An inverse method for the calculation of through-thickness fatigue crack closure behavior

An inverse technique was used to calculate through-thickness fatigue crack closure behavior. The through-thickness variation in crack opening stress-intensity factor was calculated by considering the variation in the three-dimensional stress-intensity factor, the variation in crack growth rate along the crack front, and a relationship between the crack growth rate and effective stress-intensity factor range (da/dN-Delta-K(eff)). The three-dimensional stress-intensity factor variation was obtained from an elastic finite element analysis of specific crack-front profiles observed experimentally. The variation in crack growth rate along the crack front was obtained experimentally from comparison of observed crack front changes. The da/dN-Delta-K(eff) relationship was estimated from high stress ratio, constant load amplitude, and fatigue crack growth tests. The through-thickness crack opening stress-intensity factor results agreed with crack opening measurements obtained from fatigue striations, near-tip strain gages, and remote strain and displacement gages.

Dawicke, D. S.↗

Small Crack Growth and Fatigue Life Predictions for High-Strength Aluminium Alloys: Experimental and Fracture Mechanics Analysis - Part 1

The small crack effect was investigated in two high-strength aluminium alloys: 7075-T6 bare and LC9cs clad alloy. Both experimental and analytical investigations were conducted to study crack initiation and growth of small cracks. In the experimental program, fatigue tests, small crack and large crack tests A,ere conducted under constant amplitude and Mini-TWIST spectrum loading conditions. A pronounced small crack effect was observed in both materials, especially for the negative stress ratios. For all loading conditions, most of the fatigue life of the SENT specimens was shown to be crack propagation from initial material defects or from the cladding layer. In the analysis program, three-dimensional finite element and A weight function methods were used to determine stress intensity factors and to develop SIF equations for surface and corner cracks at the notch in the SENT specimens. A plastisity-induced crack-closure model was used to correlate small and large crack data, and to make fatigue life predictions, Predicted crack-growth rates and fatigue lives agreed well with experiments. A total fatigue life prediction method for the aluminum alloys was developed and demonstrated using the crack-closure model.

Wu, X. R.↗

The Significance of Small Cracks in Fatigue Design Concepts as Related to Rotorcraft Metallic Dynamic Components

In this paper the significance of the "small" crack effect as defined in fracture mechanics will be discussed as it relates to life managing rotorcraft dynamic components using the conventional safe-life, the flaw tolerant safe-life, and the damage tolerance design philosophies. These topics will be introduced starting with an explanation of the small-crack theory, then showing how small-crack theory has been used to predict the total fatigue life of fatigue laboratory test coupons with and without flaws, and concluding with how small cracks can affect the crack-growth damage tolerance design philosophy. As stated in this paper the "small" crack effect is defined in fracture mechanics where it has been observed that cracks on the order of 300 microns or less in length will propagate at higher growth rates than long cracks and also will grow at AK values below the long crack AK threshold. The small-crack effect is illustrated herein as resulting from a lack of crack closure and is explained based on continuum mechanics principles using crack-closure concepts in fracture mechanics.

Everett, R. A., Jr.↗

On Generating Fatigue Crack Growth Thresholds

The fatigue crack growth threshold, defining crack growth as either very slow or nonexistent, has been traditionally determined with standardized load reduction methodologies. These experimental procedures can induce load history effects that result in crack closure. This history can affect the crack driving force, i.e. during the unloading process the crack will close first at some point along the wake or blunt at the crack tip, reducing the effective load at the crack tip. One way to reduce the effects of load history is to propagate a crack under constant amplitude loading. As a crack propagates under constant amplitude loading, the stress intensity factor range, Delta K, will increase, as will the crack growth rate. da/dN. A fatigue crack growth threshold test procedure is experimentally validated that does not produce load history effects and can be conducted at a specified stress ratio, R. The authors have chosen to study a ductile aluminum alloy where the plastic deformations generated during testing may be of the magnitude to impact the crack opening.

