Evaluating the grain-scale deformation behavior of a single-phase FCC high entropy alloy using synchrotron high energy diffraction microscopy

We report although the deformation behavior of high-entropy alloys (HEAs) has been extensively studied at the macroscale, many important properties have yet to be explored for these alloys at the microscale, thus hampering accurate prediction of damage and failure processes. Synchrotron high-energy diffraction microscopy (HEDM) and fast-Fourier transform-based crystal plasticity modeling was conducted to investigate the three-dimensional (3D) grain-resolved micromechanical response for approximately 1,900 constituent grains within a single-phase FCC HEA up to 1% applied strain. The evolution of grain-resolved elastic strains, lattice reorientations, and maximum resolved shear stresses (mRSS) were evaluated to quantify elastic, yield, and fully plastic behavior. Overall, the initial critical resolved shear stress (CRSS), determined via in situ HEDM and companion modeling, was found to be > 20% higher than estimated using the classical polycrystalline Taylor factor (M = 3.06). However, a descriptive parameter based on the average grain-resolved Taylor factor ($\overline{M}$) was found to show excellent agreement with plastic yielding behavior observed within HEDM datasets. Noticeable deviations in HEDM lattice reorientations compared to both EVP-FFT simulations and classical predictions for FCC polycrystals were discovered, highlighting the complexity in correlating local lattice reorientations, Taylor, and Schmid factors with plastic response for this material at the grain-scale. Therefore, it is anticipated that the overall trends and parameter identification of 3D grain-resolved properties in this study can serve as an important foundation for continued mesoscale investigation on both well-established and newly developed Cantor-like HEAs.

36 MATERIALS SCIENCE↗

Correlating hidden local structural distortion with antiferroelectric-ferroelectric transition in PbZrO 3 -based perovskites

Externally stimulated antiferroelectric-ferroelectric (AFE-FE) transition makes AFE materials attractive for many applications ranging from energy storage to sensing. This transition-mediated macroscopic electrical characteristics have been extensively investigated, yet the underlying structural evolution remains poorly understood. Herein, we study the local- and long-range structural evolutions in the Nb-doped Pb(Zr,Sn,Ti)O 3 perovskites by in-situ X-ray total scattering and diffraction, which show three different types of AFE-FE transitions. The evolution of long-range structure from diffraction and local structure identified by atomic pair distribution function (PDF) are consistent well with the phase transition behavior indicated by macroscopic polarization/strain measurements, while discrepancies exist. Interestingly, frequently employed long-range structure picture that the uniform AFE pseudo-tetragonal to FE rhombohedral transformation is insufficient to understand the distinct composition-dependent AFE-FE transition behaviours. Instead, the reversibility of this transition correlates with the chemically sensitive local atomic displacements revealed by newly developed in-situ PDF. The critical electric field of transition is associated with the local structural differences between the AFE and FE state. The macroscopic electrostrains can be well estimated by the phase transition associated lattice strain and domain alignment from in-situ synchrotron XRD data, while the local strains calculated from in-situ PDFs are found to be much lower. Finally, these results provide a fresh insight into the AFE-FE transition, and advance the understanding of structure-property relationships in AFE materials.

36 MATERIALS SCIENCE↗

Load shuffling during creep deformation of an additively manufactured AlCuMnZr alloy

Here, the high-temperature deformation behavior of an additively manufactured Al-Cu-Mn-Zr alloy is evaluated in the as-fabricated and heat-treated states using traditional ex-situ and in-situ neutron diffraction creep experiments performed at 300 °C. The dominant reinforcement phase in the alloy, θ-Al 2 Cu, despite its high volume fraction of ~10%, does not provide load transfer strengthening during creep deformation. Instead, the lattice strain evolution suggests a new mechanism we term “load shuffling” wherein the initial load is transferred away from precipitate-free zones along the grain boundaries where most of the θ-Al 2 Cu particles are located to precipitate-strengthened grain interiors. Notwithstanding the lack of load transfer strengthening, the as-fabricated AM Al-Cu-Mn-Zr alloy still possesses improved creep resistance at 300 °C relative to a cast alloy with similar composition. The proposed load shuffling mechanism explains the lack of observed L1 2 -Al 3 Zr strengthening at 300 °C and helps identify several strategies for improvement of elevated-temperature mechanical response of AM Al alloys.

