Search NASA⌕ Search

SEARCH · Search NASA

Results for “divertor ;fusion materials”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Comparison of divertor behavior and plasma confinement between argon and neon seeding in EAST

The exhaust of excessively high heat and particle fluxes on the divertor target is crucial for EAST long-pulse operation. In the recent EAST experiments, stable partial energy detachment around the upper outer strike point with H 98,y2 ~ 1 was achieved with either Ne or Ar seeding from the upper outer divetor target in the upper single null configuration with ITER-like tungsten divertor. With either Ar or Ne seeding, the electron temperature around the upper outer strike point (T et,UOSP ) was maintained at around 5 eV, the peak temperature of divertor target surface around the upper outer strike point (T div,UO ) decreased significantly, and material sputtering was well suppressed. Here, it was observed that there was less Ar seeding needed for partial energy detachment onset than Ne seeding, which shows that Ar is more efficient in the cooling of T et on the upper outer divertor than Ne. However, there was no detachment on the upper inner divertor with T et around strike point (T et,UISP ) remaining >10 eV with either Ar or Ne seeding from the upper outer divertor. Accompanied with the disappearance of double peak phenomenon of ion flux density on the upper inner divertor target (j s,UI ), the peak T div,UI around the strike point increased to around 300 °C. Although the heat flux on the upper inner divertor target (q t,UI ) is still in the acceptable level, either Ar or Ne seeding only from the upper outer divertor target is not enough to protect the upper inner divertor target from sputtering under current EAST conditions. On the other hand, Ar seeding always causes confinement degradation in the partial energy detachment state. It was observed that there is a slight confinement improvement (~10%) with Ne seeding, which may be due to density peaking, dilution effects and stabilization of the ion temperature gradient mode.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Developing solid-surface plasma facing components for pilot plants and reactors with replenishable wall claddings and continuous surface conditioning. Part A: concepts and questions

Abstract It is estimated that pilot plants and reactors may experience rates of net erosion and deposition of solid plasma facing component (PFC) material of 10 3 –10 5 kg yr −1 . Even if the net erosion (wear) problem can be solved, the redeposition of so much material has the potential for major interference with operation, including disruptions due to so-called ‘unidentified flying objects (UFOs)’ and unsafe dust levels. The potential implications appear to be no less serious than for plasma contact with the divertor target: a dust explosion or a major UFO-disruption could be as damaging for an actively-cooled deuterium-tritium (DT) tokamak as target failure. It will therefore be necessary to manage material deposits to prevent their fouling operation. This situation appears to require a fundamental paradigm shift with regard to meeting the challenge of taming the plasma–material interface: it appears that any acceptable solid PFC material will in effect be flow-through , like liquid–metal PFCs, although at far lower mass flow rates. Solid PFC material will have to be treated as a consumable , like brake pads in cars. ITER will use high-Z (tungsten) armor on the divertor targets and low-Z (beryllium) on the main walls. The ARIES-AT reactor design calls for a similar arrangement, but with SiC cladding on the main walls. Non-metallic low-Z refractory materials such as ceramics (graphite, SiC, etc) used as in situ replenishable, relatively thin—of order mm—claddings on a substrate which is resistant to neutron damage could provide a potential solution for the main walls, while reducing the risk of degrading the confined plasma. Separately, wall conditioning has proven essential for achieving high performance. For DT devices, however, standard methods appear to be unworkable, but recently powder droppers injecting low-Z material ∼continuously into discharges have been quite effective and may be usable in DT devices as well. The resulting massive generation of low-Z debris, however, has the same potential to seriously disrupt operation as noted above. Powder droppers provide a unique opportunity to carry out controlled studies on the management of low-Z slag in all current tokamaks, independent of whether their protection tiles use low-Z or high-Z material.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Lithium splashing from flowing liquid lithium limiter and its effect on high confinement plasma performance in EAST tokamak