Forth, Scott C.↗

Simulating Fatigue Crack Growth in Spiral Bevel Pinion

This project investigates computational modeling of fatigue crack growth in spiral bevel gears. Current work is a continuation of the previous efforts made to use the Boundary Element Method (BEM) to simulate tooth-bending fatigue failure in spiral bevel gears. This report summarizes new results predicting crack trajectory and fatigue life for a spiral bevel pinion using the Finite Element Method (FEM). Predicting crack trajectories is important in determining the failure mode of a gear. Cracks propagating through the rim may result in catastrophic failure, whereas the gear may remain intact if one tooth fails and this may allow for early detection of failure. Being able to predict crack trajectories is insightful for the designer. However, predicting growth of three-dimensional arbitrary cracks is complicated due to the difficulty of creating three-dimensional models, the computing power required, and absence of closed- form solutions of the problem. Another focus of this project was performing three-dimensional contact analysis of a spiral bevel gear set incorporating cracks. These analyses were significant in determining the influence of change of tooth flexibility due to crack growth on the magnitude and location of contact loads. This is an important concern since change in contact loads might lead to differences in SIFs and therefore result in alteration of the crack trajectory. Contact analyses performed in this report showed the expected trend of decreasing tooth loads carried by the cracked tooth with increasing crack length. Decrease in tooth loads lead to differences between SIFs extracted from finite element contact analysis and finite element analysis with Hertz contact loads. This effect became more pronounced as the crack grew.

Ural, Ani↗

Application of Self Nulling Eddy Current Probe Technique to the Detection of Fatigue Crack Initiation and Control of Test Procedures

A major part of fracture mechanics is concerned with studying the initiation and propagation of fatigue cracks. This typically requires constant monitoring of crack growth during fatigue cycles and the knowledge of the precise location of the crack tip at any given time. One technique currently available for measuring fatigue crack length is the Potential Drop method. The method, however, may be inaccurate if the direction of crack growth deviates considerably from what was assumed initially or the curvature of the crack becomes significant. Another popular approach is to optically view the crack using a high magnification microscope, but this entails a person constantly monitoring it. The present proposed technique uses an automated scheme, in order to eliminate the need for a person to constantly monitor the experiment. Another technique under development elsewhere is to digitize an optical image of the test specimen surface and then apply a pattern recognition algorithm to locate the crack tip. A previous publication showed that the self nulling eddy current probe successfully tracked a simulated crack in an aluminum sample. This was the impetus to develop an online real time crack monitoring system. An automated system has been developed which includes a two axis scanner mounted on the tensile testing machine, the probe and its instrumentation and a personal computer (PC) to communicate and control all the parameters. The system software controls the testing parameters as well as monitoring the fatigue crack as it propagates. This paper will discuss the experimental setup in detail and demonstrate its capabilities. A three dimensional finite element model is utilized to model the magnetic field distribution due to the probe and how the probe voltage changes as it scans the crack. Experimental data of the probe for different samples under zero load, static load and high cycle fatigue load will be discussed. The final section summarizes the major accomplishments of the present work, the elements of the future R&D needs and the advantages and disadvantages of using this system in the laboratory and field.

Namkung, M.↗

An Application of a New Electromagnetic Sensor to Real-Time Monitoring of Fatigue Crack Growth in Thin Metal Plates