36 MATERIALS SCIENCE↗

Structural origin of size effect on piezoelectric performance of Pb(Zr,Ti)O 3

Grain size effect plays a vital role in piezoelectric performance from both scientific and technological view. However, the underlying structural mechanism related to grain size is still unclear. In the present study, the structural mechanism of grain size effect on piezoelectric performance has been revealed in the prototype Pb(Zr, Ti)O 3 system by using in-situ synchrotron X-ray diffraction. The miniaturization of grain size tends to favor the appearance of higher symmetric tetragonal phase, while a single monoclinic phase is determined in the coarse-grained ceramics. The direct structural evidence reveals that both tetragonal and monoclinic phases in the fine-grained ceramics are less sensitive to the electric field, corresponding to the inferior piezoelectric performance, while the single monoclinic phase in the coarse-grained ceramics is more active to be driven by the electric field, generating good piezoelectric behavior. Both domain switching ability and lattice strain are suppressed with decreasing grain size, which directly leads to the deterioration in piezoelectric performance. In conclusion, the current results will benefit the structural understanding of the size effect of piezoelectric and other related systems.

36 MATERIALS SCIENCE↗

Sectoral and growth rate control on elemental uptake by individual calcite crystals

Heterogeneous distribution of trace elements (impurities) within individual calcite crystals is a phenomenon commonly observed in natural and laboratory systems. Changes in thermodynamic intensive parameters (mostly chemical potential and temperature) cannot always explain the inhomogeneous impurity patterns in calcite crystals and it has been suggested that growth rate and crystallographic orientation may exert strong effects on elemental incorporation into calcite. In addition, there are a number of experimental studies on micro-scale element (E) distribution between non-equivalent pairs of calcite vicinal faces (known as sectoral zoning); however, the variability of partition coefficients (e.g., K E = (E/Ca) calcite /(E/Ca) fluid ) within individual crystals remains undetermined. In this study, we have extended the work on elemental distribution between crystal sectors to evaluation of partition coefficients of trace and minor elements (Li, B, Mg, and Sr) in calcite crystal faces (10–14) and (01-12), whose growth rates were assessed. Growth entrapment model (GEM) and lattice strain theory were applied to explain K E heterogeneity by varying near-surface diffusivity of Mg and Sr and by varying surface enrichment factor for Li, B, Mg, and Sr. Decoupling of sectoral and growth rate effects reveals that sectoral zoning plays a key role in elemental distribution. More specifically, K Li and K B vary by more than one order of magnitude and K Mg varies by a factor of two within individual crystal faces. Strontium sectoral distribution is different from those of Li, B, and Mg and K Sr varies by up to a factor of two. Finally, these behaviors likely reflect different mechanisms of incorporation of Li, B, Mg, and Sr into calcite.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

From ammonium Hexahalorhenates(IV) to nanocrystalline rhenium metal: A combined thermal, diffraction and microscopic analysis

Rhenium metal powder is a material of industrial importance. Several industrial and laboratory methods have been developed for the preparation of ultrafine Re metal powder and nanoparticles. The present study provides a better understanding of the characteristic and formation of Re metal powder from the decomposition of (NH4)2ReX6 salt (X = F, Cl, Br, I) at high temperature in inert atmosphere. Such analysis resulted in the formation of nanocrystalline Re metal as characterized by powder XRD. Williamson-Hall, Scherrer, and Williamson-Smallman methods were employed to study the effect of crystallize size, lattice strain, and dislocation density as analyzed from powder XRD peak broadening. Here, the morphology and composition of the metal were analyzed using scanning electron microscopy (SEM) and energy dispersive X-ray (EDX) spectroscopy.

36 MATERIALS SCIENCE↗

Conversion of (NH 4 ) 2 [ReF 6 ] into ReO 2 mixed phases: A thermal analysis study

We report the thermal behavior of (NH 4 ) 2 [ReF 6 ] was evaluated in an alumina crucible using simultaneous thermal gravimetric analysis (TGA) and differential scanning calorimetry (DSC) in an argon atmosphere. The TGA of (NH 4 ) 2 [ReF 6 ] is characterized by a single step decomposition while the DSC exhibits two exothermic peaks. Powder X-ray diffraction (PXRD) analyses of the decomposition products show the presence of a mixed ReO 2 phase. The formation of ReO2 is driven by the reaction of (NH 4 ) 2 [ReF 6 ] with Al 2 O 3 at the grain boundary of the alumina crucible. XRD peak broadenings due to the combined effect of crystallite size and lattice strain were evaluated using both Scherrer and Williamson-Hall methods.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

In situ neutron diffraction study of fatigue behavior of CrFeCoNiMo 0.2 high entropy alloy

In situ neutron diffraction measurement was applied to study the low-cycle fatigue behavior of CrFeCoNiMo 0.2 high entropy alloy. A two-step stress-controlled fatigue test with a stress range of 100–460 and 20–500 MPa was employed. The as-cast sample was cycled 129,000 and 61,000 times, respectively, before fracture. The evolution of the lattice strain and peak intensity demonstrates that the main deformation mechanism is dislocation slip, while no evidence of stacking fault was found. A three-stage ratcheting was clearly observed. Under the stress-controlled mode, the experimentally determined dislocation density increases linearly with the ratcheting strain. Here, the increase of the dislocation density results in a decay of the ratcheting strain rate, which stabilizes the structure and is beneficial for fatigue resistance.

