Structure of tetragonal martensite in the In{sub 95.42}Cd{sub 4.58} cast alloy

The structure of martensite in the In{sub 95.42}Cd{sub 4.58} alloy has been studied by metallography, X-ray diffraction, dilatometry, and transmission electron microscopy. It has been shown that a massive structure built of colonies of tetragonal lamellar plates divided by a twin boundary {101}FCT is formed in the alloy under cooling below the martensite FCC → FCT transition temperature. The alloy recrystallizes after a cycle of FCT → FCC → FCT transitions with a decrease in the grain size by several times compared with the initial structure such fashion that the size of massifs and individual martensite lamella in the massif correlates with the change in the size of the alloy grain. Using thermal cycling, it has been revealed that the alloy tends to stabilize the high-temperature phase.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Development of Novel Ferritic-Martensitic Steels with Superior Creep Properties for Power Plant Applications

A creep resistant martensitic steel, CPJ-7, was developed with an operating temperature approaching 650°C. Subsequently, another creep resistant martensitic steel, JMP, was designed with the potential to operate at, or slightly above, 650°C. This report describes the development of these alloys from early iterations of CPJ steels to the final CPJ-7 formulation as well as the more heat resistant JMP steel formulation. The design originated from computational modeling for phase stability and precipitate strengthening using fifteen constituent elements. Approximately forty heats of CPJ and ten of JMP, each weighing ~7 kg, were vacuum induction melted. A computationally optimized heat treatment schedule was developed to homogenize the ingots prior to hot forging and rolling prior to final normalization and tempering. Overall, wrought and cast versions of CPJ-7 present superior creep properties when compared to wrought and cast versions of COST alloys for steam turbine and wrought and cast versions of P91/92 for boiler applications. For instance, the Larson Miller Parameter curve for CPJ-7 at 650°C almost coincides with that of COST E at 620°C. The prolonged creep life was attributed to slowing down the process of the destabilization of the MX and M 23 C 6 precipitates at 650°C. On the other hand, the cast version of CPJ-7 also revealed superior mechanical performance, well above commercially available cast 9% Cr martensitic steel or derivatives, especially for creep life at 650°C. The casting process employed slow cooling to simulate the conditions of a thick wall full-size steam turbine casing but utilized a separate homogenization step prior to final normalization and tempering. To advance the development of CPJ-7 for commercial applications, a process was used to scale up the production of the alloy using vacuum induction melting (VIM) and electroslag remelting (ESR), which underlined the importance of melt processing control of intentionally designed minor and trace elements in these advanced alloys. Following the work on CPJ-7, the JMP steels were designed with higher Co for increased solid solution strengthening, Si for oxidation resistance and increased W (with low Mo content) for matrix strength and stability as well as solid solution strengthening. The JMP steels showed increases in creep life compared to CPJ-7 between 118 to 150% at 650°C for testing at various stresses between 138 MPa and 207 MPa. On a Larson-Miller plot, the performance of the JMP steels surpasses that of state-of-the-art MARBN and other MARBN-type steels. The influence of various elements within the composition of the alloys on the microstructure and mechanical properties are discussed. This report presents approximately 420,000 h of in-house creep testing, the equivalent of almost 50 years of cumulative creep tests.

36 MATERIALS SCIENCE↗

Isothermal Martensitic and Pressure-Induced Delta to Alpha-Prime Phase Transformations in a Pu-Ga Alloy

