Search NASA⌕ Search

SEARCH · Search NASA

Results for “batch crystallization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

148 records · Page 9

FRIT DEVELOPMENT FOR HIGH LEVEL WASTE SLUDGE BATCH 5: COMPOSITIONAL TRENDS FOR VARYING ALUMINUM CONCENTRATIONS

The objective of this study was to experimentally measure the properties and performance of a series of glasses with compositions that could represent Sludge Batch 5 (SB5) as processed at the Defense Waste Processing Facility (DWPF). The data was used to provide recommendations to the Liquid Waste Organization (LWO) regarding blending and washing strategies in preparing SB5 based on acceptability of the glass compositions. These data were also used to guide frit optimization efforts as the SB5 composition was finalized. Glass compositions for this study were developed by combining a series of SB5 composition projections with a group of frits. Three composition projections for SB5 were developed using a model-based approach at Savannah River National Laboratory (SRNL). These compositions, referred to as SB5 Cases B, C and D, projected removal of 25, 50 and 75% (respectively) of the aluminum in Tank 51 through the low temperature aluminum dissolution process. The frits for this study (Frits 530 through 537) were selected based on their predicted operating windows (i.e., ranges of waste loadings over which the predicted properties of the glasses were acceptable) and their potential (based on historical trends) to provide acceptable melt rates for SB5. Six additional glasses were designed to evaluate alternatives for uranium in DWPF-type glasses used for variability studies and some scoping studies. Since special measures are necessary when working with uranium-containing glasses in the laboratory, it is desirable as a cost and time saving measure to find an alternative for uranium to support frit optimization efforts. Hafnium and neodymium were investigated as potential surrogates for uranium, and other glasses were made by simply excluding the radioactive components and renormalizing the glass composition. The study glasses were fabricated and characterized at SRNL. Chemical composition analyses suggested only minor difficulties in meeting the targeted compositions for some of the oxides for some of the glasses. Although minor differences were observed, they did not have a significant impact on the conclusions made in this study. Several of the study compositions showed retention of more than 0.5 wt% SO{sub 4}{sup 2-} in glass. Trevorite (a spinel) was the only crystalline phase that was positively identified in a few of the study glasses after the canister centerline cooled (CCC) heat treatment. Spinels are not of concern as they have been shown to have little impact on the durability of high level waste glasses. The crystallization behavior of the surrogate glasses was generally the same as that of their U{sub 3}O{sub 8}-containing counterparts. There are two pairs that were exceptions: SB5-04 (amorphous) and SB5-24 (possible trevorite), along with SB5-07 (amorphous) and SB5-25 (trevorite). In these cases, the surrogate glasses (SB5-24 and SB5-25) appear to be more conservative (more prone to crystallization) than their U{sub 3}O{sub 8}-containing counterparts. Chemical durability was quantified using the Product Consistency Test (PCT). The normalized leachate (NL) values for B, Li, Na and Si for all of the study glasses were well below those of the Environmental Assessment (EA) benchmark glass, regardless of heat treatment or compositional view. This indicates that all of the glasses had very acceptable durability performance. The highest NL [B] for the study glasses was 0.914 g/L (the quenched version of glass SB5-13), normalized using the measured, bias-correct composition. There was little practical impact of the CCC heat treatment on the PCT responses of the study glasses. The measured PCT responses were predictable by the current {Delta}G{sub p} models. In general, the PCT responses for the surrogate glasses or the glasses without U{sub 3}O{sub 8} were quite similar to their U{sub 3}O{sub 8}-containing counterparts. The average percent error in NL [B] normalized by the measured, bias-corrected compositions for the surrogate glasses compared with their radioactive counterparts was 8.8%. The largest difference in NL [B] was 0.152 g/L. While similarities existed in crystallization behavior and PCT response for both the surrogates and the glasses renormalized without U{sub 3}O{sub 8}, additional data must be collected before the best solution to fabricating test glasses without radioactive components can be identified. Further surrogate studies are currently underway at SRNL. The results of this study indicate that a frit composition can be identified that will provide a processable and durable glass when combined with SB5 at the DWPF. Additional studies are underway to recommend a frit that continues to meet process and performance requirements as well as to provide an enhanced melt rate for improved waste throughput.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Integrated Experimental and Modeling Studies of Mineral Carbonation as a Mechanism for Permanent Carbon Sequestration in Mafic/Ultramafic Rocks

