At least 163 records · Page 9

Enabling Stable High‐Voltage LiCoO 2 Operation by Using Synergetic Interfacial Modification Strategy

Abstract Structural and interfacial instability of the LiCoO 2 cathode under a voltage exceeding 4.5 V (vs Li/Li + ) severely hinders its practical applications for high‐energy‐density lithium batteries. Herein, a modified electrolyte with nitriles (suberonitrile or 1,3,6‐hexanetricarbonitrile) and fluoroethylene carbonate (FEC) coadditives is demonstrated to form an ultrathin and uniform interface layer on LiCoO 2 cathode under a synergetic effect. As such, LiCoO 2 /Li cells display excellent cyclability at a cutoff voltage of 4.6 V with a capacity retention over 72% after 300 cycles and 60% after 200 cycles at 30 and 55 °C, respectively, even achieving operation at a high current rate (10 C) upon 500 cycles as compared to the controls with fast‐falling capacity to zero. Furthermore, an adsorption‐coordination mechanism between nitriles and cobalt and synergetic effect of coadditives are explored by the alliance of spectroscopic analysis and theoretical calculations. The contributed lone‐pairs on the N 2p orbital of nitriles in coordination lowers the real oxidation state of Co 3+/4+ so that it decreases its catalysis on electrolytes, and the synergy from nitrile‐derived species regulates FEC to form an LiF‐containing electron‐insulated interface layer. This work shares a new insight to nitriles with the synergy of coadditives and paves a way to refine (ultra)high‐voltage LiCoO 2 cathode for high‐energy‐density energy storages.

Yang, Xuerui↗

Cobalt-free and high-rate stable 5V lithium nickel manganese oxide spinel cathodes enabled via surface oxygen vacancies

Spinel LiNi 0.5 Mn 1.5 O 4 offers both the high-rate, low-cost and safety advantages of LiFePO 4 and the high energy density of LiNiₓMnᵧCo₁₋ₓ₋ᵧO₂ and LiNiₓCoᵧAlzO₂ cathodes. However, the large operating voltage of these materials induces electrolyte oxidation, which degrades the interface and drives Mn dissolution. These reactions are further exacerbated at high rates due to temperature rise. In this study, we discover that ammoniacal treatment followed by annealing introduces a high density of oxygen vacancies in the “near-surface region” of LiNi 0.5 Mn 1.5 O 4 particles. These vacancies release electrons changing the oxidation state of Mn and suppressing its tendency to oxidize the electrolyte. Further, these vacancies enhance the electrode’s electronic conductivity (by ∼3-fold) and Li + diffusivity (by ∼2-fold) greatly improving charge transport, especially when operated at high rates. This results in an across-the-board improvement in self-discharge, specific capacity, energy density, rate capability, coulombic efficiency and cycling stability. When cycled at ∼200 mA g −1 , the capacity fade averaged over 3000 cycles for the surface vacancy-enriched material is ∼0.0167% per cycle compared to an order of magnitude higher fade rate for the baseline material. In conclusion, these findings reveal the potential of targeted surface oxygen vacancy doping to develop cobalt-free and high energy density cathodes that tolerate fast charging and deliver improved cycle life.

Cobalt-free cathodes↗

Direct Recycling of Lithium-Ion Battery Cathodes: A Multi-Stage Annealing Process to Recover the Pristine Structure and Performance

Direct recycling is an alternative low-cost process that retains the structure of the lithium-ion battery cathode rather than going through materials dissolution and repurification. While the process shows promise, various steps need to be better understood and studied to identify possible roadblocks, cost intensive steps, and needed variations in protocol that may be necessary based on the feedstock of recycled cathodes available. In this study, we have evaluated the process of thermal relithiation as it applies to end-of-life cathode materials. For recovered end-of-life cathodes, approximately 20% of the useable lithium has been lost due to solid electrolyte interface formation, parasitic reactions, and particle isolation; this lost lithium contributes to higher cell impedance and a gradual shift in electrode potentials. As a first step in the direct recycling process, this lithium needs to be restored not only to recover capacity but also to eliminate surface vacancies and hinder surface reconstruction that may increase impedance and impact performance. Here, we have optimized a coating method followed by a two-stage annealing process that restores a model delithiated NMC333 material to pristine performance. Comparisons to single-stage processes are made, and new characterization tools have been used to better understand the processes.

