At least 163 records · Page 9

Phase Transformations and Formation of Ultra-Fine Microstructure During Hydrogen Sintering and Phase Transformation (HSPT) Processing of Ti-6Al-4V

The hydrogen sintering and phase transformation (HSPT) process is a novel powder metallurgy method for producing Ti alloys, particularly the Ti-6Al-4V alloy, with ultra-fine microstructure in the as-sintered state. The ultra-fine microstructure is obtained as a direct result of the use of H-2 gas during sintering. The refinement of the microstructure during HSPT is similar to that of thermal hydrogen processing (THP) of bulk Ti alloys. For both THP and HSPT of Ti-6Al-4V alloy, the mechanisms of the grain refinement depend on the phase equilibria and phase transformations in the presence of hydrogen, which are surprisingly still not well established to date and are still subjected to research and debate. In recent work by the present authors, a pseudo-binary phase diagram of (Ti-6Al-4V)-H has been determined by using in situ synchrotron XRD and TGA/DSC techniques. Aided by this phase diagram, the current paper focuses on the series of phase transformations during sintering and cooling of Ti-6Al-4V in a hydrogen atmosphere and the mechanisms for the formation of the ultra-fine microstructures obtained. Using experimental techniques, including in situ synchrotron XRD, SEM, EBSD, and TEM, the microstructural refinement was found to be the result of (1) the precipitation of ultra-fine alpha/alpha(2) within coarse beta grains during an isothermal hold at intermediate temperatures, and (2) the eutectoid transformation of beta -> alpha + delta d at approximately 473 K (200 degrees C). (C) The Minerals, Metals & Materials Society and ASM International 2015

Sun, Pei↗

Effect of Electropulsing-Assisted Ultrasonic Nanocrystalline Surface Modification on the Surface Mechanical Properties and Microstructure of Ti-6Al-4V Alloy

The effect of electropulsing-assisted ultrasonic nanocrystalline surface modification (EP-UNSM) on surface mechanical properties and microstructure of Ti-6Al-4V alloy is investigated. Compared to conventional ultrasonic nanocrystalline surface modification (UNSM), EP-UNSM can effectively facilitate surface roughness and morphology, leading to excellent surface roughness (reduced from Ra 0.918 to Ra 0.028 μm by UNSM and Ra 0.019 μm by EP-UNSM) and smoother morphology with less cracks and defects. Surface friction coefficients are enhanced, resulting in lower and smoother friction coefficients. In addition, the surface-strengthened layer and ultra-refined grains are significantly enhanced with more severe plastic deformation and a greater surface hardness (a maximum hardness value of 407 HV and an effective depth of 550 μm, in comparison with the maximum hardness value of 364 HV and effective depth of 300 μm obtained by conventional UNSM). Remarkable enhancement of surface mechanical properties can be attributed to the refined gradient microstructure and the enhanced severe plastic deformation layer induced by coupling the effects of UNSM and electropulsing. The accelerated dislocation mobility and atom diffusion caused by the thermal and athermal effects of electropulsing treatment may be the primary intrinsic reasons for these improvements.

36 MATERIALS SCIENCE↗

An Integrated Study on the Evolution of Inclusions in EH36 Shipbuilding Steel with Mg Addition: From Casting to Welding

Inclusion evolution behaviors, in terms of composition, size, and number density, and associated influence on the microstructures of the as-cast slabs, rolled plates, and simulated welded samples of plain EH36 and EH36-Mg shipbuilding steels have been systematically investigated. The results indicate that the inclusions in the as-cast plain EH36 are almost Al-Ca-S-O-(Mn) complex oxides with sizes ranging from 1.0 to 2.0 μm. After Mg addition, a large amount of individually fine MnS precipitates and Mg-containing Ti-Al-Mg-O-(Mn-S) complex inclusions are generated, which significantly refine the microstructure and are conducive to the nucleation of acicular ferrite in the rolled and welded sample. Moreover, after rolling and welding thermal simulation, the number of individual MnS decreases gradually due to its precipitation on the surface of Ti-Al-Mg-O oxides.