To study the potential applications of liquid lithium (Li) as plasma facing material, the third generation of flowing liquid Li (FLiLi) limiter has been designed and successfully tested in EAST tokamak H-mode discharges in the 2018 run campaign. Here, the stability of liquid Li on FLiLi surface, and Li splashing and its effect on the plasma performance are investigated in detail. Li splashing was observed in L-mode and H-mode discharges due to Rayleigh-Taylor (R-T) instability, resulting from electromagnetic forces J → x B → . Li splashing in low-parameter plasma decreased both core and edge electron temperatures, resulting in the degradation of plasma energy confinement and even H-L back transition, however, it almost did not influence plasma confinement performance in high-parameter plasma. These findings indicate that high-parameter plasma has higher tolerance to Li impurities than low-parameter plasma. By contrast, tungsten splashing from the melted layer on the upper divertor was also induced by the R-T instability but generally resulted in plasma disruption, which suggests lower tolerance to tungsten impurities in EAST tokamak.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Ion cyclotron heating at high plasma density in Proto-MPEX

The physics of ion cyclotron heating (ICH) relevant to the steady-state linear machine MPEX (Material Plasma Exposure eXperiment) has been explored in its predecessor, short-pulse device: Proto-MPEX. MPEX will utilize fundamental ICH to increase heat flux at the target and produce ion temperatures and velocity distributions with improved fidelity to those found in a tokamak divertor region, in comparison to those produced by substrate biasing. In the experiments on Proto-MPEX described here, bulk ion temperatures up to ~15 eV have been achieved with 20 kW net ICH power at 6.5 MHz, using ICH heating of a deuterium plasma produced by a helicon plasma source. The heat flux at the target has been observed to increase throughout the plasma cross section, including in the core region. Core $T_i$ and target heat flux are observed to scale linearly with injected ICH power. Further, measurements of plasma loading and target heat flux as a function of the magnetic field strength at the antenna, together with modeling of the wave propagation from the antenna to the ion cyclotron resonance using the ANTENA and COMSOL codes with a warm plasma dielectric tensor, indicate that power is coupled to the core plasma via fast wave excitation of a kinetic Alfvén wave.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Alcator C-Mod: Research in support of ITER and steps beyond

This paper presents an overview of recent highlights from research on Alcator C-Mod. Significant progress has been made across all research areas over the last two years, with particular emphasis on divertor physics and power handling, plasma-material-interaction studies, ELM-suppressed pedestal dynamics, core transport and turbulence, and RF heating and current drive utilizing Ion Cyclotron and Lower Hybrid tools. Specific results of particular relevance to ITER include: inner wall SOL transport studies that have led, together with results from other experiments, to the change of the detailed shape of the inner wall in ITER; runaway electron studies showing that the critical electric field required for runaway generation is much higher than predicted from collisional theory; core tungsten impurity transport studies reveal that tungsten accumulation is naturally avoided in typical C-Mod conditions.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Improving the Fracture Toughness and Ductility of Liquid-Phase Sintered WNiFe Tungsten Heavy Alloys by High-Temperature Annealing

Tungsten heavy alloys (WHAs) are candidates for use in fusion reactor divertors. Here, we characterize liquid-phase sintered WHAs with 90, 92.5, 95, and 97 (wt.%) tungsten (W), with a balance of a 0.7Ni–0.3Fe ductile phase. These WHAs show remarkable room temperature (RT) fracture toughness at the maximum load, K Jm , ranging from ≈ 38 to 107 MPa√m, compared to a monolithic W toughness of ≈ 8 MPa√m. In most cases, the fracture of WHAs occurs through stable crack tearing. However, the 97W WHA has the lowest toughness and fracture elastically in all but the smallest specimens. As lower Ni contents are desirable for fusion application, we explore the potential for improving the ductility and K Jm of WHAs using vacuum annealing at 1300 °C for 24 h. The microstructural observations reveal negligible changes in the WHA microstructure and constituent compositions. While annealing reduces the Vickers microhardness (HV), it does not significantly change the RT yield (σ y ) and ultimate (σ u ) strengths but results in beneficial increases in total elongation in the 95 and 97W WHAs by a factor of 2. RT tests on the precracked three-point-bend (3PB) bars show that annealing increases the K Jm of these WHAs, and in the case of the 97W WHA, the increase is from 42 to 92%, depending on the size of the specimen. Toughening is due to enhanced crack tip process zone microcracking and dilatation.

