Search NASA⌕ Search

SEARCH · Search NASA

Results for “Photovoltaic Module”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Life Cycle Inventory of Current Photovoltaic Module Recycling Processes in Europe

Solar photovoltaic (PV) installations must be properly dismantled and any waste treated and disposed at the end of project life. However, because most of the world's nearly 400 GW of PV systems have been built in the past decade - each expected to operate for between 20 and 30 years - current PV module waste volumes do not yet justify widespread operation of PV recycling facilities. The necessary policies and technologies for recycling PV systems are currently under rapid development. With modifications to the European waste electrical and electronic equipment directive (WEEE 2012/19/EU) in 2012, take back and recycling of PV modules is, in fact, already mandatory in Europe. There, take back and recycling is currently performed in small but annually-increasing quantities. Even though waste treatment is considered part of a module's life cycle, only a few life cycle inventories (LCI) of energy and materials flows are available for the industrial recycling processes that are used today to recycle crystalline silicon-based (c-Si) PV modules. LCI are the data inputs that inform lifecycle assessments which quantify the environmental impacts across the full life cycle of PV modules - from manufacturing and use to end of life. To help progress the industry forward, a survey of European recyclers was performed to characterize existing commercial recycling processes and share associated life cycle inventory data. System Boundaries: The reference unit, or "functional unit" in the vocabulary of life cycle assessment, is defined as the processing of one metric ton of crystalline silicon PV modules in recycling lines for laminated glass, metals, and electronic wastes. Today, all modules are processed in discrete batches, yet not metered at that scale. Thus the process energy for a batch is estimated based on scaled annual production data as well as on input and output streams.

14 SOLAR ENERGY↗

Durability of ionomer encapsulants in photovoltaic modules

Ethylene vinyl acetate (EVA) has for decades been the preferred material for photovoltaic (PV) module encapsulation. However, while it is relatively inexpensive and initially adheres well to module components, EVA discolors with age and - as interfacial adhesion degrades - becomes susceptible to delamination, ultimately resulting in reduced module efficiency and shortened service lifetimes. As potential replacements for EVA, ionomer thermoplastic materials cure faster, are more resistant to discoloration and potential induced degradation, and do not evolve corrosive acetic acid, making them compatible with new device materials such as perovskites. Since there is limited information on ionomer durability for PV module applications, a series of field and accelerated laboratory aging studies were conducted to assess ionomer interface stability in the presence of terrestrial environmental stressors. It is shown that adhesion to the glass and cell interfaces of PV modules is inferior to EVA, both before and after aging, rendering ionomers particularly susceptible to delamination after short timeframes. Potential solutions to improve ionomer adhesion are discussed.

14 SOLAR ENERGY↗

Task 12 PV Sustainability - Life Cycle Assessment of Crystalline Silicon Photovoltaic Module Delamination with Hot Knife Technology

The objective of this study is to complete a life cycle assessment (LCA) of a novel technology that separates the crystalline silicon (c-Si) photovoltaic (PV) module front glass from the backsheet using hot knife technology. This is known to be the most challenging step in module recycling, where the choice of delamination approach can determine the process selection for the next steps of the recycling process, the economic value of the recovered materials, and environmental performance. The life cycle inventory (LCI) reported here is based on primary data from the technology manufacturer. Different LCIs are established following the cut-off approach and the end-of-life (EOL) approach. The environmental impacts of the hot knife delamination process are analysed based on six indicators, and the main contributors to delamination efforts are identified. For the EOL approach, the potential environmental benefits from the recovered materials are compared to the environmental impacts caused by the delamination process. The functional unit of this analysis is the delamination of 1 kg of used framed c-Si PV modules at the place of installation.

14 SOLAR ENERGY↗

Diffractive Multiplexing for High-Throughput Roll-to-Roll Laser Patterning of Flexible Organic Photovoltaic Modules (Final Report)

The purpose of this project is to demonstrate a cost-effective, high-throughput roll-to-roll (R2R) process for patterning of flexible, semitransparent organic photovoltaic (OPV) modules by developing diffractive optics-based laser multiplexing (DOL Multiplexing). DOL Multiplexing allows a single, high-powered laser source to perform parallel scribing across the R2R web width in a manner compatible with high process speeds. Such a process could have enormous benefits in terms of increased process speeds and reduced costs, both up-front capital costs, and long-term operational costs, over galvanometer-based step and scan methods or many-laser systems.