A major part of fracture mechanics is concerned with studying the initiation and propagation of fatigue cracks. This typically requires constant monitoring of crack growth during fatigue cycles which necessitates automation of the whole process. If the rate of crack growth can be determined the experimenter can vary externally controlled parameters such as load level, load cycle frequency and so on. Hence, knowledge of the precise location of the crack tip at any given time is very valuable. One technique currently available for measuring fatigue crack length is the DC potential drop method. The method, however, may be inaccurate if the direction of crack growth deviates considerably from what was assumed initially or the curvature of the crack becomes significant. Another approach is to digitize an optical image of the test specimen surface and then apply a pattern recognition technique to locate the crack tip, but this method is still under development. The present work is an initial study on applying eddy current-type probes to monitoring fatigue crack growth. The performance of two types of electromagnetic probes, a conventional eddy current probe and a newly developed self-nulling probe, was evaluated for the detection characteristics at and near the tips of fatigue cracks. The scan results show that the latter probe provides a very well defined local maximum in its output in the crack tip region suggesting the definite possibility of precisely locating the tip, while the former provides a somewhat ambiguous distribution of the sensor output in the same region. The paper is organized as follows: We start by reviewing the design and performance characteristics of the self-nulling probe and then describe the scan results which demonstrate the basic properties of the self-nulling probe. Next, we provide a brief description of the software developed for tracing a simulated crack and give a brief discussion of the main results of the test. The final section summarizes the major accomplishments of the present work and the elements of the future R&D needs.

Namkung, M.↗

Experimental and Finite Element Modeling of Near-Threshold Fatigue Crack Growth for the K-Decreasing Test Method

The experimental methods to determine near-threshold fatigue crack growth rate data are prescribed in ASTM standard E647. To produce near-threshold data at a constant stress ratio (R), the applied stress-intensity factor (K) is decreased as the crack grows based on a specified K-gradient. Consequently, as the fatigue crack growth rate threshold is approached and the crack tip opening displacement decreases, remote crack wake contact may occur due to the plastically deformed crack wake surfaces and shield the growing crack tip resulting in a reduced crack tip driving force and non-representative crack growth rate data. If such data are used to life a component, the evaluation could yield highly non-conservative predictions. Although this anomalous behavior has been shown to be affected by K-gradient, starting K level, residual stresses, environmental assisted cracking, specimen geometry, and material type, the specifications within the standard to avoid this effect are limited to a maximum fatigue crack growth rate and a suggestion for the K-gradient value. This paper provides parallel experimental and computational simulations for the K-decreasing method for two materials (an aluminum alloy, AA 2024-T3 and a titanium alloy, Ti 6-2-2-2-2) to aid in establishing clear understanding of appropriate testing requirements. These simulations investigate the effect of K-gradient, the maximum value of stress-intensity factor applied, and material type. A material independent term is developed to guide in the selection of appropriate test conditions for most engineering alloys. With the use of such a term, near-threshold fatigue crack growth rate tests can be performed at accelerated rates, near-threshold data can be acquired in days instead of weeks without having to establish testing criteria through trial and error, and these data can be acquired for most engineering materials, even those that are produced in relatively small product forms.

Smith, Stephen W.↗

Dye Penetrant Crack Detectability in External Corners in Presence of Fillet Radius

NASA uses special dye penetrant nondestructive evaluation process to provide reliable detection of very small cracks. Typically the surface crack lengths sizes are 0.030' and 0.050' for special dye penetrant process. Qualification requires demonstration of crack detection on a set of cracks with average crack size smaller than or equal to the qualification crack size. The demonstration is called point estimate demonstration. A set of corner cracks can be used to determine reliably detectable corner crack using the point estimate demonstration method. However, dye penetrant demonstration on surface cracks can be used to assess reliably detectable corner crack sizes by using similarity in the penetrant process. The paper provides similarity analysis approach for determining the reliably detectable corner crack sizes for given a point estimate demonstrated surface crack size.

Koshti, Ajay M.↗

Implementation of J-A Methodology Elastic-Plastic Crack Instability Analysis Capability into the WARP-3D Code

