SEARCH · Search NASA
Results for “SINTERED INTERFACES”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Effects of Holding Time on the Sintering of Cemented Tungsten Carbide Powder and Bonding with High-Strength Steel Wire
Cemented tungsten carbide (WC-10Co) and high-strength (AISI 4340) steel were successfully bonded by hot compaction diffusion bonding at a low temperature. The effects of holding time (5-50 min) on microstructure and mechanical properties of the sintered carbides and bonding strengths of the dissimilar bilayered composite materials were examined. The results show that the mechanical properties of the carbides increase, but the bonding strength increases firstly and then decreases with the increase in holding time. The maximum density and hardness achieved are 95.92 and 99.5%, respectively. A transitional layer forms at the interface as a result of elemental interdiffusion. The depth of the layer increases with the increase in holding time. The optimal bonding time is determined to be 40 min at a temperature of 1200°C and a pressure 160 MPa, by which the maximum bonding strength of 204 MPa of the WC-10Co/4340 steel joints can be achieved.
A high conductivity oxide–sulfide composite lithium superionic conductor
We fabricated a hybrid superionic conductor using the space charge effect between the LLZO and LPS interfaces. This space-charge effect resulted in an improvement over the individual bulk conductivities of the two systems. Sample with higher weight fractions of LLZO are limited by the porosity and grain boundary resistance arising from non-sintered membranes. Furthermore, by combining the properties of LLZO and LPS, the high temperature sintering step has been avoided thus facilitating easier materials processing. The interfacial resistances were also measured to be minimal at ambient conditions. Our procedure thus opens a new avenue for improving the ionic conductivity and electrochemical properties of existing solid state electrolytes. High frequency impedance analyses could aid in resolving the ionic conductivity contributions from the space charge layer in the higher conducting composites while mechanical property investigations could illustrate an improvement in the composite electrolyte in comparison with the crystalline LPS membranes.
Critical Causes of Degradation in Integrated Laboratory Scale Cells during High Temperature Electrolysis
An ongoing project at Idaho National Laboratory involves generating hydrogen from steam using solid oxide electrolysis cells (SOEC). This report describes background information about SOECs, the Integrated Laboratory Scale (ILS) testing of solid-oxide electrolysis stacks, ILS performance degradation, and post-test examination of SOECs by various researchers. The ILS test was a 720- cell, three-module test comprised of 12 stacks of 60 cells each. A peak H2 production rate of 5.7 Nm3/hr was achieved. Initially, the module area-specific resistance ranged from 1.25 Ocm2 to just over 2 Ocm2. Total H2 production rate decreased from 5.7 Nm3/hr to a steady state value of 0.7 Nm3/hr. The decrease was primarily due to cell degradation. Post test examination by Ceramatec showed that the hydrogen electrode appeared to be in good condition. The oxygen evolution electrode does show delamination in operation and an apparent foreign layer deposited at the electrolyte interface. Post test examination by Argonne National Laboratory showed that the O2-electrode delaminated from the electrolyte near the edge. One possible reason for this delamination is excessive pressure buildup with high O2 flow in the over-sintered region. According to post test examination at the Massachusetts Institute of Technology, the electrochemical reactions have been recognized as one of the prevalent causes of their degradation. Specifically, two important degradation mechanisms were examined: (1) transport of Crcontaining species from steel interconnects into the oxygen electrode and LSC bond layers in SOECs, and (2) cation segregation and phase separation in the bond layer. INL conducted a workshop October 27, 2008 to discuss possible causes of degradation in a SOEC stack. Generally, it was agreed that the following are major degradation issues relating to SOECs: • Delamination of the O2-electrode and bond layer on the steam/O2-electrode side • Contaminants (Ni, Cr, Si, etc.) on reaction sites (triple phase boundary) • Loss of electrical/ionic conductivity of electrolyte.