A program of laboratory experiments, modeling and fieldwork was carried out at Yale University, University of Maryland, and University of Hawai‘i, under a DOE Award (DE-FE0004375) to study mineral carbonation as a practical method of geologic carbon sequestration. Mineral carbonation, also called carbon mineralization, is the conversion of (fluid) carbon dioxide into (solid) carbonate minerals in rocks, by way of naturally occurring chemical reactions. Mafic and ultramafic rocks, such as volcanic basalt, are natural candidates for carbonation, because the magnesium and iron silicate minerals in these rocks react with brines of dissolved carbon dioxide to form carbonate minerals. By trapping carbon dioxide (CO 2 ) underground as a constituent of solid rock, carbonation of natural basalt formations would be a secure method of sequestering CO 2 captured at power plants in efforts to mitigate climate change. Geochemical laboratory experiments at Yale, carried out in a batch reactor at 200°C and 150 bar (15 MPa), studied carbonation of the olivine mineral forsterite (Mg 2 SiO 4 ) reacting with CO 2 brines in the form of sodium bicarbonate (NaHCO 3 ) solutions. The main carbonation product in these reactions is the carbonate mineral magnesite (MgCO 3 ). A series of 32 runs varied the reaction time, the reactive surface area of olivine grains and powders, the concentration of the reacting fluid, and the starting ratio of fluid to olivine mass. These experiments were the first to study the rate of olivine carbonation under passive conditions approaching equilibrium. The results show that, in a simple batch reaction, olivine carbonation is fastest during the first 24 hours and then slows significantly and even reverses. A natural measure of the extent of carbonation is a quantity called the carbonation fraction, which compares the amount of carbon removed from solution, during a run, to the maximum amount that could have been removed if the olivine initially present had fully dissolved and the cations released had subsequently precipitated in carbonate minerals. The carbonation fractions observed in batch experiments with olivine grains and powders varied significantly, from less than 0.01 (1%) to more than 0.5 (50%). Over time, the carbonation fractions reached an upper limit after about 24 to 72 hours of reaction, then stayed constant or decreased. The peak Final Scientific/Technical Report DE-FE0004275 | Mineral Carbonation | 4 coincided with the appearance of secondary magnesium-bearing silicate minerals, whose formation competes for magnesium ions in solution and can even promote conditions that dissolve magnesite. The highest carbonation fractions resulted from experiments with low ratios of concentrated solution to olivine, during which amorphous silica spheres or meshes formed, instead of secondary silicate minerals. The highest carbonation fractions appear to result from competing effects. Precipitation of silica layers on olivine reduces the reactive surface area and, thus, the rate of olivine dissolution (which ultimately limits the carbonation rate), but these same silica layers can also inhibit the formation of secondary silicate minerals that consume magnesite formed in earlier stages of carbonation. Simulation of these experiments with simple geochemical models using the software program EQ3/6 reproduces the general trends observed—especially the results for the carbonation fraction in short-run experiments. Although further experimentation and better models are needed, this study nevertheless provides a framework for understanding the optimal conditions for sequestering carbon dioxide by reacting CO 2 -bearing fluids with rocks containing olivine minerals. A series of experiments at the Rock Physics Laboratory at the University of Maryland studied the carbonation process during deformation of thermally cracked olivine-rich rock samples (dunite) saturated with CO 2 brines of varying compositions. A goal of these geomechanical experiments was to see if flow and deformation processes, which accompany natural carbonation reactions in underground settings, work to enhance or inhibit the reactions. The experiments involved hydrostatic compaction, followed by deformation at a constant rate of strain. Sample permeability was monitored during the reactions. Comparison of the samples’ volume changes to their axial strains (shortening) during deformation indicates that samples reacted with CO 2 -saturated brines accommodate more axial compaction, before the onset of dilation (a swelling that precedes rock failure), than samples reacted with distilled water. Analyses of the reacted samples with scanning electron microscope (SEM) images indicate, first, that dissolution of olivine occurring in the initial stages of carbonation can provide pathways to fluid flow that sustain the reaction, and, second, that carbonate minerals precipitated along existing fractures in the rocks may serve as asperities, or roughness on a crack’s surface that restricts its closure. Final Scientific/Technical Report DE-FE0004275 | Mineral Carbonation | 5 In a related study undertaken by one of the principal investigators as a spin-off of the main project, a simple model of (magnesite) crystal growth in the pore space of basalts undergoing carbonation was developed. The model suggests that, under a carefully controlled program of CO 2 injection, carbonate mineral growth can harden the rock formation against earthquakes that might otherwise be induced by the injection of large fluid volumes (Yarushina and Bercovici, 2013). The overall conclusion of the research project is that mineral carbonation of underground mafic and ultramafic rock formations is a viable candidate for long-term sequestration of man-made carbon dioxide. No results obtained during the project indicate that the method is inherently intractable in its implementation; moreover, enormous volumes of basalt near Earth’s surface are candidate locations for large-scale injection programs. The geochemical experiments do indicate, however, that there will be significant engineering challenges in maintaining high rates of carbonation, by delaying the onset of chemical conditions that promote formation of secondary silicate minerals and, therefore, slow down, or even reverse, the carbonation process. It remains an open question as to whether carbonation processes can be sustained for many years in an engineered system operating on a large scale—a scale capable of accommodating millions of tons of CO 2 annually. The development of realistic theoretical models that can systematically describe the combined effects of reactive flow, precipitation and geomechanical deformation is a major barrier to further understanding of the practical viability of mineral carbonation as large-scale method of carbon sequestration.