25 ENERGY STORAGE↗

Pristine Interface between Lithium Lanthanum Zirconate and Lithium Manganese Oxide by Pulsed Laser Deposition

Solid state lithium-ion batteries have garnered increasing interest in recent years due to several potential advantages over liquid-electrolyte based systems. The possibility of integrating the lithium garnet oxide, Li 6.75 La 3 Zr 1.75 Ta 0.25 O 12 (LLZTO), with the high voltage cathode, spinel Li x Mn 2 O 4 (LMO), is evaluated here. Thin film bilayer structures are prepared by pulsed laser deposition on MgO (001) substrates and characterized by x-ray diffraction and transmission electron microscopy. The LLZTO is grown by an alternating layer-by-layer deposition of LLZTO and Li 3 N and subsequently annealed for several hours at 575 °C to promote crystallinity. Growth of crystalline LMO with a pristine interface to LLZTO is achieved by gentle heat treatment (500 °C) to remove surface carbonate from the electrolyte and by cathode growth at a low temperature of 250 °C. Higher temperature depositions (330 – 450 °C) result in reaction between the two materials and the appearance of Li 2 MnO 3 , which may be in part due to the presence of excess lithium in the electrolyte layer. Because fully lithiated LiMn 2 O 4 has a voltage of ≈3.7 V versus Li+/Li, the observation of a well-defined interface, free of impurity phases and with no interdiffusion of elements, indicates LLZTO is stable to at least 3.7 V.

Garnet LLZO↗

Single-Crystalline Ni-Rich LiNi x Mn y Co 1– x – y O 2 Cathode Materials: A Perspective

To drive electrical vehicles for long-range, the energy density of Li-ion batteries must be further enhanced, which requires high-energy cathode materials. Among them, Ni-rich LiNi x Mn y Co 1–x–y O 2 (x > 0.5, NMC) is one of the most promising candidates. However, traditional poly-crystal (PC) NMC materials, whose particles are secondary clusters consisting of many primary crystalline particles, are susceptible to pulverization along the inter grain/particle boundaries, resulting in poor cycle stability. Recently, single crystal (SC)-NMC cathodes are proposed as they are believed to have several merits such as high structural integrity, lower interface with electrolyte, and potentially better energy storage performance. Nevertheless, several queries, such as the merits of SC structure and the mechanism for their structure degradation, are still controversial and required to be addressed. Here, in this study, the synthesis parameters, properties, energy storage as well as safety of SC- and PC-NMC cathodes with various Ni contents are critically reviewed, for clarifying the merits and drawbacks of SC. Furthermore, the study focuses on the recent advances of insight mechanisms and strategies for stabilizing the structure/interface by doping, morphology engineering, surface coating, and composition tailoring. The remaining challenges, safety concerns, and perspectives to enhance the electrochemical performance of SC-NMC cathodes for electric vehicle application are followed.

25 ENERGY STORAGE↗

Unveiling the High-valence Oxygen Degradation Across the Delithiated Cathode Surface

Charge compensation on anionic redox reaction (ARR) has been promising to realize extra capacity beyond transition metal redox in battery cathodes. The practical development of ARR capacity has been hindered by high-valence oxygen instability, particularly at cathode surfaces. However, the direct probe of surface oxygen behavior has been challenging. Here, the electronic states of surface oxygen are investigated by combining mapping of resonant Auger electronic spectroscopy (mRAS) and ambient pressure X-ray photoelectron spectroscopy (APXPS) on a model LiCoO 2 cathode. The mRAS verified that no high-valence oxygen can sustain at cathode surfaces, while APXPS proves that cathode electrolyte interphase (CEI) layer evolves and oxidizes upon oxygen gas contact. In conclusion, this work provides valuable insights into the high-valence oxygen degradation mode across the interface. Oxygen stabilization from surface architecture is proven a prerequisite to the practical development of ARR active cathodes.

