Search NASA⌕ Search

SEARCH · Search NASA

Results for “SILICONES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Charge Transfer and Built-in Electric Fields between a Crystalline Oxide and Silicon

Built-in electric fields across heterojunctions between semiconducting materials underpin the functionality of modern device technologies. Heterojunctions between semiconductors and epitaxially grown crystalline oxides provide a rich setting in which built-in fields can be explored. Here, we present an electrical transport and hard X-ray photoelectron spectroscopy study of epitaxial SrNbxTi1-xO3-d / Si heterojunctions.

Lim, Zhenghui↗

Datasheet Driven Silicon Carbide Power MOSFET Model

A compact model for SiC Power MOSFETs is presented. The model features a physical description of the channel current and internal capacitances and has been validated for dc, CV, and switching characteristics with measured data from a 1200-V, 20-A SiC power MOSFET in a temperature range of 25 degrees C to 225 degrees C. The peculiar variation of on-state resistance with temperature for SiC power MOSFETs has also been demonstrated through measurements and accounted for in the developed model. In order to improve the user experience with the model, a new datasheet driven parameter extraction strategy has been presented which requires only data available in device datasheets, to enable quick parameter extraction for off-the-shelf devices. Excellent agreement is shown between measurement and simulation using the presented model over the entire temperature range.

Mudholkar, M↗

Determination of the pure silicon monocarbide content of silicon carbide and products based on silicon carbide

Experience has shown that different methods of analysis of SiC products give different results. Methods identified as AFNOR, FEPA, and manufacturer P, currently used to detect SiC, free C, free Si, free Fe, and SiO2 are reviewed. The AFNOR method gives lower SiC content, attributed to destruction of SiC by grinding. Two products sent to independent labs for analysis by the AFNOR and FEPA methods showed somewhat different results, especially for SiC, SiO2, and Al2O3 content, whereas an X-ray analysis showed a SiC content approximately 10 points lower than by chemical methods.

Prost, L.↗

Continuous Czochralski growth: Silicon sheet growth development of the large area silicon sheet task of the Low Cost Silicon Solar Array project

The primary objective of this contract is to develop equipment and methods for the economic production of single crystal ingot material by the continuous Czochralski (CZ) process. Continuous CZ is defined for the purpose of this work as the growth of at least 100 kilograms of ingot from only one melt container. During the reporting period (October, 1977 - September, 1978), a modified grower was made fully functional and several recharge runs were performed. The largest run lasted 44 hours and over 42 kg of ingot was produced. Little, if any, degradation in efficiency was observed as a result of pulling multiple crystals from one crucible. Solar efficiencies observed were between 9.3 and 10.4% AMO (13.0 and 14.6% AMI) compared to 10.5% (14.7% AMI) for optimum CZ material control samples. Using the SAMICS/IPEG format, economic analysis of continuous CZ suggests that 1986 DoE cost goals can only be met by the growth of large diameter, large mass crystals.

Source record↗

Silicon-on-ceramic Process: Silicon Sheet Growth and Device Development for the Large-area Silicon Sheet and Cell Development Tasks of the Low-cost Solar Array Project

Significant progress is reported in fabricating a 4 sq cm cell having a 10.1 percent conversion efficiency and a 10 sq cm cell having a 9.2 percent conversion efficiency. The continuous (SCIM) coater succeeded in producing a 16 sq cm coating exhibiting unidirectional solidification and large grain size. A layer was grown at 0.2 cm/sec in the experimental coater which was partially dendritic but also contained a large smooth area approximately 100 micron m thick. The dark characteristic measurements of a typical SCC solar cell yield shunt resistance values of 10K ohms and series resistance values and 0.4 ohm. The production dip-coater is operating at over 50 percent yield in terms of good cell quality material. The most recent run yielded 13 good substrates out of 15.

Chapman, P. W.↗

Continuous Czochralski Growth. Silicon Sheet Growth Development of the Large Area Silicon Sheet Task of the Low Cost Silicon Solar Array Project

During the reporting period, a successful 100 kilogram run was performed. Six ingots of 13 cm diameter were grown, ranging in size from 15.5 kg to 17.7 kg. Melt replenishment methods included both poly rod and lump feed material. Samples from each ingot were prepared for solar cell fabrication and analyses, impurity analysis, and structural studies. The furnace was converted to the 14-inch hot zone and preliminary heat runs were performed. Two sucessful runs were demonstrated, by growing 25 kg ingots from 30 kg melts. Also, a 100 kg run was attempted, utilizing the 14 inch crucible hot zone, but was prematurely terminated due to excessive monoxide which accumulated on the viewports and a seed failure.

Merz, F.↗

Analysis of defect structure in silicon. Characterization of SEMIX material. Silicon sheet growth development for the large area silicon sheet task of the low-cost solar array project

Statistically significant quantitative structural imperfection measurements were made on samples from ubiquitous crystalline process (UCP) Ingot 5848 - 13C. Important correlation was obtained between defect densities, cell efficiency, and diffusion length. Grain boundary substructure displayed a strong influence on the conversion efficiency of solar cells from Semix material. Quantitative microscopy measurements gave statistically significant information compared to other microanalytical techniques. A surface preparation technique to obtain proper contrast of structural defects suitable for quantimet quantitative image analyzer (QTM) analysis was perfected and is used routinely. The relationships between hole mobility and grain boundary density was determined. Mobility was measured using the van der Pauw technique, and grain boundary density was measured using quantitative microscopy technique. Mobility was found to decrease with increasing grain boundary density.

Natesh, R.↗

Solid‐State Prealkylation of Electrode Architectures (SPEAR): Direct Control of Prelithiation Levels in Silicon Anodes and Electrochemical Cycling

The Solid-state Prealkylation of Electrode ARchitectures (SPEAR) is different than traditional electrochemical prealkylation processes. Through SPEAR, alkylation is driven by solid-state diffusion without the simultaneous SEI formation concomitant with polarization. Here, we investigate the prelithiation of 80 wt. % Si-based anodes to varying amounts (up to Li 1.38 Si) to understand the trade-off between improved Li capacity and expansion-induced stress. Through dilatometry, we found that solid-state lithiation led to filling of the electrode pores through silicon expansion. This swelling changed the SEI formation process and accessibility of the silicon compared to an electrochemically lithiated electrode. Indeed, optimal prelithiation to Li 0.82 Si increases the initial C/3 cycling capacity post-SEI formation up to 43%, consistent with deeper Si activation through the electrode bulk. Prelithiation and cycling cells prelithiated beyond Li 0.82 Si results in a state of charge (SOC) close to 100% which facilitates parasitic degradation mechanisms and volume expansion of the Si electrode. The results demonstrate a pathway to modify silicon activation/SEI formation to enable high-energy electrodes.

Musgrove, Amanda L. [Oak Ridge National Laboratory↗