Towards understanding particle rigid-body motion during solid-state sintering
A quantitative understanding of particle rigid body (RB) motion that inherently accompanies grain boundary (GB) diffusion is highly desirable to understand and control the dynamic interplay between coarsening and densification during solid state sintering. In this work, by computer simulation using a multi-phase-field approach, we analyze systematically the roles played by each of these processes at different stages of the shrinkage of the internal pore in a three-particle green body as a function of particle size as well as thermodynamic and kinetic factors of interfaces. We demonstrate that particle RB translation promotes both neck growth, and pore rounding and shrinkage. Moreover, the forces acting at GBs and pulling neighboring particles towards one another dynamically evolve as particles fuse. In contrast, particle RB rotation has no contribution to pore shrinkage. The translational force acting on an individual particle varies with not only its size, but also the number and sizes of its neighboring particles.
Nano-Engineered Interfaces in Dual-Layer Electrodes for Protonic Ceramic Cells with Enhanced Stability and Kinetics
Enhancing interfacial stability and charge transfer in protonic ceramic cells (PCCs) remains a critical challenge, as structural degradation and interfacial resistance often compromise durability and efficiency. Here, we report a nanoengineered dual-layer oxygen electrode architecture designed to address these limitations by introducing a fine-grained nanoparticle interfacial contact layer beneath a porous catalytic backbone. The nanoscale powders, through enhanced sintering activity, densify into a robust interfacial layer that promotes strong chemical bonding, uniform adhesion, and continuous ionic/electronic pathways with the BCZYYb electrolyte. This hierarchical architecture mitigates delamination, redistributes mechanical stress, and establishes efficient charge and mass transport channels without relying on corrosive surface treatments. Electrochemical evaluation demonstrates that the dual-layer design markedly reduces interfacial polarization resistance and accelerates electrode kinetics. Compared to the single-layer counterpart, the architecture achieves a peel strength of 44.53 N/cm 2 , a 40% improvement in peak power density (0.96 W cm –2 at 600 °C), and a 130% enhancement in electrolysis current density (4.78 A cm –2 at 1.57 V). Faradaic efficiency remains as high as 88% under high steam concentrations, underscoring minimal charge loss during practical operation. Notably, the electrode retains stability across 450–600 °C and under transient voltage cycling, with impedance spectra confirming suppressed interfacial resistance growth over prolonged use. These results highlight nanoscale interface engineering as a powerful route to enhance both mechanical robustness and electrochemical kinetics in PCCs. The demonstrated scalability and durability of this architecture provide a versatile platform for advancing solid-state electrochemical systems, including reversible fuel cells and high-efficiency hydrogen production technologies.
Power Electronics Materials and Bonded Interfaces - Reliability and Lifetime
Wide-bandgap devices have pushed the operational limit of semiconductor devices in automotive power electronics packages to higher temperatures (>200 C). While a higher efficiency can be achieved through the use of wide-bandgap devices, the entire package must be re-designed with components that can withstand the higher temperature limits. Sintered silver and transient liquid phase bonds are potential candidates as bonded materials for use in higher temperatures however, the underlying mechanics of deformation under thermal loads and the resulting failure mechanisms in these materials are not well understood. Accelerated experiments conducted at NREL reveal that high-lead solder joints have better reliability than sintered silver under extreme thermal cycling conditions. Furthermore, efforts to develop a crack propagation model for the high-temperature materials are described.
High thermoelectric performance BiSbTe alloy with unique low-dimensional structure
We report a detailed description of an innovative route of a melt spinning (MS) technique combined with a subsequent spark plasma sintering process in order to obtain high performance p-type Bi{sub 0.52}Sb{sub 1.48}Te{sub 3} bulk material, which possesses a unique low-dimensional structure. The unique structure consists of an amorphous structure, 5-15 nm fine nanocrystalline regions, and coherent interfaces between the resulting nanocrystalline regions. Measurements of the thermopower, electrical conductivity, and thermal conductivity have been performed over a range of temperature of 300-400 K. We found that MS technique can give us considerable control over the resulting nanostructure with good thermal stability during the temperature range of 300-400 K and this unique structure can effectively adjust the transport of phonons and electrons, in a manner such that it is beneficial to the overall thermoelectric performance of the material, primarily a reduction in the lattice thermal conductivity. Subsequently, this results in a maximum figure of merit ZT value of 1.56 at 300 K for p-type Bi{sub 0.52}Sb{sub 1.48}Te{sub 3} bulk material. This ZT value is over a 50% improvement of that of the state of the art commercial Bi{sub 2}Te{sub 3} materials. We also report results of thermal cycling of this material for over one hundred cycles between 300-400 K. Our work offers an innovative route for developing high performance bismuth telluride based alloys and devices, which have even broader prospects for commercial applications. This technique may also be applicable to other thermoelectric materials.
