Search NASA⌕ Search

SEARCH · Search NASA

Results for “electrode processing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Characterization of dynamic morphological changes of tin anode electrode during (de)lithiation processes using in operando synchrotron transmission X-ray microscopy

The morphological evolution of tin particles with different sizes during the first lithiation and delithiation processes has been visualized by an in operando synchrotron transmission X-ray microscope (TXM). Here, the in operando lithium ion battery cell was operated at constant current condition during TXM imaging. Two-dimensional projection images with 40 nm resolution showing morphological evolution were obtained and analyzed. The analysis of relative area change shows that the morphology of tin particles with different sizes changed simultaneously. This phenomenon is mainly because of a negative feedback mechanism among tin particles in the battery electrode at a constant current operating condition. For irregular-shaped tin particles, the contour analysis demonstrates that the regions with higher curvature started volume expansion first, and then the entire particle expanded almost homogeneously. This study provides insights for understanding the dynamic morphological change and the particle-particle interactions in high capacity lithium ion battery electrodes.

25 ENERGY STORAGE↗

Ultra-High Temperature Materials Characterization for Space and Missile Applications

Numerous advanced space and missile technologies including propulsion systems require operations at high temperatures. Some very high-temperature materials are being developed to meet these needs, including refractory metal alloys, carbides, borides, and silicides. System design requires data for materials properties at operating temperatures. Materials property data are not available at the desired operating temperatures for many materials of interest. The objective of this work is to provide important physical property data at ultra-high temperatures. The MSFC Electrostatic Levitation (ESL) facility can provide measurements of thermophysical properties which include: creep strength, emissivity, density and thermal expansion. ESL uses electrostatic fields to position samples between electrodes during processing and characterization experiments. Samples float between the electrodes during studies and are free from any contact with a container or test apparatus. This provides a high purity environment for the study of high-temperature, reactive materials. ESL can be used to process a wide variety of materials including metals, alloys, ceramics, glasses and semiconductors. A system for the determination of total hemispherical emissivity is being developed for the MSFC ESL facility by AZ Technology Inc. The instrument has been designed to provide emissivity measurements for samples during ESL experiments over the temperature range 700-3400K. A novel non-contact technique for the determination of high-temperature creep strength has been developed. Data from selected ESL-based characterization studies will be presented. The ESL technique could advance space and missile technologies by advancing the knowledge base and the technology readiness level for ultra-high temperature materials. Applications include non-eroding nozzle materials and lightweight, high-temperature alloys for turbines and structures.

Rogers, Jan↗

Composite Thermal Switch

Lithium primary and lithium ion secondary batteries provide high specific energy and energy density. The use of these batteries also helps to reduce launch weight. Both primary and secondary cells can be packaged as high-rate cells, which can present a threat to crew and equipment in the event of external or internal short circuits. Overheating of the cell interior from high current flows induced by short circuits can result in exothermic reactions in lithium primary cells and fully charged lithium ion secondary cells. Venting of the cell case, ejection of cell components, and fire have been reported in both types of cells, resulting from abuse, cell imperfections, or faulty electronic control design. A switch has been developed that consists of a thin layer of composite material made from nanoscale particles of nickel and Teflon that conducts electrons at room temperature and switches to an insulator at an elevated temperature, thus interrupting current flow to prevent thermal runaway caused by internal short circuits. The material is placed within the cell, as a thin layer incorporated within the anode and/or the cathode, to control excess currents from metal-to-metal or metal-to-carbon shorts that might result from cell crush or a manufacturing defect. The safety of high-rate cells is thus improved, preventing serious injury to personnel and sensitive equipment located near the battery. The use of recently available nanoscale particles of nickel and Teflon permits an improved, homogeneous material with the potential to be fine-tuned to a unique switch temperature, sufficiently below the onset of a catastrophic chemical reaction. The smaller particles also permit the formation of a thinner control film layer (<50 m), which can be incorporated into commercial high-rate lithium primary and secondary cells. The innovation permits incorporation in current lithium and lithium-ion cell designs with a minimal impact on cell weight and volume. The composite thermal switch (CTS(TradeMark)) coating can be incorporated in either the anode or cathode or both. The coating can be applied in a variety of different processes that permits incorporation in the cell and electrode manufacturing processes. The CTS responds quickly and halts current flow in the hottest parts of the cell first. The coating can be applied to metal foil and supplied as a cell component onto which the active electrode materials are coated.