A well-homogenized Pu-2 at.% Ga alloy can be retained in the metastable face-centered cubic {delta} phase at room temperature. Ultimately, this metastable {delta} phase will decompose via a eutectoid transformation to the thermodynamically stable monoclinic {alpha} phase and the intermetallic compound Pu{sub 3}Ga over a period of approximately 10,000 years [1]. In addition, these low solute-containing {delta}-phase Pu alloys are metastable with respect to an isothermal martensitic phase transformation to the {alpha}{prime} phase during low temperature excursions [2, 3] and are also metastable with respect to a {delta} {yields} {alpha}{prime} phase transformation with increases in pressure [3-5]. The low temperature {delta} {yields} {alpha}{prime} isothermal martensitic phase transformation in the Pu-2 at.% Ga alloy only goes to {approx}25% completion with the resultant {approx}20 {micro}m long by 2 {micro}m wide lath-shaped {alpha}{prime} particles dispersed within the {delta} matrix. In recently reported studies, Faure et al. [4] have observed a {delta} {yields} {gamma} {yields} {alpha}{prime} pressure-induced phase transformation sequence during a diamond anvil cell investigation and, based on x-ray diffraction and density and compressibility experiments, Harbur [5] has concluded that both {alpha}{prime} and an amorphous phase are present in samples that were pressurized and recovered. In this work, a large volume moissanite anvil cell is constructed to permit the pressurization and recovery of specimens of a size suitable for TEM and electron diffraction studies. The cell, shown in Fig. 1, has an overall diameter of 101.6 mm, a moissanite anvil diameter of 9.00 mm, a culet size of 3 mm, and a spring steel gasket 0.5 mm thick with a hole diameter of 2.5 mm. A 2.3 mm diameter by 100 {micro}m thick sample of {delta}-phase Pu-2 at.% Ga is compressed at a rate of approximately 0.05 GPa/minute to {approx}1 GPa to induce the phase transformation to {alpha}{prime}. Optical microscopy of the recovered specimen reveals a very fine microstructure that appears to be single phase, although the resolution of this technique is insufficient to differentiate between single and multiple phases if the grain size is below approximately 1 {micro}m. X-ray diffraction, using a laboratory Cu K{sub {alpha}} source with wavelength of 1.542{angstrom}, shows the monoclinic reflections from the {alpha}{prime} phase, strong peaks from the aluminum specimen holder, and weak peaks from the face-centered cubic {delta} phase as shown in Fig. 2. The recovered specimen is prepared for TEM and electron diffraction studies as described in Moore et al. [6]. TEM reveals small regions of {delta} phase with a very high dislocation density interspersed between the 10-100's nm {alpha}{prime} grains as shown in Fig. 3. Electron diffraction, shown in the insert in Fig. 3, clearly reveals the presence of the {delta} phase. This microstructure is in contrast to the {alpha}{prime} particles that form as a result of the low-temperature isothermal martensite in which the {alpha}{prime} particles are lath-shaped and significantly larger as shown in the optical micrograph in Fig. 4 of a sample cooled to -120 C and held for 10 hours. In these preliminary results, there is no evidence of either an amorphous phase, as suggested by Harbur [5], or the presence of a {gamma} phase. We expected to observe an amorphous phase based on the similarity of this experiment to that of Harbur [5]. It is possible that the {gamma} phase, as reported by Faure et al. [4], does form as an intermediate, but it is not retained to ambient pressure.

36 MATERIALS SCIENCE↗

Time-temperature equivalence in Martensite tempering

The relationship between time and temperature is of great consequence in many materials-related processes including the tempering of martensite. In 1945, Hollomon and Jaffe quantified the 'degree of tempering' as a function of both tempering time, t, and tempering temperature, T, using the expression, T(log t + c). Here, c is thought to be a material constant and appears to decrease linearly with increasing carbon content. The Hollomon-Jaffe tempering parameter is frequently cited in the literature. This work reviews the original derivation of the tempering parameter concept, and presents the use of the characteristics diffusion distance as an alternative time-temperature relationship during martensite tempering. During the tempering of martensite, interstitial carbon atoms diffuse to form carbides. In addition, austenite decomposes, dislocations and grain boundaries rearrange, associated with iron self diffusion. Since these are all diffusional processes, it is reasonable to expect the degree of tempering to relate to the extent of diffusion.

36 MATERIALS SCIENCE↗

Effect of tailored martensitic transformation in a thick weld: Residual stresses mitigation, heterogeneous microstructure, and mechanical properties

The residual stresses, microstructural heterogeneities, and mechanical properties were extensively examined in a 25 mm thick weld consisting of two regions which respectively undergo phase transformation at relatively low (100 °C) temperature (LTT) and high (670 °C) temperature (HTT) during cooling. Due to the LTT martensitic transformation, which features a transformation strain of ~4000 με, large compressive residual stress (−510 MPa) was generated as confirmed by neutron diffraction and contour method. Meanwhile, significant heterogeneities were observed in terms of the chemical composition, yield strength, and microhardness across the interface between the LTT and HTT regions. The dependency of martensitic transformation starting temperature (M{sub s}) on chemical composition is empirically formulated, and it reveals that the dependency of M{sub s} on the Ni and Cr compositions becomes stronger when the temperature is lower than 200 °C. The maximum change of residual stresses (σ{sub x}{sup max}) exponentially decreases as M{sub s} decreases in the manner of σ{sub x}{sup max} = 97.5 exp(M{sub s}/227)-649. The fracture behavior was found highly dependent upon the volume fraction of retained austenite influenced by M{sub s}. While a ductile fracture mode was found in the cellular LTT region containing relatively higher amount of retained austenite (~10%), the interface shows transgranular brittle fracture features and sub-cracking due to the relatively small amount of retained austenite and the predominant martensite constituent.