36 MATERIALS SCIENCE↗

Overview of the COMPASS results *

COMPASS addressed several physical processes that may explain the behaviour of important phenomena. This paper presents results related to the main fields of COMPASS research obtained in the recent two years, including studies of turbulence, L–H transition, plasma material interaction, runaway electron, and disruption physics: Tomographic reconstruction of the edge/SOL turbulence observed by a fast visible camera allowed to visualize turbulent structures without perturbing the plasma. Dependence of the power threshold on the X-point height was studied and related role of radial electric field in the edge/SOL plasma was identified. The effect of high-field-side error fields on the L–H transition was investigated in order to assess the influence of the central solenoid misalignment and the possibility to compensate these error fields by low-field-side coils. Results of fast measurements of electron temperature during ELMs show the ELM peak values at the divertor are around 80% of the initial temperature at the pedestal. Liquid metals were used for the first time as plasma facing material in ELMy H-mode in the tokamak divertor. Good power handling capability was observed for heat fluxes up to 12 MW m –2 and no direct droplet ejection was observed. Partial detachment regime was achieved by impurity seeding in the divertor. The evolution of the heat flux footprint at the outer target was studied. Runaway electrons were studied using new unique systems—impact calorimetry, carbon pellet injection technique, wide variety of magnetic perturbations. Radial feedback control was imposed on the beam. Forces during plasma disruptions were monitored by a number of new diagnostics for vacuum vessel (VV) motion in order to contribute to the scaling laws of sideways disruption forces for ITER. Current flows towards the divertor tiles, incl. possible short-circuiting through PFCs, were investigated during the VDE experiments. The results support ATEC model and improve understanding of disruption loads.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Characterisation of divertor detachment onset in JET-ILW hydrogen, deuterium, tritium and deuterium–tritium low-confinement mode plasmas

Measurements of the ion currents to and plasma conditions at the low-field side (LFS) divertor target plate in low-confinement mode plasmas in the JET ITER-like wall materials configuration show that the core plasma density required to detach the LFS divertor plasma is independent of the hydrogenic species protium, deuterium and tritium, and a 40 %/60 % deuterium–tritium mixture. This observation applies to a divertor plasma configuration with the LFS strike line connected to the horizontal part of the LFS divertor chosen because of its superior diagnostic coverage. The finding is independent of the operational status of the JET cryogenic pump. The electron temperature (T e ) at the LFS strike line was markedly reduced from 25 eV to 5 eV over a narrow range of increasing core plasma density, and observed to be between 2 eV and 3 eV at the onset of detachment. The electron density (n e ) peaks across the LFS plasma when T e at the target plate is 1 eV, and spatially moves to the X-point for higher core densities. The density limit was found approximately 20 % higher in protium than in tritium and deuterium–tritium plasmas.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Exploring the effect of ELM and code-coupling frequencies on plasma and material modeling of dynamic recycling in divertors

Abstract Integrated modeling of plasma-surface interactions provides a comprehensive and self-consistent description of the system, moving the field closer to developing predictive and design capabilities for plasma facing components. One such workflow, including descriptions for the scrape-off-layer plasma, ion-surface interactions and the sub-surface evolution, was previously used to address steady-state scenarios and has recently been extended to incorporate time-dependence and two-way information flow. The new model can address dynamic recycling in transient scenarios, such as the application presented in this paper: the evolution of W samples pre-damaged by helium and exposed to ELMy H-mode plasmas in the DIII-D DiMES. A first set of simulations explored the effect of ELM frequency. This study was discussed in detail in this conference’s proceedings and is summarized here. The 2nd set of simulations, which is the focus of this paper, explores the effect of code-coupling frequency. These simulations include initial SOLPS solutions converged to the inter-ELM state, ion impact energy ( E in ) and angles ( A in ) calculated by hPIC2, and an improved heat transfer description in Xolotl. The model predicts increases in particle fluxes and decreases in heat fluxes by 10%–20% with the coupling time-step. Compared with the first set of simulations, the less shallow impact angle leads to smaller reflection rates and significant D implantation. The higher fraction of implanted flux (and deeper), in particular during ELMs, increases the accumulated D content in the W near-surface region. Future expansion of the workflow includes coupling to hPIC2 and GITR to ensure accurate descriptions of E in and A in , and W impurity transport.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Computational investigation of incident ion angles and material erosion at rough graphite and silicon carbide divertor surfaces

