Multi-Pronged Analysis of Degradation Rates of Photovoltaic Modules and Arrays Deployed in Florida
Abstract not provided
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided
There are relatively few field studies on the degradation of non-fluoropolymer-based backsheets, and understanding their in-field behavior is critical for further development of such products. In this paper, backsheet degradation of modules with one of these new types of backsheets (polyethylene naphthalate (PEN)-based) was documented at a four-year old utility-scale array located in Maryland (USA). Visual inspection, colorimetry, glossimetry, and Fourier-transform infrared spectroscopy (FTIR) revealed highly varied properties depending on module position within the array. Specifically, modules near the edge of the array and with higher mounting elevations underwent greater amounts of backsheet degradation, as indicated by yellowing and gloss-loss. The reason for these unique degradation patterns were differential backside exposure conditions, especially of ultraviolet light. This was strongly influenced by the array design, including array structural and environmental factors, such as module spacing and ground cover, respectively. Within the array, no clear link between backsheet degradation and module output or safety has been identified. However, such a relationship may be expected to become more pronounced with time, affecting system lifetime and ultimately the levelized cost of electricity (LCOE). Finally, the observed phenomena have implications for both backsheet product development and array design, especially for modules that utilize newer classes of non-fluoropolymer-based backsheets which are typically more susceptible to environmental degradation.
As it is considered economically favorable to serially connect modules to build arrays with high system voltage, it is necessary to explore potential long-term degradation mechanisms the modules may incur under such electrical potential. We performed accelerated lifetime testing of multicrystalline silicon PV modules in 85 degrees C/ 85% relative humidity and 45 degrees C/ 30% relative humiditywhile placing the active layer in either positive or negative 600 V bias with respect to the grounded module frame. Negative bias applied to the active layer in some cases leads to more rapid and catastrophic module power degradation. This is associated with significant shunting of individual cells as indicated by electroluminescence, thermal imaging, and I-V curves. Mass spectroscopy resultssupport ion migration as one of the causes. Electrolytic corrosion is seen occurring with the silicon nitride antireflective coating and silver gridlines, and there is ionic transport of metallization at the encapsulant interface observed with damp heat and applied bias. Leakage current and module degradation is found to be highly dependent upon the module construction, with factors such asencapsulant and front glass resistivity affecting performance. Measured leakage currents range from about the same seen in published reports of modules deployed in Florida (USA) and is accelerated to up to 100 times higher in the environmental chamber testing.
A CPV module containing 30 III-V multijunction cells was operated on--sun for one year in Golden, Colorado. Each cell was characterized prior to and following exposure. A module power degradation of 10% was observed and found to be a result as an overall decrease in cell short circuit current and the presence of at least one shunted cell. A positive correlation between initial shunt current and an increase in shunt current following exposure was also found. Cell exfoliation was also observed and found to be coincident with the presence of water and/or charring of the cell package due to an off-sun event.
Potential-induced degradation (PID) has recently been shown as an important failure mode in c-Si modules. We demonstrate the utility of Suns-Voc analysis for measuring shunt effects caused by PID at the module level. Our results show module shunt resistance increasing in step with module power during recovery from the degraded state.
Abstract not provided.
Abstract not provided.
Reliability and durability tests play a key role in the photovoltaic (PV) industry by minimizing potential failure risks for both existing and new cell and module technologies. In this work, a detailed study of contact degradation in monocrystalline and multicrystalline PV modules is performed. The modules are subjected to a sequence of damp heat (DH) exposures followed by electrical characterization after each step. Electroluminescence (EL) imaging shows different darkening patterns for monocrystalline modules compared to multicrystalline modules; the former shows darkening near the busbars and the latter shows it across virtually the entire cell surface. The primary loss mechanism is confirmed to be resistive after comparing the current-voltage (I–V) characteristics at each DH exposure step. Representative samples have been cored out from both the degraded modules and controls for materials characterization to gain further insights into the degradation mechanism. Top-down and cross-sectional scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and top-down high-resolution X-ray photoelectron spectroscopy (XPS) analysis performed on the cored samples confirm the degradation is due to metallization corrosion. Our study suggests that the difference in the darkening pattern can most likely be attributed to the different silver paste composition used for contacting each cell technology, particularly the composition of the glass frit.