36 MATERIALS SCIENCE↗

Austenite formation and cementite dissolution during intercritical annealing of a medium-manganese steel from a martensitic condition

In the present study, in situ high-energy X-ray diffraction (HEXRD), dilatometry, and metallography were conducted for the purpose of understanding microstructure evolution during intercritical annealing of a Fe-0.19C-4.39Mn steel from a martensitic initial condition. Three different simulations for austenite growth and solute partitioning during isothermal holding were conducted using the DICTRA™ module of Thermo-Calc®. The microstructures after intercritical annealing exhibit film-like retained austenite; however, in situ HEXRD indicates that retained austenite in the initial martensitic microstructure had decomposed upon heating to the isothermal holding temperature, suggesting that film-like austenite may be generated during intercritical annealing via nucleation and growth of new austenite and without necessarily preserving initial retained austenite films in the martensitic microstructure. Metallography and in situ HEXRD also indicate that cementite had formed upon heating but did not readily dissolve during an 1800 s isothermal hold although considerable growth of austenite had occurred during the isothermal hold, suggesting that austenite nucleation and initial growth during intercritical annealing does not solely occur due to carbon partitioning. A simulation incorporating cementite suggests that the increase in austenite fraction during intercritical annealing initially occurs in association with Mn partitioning followed by austenite growth induced by gradual cementite dissolution.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of high Mn-containing ferritic-martensitic alloys exposed to cyclical thermal treatment

Substantial residual tensile stress tends to accumulate in currently available high-Cr ferritic martensitic steels that are subjected to cyclical heat treatment, which leads to premature brittle fracture. By tailoring the alloy composition, this thermal cycling can be exploited to induce a high number density of nanoprecipitates and phase transformations countering residual tensile stresses. In this work, three new variants of ferritic-martensitic steels have been designed with computational thermodynamics to meet the goals of mitigating residual tensile stresses by lowering martensite start temperatures and of enhancing mechanical strength and irradiation sink strength by increasing the number density of nanoprecipitates. Furthermore, ctenast materials were subjected to cyclical heat treatment. The thermally cycled samples were evaluated with mechanical testing and microstructural analysis to identify the optimal composition in which figures of merit include low residual stress and a high density of nanoscale MX (M = metal, X = C/N) precipitates, leading to high yield strength with reasonable ductility. The noticeably higher density of nanoprecipitates in the optimal alloy favor its higher yield strength, which is supported by the microstructure-derived yield strength calculation and precipitation kinetics simulation.

36 MATERIALS SCIENCE↗

Two-step deformation-induced martensitic transformation in additively manufactured High-Si stainless steel

Deformation-induced phase transformation in the additively manufactured (AM) Fe–18Cr–8Ni-5.5Si (in wt.%) alloy was analyzed using the in-situ electron backscattered diffraction (EBSD) record during uniaxial tensile testing in a scanning electron microscope (SEM). Analysis of EBSD data was focused to investigate phase transformation behavior during deformation with consideration of mechanical interactions among phases and grains in the ultrafine AM microstructure. The initial EBSD phase map illustrated that the as-built microstructure was a duplex structure consisting of major austenite (γ) and minor ferrite phases, some of which showed non-traditional orientation relationship since the rapid solidification in the AM process has produced non-equilibrium state in phase formation. In the deformed as-built AM alloy, the two-step martensitic transformation (γ→ε→α´) was identified as the main deformation-induced transformation mechanism. Martensitic transformation steps were found to be associated with glides of Shockley partial dislocations on closed packed (111) planes under the influence of atomic disturbance in the γ and ε phases, respectively. Using the closed-packed plane pole figures and unit cell orientations, their evolutions and mechanisms accompanying with the transformation were analyzed. Finally, the results indicate that one variant of ε-martensite forms from their parent γ phase, while two variants of α´ form from their parent ε phase.