58 GEOSCIENCES↗

INITIAL SLUDGE BATCH 4 TANK 40 DECANT VARIABILITY STUDY WITH FRIT 510

Sludge Batch 4 (SB4) is currently being processed in the Defense Waste Processing Facility (DWPF) using Frit 510. The slurry pumps in Tank 40 are experiencing in-leakage of bearing water, which is causing the sludge slurry feed in Tank 40 to become dilute at a rapid rate. Currently, the DWPF is removing this dilution water by performing caustic boiling during the Sludge Receipt and Adjustment Tank (SRAT) cycle. In order to alleviate prolonged SRAT cycle times that may eventually impact canister production rates, decant scenarios of 100, 150, and 200 kilogallons of supernate were proposed for Tank 40 during the DWPF March outage. Based on the results of the preliminary assessment issued by the Savannah River National Laboratory (SRNL), the Liquid Waste Organization (LWO) issued a Technical Task Request (TTR) for SRNL to (1) perform a more detailed evaluation using updated SB4 compositional information and (2) assess the viability of Frit 510 and determine any potential impacts on the SB4 system. As defined in the TTR, LWO requested that SRNL validate the sludge--only SB4 flowsheet and the coupled operations flowsheet using the 100K gallon decant volume as well as the addition of 3 wt% sodium on a calcined oxide basis. Approximately 12 historical glasses were identified during a search of the ComProTM database that are located within at least one of the five glass regions defined by the proposed SB4 flowsheet options. While these glasses meet the requirements of a variability study there was some concern that the compositional coverage did not adequately bound all cases. Therefore, SRNL recommended that a supplemental experimental variability study be performed to support the various SB4 flowsheet options that may be implemented for future SB4 operations in DWPF. Eighteen glasses were selected based on nominal sludge projections representing the current as well as the proposed flowsheets over a WL interval of interest to DWPF (32-42%). The intent of the experimental portion of the variability study is to demonstrate that the glasses of the Frit 510-modified SB4 compositional region (Cases No.1-5) are both acceptable relative to the Environmental Assessment (EA) reference glass and predictable by the current DWPF process control models for durability. Frit 510 is a viable option for the processing of SB4 after a Tank 40 decant and the addition of products from the Actinide Removal Process (ARP). The addition of ARP did not have any negative impacts on the acceptability and predictability of the variability study glasses. The results of the variability study indicate that all of the study glasses (both quenched and centerline canister cooled (ccc)) have normalized releases for boron that are well below the reference EA glass (16.695 g/L). The durabilities of all of the study glasses are predictable using the current Product Composition Control System (PCCS) durability models with the exception of SB4VAR24ccc (Case No.2 at 41%). PCCS is not applicable to non-homogeneous glasses (i.e. glasses containing crystals such as acmite and nepheline), thus SB4VAR24ccc should not be predictable as it contains nepheline. The presence of nepheline