36 MATERIALS SCIENCE↗

Effect of graphite nanoplatelets and carbon nanofibers on rheology, hydration, shrinkage, mechanical properties, and microstructure of UHPC

This study evaluates the effects of two types of graphite nanoplatelet (GNP-C and GNP-M) and one type of carbon nanofiber (CNF) on rheological properties, hydration kinetics, autogenous shrinkage, and pore structure of ultra-high-performance concrete (UHPC). The dispersion method was optimized to secure uniform dispersion of the nanomaterials in the UHPC. The plastic viscosity decreased with the nanomaterials content as the content was increased from 0 to 0.05%. As the nanomaterials content increased from 0 to 0.3%, the duration of induction period was extended by the addition of CNF, but shortened by use of GNP-C or GNP-M; cumulative hydration heat release was increased by introduction of nanomaterials; the autogenous shrinkage of UHPC with CNF, GNP-C, and GNP-M was increased by 30%, 20%, and 20%, respectively. The use of 0.3% CNFs reduced the total porosity of the UHPC by approximately 35%, indicating that the presence of CNFs refined the microstructure of UHPC.

36 MATERIALS SCIENCE↗

Laser shock peening effect on the dislocation transitions and grain refinement of Al–Mg–Si alloy

This paper systematically investigates the effect of laser shock peening without coating parameters on the microstructural evolution, and dislocation configurations induced by ultra-high plastic strains and strain rates. Based on an analysis of optical microscopy, polarized light microscopy, transmission electron microscopy observations and residual stress analysis, the significant influence of laser shock peening parameters due to the effect of plasma generation and shock wave propagation has been confirmed. Although the optical microscopy results revealed no significant microstructural changes after laser shock peening, i.e. no heat effect zone and differences in the distribution of second-phase particles, expressive influence of laser treatment parameters on the laser shock induced craters was confirmed. Moreover, polarized light microscopy results have confirmed the existence of well-defined longish grains up to 455 μm in length in the centre of the plate due to the rolling effect, and randomly oriented smaller grains (20 μm × 50 μm) in the surface due to the static recrystallization effect. Laser shock peening is reflected in an exceptional increase in dislocation density with various configurations, i.e. dislocation lines, dislocation cells, dislocation tangles, and the formation of dense dislocation walls. More importantly, the microstructure is considerably refined due to the effect of strain deformations induced by laser shock peening process. The results have confirmed that dense dislocation structures during ultra-high plastic deformation with the addition of shear bands producing ultra-fine (60–200 nm) and nano-grains (20–50 nm). Furthermore, dislocation density was increased by a factor of 2.5 compared to the untreated material (29 × 10{sup 13} m{sup −2} vs. 12 × 10{sup 13} m{sup −2}). - Highlights: • LSPwC imparts high compressive residual stresses up to − 362 ± 31 MPa. • After LSPwC the microstructure is considerably refined via dislocation transitions. • Results confirmed ultra-fine (60–200 nm) and nano-grains (20–50 nm) after LSPwC. • Reasonable agreements between dislocation density and residual stress are obtained.

36 MATERIALS SCIENCE↗

Microstructures of magnetically assisted dual-phase steel resistance spot welds

Traditional spot welds and magnetically assisted spot welds were made in 2.25 mm thick galvanised dual-phase steel, and the weld microstructures were compared. The magnetically assisted weld nugget had a ‘dog bone’ shape, and it had an increased diameter, which indicates a larger load-bearing area that will improve mechanical performance. The fusion zone of the magnetically assisted welds had a finer and less-directional grain structure than the conventional welds, which would improve weld strength, plastic strains, and ductility. Both types of welds contained an unusual soft zone very close to the fusion zone that is thought to be an integral part of the fusion zone. Furthermore, the soft zone of the magnetically assisted welds was wider than the conventional welds.