14 SOLAR ENERGY↗

Advancing reliability assessments of photovoltaic modules and materials using combined-accelerated stress testing

Previously undiscovered failure modes in photovoltaic (PV) modules continue to emerge in field installations despite passing protocols for design qualification and quality assurance. Failure to detect these modes prior to widespread use could be attributed to the limitations of present-day standard accelerated stress tests (ASTs), which are primarily designed to identify known degradation or failure modes at the time of development by applying simultaneous or sequential stress factors (usually two at most). Here, we introduce an accelerated testing method known as the combined-accelerated stress test (C-AST), which simultaneously combines multiple stress factors of the natural environment. Simultaneous combination of multiple stress factors allows for improved identification of failure modes with better ability to detect modes not known a priori. A demonstration experiment was conducted that reproduced the field-observed cracking of polyamide- (PA-) and polyvinylidene fluoride (PVDF)–based backsheet films, a failure mode that was not detected by current design qualification and quality assurance testing requirements. In this work, a two-phase testing protocol was implemented. The first cycle (“Tropical”) is a predominantly high-humidity and high-temperature test designed to replicate harsh tropical climates. The second cycle (“Multi-season”) was designed to replicate drier and more temperate conditions found in continental or desert climates. Testing was conducted on 2 × 2-cell crystalline-silicon cell miniature modules constructed with both ultraviolet (UV)–transmitting and UV-blocking encapsulants. Cracking failures were observed within a cumulative 120 days of the Tropical condition for one of the PA-based backsheets and after 84 days of Tropical cycle followed by 42 days of the Multi-season cycle for the PVDF-based backsheet, which are both consistent with failures seen in fielded modules. In addition to backsheet cracking, degradation modes were observed including solder/interconnect fatigue, various light-induced degradation modes, backsheet delamination, discoloration, corrosion, and cell cracking. The ability to simultaneously apply multiple stress factors may allow many of the test sequences within the standardized design qualification procedure to be performed using a single test setup.

14 SOLAR ENERGY↗

Advanced Photovoltaic Module Characterization: Using Image Transformers for Current–Voltage Curve Prediction From Electroluminescence Images

Individual photovoltaic (PV) module health monitoring can be a daunting task for operation and maintenance of solar farms. Modules can be inspected through luminescence, thermal imaging, and current–voltage (I–V) curve analyzes for identification of damage and power loss. I–V curves provide easily interpretable data to determine module health as they directly provide electrical performance metrics. However, in order to obtain these curves, modules must be disconnected from the array and either removed to a solar simulator or characterized in situ with corrections for module temperature, the incident solar spectrum, and intensity. Luminescence or thermal images of a module are relatively easy to acquire in situ. Electroluminescence (EL) images highlight physical defects in the modules but do not provide easily interpretable features to correlate with electrical performance. This work presents a SWin transformer network to predict I–V curves for PV modules from their corresponding EL images. The predicted I–V curves allow the accurate prediction of the maximum power point (MPP), short-circuit current I sc , and open-circuit voltage V oc with a mean error less of than 1%. Comparing single diode model (SDM) parameters extracted from the predicted curves to those extracted from the true curves, the series resistance R s demonstrates a mean error of 5.19%, and the photocurrent I a mean error of 0.197%. The shunt resistance R sh and dark current Io parameters are predicted with larger errors because of their sensitivity to small changes in the I–V curve.