25 ENERGY STORAGE↗

Conformal LiF Stabilized Interfaces via Electrochemical Fluorination on High Voltage Spinel Cathodes (≈4.9 V) for Lithium-Ion Batteries

The high voltage LiNi 0.5 Mn 1.5 O 4 (LNMO) spinel is one of the promising cathodes for the lithium-ion batteries due to its high energy densities, good rate performance. However, its high operating potential (≈4.75 V) causes extensive oxidation of conventional carbonate electrolytes, resulting an unstable and thick cathode electrolyte interphase (CEI) layer with a large irreversible capacity and low coulombic efficiency. In this work, we report the formation of thin LiF stabilized interfaces on LNMO via electrochemical fluorination that significantly improves the cycling stability and enhanced the capacity. An electrochemically induced conformal LiF layer acts as a part of a robust CEI by reducing the leakage of electrons and allowing the conduction of Li ions through it. Because of the robust LiF stabilized CEI, LNMO delivers a discharge capacity of ≈148.5 and ≈117.1 mAh g -1 at 0.1 and 1 C rate, respectively. It exhibits excellent cyclability with 80% capacity retention (CR) after 600 cycles in lithium-half cell and ≈90% CR after 200 cycles in full cell with only 0.03% and 0.05% capacity decay per cycle in conventional carbonate electrolytes without additives. Such an excellent electrochemical performance could lead to the potential development of high energy density batteries with high voltage cathodes for grid-based applications.

25 ENERGY STORAGE↗

Elucidating the Link Between Alkali Metal Ions and Reaction-Transport Mechanisms in Cathode Electrodes for Alkali-ion Batteries

Our long-term goal is to improve the reliability of electrode materials and their ability to transport and store various metal ions for electrochemical energy storage applications. The main objective of this work was to investigate the intrinsic relationship between the role of alkali metal ions and electrochemically driven mechanical stability and kinetic properties of battery materials. The overall question was “What is the role of alkali metal ions on the electrochemical and mechanical behavior of cathode electrodes? Our guiding hypothesis was that intercalation of larger alkali metal ions (Na and K) inevitably alters the coupled transport-reaction processes during battery operation in organic electrolytes, leading to more intensive chemo-mechanical instabilities in cathode electrodes, resulting in rapid capacity fade. To validate the hypothesis, we experimentally characterized the reaction-transport processes and governing forces driving the instability of electrode materials in different alkali metal-ion environments. The project had three main tasks. The first one was to investigate intercalation-induced strains and associated stress generation, and their impact on structural deformations in composite cathode electrodes. The second task focused on identifying potential-dependent dynamic changes in the electrode-electrolyte interface in alkali metal ion batteries. The last task was focused on determining how larger alkali metal ions with slower diffusivity affect the transport-mechanics coupling at faster scan rates, compared to smaller ions with faster diffusivity in electrodes. We shortly provided the outcome of each task in the accomplishment section. This project produced 10 peer-reviewed publications (9 research papers and one review manuscript) and supported two Ph.D. students, who graduated from Oklahoma State University.

25 ENERGY STORAGE↗

Enabling High Capacity and Coulombic Efficiency for Li-NCM811 Cells Using a Highly Concentrated Electrolyte

Lithium metal batteries suffer from dendrite formation and the associated safety hazards of thermal runaway reactions. In this study, we report the performances of a highly concentrated electrolyte (HCE) and a dilute LiPF6 electrolyte in lithium metal cells using LiNi 0.8 Co 0.1 Mn0.1O 2 . While the HCE exhibits lower bulk ionic conductivity than the dilute LiPF6 electrolyte, the cell conductivity is higher for the HCE system, indicating higher thermodynamic stability of the electrolyte against the electrodes. Full cell cycling demonstrates higher capacity for the HCE system, which declines as a function of cycle number due to the formation of decomposition products, similar to the dilute LiPF 6 system. The origin of the enhanced performance is the higher stability of the HCE against a Li metal anode as compared to the dilute LiPF 6 electrolyte. Cycling at higher temperatures further enhances the performance of the HCE, which is more thermally stable than the dilute LiPF 6 electrolyte.

