Microstructure of Friction Stir Welded AlSi9Mg Cast with 5083 and 2017A Wrought Aluminum Alloys

Wrought aluminum alloys 5083 and 2017A were each joined with cast aluminum alloy AlSi9Mg through friction stir welding in butt weld configurations. For each material system, the wrought and cast alloy positions, i.e., the advancing side or the retreating side, were exchanged between welding trials. The produced weldments were free from cracks and discontinuities. For each alloy configuration, a well-defined nugget comprised of alternating bands of the welded alloys characterized the microstructure. The degree of mixing, however, strongly depended on which wrought alloy was present and on its position during processing. In all cases, the cast AlSi9Mg alloy dominated the weld center regardless of its position during welding. Electron backscattered diffraction analysis showed that the grain size in both alloys (bands) constituting the nugget was similar and that the majority of grain boundaries exhibited a high angle character (20°-60°). Regardless of the alloy, however, all grains were elongated along the direction of the material plastic flow during welding. A numerical simulation of the joining process visualized the material flow patterns and temperature distribution and helped to rationalize the microstructural observations. The hardness profiles across the weld reflected the microstructure formed during welding and correlated well with the temperature changes predicted by the numerical model. Tensile specimens consistently fractured in the cast alloy near the weld nugget.

36 MATERIALS SCIENCE↗

The Role of Friction Stir Welding on the Microstructure and Mechanical Properties of AZ31B-H24 Mg alloy

In this study, an attempt was made to join AZ31B magnesium alloy by friction stir welding (FSW) process. A single tool with cylindrical screw threaded pin was used to investigate the effect of welding parameters on microstructure and mechanical properties of stir zone (SZ). Several welds were made at different rotational ({omega}) and traverse ({upsilon}) speeds, while the {omega}/{upsilon} ratios were kept constant. The optical and scanning electron microscopy were used to study the variation of microstructure across the welds. Moreover, micro-hardness and tensile tests were carried out to evaluate the mechanical properties of joints. It was found that {omega} plays more significant role on the resulted grain structure than {upsilon}, and at a constant {omega}/{upsilon} ratio, decreasing rotational speed decreased the size of grains, and hence, improved the hardness value and the tensile strength of the SZ.

36 MATERIALS SCIENCE↗

Adaptive relay autotuning under static and non-static disturbances with application to friction stir welding

When a traditional relay feedback test is biased, asymmetry is induced, erroneous system identification occurs, and the test may stop oscillating. Adaptive methods which restore symmetry to the relay test are developed, and additional methods are presented to detect and recover from a non-oscillation condition. This is demonstrated both in simulation and in a process with significant transients and disturbances - friction stir welding (FSW). In testing, it is shown that the adaptive method is able to restore symmetry even in the presence of severe and changing disturbances, including after the weld plunge where temperature gradients change rapidly. Finally, these improvements enable system identification of systems such as FSW in a more robust and accurate manner.

42 ENGINEERING↗

Microstructure evolution in the conventional single side and bobbin tool friction stir welding of thick rolled 7085-T7452 aluminum alloy

Highlights: • Comparison of microstructure evolution via EBSD of SS-FSW and BB-FSW was investigated. • Friction heat, strain rate and degree of recrystallization affected grain size. • Discontinuously dynamic recrystallization occurred in the weld nugget zone. • The degree of recrystallization was mainly controlled by the strain rate. - Abstract: The microstructure evolution during the conventional single side friction stir welding (SS-FSW) and the bobbin tool FSW (BB-FSW) of 7085-T7452 alloy thick plate was extensively studied by using the state-of-the-art materials characterization techniques. The Electron backscattering diffraction results reveal that a significant grain refinement and a larger percentage of high angle grain boundaries (HAGBs) exist in the weld nugget zone (WNZ) and the thermal-mechanical affected zone (TMAZ) compared with the base material. Meanwhile, more obviously inhomogeneous refined grains and HAGBs in WNZ along the thickness direction and a larger percentage of low angle grain boundaries (LAGBs) were observed in SS-FSW joint than that in BB-FSW joint. The change of the average grain size is the result of friction heat and strain rate of plastic deformation combined with a certain degree of recrystallization. Moreover, the recrystallization is mainly controlled by the strain rate during the FSW process. The presence of Cube and Cube ND after welding shows that the discontinuously dynamic recrystallization (DDRX) is a major factor in the final microstructural response. The research and findings help the understanding of the mechanism of microstructure homogenization and further optimizing the welding process for application.