Characterization of the near crack-tip stress/strain fields is the foundation of fracture mechanics. The description of the near tip stress field and the prediction of when fracture occurs is well established for brittle materials that exhibit linear elastic behavior. However, in ductile materials or conditions that violate linear elastic assumptions (Aluminum alloys, Al 2024-T3, Al 2024- T351 etc.), the elastic-plastic crack-tip stress fields are characterized by the Hutchison-Rice-Rosengren (HRR) field. The J-integral is commonly used to characterize amplitude of the HRR field under elastic-plastic conditions. The J-integral has been demonstrated for crack-tip fields that are under high constraint conditions (i.e., small-scale plasticity where the J-dominance is maintained). However, as the external load increases, yielding changes from small- to largescale plasticity and usually a loss of constraint (i.e., reduction in the triaxial stress field along the crack front). The loss of constraint leads to the deviation of the crack-tip stress fields from that given by the HRR field. Hence, the J-dominance will be gradually lost and additional parameter(s) are required to quantify the crack-tip stress fields and predict fracture behavior. The assessment objectives were to: 1) implement a two-parameter (i.e., J-A) fracture criterion into an elastic-plastic three-dimensional (3D) finite element analysis (FEA), 2) validate the implementation by comparison with the A parameter from literature data, 3) conduct material characterization tests to quantify the material behavior and provide fracture data for validation of the J-A fracture criteria, and (4) perform evaluations to establish if the J-A criteria can be used to predict fracture in a ductile metallic material (e.g., aluminum alloys). The A parameter in these criteria is the second parameter in a three-term elastic-plastic asymptotic expansion of the neartip stress behavior. A series of extensive FEAs were performed using WARP3D software package to obtain solutions for the A parameter for different specimen configurations. The methodology needed for the estimation of the A parameter in the asymptotic expansion was developed and implemented using Matlab®. A user material (UMAT) routine was used to model the material stress-strain response using a Ramberg-Osgood power law with a hardening exponent (n) and a material coefficient (alpha). This UMAT routine was successfully implemented in WARP3D software and validated through comparison with the experimental data. Three configurations were extracted from published results: 1) center cracked plate (CCP), 2) single edge-cracked plate (SECP), and 3) double edge-cracked plate (DECP). These configurations and four other configurations (three-hole tension (THT)), three-point bend (3PTB), three-hole compact tension (3PCT), and compact tension (CT)) were analyzed to verify the methodology that was developed and implemented into WARP3D. Solutions of the A parameter were obtained for remote tension loading conditions that started with small-scale yielding and continued into the large-scale plasticity regime. The results indicate that the methodology developed can be used to calculate the elastic-plastic J-A parameters for test specimens with a range of crack geometries, material strain hardening behaviors, and loading conditions. The J-A parameters were implemented as fracture criteria and used to predict the test results. For comparison, other fracture criteria were used to predict the same test results. Major findings include: The A constraint parameter A varies with specimen type and applied load thus accurate determination is crucial in predicting the failure load, and the A parameter is asymptotic as the failure load is approached, making an accurate determination difficult (i.e., small differences in the A parameter can cause large variations in failure load) for materials exhibiting elastic-plastic behavior. The failure predictions from J-A methodology were more accurate than the traditionally used KC and J methods, and have comparable scatter to that observed when using the crack-tip opening angle (CTOA) method. However, the J-A methodology requires considerable effort (expertise level and labor) to implement and to evaluate the A parameter for different specimen types and materials, or to apply this methodology to part-through crack (e.g., 3D problems) structural applications.

Hamm, Kenneth R., Jr.↗

Review of modelling small-crack behavior and fatigue-life predictions for aluminum alloys

The small-crack effect, where small fatigue cracks grow faster and at lower stress-intensity factors than large cracks, has been found to be significant for many materials and loading conditions. In this paper, plasticity effects and crack-closure modelling of small fatigue cracks are reviewed. A crack-closure model with a cyclic-plastic-zone-corrected effective stress-intensity factor range (related to the cyclic J-integral) and microstructural data on crack-initiation sites were used to calculate small-crack growth rates and fatigue lives for unnotched and notched specimens made of two aluminum alloys. The crack-closure transient from the plastic wake was shown to be the dominant cause of the small-crack effect and plasticity effects on the cyclic-plastic-zone-corrected stress-intensity factor range were negligible except at extremely high stress levels. Small-crack growth rates and fatigue lives under both constant-amplitude and spectrum loading from tests and analyses agreed well.