25 ENERGY STORAGE↗

Fluorinated High-Voltage Electrolytes To Stabilize Nickel-Rich Lithium Batteries

As state-of-the-art (SOA) lithium-ion (Li-ion) batteries approach their specific energy limit (~250 Wh kg -1 ), layer-structured, nickel-rich (Ni-rich) lithium transition metal oxide-based cathode materials, e. g., LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811), have attracted great interest owing to their practical high specific capacities (>200 mAhg -1 ). Coupled with their high average discharge voltages (~4 V vs Li/Li + ), Ni-rich cathode-based lithium batteries possess a great potential to achieve much higher specific energies (>350 Wh kg -1 at the cell level) than the SOA Li-ion counterparts. In addition, Ni-rich oxides are low-cost battery cathode materials due to their low cobalt contents. However, Ni-rich cathode-based lithium batteries suffer quick capacity degradations upon cycling, particularly at high upper cutoff voltages (e.g., ≥= 4.5 V vs Li/Li + ), due to crystal structure changes of the active cathode materials and parasitic side reactions at the electrolyte/electrode interfaces. In this study, a fluorinated-solvent-based, high-voltage stable electrolyte (HVE), i.e., 1 M Li bis(trifluoromethanesulfonyl)imide (LiTFSI) in fluoroethylene carbonate (FEC), bis(2,2,2-trifluoroethyl) carbonate (FDEC), and methyl (2,2,2-trifluoroethyl) carbonate (FEMC) with Li difluoro(oxalate)borate (LiDFOB) additive, was formulated and evaluated in Li/NMC811 battery cells. Further, to the best of our knowledge, this class of electrolyte has not been investigated for Ni-rich cathode-based lithium batteries. Li/NMC811 cells with HVE exhibited a superior long-term cycle performance stability, maintaining ~80% capacity after ~500 cycles at a high cutoff voltage of 4.5 V (vs Li/Li + ) than a baseline carbonate-solvent-based electrolyte (BE). The superior cycle stability of the Li/NMC811 cells is attributed to the inherently high-voltage stability of HVE, supported by the physical and electrochemical analyses. This conclusion is supported by our density functional theory (DFT) modeling where HVE shows a less tendency of deprotonation/oxidation than BE, leading to the observed cycle stability. The findings in this study are important to help tackle the technical challenges facing Ni-rich cathode-based lithium batteries to realize their high energy density potentials with a long cycle life.

25 ENERGY STORAGE↗

A Review on Solid State Batteries: Life Cycle Perspectives

This report briefly reviews the characteristics of solid-state batteries (SSBs) and the life-cycle analysis (LCA) studies that have been completed for SSBs. Compared with conventional lithium-ion batteries (LIBs), SSBs offer improved safety and potentially higher energy density — both enabled by replacing liquid electrolytes with solid electrolytes and using lithium metal anodes. Several challenges impede the commercialization of SSBs, primarily related to the stability of the interface between the solid electrolyte and the electrodes. Several options are under consideration for SSB electrolyte and cathode chemistries. As a result, the production processes for these components and the corresponding battery packs are still under development and can differ significantly from those used for conventional LIB pack production. A robust comparison of SSBs with LIBs through LCA is important to analyze the environmental benefits and challenges associated with this alternative battery system. While the literature provides only a few LCA studies focused on SSBs, with significant uncertainty in their life-cycle inventories (LCIs), those studies collectively suggest that solid electrolyte manufacturing is the major environmental hotspot, followed by cathode and anode production.

25 ENERGY STORAGE↗

Atomic-scale constituting stable interface for improved LiNi 0.6 Mn 0.2 Co 0.2 O 2 cathodes of lithium-ion batteries

Ascribed to their higher capacity and lower cost compared to conventional LiCoO 2 , the Ni-rich layered LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) is now considered as one promising cathode for lithium-ion batteries (LIBs). However, it still suffers from some evident performance degradation, especially under high cutoff voltages (i.e., >4.3 V versus Li/Li + ). The performance degradation typically is exhibited as capacity fading and voltage drop, mainly originating from an instable interface between the NMC622 and electrolyte as well as the evolution of the NMC structure. To improve the interfacial and structural stability of NMC cathodes, herein we deposited an ultrathin layer of Al 2 O 3 coatings (<5 nm) conformally over NMC622 composite electrodes directly using atomic layer deposition (ALD). It was found that, under different upper cutoff voltages (4.3, 4.5, and 4.7 V), the ALD Al 2 O 3 coatings enable enhanced performance of NMC622 cathodes with better cyclability and higher capacity. Particularly, the beneficial effects of the ALD Al 2 O 3 coatings are more remarkable at higher upper cutoff voltages (4.5 and 4.7 V). Furthermore, the ALD coatings can significantly improve the rate capability of NMC622. To this end, we utilized a suite of characterization tools and performed a series of electrochemical tests to clarify the effects of the ALD Al 2 O 3 coatings. This study revealed that the beneficial effects of the Al 2 O 3 ALD coatings are multiple: (i) serving as an artificial layer of solid electrolyte interphase to mitigate undesirable interfacial reactions; (ii) acting as a physical barrier to inhibit metal dissolution of NMC; and (iii) forming a reinforced networked overcoating to boost the mechanical integrity of NMC cathodes. This study is favorable for designing high-performance NMC cathodes.