36 MATERIALS SCIENCE↗

Texture and precipitation behavior of friction stir welded Inconel 825 alloy

The microstructure, texture pattern, and precipitation behavior of friction stir butt welded Inconel 825 alloy are highlighted here. The microstructure of bright regions and black-banded regions in the stir zone (SZ) is characterized by SEM, EBSD, and TEM with EDS. EBSD analysis justifies that the SZ exhibits a dynamic recrystallized structure. Grain boundary mapping corroborates the insignificant difference in the low- and high-angle grain boundaries fraction between the SZ, the thermo-mechanically affected zone, and the base metal. TEM analysis confirms the formation of nano twins and dispersion of nano-size precipitations in the grains, and at the grain boundaries as well. Grain refinement and nano-size precipitation formation in the SZ significantly enhanced both microhardness and tensile strength.

Das, Hrishikesh↗

Friction stir welding and self-ion irradiation effects on microstructure and mechanical properties changes within oxide dispersion strengthened steel $\mathrm{MA956}$

We report the joining process for oxide dispersion strengthened (ODS) alloys remains a key challenge facing the nuclear community. The microstructure and mechanical properties were characterized in the base material and friction stir welded ODS MA956 irradiated with 5 MeV Fe 2+ ions from 400 to 500°C up to 25 dpa. Nanoindentation was performed to assess changes in hardness and yield stress, and the dispersed barrier hardening (DBH) model was applied to described results. A combination of scanning transmission electron microscopy (STEM) and atom probe tomography (APT) were used to assess evolution of the microstructure including dispersoids, network dislocations and dislocation loops, nanoclusters, and solid solution concentrations. Overall, softening was observed as a result of increased dose, which was exacerbated at 500°C. The formation and coarsening of new dispersoids was noted while nanoclusters tended to dissolve in the base material, and were not observed in the stir zone. Solute nanocluster evolution was identified as a primary driver of the changes in mechanical properties.

36 MATERIALS SCIENCE↗

Effect of Preheating and Water Cooling on the Performance of Friction-Stir-Welded Aviation-Grade Aluminum Alloy Joints

This paper examined the effect of preheating and water cooling on the thermal, mechanical, metallurgical, and texture properties of friction-stir-welded AA6082. Joints are fabricated under different preheating (FSW-P) and water cooling (FSW-C) conditions. The experimental outcomes indicate that the preheating and water cooling enhance the mechanical properties of the joint. The maximum tensile strength of 295 MPa is obtained for FSW-P1. It is also observed that preheating has more impact on microhardness. Microstructural analysis using optical microscope and electron backscatter diffraction analysis indicated that FSW produced fine equiaxed grains in the nugget zone due to dynamic recrystallization. Texture analysis shows that finer grain grains are obtained under preheating and water cooling conditions. The minimum grain size of 5.3 µm is obtained under FSW-P1. X-ray diffraction analysis shows that Mg{sub 2}Si phase in nugget zone that is an indication of dissolution and formation of strengthening precipitates. Fracture analysis indicates that preheating also improves the ductility of the joint.

