysteretic behavior is interpreted in terms of reptation-like motion and relaxation of the effective free chains in the cured polymer network. The relaxation of the copolymer chains is slowed significantly by even a small increase in the molar ratio of the diphenyl component.

36 MATERIALS SCIENCE↗

Theory of Ion-Mediated Segmental Localization, Activated Structural Relaxation, and the Glass Transition in Polymerized Ionic Liquids

Here we combine polymer integral equation theory for structural correlations with a force-level theory for activated segmental relaxation to construct a microscopic theory for how ions modify the onset of segmental localization, the polymer alpha relaxation time, and glass transition temperature, T g , in dry polymerized ionic liquids (PolyILs). Our most important findings concerning the behavior of T g are (i) a weak dependence on anion–cation Coulomb attraction strength due to strong decoupling of ion and segmental dynamics, (ii) strong reduction with increasing mobile ion size due to both plasticization effects and weakening of ion-modified monomer caging, and (iii) increase with backbone rigidity and intrachain dynamic cooperativity. We quantitatively estimate T g variations as ion size and polymer static and dynamic rigidity are widely varied. The experimental data of 19 PolyILs are organized into a specific pattern consistent with the theoretical predictions with glass transition temperatures varying over a very wide range (~250 K) as observed experimentally. Based on the theoretical results, suggestions are made concerning the search for high conductivity Li- or Na-based PolyILs based on further lowering of T g via new polymer synthesis. Calculations of the alpha time as a function of packing fraction reveal the dynamic fragility increases for larger mobile ions, a more flexible backbone, and/or a smaller degree of intrachain dynamic cooperativity, as a consequence of the increasing importance of collective elasticity in determining the activation barrier. An analysis of transient segmental localization and a crossover to activated dynamics reveals similar, but not identical, trends as predicted at the laboratory vitrification timescale.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Molecular Dynamics Simulation and Theoretical Analysis of Structural Relaxation, Bond Exchange Dynamics, and Glass Transition in Vitrimers

Vitrimers are a class of polymer networks featuring dynamic covalent cross-links that can undergo associative bond exchange. There has been recent interest in these materials due to their promise as recyclable thermosets or self-healing polymers because of the ability of vitrimer networks to rearrange at the molecular level and undergo macroscopic flow. However, the practical use of these materials often occurs in the supercooled regime or glassy state, where the implications of dynamic bonds are complicated by the interplay between slow activated segmental dynamics, cross-link (i.e., bond-exchange) kinetics, and ultimately material properties. Here, in this paper, we combine coarse-grained molecular dynamics simulation and microscopic statistical mechanical theory to understand how cross-linking kinetics affect material dynamics and how this couples to segmental relaxation of the polymeric network strands across a spectrum of length and time scales, especially in the supercooled regime. We characterize the Kuhn segmental alpha relaxation time and bond exchange time for vitrimer systems across various cross-link densities, temperatures, and bond exchange rates. Simulation and theory both exhibit a bending-up behavior for bond exchange time upon cooling, suggesting a coupling between bond exchange dynamics and segmental relaxation that intensifies with faster bond exchange kinetics. We also found bond exchange dynamics have an impact on Kuhn segment alpha relaxation time, which is most significant at higher cross-link densities. Both these effects are most prominent when the bond exchange time is similar to the Kuhn segment alpha relaxation time, and the resulting coupling of these two relaxation processes is tied to both the probability of a free end to find a bonded pair and the time scale of the constraints imposed by the dynamic cross-links. This relationship is reflected by a cross-link dependence of a theoretical parameter which represents the quantitative degree of coupling between bond exchange and segmental dynamics. Overall, the combination of simulation and theory clarifies the intricate interaction between bond kinetics and segmental relaxation and demonstrates the ability to provide molecular-level insights into vitrimer dynamics over a wide temperature range.