25 ENERGY STORAGE↗

Lithium-Ion Battery Life Model with Electrode Cracking and Early-Life Break-in Processes

This paper develops a physically justified reduced-order capacity fade model from accelerated calendar- and cycle-aging data for 32 lithium-ion (Li-ion) graphite/nickel-manganese-cobalt (NMC) cells. The large data set reveals temperature-, charge C-rate-, depth-of-discharge-, and state of charge (SOC)-dependent degradation patterns that would be unobserved in a smaller test matrix. Model structure is informed by incremental capacity analysis that shows loss of lithium inventory and cathode-material loss as the dominant capacity fade mechanisms. The model includes terms attributable to solid-electrolyte interface (SEI) growth, electrode cracking, cycling-driven acceleration of SEI growth, and "break-in" mechanisms that slightly decrease or increase available Li inventory early in life. The study explores what mathematical couplings of these mechanisms best describe calendar aging, cycle aging, and mixed calendar/cycle aging. Various approaches are discussed for extracting relevant stress factors from complex cycling profiles to predict lifetime during real-world battery loads using models trained on constant-current laboratory test results. The complexity of the present human-driven model identification process motivates future work in machine learning to more widely search and statistically discern the optimal model that correctly extrapolates capacity fade based on physical knowledge.

25 ENERGY STORAGE↗

Interface chemistry informs about cathode and anode degradation during fast charging

Here, the aim of this study is to examine the development and makeup of the Solid Electrolyte Interphase (SEI) and Cathode Electrolyte Interphase (CEI) in lithium-ion batteries during rapid charging. Using X-ray photoelectron spectroscopy (XPS) and depth profiling, we investigate the chemical modifications occurring on the electrode surfaces during the initial formation and subsequent fast charge-discharge cycles. Our research shows that the anode's SEI initially comprises a thin layer rich in ketones, which then transforms into a thicker layer dominated by carbonaceous compounds during rapid charging cycles. Following assembly, lithium fluoride (LiF) quickly becomes a key element of the SEI, and its presence continues to grow substantially during the formation cycle, remaining the primary component throughout subsequent cycles. Initially, the cathode forms a thin oxide layer rich in ketones, with no noticeable carbonaceous CEI. The CEI primarily comprises LiF, which experiences an increase during the formation cycle and retains a thin layer of carbon coating after the initial rapid discharge. These findings show how the interphase layers impact the performance and stability of lithium-ion batteries, especially during fast charging for electric vertical take-off and landing (eVTOL) vehicles.

Fast charging↗

Study of Stable Cathodes and Electrolytes for High Specific Density Lithium-Air Battery

Future NASA missions require high specific energy battery technologies, greater than 400 Wh/kg. Current NASA missions are using "state-of-the-art" (SOA) Li-ion batteries (LIB), which consist of a metal oxide cathode, a graphite anode and an organic electrolyte. NASA Glenn Research Center is currently studying the physical and electrochemical properties of the anode-electrolyte interface for ionic liquid based Li-air batteries. The voltage-time profiles for Pyr13FSI and Pyr14TFSI ionic liquids electrolytes studies on symmetric cells show low over-potentials and no dendritic lithium morphology. Cyclic voltammetry measurements indicate that these ionic liquids have a wide electrochemical window. As a continuation of this work, sp2 carbon cathode and these low flammability electrolytes were paired and the physical and electrochemical properties were studied in a Li-air battery system under an oxygen environment.