36 MATERIALS SCIENCE↗

Fabrication of thin-walled tubes from alloy 602 CA using shear assisted processing and extrusion

Thin-walled tube is usually produced seamlessly via an expensive multi-step process or via welding of thin sheets but at reduced performance. To overcome the current process and performance inefficiencies, advanced manufacturing methods need to be investigated. In this investigation, shear assisted processing and extrusion (ShAPE) was used to fabricate thin-walled Inconel 602 tube in a single-step. Tubes measuring 0.83 m length with a 12 mm outer diameter and 1 mm wall thickness were fabricated with an average surface roughness, Ra of 1.6 µm and Rz of 15 µm. Tensile testing of tubes in the as-fabricated condition showed strength increases of 4-35% over current offerings while maintaining or improving elongation. Electron microscopy analysis revealed the recrystallized microstructure with refined inter- and intra-granular carbides. Preliminary results obtained in this investigation shows the feasibility of producing thin-wall high temperature tube in single-step via ShAPE. This achievement marks a significant step towards manufacturing larger diameter nickel alloy tubes for the U.S. Department of Energy’s Waste Treatment and Immobilization Plant.

36 MATERIALS SCIENCE↗

Friction Stir Processing for Efficient Manufacturing

Friction at contacting surfaces in relative motion is a major source of parasitic energy loss in machine systems and manufacturing processes. Consequently, friction reduction usually translates to efficiency gain and reduction in energy consumption. Furthermore, friction at surfaces eventually leads to wear and failure of the components thereby compromising reliability and durability. In order to reduce friction and wear in tribological components, material surfaces are often hardened by a variety of methods, including conventional heat treatment, laser surface hardening, and thin-film coatings. While these surface treatments are effective when used in conjunction with lubrication to prevent failure, they are all energy intensive and could potentially add significant cost. A new concept for surface hardening of metallic materials and components is Friction Stir Processing (FSP). Compared to the current surface hardening technologies, FSP is more energy efficient has no emission or waste by products and may result in better tribological performance. FSP involves plunging a rotating tool to a predetermined depth (case layer thickness) and translating the FSP tool along the area to be processed. This action of the tool produces heating and severe plastic deformation of the processed area. For steel the temperature is high enough to cause phase transformation, ultimately forming hard martensitic phase. Indeed, FSP has been used for surface modification of several metals and alloys so as to homogenize the microstructure and refine the grain size, both of which led to improved fatigue and corrosion resistance. Based on the effect of FSP on near-surface layer material, it was expected to have beneficial effects on friction and wear performance of metallic materials. However, little or no knowledge existed on the impact of FSP concerning friction and wear performance the subject of the this project and final report. Specifically for steel, which is the most dominant tribological material, FSP can replace the current conventional surface hardening techniques used for friction and wear performance. Friction Stir Link Inc. (FSL) is teamed with Argonne National Laboratory (ANL) to develop and optimize FSP for friction and wear performance enhancement. The ultimate goal is to offer FSP and an effective alternative to some of the current energy intensive and high-cost surface hardening processes.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Strong‐Yet‐Ductile Eutectic Alloys Employing Cocoon‐Like Nanometer‐Sized Dislocation Cells

Abstract Eutectic alloys (EAs) with superior fluidity are known to be the easiest to cast into high‐quality ingots, making them the alloys of choice for making large‐sized structural parts. However, conventional EAs (CEAs) have never reached strength–ductility combinations on par with the best in other alloy categories. Via thermomechanical processing of cast Ni‐32.88wt%Fe‐9.53wt%Al CEAs, a cocoon‐like nano‐meshed (as fine as 26 nm) network of dislocations (CNN‐D) is produced via recovery annealing, through the rearrangement of cold‐work‐accumulated dislocations anchored by dense pre‐existing nanoprecipitates. In lieu of traditional plasticity mechanisms, such as TWIP and TRIP, the CNN‐D is particularly effective in eutectic lamellae with alternating phases, as it instigates nanometer‐spaced planar slip bands that not only dynamically refine the microstructure but also transmit from the FCC (face‐centered‐cubic) layers into the otherwise brittle B2 layers. These additional mechanisms for strengthening and strain hardening sustain stable tensile flow, resulting in a striking elevation of both strength and ductility to outrank not only all previous CEAs, but also the state of the art—additively manufactured eutectic high‐entropy alloys. The CNN‐D thus adds a novel microstructural strategy for performance enhancement, especially for compositionally complex alloys that increasingly make use of nanoprecipitates or local chemical order.