36 MATERIALS SCIENCE↗

On the Effect of Quenching on Postweld Heat Treatment of Friction-Stir-Welded Aluminum 7075 Alloy

This work focuses on the effect of postweld heat treatment (PWHT) on the mechanical properties and microstructural evolution of aluminum 7075 alloy processed via friction stir welding (FSW). FSW is known to be capable of grain refinement in the nugget zone (NZ). Two different quench media (water and air) were employed for PWHT. Regardless of the quench media, the PWHT led to the occurrence of grain growth in the NZ of the FSWed aluminum 7075 alloy. Abnormal grain growth occurred in the water quenched specimen. It is shown that ductility and strength of FSWed aluminum 7075 alloy are strongly dependent on the quenching rate. Changes in the mechanical properties and microstructure reveal that only at lower cooling rate this alloy is prone to the formation of precipitate-free zones (PFZs) in the vicinity of grain boundaries. Eventually, the PFZs deteriorate mechanical properties of this alloy.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Friction-Stir-Welded 316L Austenitic Stainless Steels

Fusion welding of austenitic stainless steels (ASSs) causes undesirable metallographic changes. An attempt has been made to join 3-mm-thick 316L ASS plates using friction stir welding and correlate the microstructural evolution and the mechanical properties under various welding conditions. Tungsten alloy (W-Re) tool was employed for welding. Successful joints were obtained within a range of traverse speeds (45-85 mm/min) used in this work. Various zones were observed across the joint line. The stir zone exhibited considerable grain refinement and traces of delta ferrite phase. EBSD images showed a decreasing grain size with increased traverse speed. XRD patterns and TEM images confirmed the existence of delta ferrite. The mechanical properties of the joints including microhardness, tensile strength, impact toughness and bending were further reported.

36 MATERIALS SCIENCE↗

Impact of Backing Plate and Thermal Boundary Conditions for High-Speed Friction Stir Welding of 25-mm Thick Aluminum Alloy 7175-T79

Here this study demonstrates high-speed (150 mm/min) single pass friction stir butt joining of 25 mm thick aluminum alloy 7175-T79. To understand the impact of quenching and cooling rate on process responses, joint strength, and grain size distributions across the weld thickness, we performed a series of friction stir welding (FSW) trials in air and with a trailing water spray using steel and composite backing plates (BP). Welds made in air and trailing water spray exhibit significantly different hardness distributions across the nugget, heat affected zone (HAZ), and HAZ minimum hardness as evidenced by detailed microhardness mapping. The effect of trailing water spray (TWS) on joint efficiency overshadows the influence of BP composition due to the vastly different contribution to quenching. TWS also resulted in a multifaceted effect on FSW such as lowering processing temperature, increasing X and Z forces while lowering Y force, and narrow heat affecting zone. Finally, digital image correlation (DIC)-based fracture mode analysis and grain size measurements correlate with the hardness distribution.

42 ENGINEERING↗

A FEASIBILITY STUDY ON CRACK REPAIR IN AUSTENITIC STAINLESS STEEL DRY STORAGE CANISTERS USING ISOTHERMAL FRICTION STIR WELDING

In recent time, solid state crack repair techniques in spent nuclear fuel dry storage canisters (SNF-DSC) have garnered significant interest. Plates of austenitic stainless steels are usually arc welded to fabricate the cylindrical canisters which are prone to chloride-induced stress corrosion cracking. Friction stir welding (FSW) is considered to be a potential candidate for damage repair. In this work, electrical discharge machining was used to simulate cracks in 304L stainless steel plates of 12.7 mm thickness. Subsequently, isothermal FSW was carried out at two different temperatures (725 and 825°C) in order to repair the simulated crack. Microstructure-mechanical property correlations in FSWed plates were studied in detail. Significant grain refinement observed in the stir zone (SZ) was attributed to dynamic recrystallization occurring during FSW. A comparison of Vickers microhardness showed higher hardness and homogeneity in the 725°C SZ than its 825°C counterpart. The fraction of S3 boundary is found to be low in the SZ as compared to base metal (BM). Yield strength of the joints was found to be approximately 100 MPa higher than that of the BM accompanied by a drop in ductility by a factor of 2. Residual stress profile across 825°C weld was measured using x-ray diffraction.