McDonald, Robert↗

Structural phase transformation and Fe valence evolution in FeOxF2-x/C nanocomposite electrodes during lithiation and de-lithiation processes

In this study, the structural changes of FeOxF2-x/C during the first discharge and recharge cycles were studied by ex situ electron microscopy techniques including annular dark field scanning transmission electron microscopy (DF-STEM) imaging, selected area electron diffraction (SAED) and electron energy loss spectroscopy (EELS) as well as by in situ X-ray absorption spectroscopy (XAS). The evolution of the valence state of Fe was determined by combined EELS using the Fe-L edge and XAS using the Fe-K edge. The results of this investigation show that the conversion reaction path during 1st lithiation is very different from the re-conversion path during 1st delithiation. During lithiation, intercalation is first observed followed by conversion into a lithiated rocksalt (Li–Fe–O–F) structure, and metallic Fe and LiF phases. During delithiation, the rocksalt phase does not disappear, but co-exists with an amorphous (rutile type) phase formed initially by the reaction of LiF and Fe. However, a de-intercalation stage is still observed at the end of reconversion similar to a single phase process despite the coexistence of these two (rocksalt and amorphous) phases.

36 MATERIALS SCIENCE↗

Mitigating the Effects of Au-Al Intermetallic Compounds Due to High-Temperature Processing of Surface-Electrode Ion Traps

Stringent physical requirements need to be met for the high-performing surface-electrode ion traps used in quantum computing and timekeeping. In particular, these traps must survive a high-temperature environment for vacuum chamber preparation and support high RF voltage on closely spaced electrodes. Due to the use of gold wire bonds on aluminum pads, intermetallic growth can lead to wire bond failure via breakage or high resistance, limiting the lifetime of a trap assembly to a single multiday bake at 200 ° C. Using traditional thick metal stacks to prevent intermetallic growth, however, can result in trap failure due to RF breakdown events. Through high-temperature experiments, we conclude that an ideal metal stack for ion traps is Ti/Pt/Au (20/100/250 nm), which allows for a cumulative bakeable time of roughly 86 days without compromising the trap voltage performance. This increase in the bakeable lifetime of ion traps will remove the need to discard otherwise functional ion traps when vacuum hardware is upgraded, which will greatly benefit ion trap experiments.

Haltli, Raymond A.↗

Roll-To-Roll Process for Transparent Metal Electrodes in OLED Manufacturing

This program will develop and demonstrate a new manufacturing technology that can help to improve the efficiency and reduce the cost of producing the next generation solid-state lighting (OLEDs)for a broad range of commercial applications. This will not only improve US competitiveness in the manufacturing sector but will also result in a positive impact in meeting the Department of Energy’s goal of developing high efficiency lighting while reducing the environmental impact.

99 GENERAL AND MISCELLANEOUS↗

Semi-Transparent Perovskite Solar Cells in a Stacked Tandem Module: Cooperative Research and Development Final Report, CRADA Number CRD-19-00810

This project seeks to develop device design, materials composition, and processing tools and parameters to fabricate semi-transparent perovskite solar cells and modules for application in stand-alone products or added to other solar cells in a mechanically stacked tandem configuration. This technology presents significant advanced manufacturing challenges and opportunities in getting to scale, including development of perovskite inks, scalable perovskite and heterojunction deposition and annealing processes, heterojunction composition, transparent electrode composition and deposition process, anti-reflection layer composition and deposition process, and cell to module integration processes. Modification 5: The proposed project seeks to develop device design, materials composition, and processing tools and parameters to fabricate semi-transparent perovskite solar cells and modules for application in stand-alone products or added to other solar cells in a mechanically-stacked tandem configuration. This technology presents significant advanced manufacturing challenges and opportunities in getting to scale, including development of perovskite inks, scalable perovskite and heterojunction deposition and annealing processes, heterojunction composition, transparent electrode composition and deposition process, passivation layers including in module scribes, anti-reflection layer composition and deposition process, and cell to module integration processes. Advanced metrology and characterization will be performed on perovskite films, cells and module. Furthermore, we will examine module or materials recycling for circular economy considerations. Modifcation 6: Gigahertz frequency microwave pump-probe spectroscopies are highly sensitive to thin film semiconductor photoconductivity of individual and stacks of layers that comprise perovskite solar cells. As such, these techniques will be used to qualify reproducibility and quality correlations during the manufacturing process. Modification 7: Mechanical adhesion of top contacts within perovskite modules significantly impacts the durability of the module when exposed to accelerated degradation testing. The adhesion between the perovskite/transport layer interface and the transport layer/top contact interface are both very sensitive small changes in processing. ALD processing conditions of the transport layer will be tuned to optimize the mechanical adhesion within the perovskite module stack.