Chemistry↗

Microstructural evolution in Cu-Nb processed via friction consolidation

Immiscible alloys, whether in well-mixed or layered forms, are of increasing interest based on their novel structural and functional properties, such as enhanced thermal stability against grain growth or radiation-induced defect trapping at the interfaces. To address the need for new approaches to tailor microstructures, the microstructural development of an immiscible Cu-Nb alloy processed via friction consolidation of elemental powders is investigated. Friction consolidation is a solid-phase processing technique that imparts severe plastic strain into a deforming volume resulting in elevated temperatures below the melting temperature of the alloy. Two distinct processing pathways were chosen to understand the effect of thermomechanical conditions on the final microstructure. The microstructure was characterized using scanning electron microscopy, scanning transmission electron microscopy, and X-ray diffraction techniques. Path 1 exhibited larger strain, strain rate, and temperature as compared with path 2. In path 1, agglomerated Nb particles were present in the recrystallized ultrafine-grained Cu matrix, while in path 2 extremely fine and dispersed Nb particles were present in a highly deformed Cu matrix. In both pathways, supersaturation of Cu in Nb lattices was noted, but not vice-versa. The asymmetry in mixing is explained based on deformation-based, thermodynamic and kinetic factors. These findings provide a pathway for creation of novel tailored microstructures and improved properties in any number of binary immiscible alloy systems.

Cu-Nb alloys, Microstructural refinement, Friction↗

A High-Throughput Method to Define Additive Manufacturing Process Parameters: Application to Haynes 282

This paper demonstrates how an analytical and experimental method can be used to rapidly define the 45 additive manufacturing settings for a new alloy where the process parameters were previously unknown. A nickel-based superalloy, Haynes 282, was chosen for the analysis. An experimental matrix of focused processing parameters was predicted with a dimensionless number and 100 samples were printed using the Selective Laser Melting technique. High-throughput measurements validated the predicted process conditions needed to achieve desired density and hardness. The whole process was completed in 16 hours. The new technique was confirmed with analytical processing maps adopted by the metal additive manufacturing community. With the predicted set of process parameters, microstructural characterizations and tensile testing were used to confirm the predictions. The resultant as-fabricated microstructures have refined length scales of both microsegregation and secondary phase distributions. As a result, the mechanical properties were comparable within the predicted processing window and exhibited high strength and high ductility.

Laser Material Processing↗

Electrochemical Behavior of Sn-9Zn-xTi Lead-Free Solders in Neutral 0.5M NaCl Solution

Electrochemical techniques were employed to study the electrochemical corrosion behavior of Sn-9Zn-xTi (x = 0, 0.05, 0.1, 0.2 wt.%) lead-free solders in neutral 0.5M NaCl solution, aiming to figure out the effect of Ti content on the corrosion properties of Sn-9Zn, providing information for the composition design of Sn-Zn-based lead-free solders from the perspective of corrosion. EIS results reveal that Ti addition was involved in the corrosion product layer and changed electrochemical interface behavior from charge transfer control process to diffusion control process. The trace amount of Ti addition (0.05 wt.%) can refine the microstructure and improve the corrosion resistance of Sn-9Zn solder, evidenced by much lower corrosion current density (i{sub corr}) and much higher total resistance (R{sub t}). Excess Ti addition (over 0.1 wt.%) led to the formation of Ti-containing IMCs, which were confirmed as Sn{sub 3}Ti{sub 2} and Sn{sub 5}Ti{sub 6}, deteriorating the corrosion resistance of Sn-9Zn-xTi solders. The main corrosion products were confirmed as Sn{sub 3}O(OH){sub 2}Cl{sub 2} mixed with small amount of chlorine/oxide Sn compounds.