36 MATERIALS SCIENCE↗

Thermophysical properties of high-density, sintered monoliths of yttrium dihydride in the range 373–773 K

Yttrium dihydride is a promising nuclear reactor moderator for high-temperature, thermal micro-reactors due to its ability to retain hydrogen to high temperatures while having a relatively low impact on neutron economy. However, it is difficult to fabricate yttrium dihydride in high-density, near net-shape monoliths for moderator applications due to challenges associated with the hydrogen absorption process. Here, high-density monoliths of yttrium dihydride were prepared by powder metallurgical methods. The lattice strain and thermal expansion coefficient were measured using neutron diffraction of powders of directly-hydrided yttrium, while the molar heat capacity and thermal diffusivity of sintered yttrium dihydride were measured using differential scanning calorimetry (DSC) and laser flash analysis (LFA), respectively. The molar heat capacity of yttrium dihydride was also calculated using density functional theory (DFT) for comparison. These parameters were used to then calculate the thermal conductivity and resistivity of yttrium dihydride as a function of temperature. The thermophysical properties of materials produced by both methods were observed to be consistent with the values from literature for yttrium dihydride. Due to the novelty of producing yttrium dihydride by powder metallurgical methods, this result indicated that the sintered monoliths were of high quality and that powder metallurgy is a viable method for large-scale production of yttrium dihydride monoliths for nuclear reactor moderator applications.

36 MATERIALS SCIENCE↗

Enhanced superelasticity of nanocrystalline NiTi/NiTiNbFe laminar composite

This study explores a new concept of the synergy between two constituent shape memory alloys (SMAs) in a composite to achieve a wide superelastic temperature window. In this work, a nanocrystalline NiTi/NiTiNbFe dual-SMA composite is designed, in which two constituent SMAs are both capable of stress-induced martensitic transformation, but within different temperature ranges. Based on the principle of lattice strain matching between the two SMAs, superelastic martensitic transformation in one induces superelastic transformation in the other at temperatures the latter will not when standing alone. Furthermore, via this synergy the composite is able to achieve an ultra-wide superelastic temperature window of 336°C, from -196 to 140°C, with a ~5% tensile strain recovery and high superelastic stresses in the range of 700~1400 MPa. Such properties appear superior to all NiTi-based shape memory alloys to date.

36 MATERIALS SCIENCE↗

Structural stability of mechanically alloyed amorphous (FeCoNi) 70 Ti 10 B 20 under high-temperature and high-pressure

Nanostructured (FeCoNi) 70 Ti 10 B 20 (at%) alloy was synthesized by mechanical alloying from elemental powder mixture of Fe, Co, Ni, Ti and B using ball milling. The effect of ball milling time on the evolution of structure and morphology was investigated by X-ray diffraction, scanning and transmission electron microscopy and differential thermal analysis. It was observed that the formation of solid solution of (FeCoNi) 70 Ti 10 B 20 started from the very onset of the milling process. Crystallite size and lattice strains seemed to be leveled off after 20 h of milling with no further major changes. The milling process for longer periods introduced severe plastic deformations causing formation of amorphous phase of (FeCoNi) 70 Ti 10 B 20 . The amorphous alloy composition was confirmed by energy dispersive X-ray spectroscopy analysis that showed an excellent homogeneity of the alloying elements. The phase stability of the mechanically alloyed amorphous sample was further verified by employing high-temperature and high-pressure studies. The alloy samples heat-treated at 700 °C revealed crystallization of the amorphous phase. However, synchrotron-based high-pressure ambient temperature X-ray diffraction studies confirmed that the amorphous phase of the alloy remained stable up to the pressure of 30 GPa. Here, the 50 h milled sample after being annealed at 350 °C showed improvement in the soft magnetic properties of the alloy, which was due to the probable elimination of the residual stress in the amorphous phase of the alloy powders.