Byford, Brandon K. [New Mexico State Univ., Las Cr↗

Transient Weighted Moving-Average Model of Photovoltaic Module Back-Surface Temperature

Accurate modeling of photovoltaic (PV) performance requires the precise calculation of module temperature. Currently, most temperature models rely on steady-state assumptions that do not account for the transient climatic conditions and thermal mass of the module. On the other hand, complex physics-based transient models are computationally expensive and difficult to parameterize. In order to address this, a new approach to transient thermal modeling was developed, in which the steady-state predictions from previous timesteps are weighted and averaged to accurately predict the module temperature at finer time scales. This model is informed by 3-D finite-element analyses, which are used to calculate the effect of wind speed and module unit mass on module temperature. The model, in application, serves as an added filter over existing steady-state models that smooths out erroneous values that are a result of intermittency in solar resource. Validation of this moving-average model has shown that it can improve the overall PV energy performance model accuracy by as much as 0.58% over steady-state models based on mean absolute error improvements and can significantly reduce the variability between the model predictions and measured temperature times series data.

14 SOLAR ENERGY↗

Photovoltaic module antireflection coating degradation survey using color microscopy and spectral reflectance

Abstract Commercial antireflective coatings (ARCs) on photovoltaic (PV) module glass can improve module power by 2.5%–3.0%, but their long‐term field performance requires additional study. In this paper, we investigate ARC performance on fielded modules using two nondestructive techniques: reflectance spectroscopy and RGB microscopy, finding a large variation in coating durability and performance. For new coatings, the fleet average nominal power enhancement is 2.8%. This power enhancement is observed to degrade at approximately −0.05%/year absolute over the first 8 years of fielding in arrays that are not regularly cleaned. Interferometry and imaging results imply that coating loss for these modules is due to slow chemical thinning of the initial 125 nm thick coating by 1.4 to 5.0 nm/year. Due to the physics of interference coatings, the performance loss is projected to accelerate as the coating is further thinned, resulting in a coating lifetime (time to 80% of initial performance) of 7.5 to 25 years. At the higher 5.0 nm/year coating loss rates, we estimate that −0.14%/year power degradation of the module can be attributed solely to ARC degradation over the first 20 years. Extreme coating loss is observed on some modules where after 8 years fielding, the coating can be completely removed with a single wet wipe with a lens tissue. A case study is also presented comparing ARC and noncoated modules installed at a single site in 2013. We find that the ARC modules have a 2.6% higher soiling power loss than the noncoated modules; this exceeds the ARC power enhancement of 2.4% and leads to the surprising conclusion that the ARC lowers production for modules in this location due to increased soiling. These results demonstrate that RGB microscopy is a powerful, field‐capable, and quantitative characterization technique for assessing degradation of PV module ARCs.

Karin, Todd↗

Thermomechanical fatigue resistance of low temperature solder for multiwire interconnects in photovoltaic modules

Novel interconnect technologies leveraging low melting temperature solders, such as multiwire interconnects, are being deployed in photovoltaic (PV) modules for improved reliability through interconnect redundancy and lower thermal loads during interconnection and lamination. However, the equivalency of standardized accelerated testing to field conditions has not yet been established for these emerging technologies. In this study, the thermomechanical fatigue resistance of low temperature solder alloys is investigated and compared to that of conventional SnPb to assess the acceleration behavior of these alloys. While InSn is shown to have sufficient thermomechanical fatigue resistance on the order of that of SnPb, these results indicate Sn–Bi alloys may have poor thermomechanical fatigue resistance at field conditions. The results also show that Sn–Bi alloys have thermal cycling acceleration factors of less than one. This indicates that the standardized accelerated thermal cycling test, such as that in IEC 61215, will produce misleading results for Sn–Bi alloys and that unique testing is required for this PV module architecture. Though accelerated thermal cycling may be a meaningful qualification test for SnPb solder joints, these results suggest that mechanical loading may be a more appropriate test for Sn–Bi multiwire interconnects. This is due to the distinct processing and geometry of multiwire interconnects which may allow for mechanical, rather than strictly metallurgical interconnections.