36 MATERIALS SCIENCE↗

The Effects of Sc Addition on the Microstructure and Mechanical Properties of Be-Al Alloy Fabricated by Induction Melting

This study investigated the alloying effects of 0.4 wt.% Sc on the microstructure, mechanical properties, and fracture behavior of a cast Be-Al alloy prepared by vacuum induction melting. The micromechanics of Sc-containing secondary-phase particles (SPs) were characterized by nanoindentation, and the fracture behavior of the alloy was investigated via tensile fractography and optical metallography. The addition of 0.4 wt.% Sc significantly modified the alloy microstructure by decreasing the secondary dendritic arm spacing (SDAS), weakening the dendritic structure of Be, and producing an equiaxed/cellular alloy microstructure with refined Be grains. Sc alloying increased the Vickers hardness by 36%, elastic modulus by 28%, yield strength by 35%, ultimate strength by 52%, but decreased the elongation from 3.6 to 2.9%. Sc-containing SPs had a higher elastic modulus, yield strength, microhardness, and a lower plasticity index than the Be and Al matrices, resulting in interface separation during the fracture process. SPs located at the Be/Al interfaces did not act as microcrack sources for the matrices, whereas highly faceted SPs within the Be grains induced microcrack formation and decreased the elongation. The failure mode of the cast Be-Al-0.4Sc alloy still involved the brittle cleavage failure of Be regions and ductile dimple failure of Al regions, which was not the case with the cast Be-Al alloy.

36 MATERIALS SCIENCE↗

Corrosion Behavior of AZ31 Magnesium Alloy Produced by Continuous Variable Cross Section Direct Extrusion

In order to study the corrosion behavior of magnesium alloys of high performance in the simulated seawater by continuous variable cross section direct extrusion (CVCDE), an electrochemical method and weight loss method were used to study the difference between AZ31 magnesium alloys produced by CVCDE with different numbers of interim dies to examine the electrochemical corrosion behavior and corrosion rate at 3.5 wt.% NaCl solution in this paper. Scanning electron microscopy and x-ray diffraction were used to analyze the morphology of corrosion surfaces and the composition of the corrosion products of samples soaked for different times. The results show that after CVCDE with different numbers of interim dies, the size of the microstructure is refined gradually, and the grain orientation is also different; with the increase in the number of interim dies, the thermodynamic corrosion tendencies are different, and the corrosion resistance of samples extruded by conventional extrusion is relatively good; the charge transfer and material transfer process are the two main factors affecting the corrosion rate, which determines the direction of the electrochemical reaction; the corrosion form of the sample extruded by CVCDE is the local corrosion which is the filiform corrosion and pitting corrosion, and the corrosion product is mainly water-insoluble Mg(OH){sub 2}.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of pure copper wire produced by shear assisted processing and extrusion

Shear assisted processing and extrusion (ShAPE) process can consolidate powdered materials and simultaneously extrude wire or tube with improved properties. We successfully produced copper wire extrusions from powder and solid materials for the first time. The extrusion pressure of ShAPE process is at least two times less than that required for conventional extrusion. We used optical microscopy to inspect and validate the integrity of extrudates. It shows that the microstructure was refined and dynamically recrystallized to equiaxial grains. Compared to the annealed copper wire, ShAPE processed wire has 80% higher yield strength, 15% higher ultimate tensile strength and 20% higher ductility. These were correlated with refined grain size and sub-structuring observed via electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM).

Copper, Wire, Shear Assisted Processing and Extrus↗

Probabilistic fatigue life prediction model for alloys with defects: applied to A206

Presented here is a model for the prediction of fatigue life based on the statistical distribution of pores, intermetallic particles and grains. This has been applied to a cast Al alloy A206, before and after friction stir processing (FSP). The model computes the probability to initiate a small crack based on the probability of finding combinations of defects and grains on the surface. The crack initiation and propagation life of small cracks due to these defect and grain combinations are computed and summed to obtain the total fatigue life. The defect and grain combinations are ranked according to total fatigue life and the failure probability computed. Bending fatigue experiments were carried out on A206 before and after FSP. FSP eliminated the porosity, broke down the particles and refined the microstructure. The model predicted the fatigue life of A206 before and after FSP well. The cumulative probability distribution vs. fatigue life was fitted to a three parameter Weibull distribution function. The scatter reduced after FSP and the threshold of fatigue life increased. The potential improvement in the fatigue life of A206 for a microstructure consisting of a finer distribution of particle sizes after FSP was predicted using the model.