Bhattacharyya, Madhumanti↗

Prediction of hardness minimum locations during natural aging in an aluminum alloy 6061-T6 friction stir weld

This study describes a simple model that can predict the evolution of hardness distribution as a function of natural aging time in a heat-treatable 6061-T6 Al alloy plate subjected to friction stir welding (FSW). First, two dimensional thermal distributions were simulated as a function of time in the FSW plate by finite element modeling. Second, the hardness changes during natural aging were measured as a function of aging time for a number of Al specimens that had been previously isothermally heat-treated to different hold temperatures in order to determine the natural aging kinetics. Finally, the simulated temperature profiles and the natural aging kinetics were correlated to predict the hardness profiles in the FSW plate. The predicted hardness variations are consistent with measured hardness profiles in that the location of minimum hardness moves away from the centerline as the aging time and/or heat input increases. The hardness variation was also related to the location of failure in cross-weld tensile samples.

36 MATERIALS SCIENCE↗

Mechanical Properties and Wear Behavior of AA5182/WC Nanocomposite Fabricated by Friction Stir Welding at Different Tool Traverse Speeds

Grain growth inhibition at the heat-affected zone, improved weld strength and superior tribological properties of welds are desirable attributes of modern manufacturing. With the focused on these attributes, tungsten carbide (WC) nanoparticles were employed as reinforcements for the friction stir welding of 5-mm-thick AA5182 aluminum alloy by varying tool traverse speeds. The microstructure, microhardness, ultimate tensile strength, fracture and wear behavior of the resultant WC-reinforced welds were investigated, while unreinforced AA5182 welds were employed as controls for the study. The result shows that the addition of WC nanoparticles causes substantial grain refinement within the weld nugget. A decrease in traverse speed caused additional particle fragmentation, improved hardness value and enhanced weld strength in the reinforced welds. Improved wear rate and friction coefficient of welds were attained at a reduced traverse speed of 100 mm/min in the WC-reinforced welds. This improvement is attributed to the effects of reduced grain size/grain fragmentation and homogeneous dispersion of WC nanoparticles within the WC-reinforced weld nugget.

36 MATERIALS SCIENCE↗

Friction stir welding of thick 7175 aluminium alloy plates for deepwater riser applications

To substantially reduce the cost of extracting petroleum from ultra-deepwater sources, manufacturing risers from 7175 aluminium (Al) alloys rather than steels is being considered. Friction stir welding (FSW), a solid-phase joining technique, is widely applied to 7XXX Al alloys because its mechanical properties are retained within the nugget zone. And, the primary technical objective of the current study is the development of high-strength, corrosion-resistant weldments that connect 7175 Al riser flanges and pipes. However, as the welding thickness increases, the welding speed can be greatly impeded, which lowers the manufacturing efficiency and weakens the mechanical properties in the heat affected zone (next to the nugget). Therefore, obtaining high-performance thick plate 7175 Al alloy joints via FSW is challenging. To overcome this dilemma, the current work optimises the tool design and welding parameters for achieving high-performance joints between 25.4 mm thick 7175 Al alloy plates in butt joint configuration.

Wang, Tianhao↗

Effect of Zinc Interlayer in Microstructure Evolution and Mechanical Properties in Dissimilar Friction Stir Welding of Aluminum to Titanium

The welding of aluminum (Al) and titanium (Ti) is difficult and challenging due to the differences in their chemical and physical properties, and the formation of brittle intermetallic phases. In the present experiment, a zinc (Zn) interlayer was used during friction stir welding of Al to Ti. The weld was characterized in detail to understand the mechanisms associated with microstructural evolution and improvement in mechanical properties of the weld. X-ray computed tomography results reveal three-dimensional distribution of particles and flakes of titanium in the weld nugget. It was also observed that Ti particles are inhomogeneously distributed in the weld and the distribution depends on their morphology. Such a distribution of Ti was informative in understanding material flow. In addition, the consolidation of Zn in the Al matrix reveals the nature of material flow in the weld nugget as well. The importance of the Zn interlayer and mechanism of phase formation was explored in this study. It was characterized that the mechanical mixing of Zn with Al and Ti alters phase evolution and restricts the formation of conventional Al{sub 3}Ti intermetallic phase. The presence of zinc homogenizes elemental distribution and inhibits the formation of brittle intermetallic phases, which leads to a substantial improvement in mechanical properties of the weld.