CRACK CLOSURE MODELLING↗

A finite element analysis of fatigue crack closure

Experiments have shown that fatigue cracks close at positive loads during constant-amplitude load cycling. The crack-closure phenomenon is caused by residual plastic deformations remaining in the wake of an advancing crack tip. The present paper is concerned with the application of a two-dimensional, nonlinear, finite-element analysis for predicting crack-closure and crack-opening stresses during cyclic loading. A two-dimensional finite-element computer program, which accounts for both elastic-plastic material behavior and changing boundary conditions associated with crack extension and intermittent contact of the crack surfaces under cyclic loading, has been developed. An efficient technique to account for changing boundary conditions was also incorporated into the nonlinear analysis program. This program was subsequently used to study crack extension and crack closure under constant-amplitude and two-level block loading. The calculated crack-closure and crack-opening stresses were qualitatively consistent with experimental observations.

Newman, J. C., Jr.↗

Application of the line-spring model to a cylindrical shell containing a circumferential or axial part-through crack

An approximate solution was obtained for a cylindrical shell containing a part-through surface crack. It was assumed that the shell contains a circumferential or axial semi-elliptic internal or external surface crack and was subjected to a uniform membrane loading or a uniform bending moment away from the crack region. A Reissner type theory was used to account for the effects of the transverse shear deformations. The stress intensity factor at the deepest penetration point of the crack was tabulated for bending and membrane loading by varying three dimensionless length parameters of the problem formed from the shell radius, the shell thickness, the crack length, and the crack depth. The upper bounds of the stress intensity factors are provided by the results of the elasticity solution obtained from the axisymmetric crack problem for the circumferential crack, and that found from the plane strain problem for a circular ring having a radial crack for the axial crack. The line-spring model gives the expected results in comparison with the elasticity solutions. Results also compare well with the existing finite element solution of the pressurized cylinder containing an internal semi-elliptic surface crack.

Delale, F.↗

On the use of marker loads and replicas for measuring growth rates for small cracks

The initiation and growth of small cracks (5-500 microns) from edge notches in 2024-T3 aluminum alloy sheets were studied under constant-amplitude loading. Two methods were used to measure crack shape and size. In the first method, striation marker bands were periodically formed along the crack front by interrupting the constant-amplitude loading by either an elevated R-ratio load sequence, or by an overload sequence. In each case the marker loading was selected so as to have minimal influence on the growth rate under the primary loading. In the second method, the surface crack length was monitored by taking surface replicas at regular intervals. The marker band techniques did not provide reliable crack length and crack shape information for cracks smaller than 2 mm. The replica technique provided accurate information for surface crack length at all crack lengths, and fracture tests on specimens with small cracks provided crack-shape information.

Swain, M. H.↗

Short-crack growth behaviour in an aluminum alloy: An AGARD cooperative test program

An AGARD Cooperative Test Program on the growth of short fatigue cracks was conducted to define the significance of the short-crack effect, to compare test results from various laboratories, and to evaluate an existing analytical crack-growth prediction model. The initiation and growth of short fatigue cracks (5 micrometer to 2 mm) from the surface of a semi-circular notch in 2024-T3 aluminum alloy sheet material were monitored under various load histories. The cracks initiated from inclusion particle clusters or voids on the notch surface and generally grew as surface cracks. Tests were conducted under several constant-amplitude (stress ratios of -2, -1, 0, and 0.5) and spectrum (FALSTAFF and Gaussian) loading conditions at 3 stress levels each. Short crack growth was recorded using a plastic-replica technique. Over 250 edge-notched specimens were fatigue tested and nearly 950 cracks monitored by 12 participants from 9 countries. Long crack-growth rate data for cracks greater than 2 mm in length were obtained over a wide range in rates (10 to the -8 to 10 to the -1 mm/cycle) for all constant-amplitude loading conditions. Long crack-growth rate data for the FALSTAFF and Gaussian load sequences were also obtained.