14 SOLAR ENERGY↗

Nickel-hydrogen capacity loss on storage

Nickel-hydrogen batteries are rapidly becoming accepted for use in low-earth-orbit and geosynchronous orbit applications. With their increased use it has become evident that the storage procedures commonly used for nickel-cadmium cells are not adequate for the nickel-hydrogen system. The capacity loss exhibited by nickel electrodes from various manufacturers when exposed to different storage conditions was determined. A comprehensive test matrix was developed to evaluate capacity loss in nickel electrodes from four different manufacturers. Two types of tests were run; individual electrode tests, which involved flooded capacity and impedance measurements before and after storage under varied conditions of temperature, hydrogen pressure, and electrolyte concentration; and cell tests which primarily evaluated the effects of state-of-charge on storage. The cell tests evaluated capacity loss on cells stored open circuit, shorted and trickle charged at C/100 following a full charge. The results indicate that capacity loss varies with the specific electrode manufacturing process, storage temperature and hydrogen pressure. In general, electrodes stored at low temperatures or low hydrogen pressures exhibited a smaller loss in capacity over the twenty-eight day storage period than those stored at high pressure and high temperature. The capacity loss appears to correlate with the level of cobalt in the nickel electrode, with the most significant loss of capacity occurring in electrodes with higher cobalt levels. Impedance measurements appear to correlate well with the capacity loss observed for a given type of electrode but do not correlate well with the capacity loss between electrodes fabricated by different manufacturers. There was a definite correlation between the electrode potential measured immediately following storage and the measured capacity loss.

Manzo, Michelle A.↗

Process for producing nickel electrode having lightweight substrate

A nickel electrode having a lightweight porous nickel substrate is subjected to a formation cycle involving heavy overcharging and under-discharging in a KOH electrolyte having a concentration of 26% to 31%, resulting in electrodes displaying high active material utilization.

Lim, Hong S.↗

Enhanced Cyclability of Lithium-Oxygen Batteries with Electrodes Protected by Surface Films Induced via In Situ Electrochemical Process

Although the rechargeable lithium-oxygen (Li-O2) batteries have extremely high theoretical specific energy, the practical application of these batteries is still limited by the instability of their carbon-based air-electrode, Li metal anode, and electrolytes towards reduced oxygen species. Here we demonstrate a simple one-step in-situ electrochemical pre-charging strategy to generate thin protective films on both carbon nanotubes (CNTs) air-electrode and Li metal anode simultaneously under an inert atmosphere. Li-O2 cells after such pre-treatment demonstrate significantly extended cycle life of 110 and 180 cycles under the capacity-limited protocol of 1000 mAh g-1 and 500 mAh g-1, respectively, which is far more than those without pre-treatment. The thin-films formed from decomposition of electrolyte during in-situ electrochemical pre-charging process in an inert environment can protect both CNTs air-electrode and Li metal anode prior to conventional Li-O2 discharge/charge cycling where reactive reduced oxygen species are formed. This work provides a new approach for protections of carbon-based air-electrode and Li metal anode in practical Li-O2 batteries, and may also be applied to other battery systems.

Environmental Molecular Sciences Laboratory↗

Effect of calendering and temperature on electrolyte wetting in lithium-ion battery electrodes

The formation process during which the liquid electrolyte wets into the porous electrode films usually takes several days or weeks at elevated temperatures, which poses a distinct bottleneck in the manufacturing line of lithium-ion batteries, especially for large-size batteries. However, despite the significance of achieving rapid and complete wetting, reliable scientific investigation on the wettability between the porous electrode and the liquid electrolyte has rarely been reported. In this study, a systematic study of the effect of different manufacturing factors on electrolyte wetting rate is conducted. The effect of calendering degree and wetting temperature on the electrodes obtained through both organic solvent-based processing and water-based processing are studied in detail. The results presented here suggest that although increasing calendering degree increases volumetric energy density, it generally reduces electrolyte wetting rate. While switching anode manufacturing from conventional processing to aqueous processing retards the electrolyte wetting process, switching cathode processing from organic system to aqueous system can drastically influence the pore structure of the cathodes, resulting in irregularly shaped wetted regions. The results also show that while the electrolyte wetting rate of all the tested electrolytes increases with increasing temperature, the change is significant only for the electrolytes with relatively high salt concentrations.