On the solid-state-bonding mechanism in friction stir welding
This study is a critical assessment of various solid-state-bonding mechanisms is established for friction stir welding (FSW) processes of engineering alloys. The commonly assumed sintering-like diffusional-bonding hypothesis is criticized in this work as not the dominant mechanism. For the wide spectrum of material constitutive laws and FSW processing conditions examined and employed in realistic applications, the thermomechanical history on the workpiece–workpiece interface traverses in the creep-dominated regime for the growth/shrinkage of interfacial cavities. The evolution of the bonding fraction relies mainly on the creep strain rate in the adjourning workpieces, weakly on stress triaxiality, and negligibly on interfacial diffusion.
The Triple Component Interface of Ni–Co–Ce: Growth, Chemical State, and Stability of NiCo Bimetallic Particles on Reducible CeO 2 (111) Thin Films
The growth of NiCo particles at low coverages over reducible CeO 2 (111) thin films producing a triple interface between Ni-Co-Ce was investigated by scanning tunneling microscopy (STM) and X-ray photoelectron spectroscopy (XPS), which was compared to that of monometallic Ni and Co particles. XPS data show that deposition of either Ni or Co on CeO 2 at 300 K causes a partial reduction of Ce 4+ cations to Ce 3+ ions. At 0.3 monolayer (ML), XPS detects Co 2+ on CeO 2 . However, both Ni 0 and Ni 2+ are present as major species at 300 K and annealing causes a significant increase of Ni 2+ in Ni particles. Deposition of 0.3 ML Co over 0.3 ML Ni on CeO 2 at 300 K induces reduction of Ni 2+ to metallic Ni and Ni 0 was found as predominant species. Unlike for Co/CeO 2 , metallic Co was also present over the Co-Ni/CeO 2 surface in addition to Co 2+ . Further, this behavior indicates the formation of NiCo bimetallic particles with the possibility of Co diffusion to the interface of Ni/ceria. With heating, the intermixing of Ni and Co atoms in bimetallic particles on CeO 2 was facilitated. Furthermore, oxidation of both metals and ceria occurred as a result of the diffusion of lattice oxygen from the bulk of ceria to the surface. A slight increase in Ni 2+ was observed after heating Co-Ni/CeO 2 to 500 K or higher. Co became Co 2+ with heating to 800 K. Our STM results confirm the formation of NiCo bimetallic particles on CeO 2 at 300 K and further suggest that the addition of Co can help inhibit the sintering of Ni particles at higher temperatures. Bimetallic particles were also obtained by depositing Ni over existing Co particles on CeO 2 . However, our XPS data demonstrate that the deposition order of Co and Ni plays a role in the chemical state of these two metals in bimetallic particles, likely attributed to the difference in their compositions at the bimetallic particle surface as well as the metal-support interface.
Fast and Scalable Synthesis of LiNi 0.5 Mn 1.5 O 4 Cathode by Sol–Gel-Assisted Microwave Sintering
High-voltage spinel LiNi 0.5 Mn 1.5 O 4 (LNMO) is a promising cathode material for high-energy-density and high-power-density lithium-ion batteries (LIBs). The high cost of the currently available LIBs needs to be addressed urgently for wide application in the transport sector (electric vehicles, buses) and large-scale energy storage systems (ESS). Of significance, herein, novel fast and scalable microwave-assisted synthesis of LNMO is reported, which leads to a production cost cut. X-ray diffraction (XRD) analysis confirms the formation of the desired phase with high crystallinity. Field emission scanning (FE-SEM) and transmission electron microscopy (TEM) analyses indicate that the synthesized phase is of nanometric size (50–150 nm) due to an extremely short sintering time (20 min). The material synthesized at 750 °C shows a higher initial discharge capacity (130 mA h g -1 ) than that synthesized at 650 °C (115 mA h g -1 ). The materials heat treated at higher temperatures show better electrochemical performance in terms of initial capacity, rate capability, and improved cycling. The improved electrochemical performance of LNMO at 750 °C is attributed to the formation of a stable crystal structure, low charge transfer resistance at the electrode/electrolyte interface, high electrical conductivity due to the presence of a disorder structure, and improved ionic diffusivity.