14 SOLAR ENERGY↗

Quantifying spectral albedo effects on bifacial photovoltaic module measurements and system model predictions

We provide a comprehensive analysis of the effect of spectral albedo on photovoltaic (PV) module measurements and system model predictions. We demonstrate how to account for albedo in indoor bifacial device measurements by adjusting the applied irradiance using the scaled rear irradiance method, exemplified on fabricated silicon heterojunction (SHJ) modules. System model performance is studied using a detailed 3D finite-element model, DUET, for fixed-tilt and horizontal single-axis tracked (SAT) arrays between 15 and 75°N. Spectral effects cause variations in measured SHJ module short-circuit current up to 2% and efficiency variation up to 0.3% abs. We further demonstrate that rear-side spectral mismatch factors (SMMs) resulting from including or omitting spectral albedo in PV system modeling vary between ±13%, while total (front+rear) SMMs vary up to 3%, depending on the deployment configuration and latitude. SAT array SMMs are weakly correlated with latitude, while fixed-tilt array SMMs increase with latitude, driven by an increasing proportion of ground-reflected light on the front-side of modules. Ground-reflections can constitute between 2% and 32% of total incident module irradiance, with notably high (>10%) contributions for fixed-tilt arrays at high latitude. Effects of spectral albedo are most significant for: (1) fixed-tilt deployments at high latitudes, (2) wide bandgap technologies such as perovskite and cadmium telluride cells, (3) albedos which vary steeply over the technology's absorption range, and (4) high albedo ground covers. Overall, we demonstrate that omitting spectral albedo effects can result in PV measurement and system-level modeling uncertainties on the order of several percent in these cases.

14 SOLAR ENERGY↗

Optical Design and Validation of an Infrared Transmissive Spectrum Splitting Concentrator Photovoltaic Module

A new modular, hybrid solar power system is designed to generate both electrical and thermal energy by utilizing the full solar spectrum. The key element, an infrared-transparent concentrator photovoltaic (CPV) module, acts as a spectrum splitter, dividing solar radiation into two parts. The ultraviolet and visible light (“in-band”) are converted to electricity with high efficiency in CPV cells, while the infrared light (“out-of-band”) is transmitted directly to a thermal receiver, where thermal power may be converted to electricity by a suitable heat engine or used directly for industrial process heat applications whenever needed. Here, we describe the optical design, modeling, fabrication, and performance validation of this novel spectrum splitting CPV module. A transfer matrix style approach, cumulative transmission model, is built to study the reflection, absorption, and transmission in each layer of the CPV module. To optimize the optical performance, different materials for module superstrate/substrate, encapsulant, cell substrate, and cooling fluids are compared in order to enhance the transmission of out-of-band light through the CPV module by minimizing absorption. Six antireflection coatings along with front and backside electrical contact grids are designed to maximize transmittance of in-band light to the cell and out-of-band light to the thermal receiver. Here, the final design, currently being prototyped, predicts out-of-band light transmission to the thermal receiver of 74.1% (for the passively cooled version) and 65.3% (for the actively cooled version). When epitaxial liftoff technology is applied, the transmission will change to 80.8% (passively cooled) and 71.9% (actively cooled). Experimental prototypes show good agreement with modeled optical performance.

14 SOLAR ENERGY↗

Trial Run of a Junction-Box Attachment Test for Use in Photovoltaic Module Qualification (Presentation)

Engineering robust adhesion of the junction-box (j-box) is a hurdle typically encountered by photovoltaic (PV) module manufacturers during product development and manufacturing process control. There are historical incidences of adverse effects (e.g., fires), caused when the j-box/adhesive/module system has failed in the field. The addition of a weight to the j-box during the 'damp-heat', 'thermal-cycle', or 'creep' tests within the IEC qualification protocol is proposed to verify the basic robustness of the adhesion system. The details of the proposed test are described, in addition to a trial run of the test procedure. The described experiments examine 4 moisture-cured silicones, 4 foam tapes, and a hot-melt adhesive used in conjunction with glass, KPE, THV, and TPE substrates. For the purpose of validating the experiment, j-boxes were adhered to a substrate, loaded with a prescribed weight, and then subjected to aging. The replicate mock-modules were aged in an environmental chamber (at 85 deg C/85% relative humidity for 1000 hours; then 100 degrees C/<10% relative humidity for 200 hours) or fielded in Golden, Miami, and Phoenix for 1 year. Attachment strength tests, including pluck and shear test geometries, were also performed on smaller component specimens.