We present a computational investigation of the dependence of material erosion on the incident ion angle at rough graphite and silicon carbide divertor surfaces. Ion angle distributions (IADs) for D plasmas at NSTX-U and DIII-D divertors were calculated by an equation-of-motion model that traces the ion trajectories in the sheath. Then, the effective sputtering yields and ion shadowed area fractions were calculated by a Monte Carlo micro-patterning and roughness code that applied the calculated IADs to surface topographic data that were obtained from optical confocal microscopy of rough graphite and SiC divertor surfaces from NSTX-U and DIII-D experiments. The calculations found that the effective sputtering yields, the sputtering pattern, and the shadowed area are determined by the detailed surface topology rather than the root mean square roughness R RMS , which represents deviations from a flat surface. The suppression of the effective sputtering yields for rough surfaces compared to the yield for a smooth surface was accounted for by the change of the mean local incident ion angle (LIIA) (θ'). The mean surface inclination angle distribution (SIAD) (δ) was found to be a useful parameter to estimate the LIIA from the calculated IADs. We report global empirical formulas for the mean LIIA and fraction of the area shadowed from the main ions for D plasmas for rough surfaces with B-field incident angles α = 85°–89° as a function of the mean SIAD (δ). We propose the use of the mean LIIA (θ') to estimate the sputtering yield for rough surfaces from the angular dependence of the sputtering yield.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Integrated modeling of boron powder injection for real-time plasma-facing component conditioning

An integrated modeling framework for investigating the application of solid boron (B) powder injection for real-time surface conditioning of plasma-facing components (PFCs) in tokamak environments is presented. Utilizing the DIII-D impurity powder dropper (IPD) setup, this study simulates B powder injection scenarios ranging from milligrams to tens of milligrams per second, corresponding to boron flux rates of 10 20 –10 21 B/s in standard L-mode conditions. The comprehensive modeling approach combines EMC3-EIRENE for simulating the deuterium plasma background and the Dust Injection Simulator (DIS) for the ablation and transport of the boron powder particles. EMC3 trace impurity fluid modeling results show substantial boron transport to the inboard lower divertor, predominantly influenced by the main ion plasma flow. The dependency on powder particle size (5-250 µm) was found to be insignificant for the scenario considered. The effects of erosion and redeposition were considered to reconcile the discrepancies with experimental observations, which saw substantial deposition on the outer divertor plasma-facing components. For this purpose, the WallDYN3D code was updated to include boron sources within the plasma domain and integrated into the modeling framework. The mixed-material migration modeling shows evolving boron deposition patterns, suggesting the formation of mixed B-C layers or predominantly B coverage depending on the powder mass flow rate. While the modeling outcomes at lower B injection rates tend to align with DIII-D experimental observations, the prediction of near-pure boron layers at higher rates has yet to be experimentally verified in the carbon environment of the DIII-D tokamak. The extensive reach of boron layers found in the modeling suggests the need for modeling that encompasses the entire wall geometry for more accurate experimental correlations. This integrated approach sets a precedent for analyzing and applying real-time in-situ boron coating techniques in advanced tokamak scenarios, potentially extendable to ITER.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

The effect of ICRH and NBI on tungsten transport in neon edge radiation cooled discharges in TEXTOR

Tungsten is planned to be the plasma-facing material for the main chamber and divertor in future devices like ITER, SPARC, and DTT. To address risks associated with tungsten, R&D is being carried out on various toroidal confinement devices. One particular research question is related to the optimum heating mix for ITER. To investigate the influence of the heating scheme on the release and transport of tungsten, a comparison of neutral beam injection (NBI) and ion cyclotron resonance frequency (ICRF) heating was carried out in TEXTOR tungsten test limiter experiments. The experiments were performed under standard L-mode conditions and in radiative improved-mode operation with neon seeding and boronized walls covering the graphite plasma-facing components. The plasma was heated with hydrogen or deuterium NBI alone or with deuterium NBI in combination with H-minority, ion cyclotron resonance heating. A movable solid tungsten limiter was inserted through a limiter lock system into the edge plasma. The impurity release from this limiter was evaluated from visible spectroscopy. The tungsten concentrations in the plasma core were determined by extreme ultraviolet spectroscopy and bolometry. With deuterium NBI alone, strong central radiation and accumulation of W was observed. This can, however, be avoided by adding ICRF heating.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Investigation of Drift Effects in UEDGE Simulations of NSTX-U Edge Plasma With Lithium Divertors