Newman, J. C., Jr.↗

The surface and through crack problems in layered orthotropic plates

An analytical method is developed for a relatively accurate calculation of Stress Intensity Factors in a laminated orthotropic plate containing a through or part-through crack. The laminated plate is assumed to be under bending or membrane loading and the mode 1 problem is considered. First three transverse shear deformation plate theories (Mindlin's displacement based first-order theory, Reissner's stress-based first-order theory, and a simple-higher order theory due to Reddy) are reviewed and examined for homogeneous, laminated and heterogeneous orthotropic plates. Based on a general linear laminated plate theory, a method by which the stress intensity factors can be obtained in orthotropic laminated and heterogeneous plates with a through crack is developed. Examples are given for both symmetrically and unsymmetrically laminated plates and the effects of various material properties on the stress intensity factors are studied. In order to implement the line-spring model which is used later to study the surface crack problem, the corresponding plane elasticity problem of a two-bonded orthotropic plated containing a crack perpendicular to the interface is also considered. Three different crack profiles: an internal crack, an edge crack, and a crack terminating at the interface are considered. The effect of the different material combinations, geometries, and material orthotropy on the stress intensity factors and on the power of stress singularity for a crack terminating at the interface is fully examined. The Line Spring model of Rice and Levy is used for the part-through crack problem. The surface crack is assumed to lie in one of the two-layered laminated orthotropic plates due to the limitation of the available plane strain results. All problems considered are of the mixed boundary value type and are reduced to Cauchy type of singular integral equations which are then solved numerically.

Erdogan, Fazil↗

Stable tearing behavior of a thin-sheet material with multiple cracks

Fracture tests were conducted on 2.3mm thick, 305mm wide sheets of 2024-T3 aluminum alloy with 1-5 collinear cracks. The cracks were introduced (crack history) into the specimens by three methods: (1) saw cutting; (2) fatigue precracking at a low stress range; and (3) fatigue precracking at a high stress range. For the single crack tests, the initial crack history influenced the stress required for the onset of stable crack growth and the first 10mm of crack growth. The effect on failure stress was about 4 percent or less. For the multiple crack tests, the initial crack history was shown to cause differences of more than 20 percent in the link-up stress and 13 percent in failure stress. An elastic-plastic finite element analysis employing the Crack Tip Opening Angle (CTOA) fracture criterion was used to predict the fracture behavior of the single and multiple crack tests. The numerical predictions were within 7 percent of the observed link-up and failure stress in all the tests.

Dawicke, D. S.↗

Near tip stress and strain fields for short elastic cracks

Recent experimental fatigue crack growth studies have concluded an apparent anomalous behavior of short cracks. To investigate the reasons for this unexpected behavior, the present paper focuses on identifying the crack length circumstances under which the requirements for a single parameter (K(sub I) or delta K(sub I) if cyclic loading is considered) characterization are violated. Furthermore, an additional quantity, the T stress, as introduced by Rice, and the related biaxiality ratio, B, are calculated for several crack lengths and two configurations, the single-edge-cracked and the centrally-cracked specimen. It is postulated that a two-parameter characterization by K and T (or B) is needed for the adequate description of the stress and strain field around a short crack. To further verify the validity of this postulate, the influence of the third term of the Williams series on the stress, strain and displacement fields around the crack tip and in particular on the B parameter is also examined. It is found that the biaxiality ratio would be more negative if the third term effects are included in both geometries. The study is conducted using the finite element method with linearly elastic material and isoparametric elements and axial (mode I) loading. Moreover, it is clearly shown that it is not proper to postulate the crack size limits for 'short crack' behavior as a normalized ratio with the specimen width, a/w; it should instead be stated as an absolute, or normalized with respect to a small characteristic dimension such as the grain size. Finally, implications regarding the prediction of cyclic (fatigue) growth of short cracks are discussed.