dynamic relaxation↗

On electron beam-induced degradation of vinyl ester thermosets

We have demonstrated that electron beam radiolysis induces scissions of the C-O-C bonds along the backbone of the chains of unsaturated polyester thermosets of different compositions based on dicyclopentadiene, isophthalic acid, epoxy vinyl ester, and terephthalic acid. The radiolysis is imminent irrespective of the degree of crosslinking in the thermosets both in neat resins and in the presence of solvents. Electron Paramagnetic Resonance (EPR) results show the formation of the alkoxyl radicals and C-centered radicals as the primary intermediate products of the C-O-C scissions. While the alkoxyl radicals of these resins exhibit very good stability even six months after the irradiation, the C-centered radicals decay very rapidly via their reactions with oxygen that is available either as adsorbed in the resins, dissolved in solvents or from the environment. The radiolytically produced •OH radicals in the unsaturated-ester aqueous solutions play a major role in inducing scissions on the backbone of the polymer chains. The solvated electrons (e s ) from organic solvents, such as dimethyl sulfoxide and isopropyl alcohol, also induce direct scission of the C-O-C bonds, giving rise to the formation of alkoxyl radicals and C-centered radicals. However, a considerable fraction of es is scavenged by the dissolved O 2 to produce O 2 - . Despite the radiation-induced scissions, irradiation of the resins at a dose level of 1000 kGy results in an increase of the glass transition temperature, Tg. This is due to the simultaneous radiation-induced polymerization of the vinyl monomers, toluene, and styrene that are present in the resins. The increase in Tg is observed in all the resins except for the terephthalic polyester resin in aqueous solution, in which the absence of these monomers results in Tg decreasing sharply with irradiation. This work demonstrates that ionizing radiation triggers continuous free radical-chain reactions that lead to the formation of recyclable oligomers.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Viscoelastic Response of Dispersed Entangled Polymer Melts

Any polymer synthesis routes result in molecular weight dispersity DAI, depending on the polymerization mechanism. The lowest dispersity polymers are those made by anionic and atom-transfer radical polymerization, which exhibit relatively narrow distributions DM=g,„1A172 — 1.02-1.04. This small divergence from monodispersity results in significant number of molecules that differ in their molecular weight from the average and their impact on the viscoelastic response remains an open question. Here the effects of low dispersity on stress relaxation and shear viscosity of entangled melts are studied using a coarse-grained model for polyethylene. Polymer melts with chain length dispersity set to follow a Schulz-Zimm distribution of Dm = 1.0 — 1.16 for an entangled polyethylene melt using molecular dynamic simulations. The systems were studied to times up to 800 ,us which is beyond the terminal time. These systems are compared to those with binary and ternary distributions. The stress relaxation functions were extracted from the Green-Kubo relation and from stress-strain relaxation following a uniaxial extension. We find on the entanglement time scale, both the mean squared displacement and the stress relaxation are independent of D m . The tube diameter and the rubbery plateau for entangled dynamics do not depend on D m . At longer times, the terminal relaxation time decreases as the faster motion of the shorter chains results in constraint release for the longer chains. Probing this low dispersity regime opens the way to evaluate the degree of dispersity that affects mechanical properties.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrospun Separator Based on Sulfonated Polyoxadiazole with Outstanding Thermal Stability and Electrochemical Properties for Lithium-Ion Batteries

Traditional polyolefin separators used in lithium-ion batteries (LIBs) are seriously limited by the issues of inferior security and poor electrolyte wettability. Most of the very promising candidate separators based on heat-resistant polymers are, however, inherently difficult to process. Herein, a unique sulfonated aromatic heterocyclic polymer, lithiated poly(diphenyl ether oxadiazole) sulfonate (Li-SPEOD), was synthesized through a simple one-pot method and further electrospun to act as a novel separator (es-Li-SPEOD) for LIBs. In this work, the prepared Li-SPEOD possesses a high degree of sulfonation with a high molecular weight (M w = 4.31 × 10 5 ). The es-Li-SPEOD separator exhibits excellent mechanical and fire-resistance properties and is able to maintain dimensional stability at a temperature of even up to 400 °C in air. The ionic conductivity (3.57 mS cm –1 ) and lithium-ion transference number (0.37) of the es-Li-SPEOD with an electrochemical stability window of 4.5 V vs Li + /Li can be improved by 382.4 and 32.1%, respectively, compared to those of Celgard-2500 in the LiPF 6 electrolyte. The enhanced rate capability and cycle performance of the LiFePO 4 –Li half-cell are therefore obtained. Moreover, the es-Li-SPEOD displays an outstanding dendrite-suppressing effect for the lithium metal anode. This research proves that the Li-SPEOD-based separator has a broad application perspective in next-generation lithium batteries.