A system of 180 monocrystalline aluminum back-surface field modules were installed in Cocoa, Florida, for 10 years. In total, 156 modules are characterized and compared to 3 controls. Power degradation rates vary between – 0.14% to – 3.22% per year, with median and average rates of –0.92% and –1.05% per year, respectively. The losses are primarily resistive with minor optical and recombination loss contributions. Electroluminescence imaging shows a characteristic pattern, which is shown to be resistive in nature when compared to photoluminescence. Resistive losses are due to corrosion of the rear contact Ag/solder interface and, to a much lesser degree, gridline Ag oxidation. Moisture ingress through the backsheet is likely responsible for mediating corrosion. Optical losses are due mostly to a combination of antireflection coating degradation, minor encapsulant browning, and delamination. Minor front contact corrosion may contribute to recombination. Furthermore, this study expands upon previous work on this vintage of the module by examining a large sample set, comprehensive characterization including techniques not previously used on these modules, and a comparison between two other systems of different climates.
Field testing, failure analysis, and understanding of degradation mechanisms are essential to advancing metal halide perovskite (MHP) photovoltaic (PV) technology toward commercialization. Here, we present performance data from up to 1 year of outdoor testing of MHP modules in Golden, Colorado. The module encapsulation architecture and encapsulant materials have a significant impact on module reliability, with modules containing a polyolefin elastomer (POE) in addition to a desiccated polyisobutylene (PIB) edge seal outlasting modules with only a PIB edge seal or PIB blanket. Nondestructive and destructive characterization of the field-tested modules points to module scribes and interfaces as areas of potential mechanical weakness and chemical migration, resulting in shunt pathways and increased series resistance. Finally, indoor accelerated stress testing with light and elevated temperatures is performed, demonstrating failure with similar scribe degradation signatures as compared to the field-tested modules. In conclusion, under both outdoor testing and light and elevated temperature conditions, electrochemical corrosion between the copper electrode and the mobile iodine ions appeared dominant, with a significant progression at the scribes that is speculated to result from an interplay between the initial laser damage and joule heating from enhanced ion diffusion under bias.
Assessing photovoltaic module backsheet durability is critical to increasing module lifetime. Lab based accelerating testing has recently failed to predict large scale failures of widely adopted polymeric materials. Field surveyed data is critical to assess the performance of component lifetime. Using a documented field survey protocol, 13 field surveys where conducted. Each measurement is encoded with it's spatial location in respect to the other modules. By combining field survey data on degradation predictors with real time satellite weather data, data-driven predictive models of backsheet degradation were trained. LOESS models were constructed to investigate the spatial dependence of measurements. It was found that micro-climatic effects like tree-lines, ground surface changes, and elevation changes effected the magnitude and variance of the measurements. A GAM model was created to predict the value of degradation based on measured predictors. The model includes variables on the climate of the system and the location of each measurement in the PV mounting structure. The model performed well with an adj.R 2 of 0.95 for yellowness index prediction. The model was cross-validated using k-folds.
Here we automate the process to enable the creation of world maps for specific PV durability metrics. The end goal is to create a tool for the creation of world maps predicting the sensitivity of modules to degradation to inform the development and utilization of module testing standards and to provide information to module designers. TMY (Typical Meteorological Year) Data was aggregated from sites around the world to render insight into factors contributing to the degradation of solar modules. The focus of aggregating data was to create a single dataset to work with utilizing Solar Irradiance values combined with Ambient Temperature, Relative Humidity, Wind Speed and Dew-Point Temperature.
A test sequence producing potential-induced degradation-delamination (PID-d) in crystalline silicon modules has been tested and found comparable under visual inspection to cell/encapsulant delamination seen in some fielded modules. Four commercial modules were put through this sequence, 85 degrees C, 85%, 1000 h damp heat, followed by an intensive PID stress sequence of 72 degrees C, 95% RH, and -1000 V, with the module face grounded using a metal foil. The 60 cell c-Si modules exhibiting the highest current transfer (4.4 center dot 10-4 A) exhibited PID-d at the first inspection after 156 h of PID stress. Effects promoting PID-d are reduced adhesion caused by damp heat, sodium migration further reducing adhesion to the cells, and gaseous products of electrochemical reactions driven by the applied system voltage. A new work item proposal for an IEC test standard to evaluate for PID-d is anticipated.