has been confirmed in both SB4VAR13ccc and SB4VAR24ccc by X-ray diffraction (XRD). These two glasses are the first results which indicate that the current nepheline discriminator value of 0.62 is not conservative. The nepheline discriminator was implemented into PCCS for SB4 based on the fact that all of the historical glasses evaluated with nepheline values of 0.62 or greater did not contain nepheline via XRD analysis. Although these two glasses do cause some concern over the use of the 0.62 nepheline value for future DWPF glass systems, the impact to the current SB4 system is of little concern. More specifically, the formation of nepheline was observed in glasses targeting 41 or 42% WL. Current processing of the Frit 510-SB4 system in DWPF has nominally targeted 34% WL. For the SB4 variability study glasses targeting these lower WLs, nepheline formation was not observed and the minimal difference in PCT response between quenched and ccc versions supported its absence.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The Uranium from Seawater Program at the Pacific Northwest National Laboratory: Overview of Marine Testing, Adsorbent Characterization, Adsorbent Durability, Adsorbent Toxicity, and Deployment Studies

The Pacific Northwest National Laboratory’s (PNNL) Marine Science Laboratory (MSL) located along the coast of Washington State is evaluating the performance of uranium adsorption materials being developed for seawater extraction under realistic marine conditions with natural seawater. Two types of exposure systems were employed in this program: flow-through columns for testing of fixed beds of individual fibers and pellets and a recirculating water flume for testing of braided adsorbent material. Testing consists of measurements of the adsorption of uranium and other elements from seawater as a function of time, typically 42 to 56 day exposures, to determine the adsorbent capacity and adsorption rate (kinetics). Analysis of uranium and other trace elements collected by the adsorbents was conducted following strong acid digestion of the adsorbent with 50% aqua regia using either Inductively Coupled Plasma Optical Emission Spectrometry (ICP-OES) or Inductively Coupled Plasma Mass Spectrometer (ICP-MS). The ORNL 38H adsorbent had a 56 day adsorption capacity of 3.30 ± 0.68 g U/ kg adsorbent (normalized to a salinity of 35 psu), a saturation adsorption capacity of 4.89 ± 0.83 g U/kg of adsorbent material (normalized to a salinity of 35 psu) and a half-saturation time of 28 ± 10 days. The AF1 adsorbent material had a 56 day adsorption capacity of 3.9 ± 0.2 g U/kg adsorbent material (normalized to a salinity of 35 psu), a saturation capacity of 5.4 ± 0.2 g U/kg adsorbent material (normalized to a salinity of 35 psu) and a half saturation time of 23 ± 2 days. The ORNL amidoxime-based adsorbent materials are not specific for uranium, but also adsorb other elements from seawater. The major doubly charged cations in seawater (Ca and Mg) account for a majority of the cations adsorbed (61% by mass and 74% by molar percent). For the ORNL AF1 adsorbent material, U is the 4th most abundant element adsorbed by mass and 7th most abundant by molar percentage

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