36 MATERIALS SCIENCE↗

Boundaries for martensitic transition of 7 Li under pressure

We report that physical properties of lithium under extreme pressures continuously reveal unexpected features. These include a sequence of structural transitions to lower symmetry phases, metal-insulator-metal transition, superconductivity with one of the highest elemental transition temperatures, and a maximum followed by a minimum in its melting line. The instability of the bcc structure of lithium is well established by the presence of a temperature-driven martensitic phase transition. The boundaries of this phase, however, have not been previously explored above 3 GPa. All higher pressure phase boundaries are either extrapolations or inferred based on indirect evidence. Here we explore the pressure dependence of the martensitic transition of lithium up to 7 GPa using a combination of neutron and X-ray scattering. We find a rather unexpected deviation from the extrapolated boundaries of the hR3 phase of lithium. Furthermore, there is evidence that, above ~3 GPa, once in fcc phase, lithium does not undergo a martensitic transition.

36 MATERIALS SCIENCE↗

Effect of niobium addition on the martensitic transformation and magnetocaloric effect in low hysteresis NiCoMnSn magnetic shape memory alloys

The effect of Nb substitution for Ni in Ni{sub 45}Co{sub 5}Mn{sub 40}Sn{sub 10} magnetic shape memory alloys on their magnetic properties, martensitic transformation characteristics, transformation hysteresis, and magnetocaloric properties was studied using wavelength-dispersive X-ray spectroscopy, differential scanning calorimetry, and the temperature and field dependence of the magnetization. Ni{sub 45}Co{sub 5}Mn{sub 40}Sn{sub 10} alloy has a very low transformation hysteresis; however, the martensitic transformation temperatures are notably above room temperature, which is not desirable for magnetic refrigeration applications. In this study, small quantities of Nb substitution were shown to drastically shift the transformation temperatures to lower temperatures, at a rate of 68 K/at. % Nb, which is needed for household refrigeration. The austenite Curie temperature also decreased with increasing Nb content. However, a decrease in the latent heat of the martensitic transition was observed, which negatively affects the magnetic field-induced adiabatic temperature change capability. Still, the relatively large transformation entropy and the low transformation hysteresis make the Nb-doped Ni{sub 45}Co{sub 5}Mn{sub 40}Sn{sub 10} alloys potential candidates for solid state refrigeration near room temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Uncharacteristic second order martensitic transformation in metals via epitaxial stress fields

While most phase transformations, e.g., ferroelectric or ferromagnetic, can be first or second order depending on external applied fields, martensitic transformations in metallic alloys are nearly universally first order. We demonstrate that epitaxial stress originating from the incorporation of a tailored second phase can modify the free energy landscape that governs the phase transition and change its order from first to second. High-fidelity molecular dynamics simulations show a remarkable change in the character of the martensitic transformation in Ni–Al alloys near the critical point. We observe the continuous evolution of the transformation order parameter and scaling with power-law exponents comparable to those in other ferroic transitions exhibiting critical behavior. Our theoretical work provides a foundation for recent experimental and computational results on martensites near critical points.

36 MATERIALS SCIENCE↗

Magnetic field dependence of the martensitic transition and magnetocaloric effects in Ni 49 BiMn 35 In 15

The structural, magnetic, and magnetocaloric properties of the Bi-doped Heusler alloy Ni 49 BiMn 35 In 15 have been investigated using room temperature X-ray diffraction (XRD) and magnetization measurements in a temperature interval of 5-400 K. The alloy at room temperature was found to be in a mixture of a high temperature austenite phase (AP) and a low temperature martensite phase (MP). A drastic shift in the martensitic transition temperature at the rate of 16 K/T from 197 K to lower temperatures was observed. A kinetic arrest phenomenon of the AP was observed in the magnetization and electrical resistivity measurements during field-cooled (FC) measurements at 5T. A metamagnetic behavior characterized by a jump in magnetization in the isothermal M ( H ) curves near T M was observed. The maximum value of the magnetic entropy change and refrigerant capacity at Curie temperature were found to be 5.5 Jkg -1 K -1 and 312 Jkg -1 for μ o Δ H = 5T, respectively. A large magnetoresistance value of -56% was found near the martensitic transition.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Formation of hierarchically structured martensites in pure iron with ultrahigh strength and stiffness

Strong steels are primarily fabricated by introducing spatial obstacles (e.g., stacking faults and precipitates) that inhibit dislocation slips under stress to achieve high strength. However, for most low-carbon steels, such obstacles are difficult to form mainly because the martensitic transition is kinetically unfavorable by conventional methods, which precludes the attainment of high-strength materials in these steels with low solute contents. Here, we report an innovative high-pressure preparation of martensitic pure Fe with involving nano-effect, which leads to the formation of ultrastrong bulk iron with exceptionally high yield strength, ultimate strength, and hardness of 2.9 GPa, 3.7 GPa, and 9.0 GPa, respectively, exceeding those of high-speed steels. Such extraordinary mechanical properties are closely attributed to its high-density martensites with unique multiscale hierarchical structures formed due to complex phase transitions under pressure.