3D LES simulations were carried out to study the performance of a vacuum membrane distillation module. A wiggly wall profile with/without embedded stiffeners was considered to alleviate axial and radial temperature polarization, the cause of performance decrease in membrane distillation. Results of the flow field show the wiggles create unsteady vortex shedding inducing intense mixing in the channel. Vortex shedding intensity increases as the Reynolds number increases or stiffeners are added. 3D results show a 56% improvement in flux when moving from a flat sheet membrane to a wiggly membrane with stiffeners at a constant Reynolds number, corresponding to an improvement from 11.7 to 41.7 in the Nusselt number, showing that the alterations improved the flux performance by enhancing the heat transfer along the membrane surface and therefore alleviating temperature polarization, a critical bottleneck in membrane distillation systems. Further, a merit criterion was defined based on the Nusselt number and friction factor, and a 40% increase in merit was shown switching from a flat to a wiggly channel, while a 97% merit increase was seen going from flat to wiggly with stiffeners. A 42% enhancement in the flux was also seen moving from a straight channel to a wiggly channel at a higher Reynolds number which highlights the importance of strategically choosing the mass flow rate, as well as inducing flow separation and vortex shedding in the channel to promote mixing and dissipate the thermal boundary layer. The variation in results between the wiggly module with stiffeners and the wiggly module at high Reynolds numbers suggests enhancing mixing structures can be more impactful on flux for this geometry than increasing the flow rate to a turbulent/transitional regime. However, both are preferable for peak system flux performance. Furthermore, a 2D approximation was used to perform simulations on more extended channels to examine the length degradation. The modules with wiggly channels performed at the same flux level with a doubling of the length. On the other hand, the flat sheet modules experienced length degradation by temperature polarization and dropped in flux yield by around 13% of the short-channel value. This work illustrates that modeling the system and understanding how the performance decreases as the membrane surface area increases are critical for a larger module (scaling up from a lab to a prototype module) to maintain high flux performance.
The correlation between outdoor field testing and indoor chamber measurement for potential-induced degradation in crystalline silicon PV modules is unclear. The motivation of this work is to build up a direct comparison and investigate the correlation between indoor and outdoor performance. First of all, four PID indoor tests were defined from basic to premium, based on the difficulty of the test. Six groups of modules were designed and fabricated in Trina Solar, with different grades of PID resistance from weak to strong. The outdoor field test systems were built in three different climates: tropical, subtropical, and semi-arid climates in Singapore, Changzhou (China) and Golden (CO, USA) respectively, in a collaborative testing campaign involving Trina, SERIS and NREL. The system in Golden has been on-sun for more than 13 months where <4% power loss which includes PID and other reliability losses was detected and power loss of <2% is shown for all six groups of modules after 21 weeks in the field in the subtropical climate in Changzhou. However, PID of 23% was observed after 18 weeks in Singapore for the most PID-susceptible module, while the other PID module types showed degradation of only less than 5%.
In an experiment with five module designs and multiple replicas, it is found that crystalline silicon cell modules that can pass a criterion of less than 5 percent power degradation in stress test conditions of 60 degrees Celsius, 85 percent relative humidity (RH), 96 h, and nameplate-rated system voltage bias show no power degradation by potential induced degradation in the range of 4-6 years duration in the Florida, USA environment. This data suggests that this chamber stress level is useful as a pass/fail criterion for PID, and will help ensure against degradation by system voltage stress in Florida, or less stressful climates, for at least 5 years.
This paper elucidates the behavior and underlying mechanism of potential-induced degradation (PID) on the rear side of p-type monocrystalline silicon bifacial passivated emitter and rear cell (PERC) photovoltaic modules. At 50 degrees C, 30% relative humidity, and -1000 V bias to the solar cells with aluminium foil on the rear glass surface, the rear-side performance of bifacial PERC modules at standard testing conditions degraded dramatically after 40 hours with a 40.4%, 36.2%, and 7.2% loss in maximum power (Pmpp), short-circuit current (Isc), and open-circuit voltage (Voc), respectively. The front-side standard testing condition performance, on the other hand, showed less degradation; Pmpp, Isc, and Voc dropped by 12.0%, 5.2%, and 5.3%, respectively. However, negligible degradation was observed when the solar cells were positively biased. Based on I-V characteristics, electroluminescence, external quantum efficiency measurements, and the effective minority-carrier lifetime simulation, the efficiency loss is shown to be caused by the surface polarization effect; positive charges are attracted to the passivation/antireflection stack on the rear surface and reduce its field effect passivation performance. Extended PID testing to 100 hours showed an increase in device performances (relative to 40 hours) due to the formation of an inversion layer along the rear surface. In addition, replacing ethylene-vinyl acetate copolymer with polyolefin elastomer films significantly slows down the progression of PID, whereas a glass/transparent backsheet design effectively protects the rear side of bifacial PERC modules from PID. Furthermore, PID on the rear side of bifacial PERC modules is fully recoverable, and light greatly promotes recovery of the observed PID.