25 ENERGY STORAGE↗

Solution–Doped Donor–Acceptor Copolymers Based on Diketopyrrolopyrrole and 3, 3'–Bis (2–(2–(2–Methoxyethoxy) Ethoxy) ethoxy)–2, 2'–Bithiophene Exhibiting Outstanding Thermoelectric Power Factors with p –Dopants

The design of polymeric semiconductors exhibiting high electrical conductivity (σ) and thermoelectric power factor (PF) will be vital for flexible large-area electronics. In this work, four polymers based on diketopyrrolopyrrole (DPP), 2,3-dihydrothieno[3,4-b][1,4]dioxine (EDOT), thieno[3,2-b]thiophene (TT), and 3, 3'-bis (2-(2-(2-methoxyethoxy) ethoxy) ethoxy)-2, 2'-bithiophene (MEET) are investigated as side-chains, with the MEET polymers newly synthesized for this study. These polymers are systematically doped with tetrafluorotetracyanoquinodimethane ( F 4 TCNQ), CF3SO3H, and the synthesized dopant Cp(CN) 3 -(COOMe) 3 , differing in geometry and electron affinity. The DPP-EDOT-based polymer containing MEET as side-chains exhibits the highest conductivity (σ) ≈700 S cm–1 in this series with the acidic dopant (CF 3 SO 3 H). This polymer also shows the lowest oxidation potential by cyclic voltammetry (CV), the strongest intermolecular interactions evidenced by differential scanning calorimetry (DSC), and has the most oxygen-based functionality for possible hydrogen bonding and ionic screening. Other polymers exhibit high σ ≈300–500 S cm–1 and power factor up to 300 µW m –1 K –2 . The mechanism of conductivity is predominantly electronic, as validated by time-dependent conductance studies and transient thermo voltage monitoring over time, including for those doped with the acid. Furthermore, these materials maintain significant thermal stability and air stability over ≈6 weeks. Density functional theory calculations reveal molecular geometries and inform about frontier energy levels. Raman spectroscopy, in conjunction with scanning electron microscopy (SEM-EDS) and x-ray diffraction, provides insight into the solid-state microstructure and degree of phase separation of the doped polymer films. Infrared spectroscopy enables this study to further quantify the degree of charge transfer from polymer to dopant.

36 MATERIALS SCIENCE↗

High-Resolution Comonomer Sequencing of Blocky Brominated Syndiotactic Polystyrene Copolymers Using 13C NMR Spectroscopy and Computer Simulations

This work demonstrates the first high-resolution comonomer sequencing of Blocky brominated syndiotactic polystyrene (sPS-co-sPS-Br) copolymers based on pentad assign- ments of the quaternary carbon region of the nuclear magnetic resonance spectrum. Copolymers containing p-bromostyrene (Br-Sty) units were prepared in matched sets using postpolymerization bromination methods carried out in the heterogeneous gel state (Blocky) and homogeneous solution state (Random). Quantitative information from the quaternary carbon spectra, heteronuclear multiple bond correlation spectroscopy, electronic structure calculations, and simulated statistically random copolymers was correlated to confirm the carbon resonance assignments for all 20 possible pentad comonomer sequences. Using the experimental pentad sequence prevalences, a computer code was developed to simulate chains with microstructures typical of each sample as a means to visually represent the copolymer blockiness with quantitative precision. Based on the microstructure and distribution of run lengths in these chains, the simulations revealed that the Blocky copolymers contain a high degree of blockiness. By comparing the run lengths in the simulated chains to the average number of styrene units in a crystalline segment of sPS (found by small-angle X-ray scattering), copolymer crystallizability was predicted. For the simulated Blocky B-21% (21 mol % Br-Sty) chain, the probability of randomly selecting a styrene unit in a crystallizable block was 25.8%, while that in the simulated Random R-18% was zero, in excellent agreement with the experimental crystallization behavior measured by differential scanning calorimetry. Additionally, these predictions confirmed that the simulated chains accurately represent the ensemble of chains in their respective copolymer samples. Furthermore, each simulated Blocky chain contained one or more long sPS blocks that paralleled the measured 38-40 styrene units spanning a crystalline segment within the sPS/CCl4 gel. This finding affirmed that the long sPS segments originated from the precise lamellar structure within the heterogeneous gel morphology (i.e., block length is correlated with lamellar thickness). Overall, the ability to tailor the copolymer microstructure through control of the semicrystalline gel morphology opens the door to synthesizing ordered copolymers by postpolymerization functionalization processes with unprecedented levels of compositional control.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