Science & Technology - Other Topics↗

Nondissipative Martensitic Phase Transformation after Multimillion Superelastic Cycles

Superelastic alloys used for stents, biomedical implants, and solid-state cooling devices rely on their reversible stress-induced martensitic transformations. These applications require the alloy to sustain high deformability over millions of cycles without failure. Here, we report an alloy capable of enduring 10 × 10 7 tensile stress-induced phase transformations while still exhibiting over 2% recoverable elastic strains. After millions of cycles, the alloy is highly reversible with zero stress hysteresis. We show that the major martensite variant is reversible even after multimillions of cycles under tensile loadings with a highly coherent $(1\bar{1}0)_A$ interface. Finally, this discovery provides new insights into martensitic transformation, and may guide the development of superelastic alloys for multimillion cycling applications.

36 MATERIALS SCIENCE↗

Ultrafast Martensitic Phase Transition Driven by Intense Terahertz Pulses

We report on an ultrafast nonequilibrium phase transition with a strikingly long-lived martensitic anomaly driven by above-threshold single-cycle terahertz pulses with a peak field of more than 1 MV/cm. A nonthermal, terahertz-induced depletion of low-frequency conductivity in Nb 3 Sn indicates increased gap splitting of high-energy 12 bands by removal of their degeneracies, which induces the martensitic phase above their equilibrium transition temperature. In contrast, optical pumping leads to a Γ 12 gap thermal melting. Such light-induced nonequilibrium martensitic phase exhibits a substantially enhanced critical temperature up to ~100 K, i.e., more than twice the equilibrium temperature, and can be stabilized beyond technologically relevant, nanosecond time scales. Together with first-principle simulations, we identify a compelling terahertz tuning mechanism of structural order via Γ 12 phonons to achieve the ultrafast phase transition to a metastable electronic state out of equilibrium at high temperatures far exceeding those for equilibrium states.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Transformation temperatures of martensite in beta phase nickel aluminide

Resistivity and thermal arrest measurements determined that the compositional dependence of Ms (martensite state) temperatures for NiAl martensite was linear between 60 and 69 atomic percent nickel, with Ms = 124 Ni - 7410 K. Resistivity and surface relief experiments indicated the presence of thermoelastic martensite for selected alloys. Some aspects of the transformation were studied by hot stage microscopy and related to the behavior observed for alloys exhibiting the shape-memory effect.

Smialek, J. L.↗

Towards Accurate and Efficient Predictions of Martensitic Transition Temperatures for Shape Memory Alloys from First Principles

Shape memory alloys (SMAs) can remember and recover their original shapes upon heating due to the existence of a reversible martensitic transition (MT) between the high-temperature austenite (A) and low-temperature martensite (M) phases. The martensitic transition temperature (MTT) is a crucial characteristic of an SMA. SMAs have a wide range of potential applications in aerospace, civil engineering, bioengineering, etc., but their operating temperatures are limited by the available SMAs. MTT can be tuned by alloying a binary with other metals, and the multicomponent NiTi-based SMAs have attracted tremendous research efforts recently. It is not efficient to employ the trial-and-error method alone due to the dramatically increased complexity and possibilities in compositions, and thus reliable theory and accurate computations play an indispensable role in creating SMAs with desirable properties.

Zhigang Wu↗

Molecular Dynamics Simulations of Austenite-Martensite Interfaces in NiTi Shape Memory Alloys

The unique properties of shape memory alloys (SMAs) arise from a reversible martensitic transformation. The nucleation and migration of austenite-martensite interfaces are the key to understanding the SMA properties. Molecular dynamics (MD) simulations can provide important atomic-scale information about these aspects of the transformation, but their time scales prevent the interface formation under near-equilibrium conditions relevant to experiment. We present a new MD methodology which allows for the natural formation of energetically preferred austenite-martensite interfaces under near-equilibrium conditions. Our simulation demonstrates that the interfaces in NiTi are semi-coherent, composed of a series of terrace planes and structural disconnections, and they migrate rapidly through single crystals with only a small thermodynamic driving force. In bi-crystals and polycrystals, the migration of these same interfaces is significantly impeded by grain boundaries and stored elastic energy. This behavior can result in SMA hysteresis via several mechanisms associated with nucleation and non-elastic strain accommodation.

Gabriel Plummer↗