36 MATERIALS SCIENCE↗

Probing thermodynamics of radiogenic helium and defects in $δ$-plutonium alloys and interactions with adsorbed environmental gases

Differential scanning calorimetry coupled with simultaneous evolved gas analysis (DSC-EGA) on aged δ-Pu samples shows that most radiogenic helium remains trapped within the Pu matrix at temperatures very close to, or slightly above, the melting temperature. Our results indicate that helium release from 50-year-old δ-Pu occurs as a burst just below the melting temperature (>0.994 T m ), with subsequent pressure oscillations as temperature increases. Subordinate quantities of H 2 were also released along with helium. Here, the helium emission tails off and ceases above ~720 – 750°C. In a δ-Pu alloy aged 6 years, the initial helium burst occurs slightly above melting (~1.015 – 1.042 T m ), with a discrete, larger helium spike occurring between 670 and 686°C. The proximity of helium release to the liquidus transition presented challenges in the deconvolution of overlapping process enthalpies, the liquidus endotherm, and the exotherm resulting from bubble collapse, annealing and gas expulsion. Helium’s strong affinity for vacancy binding in a 2He-vac configuration is predicted by Density Functional Theory (DFT) modeling. The measured stored energy associated with the He release events in a 50-year-old δ alloy is on the order of ~ 10–11 J/g, which is significantly higher than stored energies measured in the sub-solidus regimes (~2 J/g) that are related to the solid-state annealing of processing- and radiation-induced defects. This implies that aged δ Pu alloys have a remarkable resilience to accommodate the lattice strain produced by the internal pressure of the helium bubbles and provides further insight into the thermodynamic behavior of aged δ Pu.

36 MATERIALS SCIENCE↗

Unseeded, spontaneous nucleation of spherulitic magnesium calcite

Most of the sedimentary carbonates deposited in the marine environments are composed of calcium carbonate minerals with varying amounts of incorporated Mg 2+ . However, understanding how interactions of impurities with carbonate and their incorporation affect sediments behavior remains a challenge. Here, a new insight is obtained by monitoring solution composition, morphology, and electrokinetic potential of carbonate particles formed in a spontaneous unseeded batch precipitation experiment using electrochemical and scanning electron microscopy methods. The solid composition and growth rate are extracted from changes in the bulk composition and fitted to chemical affinity rate law, revealing that the precipitation pathway consists of second-order dissolution and first-order precipitation. The molecular dynamics simulations show that the lattice strain induced by randomly substituting Ca 2+ by Mg 2+ stabilizes spherical nanoparticles and reduces their surface area and volume. Combining kinetics and thermodynamics insight, we conclude that variation in the carbonate bulk and interfacial energies, along with the solution supersaturation, lead to the dissolution-precipitation transformation pathway from Mg-rich to Mg-poor carbonate phase that preserves spherulitic morphology. Furthermore, our findings are relevant for long-standing questions of how impurities influence diagenesis of carbonate sediments and spherulitic carbonate particles' origin.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

In situ high-energy X-ray study of deformation mechanisms in additively manufactured 316L stainless steel

A key structural material planned to be used in the core of the Transformational Challenge Reactor is the additively manufactured 316L stainless steel (AM 316L SS). While the deformation of conventionally-manufactured 316 SS have been extensively studied, the deformation mechanism of AM 316L SS is less known. Here the room-temperature tensile behavior of AM 316L SS was studied in situ using high-energy X-ray diffraction and X-ray tomography. Diffraction yielded the lattice strains and the dislocation densi-ties of the AM 316L SS, which were compared to those of a conventionally processed 316H SS. It was found that while the conventional 316H SS had three distinct deformation stages, namely stage II ather-mal hardening, stage III dynamic recovery, and stage IV, the AM 316L experienced only the stages III and IV after an initial transitional period. The plastic instability stresses (PIS), i.e. the true ultimate tensile strength, were nearly the same in both materials. The AM 316L had very low dislocation barrier strength throughout the plastic deformation, which, in combination with the invariant PIS, explained its high dis-location storage capability and the attractive combination of strength and ductility. Tomography revealed morphological changes of the built-in pores in the AM 316L during deformation and fracture, and it was concluded that large pores close to the surface might have significant roles in the necking stage.