cathodes↗

Electrolyte Reactivity on the MgV 2 O 4 Cathode Surface

Predictive understanding of the solvation-dependent reactivity and molecular interaction of electrolyte ions and solvent molecules on reactive electrodes has been a major challenge but is essential for addressing instabilities and surface passivation that occur at electrode-electrolyte interface (EEI) of multivalent Mg batteries. In this work, the isolated intrinsic reactivities of prominent chemical species present in magnesium bis(trifluoromethanesulfonimide) (Mg(TFSI) 2 ) in diglyme (G2) electrolytes, including ionic (TFSI - , [Mg(TFSI)] + , [Mg(TFSI):G2] + , [Mg(TFSI):2G2] + ) as well as neutral molecules (G2) on magnesium vanadate cathode (MgV 2 O 4 ) surface has been studied using a combination of first-principles calculations and multimodal analysis of well-defined cathode electrolyte interphase (CEI) layers. Here, our calculations show that non-solvated [Mg(TFSI)] + is the strongest adsorbing species on the MgV 2 O 4 surface compared to all other ions while fully solvated [Mg(TFSI):2G2] + are least favorable to decomposition. The cleavage of C-S bonds in TFSI - to form CF 3 - is predicted to be most desired pathway for all ionic species, which is followed by the cleavage of C-O bonds of G2 to yield CH 3 + or OCH 3 - species. The strong stabilization and electron transfer between ionic electrolyte species and MgV 2 O 4 is found to significantly favor these decomposition reactions on the surface compared to intrinsic gas phase dissociation. Experimentally, we used state-of-the-art ion soft landing to selectively deposit mass-selected TFSI - , [Mg(TFSI):G2] + and [Mg(TFSI):2G2] + on MgV 2 O 4 thin film to form well-defined electrolyte-MgV 2 O 4 interface. Analysis of soft-landed interphase using X-ray photoelectron, X-ray absorption near edge structure, electron energy-loss spectroscopies as well as transmission electron microscopy confirmed the presence of decomposition species (e.g., MgFx, carbonates) formed in the interfacial region and the higher amount of MgFx with [Mg(TFSI):G2] + , which corroborates the theoretical observation. Overall, we established the mechanistic pathway for the electrolyte-induced formation of passivating fluorides on MgV 2 O 4 cathode facilitated by the surface adsorption and charge transfer, which provided essential knowledge for rational design of stable electrolytes for multivalent cathodes.

Cathode-electrolyte interphase formation↗

Detection of a Cobalt-Containing Interphase at the Li 6 PS 5 Cl-NMC111 Interface by In Situ μ XANES and EIS

Sulfide electrolyte all-solid-state lithium batteries (ASLBs) with uncoated Li-Ni x Mn y Co 1–x–y O 2 (NMC) cathodes suffer from a large capacity loss during initial cycling and an increase in cell impedance. Decomposition reactions are known to occur at the Li 6 PS 5 Cl-NMC111 interface due to incompatibility between the two materials. If a stabilizing coating is applied to the NMC, it delivers full capacity during initial charge. However, the loss in capacity during discharge still occurs. The interface was studied by μ XANES and through EIS analysis. A chemically-formed interphase was detected by μ XANES, evident from reduction of Co at an uncoated NMC particle surface. This interphase was produced by decomposition at rest. To study the effect of the interphase on electrochemically active surface area, piecewise in situ EIS was performed and the data was modeled using a transmission line model (TLM). The charge transfer resistance R CT was used to estimate the volume specific active surface area (a act ). The median value for a act was 296 cm –1 , a factor of 7.5 lower than the theoretical value of 2216 cm –1 . This provided evidence of a lower electrochemically active surface area in the ASLB.

36 MATERIALS SCIENCE↗

Non-polar ether-based electrolyte solutions for stable high-voltage non-aqueous lithium metal batteries

The electrochemical instability of ether-based electrolyte solutions hinders their practical applications in high-voltage Li metal batteries. To circumvent this issue, here, we propose a dilution strategy to lose the Li + /solvent interaction and use the dilute non-aqueous electrolyte solution in high-voltage lithium metal batteries. We demonstrate that in a non-polar dipropyl ether (DPE)-based electrolyte solution with lithium bis(fluorosulfonyl) imide salt, the decomposition order of solvated species can be adjusted to promote the Li + /salt-derived anion clusters decomposition over free ether solvent molecules. This selective mechanism favors the formation of a robust cathode electrolyte interphase (CEI) and a solvent-deficient electric double-layer structure at the positive electrode interface. When the DPE-based electrolyte is tested in combination with a Li metal negative electrode (50 μm thick) and a LiNi 0.8 Co 0.1 Mn 0.1 O 2 -based positive electrode (3.3 mAh/cm 2 ) in pouch cell configuration at 25 °C, a specific discharge capacity retention of about 74% after 150 cycles (0.33 and 1 mA/cm 2 charge and discharge, respectively) is obtained.

25 ENERGY STORAGE↗