Development of nanosized lanthanum strontium aluminum manganite as electrodes for potentiometric oxygen sensor
Nanocrystalline La 0.8 Sr 0.2 Al 0.9 Mn 0.1 O 3 (LSAM) was synthesized by a microwave-assisted citrate method, and characterized by electron microscopy and X-ray diffraction. Electrical behavior of LSAM was investigated by impedance spectroscopy and activation energy of conduction was obtained. Joining of sintered bodies of LSAM and yttria-stabilized tetragonal zirconia polycrystals (YTZP), an extensively studied oxygen ion conducting electrolyte, was examined by isostatic hot pressing methods. Characteristics of the joining region were evaluated with microprobe Raman spectroscopy, and products formed at the interface, primarily strontium zirconate, was confirmed by examination of high temperature chemical reaction between LSAM and YTZP powders. Finally, the electrical properties of the LSAM were exploited for development of a high temperature oxygen sensor in which LSAM functioned as the electrode and YTZP as electrolyte.
Joining of dissimilar materials
A method of joining dissimilar materials having different ductility, involves two principal steps: Decoration of the more ductile material's surface with particles of a less ductile material to produce a composite; and, sinter-bonding the composite produced to a joining member of a less ductile material. The joining method is suitable for joining dissimilar materials that are chemically inert towards each other (e.g., metal and ceramic), while resulting in a strong bond with a sharp interface between the two materials. The joining materials may differ greatly in form or particle size. The method is applicable to various types of materials including ceramic, metal, glass, glass-ceramic, polymer, cermet, semiconductor, etc., and the materials can be in various geometrical forms, such as powders, fibers, or bulk bodies (foil, wire, plate, etc.). Composites and devices with a decorated/sintered interface are also provided.
An ultrastable heterostructured oxide catalyst based on high-entropy materials: A new strategy toward catalyst stabilization via synergistic interfacial interaction
Designing high–performance catalysts that can stabilize catalytic active sites against sintering to deactivation at temperature higher than 900°C is significant but challenging. In this work, we report a new strategy to obtain a transition metal oxide catalyst with high temperature stability for CO oxidation. This is achieved through a synergistic interfacial interaction at the interface of a heterostructure between high– entropy oxides (HEO, high temperature stability) and CuCeO x (catalytic site). The catalytic site (CuCeO x ) for CO oxidation is realized by dissolving an amount of Cu species in HEO into CeO 2 via an entropy–driven mechanochemical process. In situ XRD and HAADF–STEM have confirmed the high temperature stability of the heterostructure CuCeO x –HEO, which can remain its CO oxidation catalytic activity at elevated temperatures. It should be expected that this innovative will offer the potential to the synthesis of catalysts with high temperature stability in industry.
Locally developed electronic conduction in a yttria stabilized zirconia (YSZ) electrolyte for durable solid oxide fuel cells
In the present work, anode supported solid oxide fuel cells (SOFCs) based on a YSZ single layer electrolyte with locally developed electronic conduction near the anode side is fabricated to improve the cell durability under negative voltage conditions. A ceria added Ni/YSZ anode functional layer is utilized and co-sintered with the YSZ electrolyte at 1460 °C. Cerium ions are diffused into a limited region of the YSZ layer (~6 μm), establishing a ceria doped YSZ region. We successfully demonstrate that this YSZ single layer cell can operate stably for ~100 h without anode/electrolyte interface delamination, even under a negative voltage. The embedded probe technique and theoretical calculation reveal that the internal oxygen partial pressure (near the anode) is substantially reduced (stabilized) by means of local electronic conduction of ceria doped YSZ. Thus, we propose an SOFC electrolyte design comprising a YSZ single layer with a ceria added anode functional layer (locally formed ceria doped YSZ in the electrolyte) as a protection method against fuel cell stack degradation caused by negative voltage operation.