25 ENERGY STORAGE↗

Ultra-High Temperature Materials Characterization for Propulsion Applications

Propulsion system efficiency increases as operating temperatures are increased. Some very high-temperature materials are being developed, including refractory metal alloys, carbides, borides, and silicides. System design requires data for materials properties at operating temperatures. Materials property data are not available for many materials of interest at the desired operating temperatures (up to approx. 3000 K). The objective of this work is to provide important physical property data at ultra-high temperatures. The MSFC Electrostatic levitation (ESL) facility can provide measurements of thermophysical properties which include: creep strength, density and thermal expansion for materials being developed for propulsion applications. The ESL facility uses electrostatic fields to position samples between electrodes during processing and characterization studies. Because the samples float between the electrodes during studies, they are free from any contact with a container or test apparatus. This provides a high purity environment for the study of high-temperature, reactive materials. ESL can be used to process a wide variety of materials including metals, alloys, ceramics, glasses and semiconductors. The MSFC ESL has provided non-contact measurements of properties of materials up to 3400 C. Density and thermal expansion are measured by analyzing digital images of the sample at different temperatures. Our novel, non-contact method for measuring creep uses rapid rotation to deform the sample. Digital images of the deformed samples are analyzed to obtain the creep properties, which match those obtained using ASTM Standard E-139 for Nb at 1985 C. Data from selected ESL-based characterization studies will be presented. The ESL technique could support numerous propulsion technologies by advancing the knowledge base and the technology readiness level for ultra-high temperature materials. Applications include non-eroding nozzle materials and lightweight, high-temperature alloys for turbines and structures.

Rogers, Jan↗

Probing local electrochemistry via mechanical cyclic voltammetry curves

Understanding the mechanical response of an electrode during electrochemical cycling and its correlation to the device electrochemical performance is crucial to improving the performance of insertion-type energy storage devices, electrochemical actuators, water purification, ion separation and neuromorphic computing applications. Here, we visualized the electro-chemo-mechanical coupling behaviors during charge storage of anhydrous and hydrated WO 3 electrodes via in situ atomic force microscopy (AFM) and developed the concept of mechanical cyclic voltammetry (mCV) curves. The relationship between electrochemical current and strain was investigated with simplified models and the results revealed that the proton insertion/deinsertion process could be described through potential-dependent electro-chemo-mechanical coupling coefficients which might indicate changes in insertion processes during electrode cycling. The mCV mapping results highlight the local heterogeneity and show that the charging processes varied across the electrode. These local variations could be further correlated to local morphology, crystal orientations or chemical compositions with proper electrode designs.

36 MATERIALS SCIENCE↗

Characterization of Surface Free Energy of Composite Electrodes for Lithium-Ion Batteries

One critical step in lithium-ion battery manufacturing process is the electrolyte wetting step, which usually takes up to several days at elevated temperatures, posing a distinctive bottleneck in the manufacturing process especially for large-size cells. The electrode wettability depends on both the surface tension of electrolyte and the surface free energy of electrodes. This work reports a systematic study on the characterization of surface free energy of battery electrodes and the correlation between surface free energy and electrode processing. It shows that, when switching manufacturing from conventional solvent based processing to aqueous processing, the polar component of surface free energy increases 74.1% for NMC532 electrodes and 48.2% for A12 graphite electrodes. The results provide valuable guidance for electrode processing to optimize the electrolyte wetting process, helping lower processing costs and enable higher product quality and throughput.

25 ENERGY STORAGE↗

Electrodeposition for Low-Cost, Water-Based Electrode Manufacturing. Research Performance Progress Report, Jan. 1, 2016 - Dec. 31, 2019

The viability of electrocoat to fabricate battery electrodes at commercially relevant formulations has been demonstrated using both bench-scale equipment and a small pilot-scale roll-to-roll system (mini-coater). Through this, we show that an electrodeposited lithium-ion battery electrode coating system and manufacturing process is capable of reducing cell costs. Specifically, >60% decrease in capital costs is expected when transitioning from slot-die to electrocoat-based coating systems due to the removal of a solvent recovery system. In addition, a 50% reduction in operating costs in also expected as we enable 2-coat/2-cure processing of cathode electrodes.

25 ENERGY STORAGE↗

Dry-pressed lithium nickel cobalt manganese oxide (NCM) cathodes enabled by holey graphene host

There is an increasing demand for electric vehicle batteries with higher energy densities that can be manufactured with low cost utilizing environmentally friendly processes. Lithium nickel cobalt manganese oxides (NCM), such as LiNi(0.5)Co(0.2)Mr(0.3)O(2) (NCM523), are commonly used in commercial lithium ion batteries for electric vehicle applications. These cathodes are typically fabricated using environmentally hazardous, energy intensive, and time-consuming solvent-based slurry casting processes. Polymeric binders, also required for cathode preparation, add weight and can undergo parasitic reactions during battery cycling. Here we report a facile, solvent-free, binder-free, and rapid cold-press electrode fabrication process to prepare high mass loading NCM cathodes within minutes. This process is enabled by the use of holey graphene, a unique lightweight, compressible carbon nanomaterial that serves as both a binder and an electrically conductive matrix. NCM cathodes fabricated by this method are stable and exhibit good active material utilization. A significant advantage for the dry-press process is that the electrode mass loadings can be readily increased simply by adding more composite powder to the compression molding die, resulting in improved areal capacities that are attractive for applications requiring high energy per unit footprint. (C) 2020 Elsevier Ltd. All rights reserved.

25 ENERGY STORAGE↗