14 SOLAR ENERGY↗

Dynamic Material Flow Analysis of Silicon Photovoltaic Modules to Support a Circular Economy Transition

Solar photovoltaics (PV) are the fastest growing renewable energy technologies for clean, cheap, and sustainable electricity generation. To prepare for rapid scale-up, the PV industry needs to project material requirements to build out all aspects of the supply chain appropriately and plan to handle large volumes of module waste. Impacts of deploying different material circularity strategies to reduce waste and conserve primary resources need to be quantified to inform sustainable material management. Here, we introduce the photovoltaic dynamic material flow analysis (PV DMFA) model based on PV electricity generation. The model quantifies material flows and stocks in the cradle-to-cradle life cycles of utility-scale c-Si PV systems in the United States through 2100. We present case studies for solar flat glass and aluminum frame materials under various scenarios to project the impacts of PV performance, reliability, and processing parameters, material circularity strategies, and module design shifts. In the absence of circularity measures, ~100 million MT of flat glass and ~12 million MT of aluminum would be needed for PV installations by 2100 to meet projected growth in domestic utility PV demand to nearly 1000 TWh in 2100. With optimistic but feasible improvements in efficiency, reliability, and circularity, material intensity and waste could be reduced by nearly 50%. Efficient module collection, minimally intrusive recycling, and careful scrap handling and cleaning could improve material circularity in the PV value chain. This model serves as a sustainability data support tool that may aid in the circular economy transition for PV systems.

circular economy↗

Potential-induced degradation in photovoltaic modules: a critical review

Potential-induced degradation (PID) has received considerable attention in recent years due to its detrimental impact on photovoltaic (PV) module performance under field conditions. Both crystalline silicon (c-Si) and thin-film PV modules are susceptible to PID. While extensive studies have already been conducted in this area, the understanding of the PID phenomena is still incomplete and it remains a major problem in the PV industry. Herein, a critical review of the available literature is given to serve as a one-stop source for understanding the current status of PID research. This article also aims to provide an overview of future research paths to address PID-related issues. This paper consists of three parts. In the first part, the modelling of leakage current paths in the module package is discussed. The PID mechanisms in both c-Si and thin-film PV modules are also comprehensively reviewed. The second part summarizes various test methods to evaluate PV modules for PID. The last part focuses on studies related to PID in the omnipresent p-type c-Si PV modules. The dependence of temperature, humidity and voltage on the progression of PID is examined. Preventive measures against PID at the cell, module and system levels are illustrated. Moreover, PID recovery in standard p-type c-Si PV modules is also studied. Most of the findings from p-type c-Si PV modules are also applicable to other PV module technologies.

14 SOLAR ENERGY↗

Numerical method for angle-of-incidence correction factors for diffuse radiation incident photovoltaic modules

Here, a numerical method is provided for solving the integral equation for the angle-of-incidence (AOI) correction factor for diffuse radiation incident photovoltaic (PV) modules. The types of diffuse radiation considered include sky, circumsolar, horizon, and ground-reflected. The method permits PV module AOI characteristics to be addressed when calculating AOI losses associated with diffuse radiation. Pseudo code is provided to aid users in the implementation, and results are shown for PV modules with tilt angles from 0° to 90°. Diffuse AOI losses are greatest for small PV module tilt angles. Including AOI losses associated with the diffuse irradiance will improve predictions of PV system performance.

14 SOLAR ENERGY↗

Ultraviolet Radiation Round-Robin Testing of Various Backsheets for Photovoltaic Modules

Durability testing of materials exposed to natural weathering requires testing of the ultraviolet (UV) stability, especially for polymeric materials. The type approval testing of photovoltaic (PV) modules according to standards IEC 61215 and IEC 61646, which includes a so-called UV preconditioning test with a total UV dose of 15 kWh/m2, does not correspond to the real loads during lifetime. Between 3%-10% of the UV radiation has to be in the spectral range between 280 and 320 nm (UV-B) in the recent editions of the standards. However, the spectral distribution of the radiation source is very important because different samples show very individual spectral sensitivity for the radiation offered. Less than 6% of the intensity of solar radiation exists in the UV range. In the case of an increase of the intensity of the light source for accelerating the UV test, overheating of the samples would have to be prevented more rigorously and the temperature of the samples have to be measured to avoid misinterpretation of the test results.