Different Radiation Tolerances of Ultrafine-Grained Zirconia–Magnesia Composite Ceramics with Different Grain Sizes
Developing high-radiation-tolerant inert matrix fuel (IMF) with a long lifetime is important for advanced fission nuclear systems. In this work, we combined zirconia (ZrO 2 ) with magnesia (M g O) to form ultrafine-grained ZrO 2 –M g O composite ceramics. On the one hand, the formation of phase interfaces can stabilize the structure of ZrO 2 as well as inhibiting excessive coarsening of grains. On the other hand, the grain refinement of the composite ceramics can increase the defect sinks. Two kinds of composite ceramics with different grain sizes were prepared by spark plasma sintering (SPS), and their radiation damage behaviors were evaluated by helium (He) and xenon (Xe) ion irradiation. It was found that these dual-phase composite ceramics had better radiation tolerance than the pure yttria-stabilized ZrO 2 (YSZ) and M g O. Regarding He+ ion irradiation with low displacement damage, the ZrO 2 –M g composite ceramic with smaller grain size had a better ability to manage He bubbles than the composite ceramic with larger grain size. However, the ZrO 2 –M g composite ceramic with a larger grain size could withstand higher displacement damage in the phase transformation under heavy ion irradiation. Therefore, the balance in managing He bubbles and phase stability should be considered in choosing suitable grain sizes.
Identifying higher oxygenate synthesis sites in Cu catalysts promoted and stabilized by atomic layer deposited Fe 2 O 3
The conversion of syngas to higher oxygenates is an important step in the pathway towards the long-term sustainable production of fuels and chemicals. Mixed Cu/Fe catalysts combine metals with different CO activation characteristics, a property that makes them promising candidates for higher oxygenate production. However, Cu/Fe catalysts suffer from instability due to sintering and phase separation, and the active sites for higher oxygenate formation on these materials are not well understood. In this work, we use atomic layer deposition (ALD) to modify silica-supported Cu nanoparticles with monolayer precise amounts of Fe 2 O 3 and study the effects on catalyst structure, reactivity, and stability. We demonstrate that the Fe 2 O 3 ALD process is inherently selective towards deposition on the SiO 2 surface versus the Cu nanoparticles. As a result, a sufficiently thick Fe 2 O 3 layer surrounding the Cu nanoparticles acts as a barrier against Cu migration, preventing catalyst deactivation through sintering without covering the Cu. In syngas conversion reactions, we find that higher oxygenate selectivity increases with Fe 2 O 3 loading at low and intermediate ALD cycle numbers. Furthermore, using in situ X-ray absorption spectroscopy, we demonstrate that the Fe near the Cu nanoparticles is reduced to a metallic state under reaction conditions. From these measurements, we identify these metallic Cu/Fe interfaces as the active sites for higher oxygenate formation, which are most abundant at intermediate Fe 2 O 3 ALD cycle numbers. As the Fe 2 O 3 loading increases, higher oxygenate selectivity falls, resulting from encapsulation of the Cu nanoparticles by thick Fe 2 O 3 layers. Overall, the results demonstrate how thickness-controlled ALD Fe 2 O 3 can be used as both a promoter and stabilizer of Cu-based higher oxygenate synthesis catalysts.
Enhanced Thermal Stability and Magnetic Properties in NaCl-Type FePt-MnO Binary Nanocrystal Superlattices
We report the growth of NaCl-type binary nanocrystal (NC) superlattice membranes by coassembly of FePt and MnO NCs at the liquid-air interface. The constituent FePt NCs were converted into the hard magnetic L1(0) phase by thermal annealing at 650 degrees C without degradation of the long-range NC ordering. In contrast, both FePt-only NC superlattices and FePt-MnO disordered NC mixtures showed substantial FePt sintering under the same annealing conditions. Our results demonstrate that the incorporation of FePt NCs into binary superlattices can solve the problems of FePt sintering during conversion to the L1(0) phase, opening a new route to the fabrication of ordered ferromagnetic NC arrays on a desired substrate for high-density data storage applications.