Lithium is a low-Z material, and lithium-based plasma-facing components (PFCs) are planned for the National Spherical Torus Experiment Upgrade (NSTX-U) to explore potential benefits for divertor power exhaust and core plasma management. NSTX-U is a medium-sized spherical tokamak with up to 12 MW of auxiliary heating, capable of generating reactor-relevant plasma conditions. This work presents boundary plasma simulations for NSTX-U with lithium PFCs using the UEDGE code, incorporating full magnetic and 𝐄 ×𝐁 drift physics. The simulations show that drifts strongly influence heat and particle transport: they enhance convective transport, broaden the scrape-off layer heat-flux width 𝜆 𝑞 , and reduce the anomalous heat diffusivity 𝜒 required to reproduce predicted SOL heat-flux width. 𝐄 ×𝐁 drifts provide poloidal transport, while ∇𝐵 (which includes both gradB and curvature) drifts provide radial heat and particle transport. Lithium transport is also affected by drifts, with lithium ions migrating from the outer divertor to the inner divertor through the private flux region (PFR) following the 𝐄 ×𝐁 drifts flow, lowering upstream impurity lithium densities. UEDGE is self-consistently coupled with the Wall-Li model to study plasma lithium PFC interactions depending on the local lithium sourcing based on local plasma conditions and lithium surface temperature. In these simulations, lithium evaporation shows a vapor-shielding effect that reduces divertor heat flux and increases radiative losses once surface temperatures exceed 450°C. This research work provides a first step toward self-consistent modeling of lithium PFCs in NSTX-U, demonstrating the impact of drift-driven plasma transport in SOL and divertor regions.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Wall conditioning effects of boron powder injection in KSTAR with a tungsten divertor

Boron powder dropped into KSTAR plasmas decreased the radiated power, core electron density, and Z eff , indicating that the ablated and redeposited boron powder helped to condition the plasma-facing surfaces. Visible line emission of oxygen and tungsten were also reduced by 50% (80%) with boron injection into H-mode (L-mode) discharges that used the new KSTAR tungsten monoblock lower divertor. Dynamic particle balance analysis found a negligible difference in the inferred wall pumping rate during the steady portion of the discharges. It is inferred that the observed conditioning effects were principally caused by a reduction in intrinsic impurities as opposed to a reduction in wall recycling. These results are in qualitative agreement with low-Z injected powder experiments across many fusion devices, confirming the utility of low-Z powder injection as a real-time wall conditioning tool.

boron powder injection↗

First lithium experiments in HIDRA and evidence of helium retention during quasi-steady-state stellarator plasma operations