316 stainless steel↗

High energy X-ray characterization of the microstructure of PuGa alloy samples at macroscopic depths and non-ambient conditions

High energy (95 keV) X-rays were utilized to characterize the microstructure of eight PuGa alloy samples at room temperature and during cooling to ∼10 K. The samples had different Ga content (nominally 0-3.4 at.%), age, and history. A ninth sample, similarly characterized with neutron diffraction, was included to extend the Ga range to 7 at.%. The samples span the range from single phase α (monoclinic) to δ (face-centered cubic) PuGa, as well as a two-phase α′/δ sample. The crystallographic textures, phase fractions, lattice parameters and dislocation densities of each sample were evaluated through distinct analysis techniques. The textures of the samples were modest. In each case, the dislocation densities were relatively high, comparable to cold worked metals and metals exposed to similar radiation dose. At room temperature, the lattice parameters determined in the predominantly single-phase samples were larger than expected based on the nominal Ga concentration. The observed lattice thermal expansions of the single-phase δ samples to 10 K are self-consistent across the samples and consistent with previous measurements reported in the literature. Significantly larger thermal lattice strain is observed in the δ phase of the two-phase material due to mechanical constraint from the α′ phase, which has a three times larger thermal expansion and is much harder than the δ phase. In conclusion, the results demonstrate the unique value of high-energy X-rays for relatively routine microstructural characterization of Pu alloy samples.

36 MATERIALS SCIENCE↗

Interplay of molten salt and dopants in tuning the performance of single-crystalline LiNiO 2

Single-crystalline layered oxide cathodes have seen great research interest in recent years. Adoption of single-crystal morphology improves mechanical robustness and eliminates intergranular boundaries, improving the chemical stability of the cathode. Furthermore, single-crystal cathodes also suffer from worsened lithium-diffusion kinetics stemming from the significantly increased diffusion path lengths. Sluggish lithiation kinetics induce concentration gradients within the cathode particle during cell operation, resulting in the accumulation of lattice strain, which deteriorates cell performance. Foreign dopants have been shown to greatly improve ion diffusion in many high-Ni layered oxide cathode systems. In particular, we identify Ti and Te as promising dopants to ameliorate the slow diffusion kinetics. We find that doping 1 mol.% Te into single crystal LiNiO 2 greatly improves Li + diffusivity, as determined through galvanostatic intermittent titration technique. Further incorporating 2 mol.% Al and pairing with lithium-metal anode in a localized high concentration electrolyte (LHCE) delivers 206 mA h g -1 at C/3 rate and retains 94% capacity after 100 cycles in Li metal half cells. By addressing kinetically mediated degradation with Te doping, and surface-based degradation with Al and LHCE, the cathode experiences very little polarization and overpotential growth, enabling stable cycling with high accessible capacity.

25 ENERGY STORAGE↗

Strengthening mechanisms, hardening/softening behavior, and microstructure evolution in an LPSO magnesium alloy at elevated temperatures

Here, rapid degradation of the mechanical properties of conventional Mg alloys with temperature precludes their wide application in industry. The LPSO (long period stacking ordered) Mg alloys, on the other hand, show considerable potential to achieve excellent high-temperature mechanical performance. In this study, a Mg-5.1Y-2.4Zn (wt.%) extrusion alloy with the microstructure comprising of α-Mg matrix and LPSO phase was prepared. It is shown that the yield strength of the alloy at 200 °C retained ~83% of the yield strength of 198 MPa at room temperature (RT). Importantly, the ductility also improved, owing to the increased non-basal slip activities at elevated temperatures. In contrast to RT and 200 °C, the alloy exhibited softening tensile behavior with an apparent loss of yield strength at 300 °C. In-situ lattice strain analysis revealed that load transfer from α-Mg to LPSO remains effective at temperatures up to 200 °C, governing the high yield strength of the alloy. The post-mortem analysis by means of electron microscopy confirmed that the LPSO phase is structurally stable at 200 °C. In particular, the high strain hardenability is rationalized by the sandwiched LPSO structures together with stacking faults serving as effective obstacles to the motion of non-basal dislocations. The load transfer effect disappears at the temperature of 300 °C, resulting in the fast deterioration of strength of the alloy. The cracking of the LPSO phase along with the recrystallizing of α-Mg grains were found to be the main causes for the softening behavior of the alloy at 300 °C.

36 MATERIALS SCIENCE↗

In-situ neutron diffraction investigation of two-stage martensitic transformation in a 13%Mn steel with serrated deformation

Two stage austenite →ε-martensite →α-martensite phase transformation, phase-specific lattice strain evolution and load sharing during tensile deformation of a 13%Mn hot-rolled austenitic steel are revealed by in-situ neutron diffraction. In conclusion, direct evidence is provided that serrated deformation behavior is attributed to discontinuous martensitic transformation.

Austenitic steel↗