36 MATERIALS SCIENCE↗

Effect of niobium interlayer in dissimilar friction stir welding of aluminum to titanium

Highlights: • In the present study, FSW of Al to Ti with Nb interlayer has been characterized. • Fragmentation and distribution of Nb and Ti have been correlated with properties. • Ternary mixing and chemical reaction reduced the brittleness of the joint. • Al in the weld nugget showed a gradient in microstructural features. • The weld with Nb interlayer exhibited higher ductility. - Abstract: The most important issue associated with dissimilar welding is the formation of detrimental intermetallics and consequent reduction in mechanical properties of the weld. It was expected that addition of an interlayer would modify the pattern of the intermetallic formation. The present investigation deals with Friction Stir Welding of aluminum (Al) to titanium (Ti) in presence of niobium (Nb) interlayer. X-ray Computed Tomography results highlighted that fine particles of both Ti and Nb are homogeneously distributed. Large Ti particles are substantially fragmented whereas large Nb particles remain as flakes. Microstructural features of the nugget zone indicated a complex mixing of materials. Jointing had been perceived through elemental diffusion at the interfaces of Al/Ti and Ti/Nb. However, Nb restricted the reaction between Al and Ti, and acted as an efficient interlayer to retard the formation of brittle Al{sub 3}Ti intermetallic phase. Mechanisms of microstructural evolution in Al side of the weld have been identified as Dynamic Recovery, Dynamic Recrystallization and particle stimulated nucleation. Significant improvement in the tensile ductility had been observed due to the presence of finer particles. The presence of Nb in the weld nugget influences the microstructural evolution and tensile properties of the weld by reducing the formation of intermetallics.

36 MATERIALS SCIENCE↗

Dissimilar Friction Stir Welds in Al5186-Al2024: The Effect of Process Parameters on Microstructures and Mechanical Properties

The effect of tool traverse and rotation speeds on the microstructures and mechanical properties are quantified for welds between non-age-hardening Al5083 and age hardening Al2024 and compared to single alloy joints made from each of the two constituents. In this paper, we report the results of microstructural, mechanical property investigations of Al5186-Al2024 friction stir welds produced using various rotations and traveling speeds of the tool to investigate the effects of the welding parameters on the joint strength. Metallographic studies by optical microscopy, electron probe microscopy, and the utilization of the X-ray diffraction technique have been conducted. It was found that the weld properties were dominated by the thermal input rather than the mechanical deformation by the tool. In particular the larger stresses under the weld tool on the AA5186 side compared to the AA2024 side are related to a transient reduction in yield stress due to dissolution of the hardening precipitates during welding prior to natural aging after welding.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Rapidly Cooled Friction Stir Welded Ti-6Al-4V Alloys

Two mm-thick Ti-6Al-4V alloy plates were friction stir butt welded under natural- and rapid-cooling conditions. The microstructures and mechanical properties of joints were investigated and compared. The rapid cooling via spraying cooling liquid nitrogen on the plate top surface was beneficial to obtaining a narrower cross section and finer and more uniform grains in the stir zone than those obtained by natural cooling. Joint tensile strength of 1021 MPa and elongation of 1.88% under the rapid-cooling condition respectively reached 102.7 and 150.4% of those under the natural-cooling condition, respectively. The uniform-and-compact equiaxed grains led to equiaxed dimples on the fracture surface, which demonstrated a ductile fracture of the welding joints.