Recent experiments in Hybrid Illinois Device for Research and Applications (HIDRA) have had operational discharges between t discharge = 60 and 1000 s using electron cyclotron resonant heating (ECRH) of the plasma. This means that quasi-steady-state plasma discharges reach conditions to study long-pulse plasma material interactions (PMIs). The newly commissioned HIDRA-Material Analysis Test-stand PMI diagnostic is used to place a drop of lithium onto a heated tungsten surface, transfer the sample in-vacuo and expose it in a helium plasma. Helium is of interest as there is an open question to whether lithium will be able to remove helium ash in real fusion devices. The introduction of the W-Li sample in HIDRA resulted in evaporation of lithium into the helium plasma during a 600 s pulse and caused a reduction of over 90% in neutral pressure during the discharge. It was also observed that the plasma density and temperature increased by over 2.5 times. Using spectroscopy and a helium collisional radiative model, the peak temperature and density of the helium plasma can be monitored during the discharge. During lithium evaporation, as significant lithium ionization occurs, there is a 85% drop in the HIDRA vessel neutral pressure, despite a constant flow rate of He gas. This reduction in neutral pressure is supported by spectroscopy data with corresponding reductions in He I line intensities (587 nm, 667 nm, 706 nm, and 728 nm), as well as those of other impurities. At one point in the discharge a lithium plasma is created, as indicated by an increase in Li + emission and a complete reduction in He + emission, but the electron density jumps from ne = 3 × 10 18 m –3 to over ne = 8 × 10 18 m –3 while the core temperature stays relatively constant between Te = 16 eV and 20 eV. Once lithium has completely evaporated from the sample and the majority of the ionized lithium has diffused from the plasma to the vessel walls, pressure and spectroscopy data paired with He collisional radiative model calculations shows a re-establishment of a helium plasma in a low recycling regime. In this regime, the density drops down to ne = 2 × 10 18 m –3 and the electron temperature increases from T e = 20 eV to over T e = 50 eV indicating an increase in helium heating efficiency. This is also indicated by the He+ emission re-establishing and having a higher intensity. Here, we show the results from the first lithium campaign in HIDRA. In the presence of lithium, and in particular when lithium ions are present, the helium disappears from the plasma via an as of yet unknown complex relationship that needs to be further studied. The most likely explanation is that the lithium ions are distributed around the vessel and able to trap helium to the surface turning HIDRA into a large gettering surface. These results have potential implications on future plasma facing component design using liquid lithium for impurity and recycling control using limiters and divertors.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Innovative laser-based methods for monitoring fuel retention in ITER

This paper addresses the challenge of tritium inventory management in ITER and future fusion reactors, highlighting the importance of accurate tritium measurement and its spatial distribution within the vacuum vessel. Given ITER’s operational constraints, especially the limit on tritium retention, precise measurement is essential for both safety and regulatory compliance. To tackle these questions, the paper presents the T-monitor diagnostic system developed by Forschungszentrum Jülich, which uses Laser-Induced Desorption (LID) in combination with Diagnostic Residual Gas Analysis (DRGA) to measure hydrogen isotope concentrations on the surface of divertor tiles. The system integrates a high-power laser, advanced optical components, and a Fast Scanning Mirror Unit (FSMU) for accurate laser spot positioning with rapid response. Designed to measure in situ tritium retention, the diagnostic provides high-resolution spatial mapping, vital for evaluating detritiation strategies. The laser heating process increases the divertor surface temperature to 1600 K within the laser spot, promoting hydrogen isotope desorption. Accurate measurements require the precise control of laser parameters, including pulse duration and spot size, with a target relative accuracy of 20%. The optical design includes both in-vessel and ex-vessel components, such as durable high-reflectivity mirrors made of gold and copper, selected not only for their infrared performance but also for their transmission of visible wavelengths for observation purposes. To protect optical components from contamination, a pneumatic shutter is used.

Hydrogen isotopes↗

Particle balance of deuterium during deuterium shattered pellet injection shutdown in DIII-D

A particle balance analysis was conducted during a deuterium (D 2 ) shattered pellet injection-induced plasma shutdown on the DIII-D tokamak to determine why less than 20% of the pellet material is assimilated into the core plasma by the mid-current quench (CQ). Initially, most of the D 2 is injected as frozen shards and ionized upon entering the vessel. During the thermal quench, ionized particles move to the divertors and subsequently to the center post (CP) walls, where they rapidly recycle and partially accumulate as neutrals without assimilating into the core plasma. In contrast, the particle flux to the outer midplane walls is negligible, despite being accompanied by hot plasma with electron temperatures exceeding 100 eV. During mid-CQ, volume recombination effects, although not large enough to impact overall particle balance, were significant enough to require accounting for accurate interpretation of fast-framing camera D-alpha signals and the estimation of the CP wall particle flux. In addition, toroidal asymmetries, observed in measurements of toroidal electron density perturbations and the phase of magnetohydrodynamic modes, are present throughout the shutdown and can account for a discrepancy in the assimilation rate for up to 50% of the observed D 2 particle inventory. These sources and sinks of particles and fluxes were identified using absolutely calibrated D-alpha brightness and Langmuir probes.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