Search NASA⌕ Search

SEARCH · Search NASA

Results for “polymer oxidation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Polymeric membrane systems of potential use for battery separators

Two membrane systems were investigated that may have potential use as alkaline battery separators. One system comprises two miscible polymers: a support polymer (e.g., polyvinyl formal) and an ion conductor such as polyacrylic acid. The other system involves a film composed of two immiscible polymers: a conducting polymer (e.g., calcium polyacrylate) suspended in an inert polymer support matrix, polyphenylene oxide. Resistivities in 45-percent potassium hydroxide and qualitative mechanical properties are presented for films comprising various proportions of conducting and support polymers. In terms of these parameters, the results are encouraging for optimum ratios of conducting to support polymers.

Philipp, W. H.↗

Concentrations and behavior of oxygen and oxide ion in melts of composition CaO.MgO.xSiO2

The behavior of oxygen and oxide ion in silicate melts was investigated through their electrochemical reactions at a platinum electrode. Values are given for the diffusion coefficient for molecular oxygen in diopside melt and the activation energy of diffusion. It is shown that molecular oxygen dissociates prior to undergoing reduction and that oxide ion reacts quickly with silicate polymers when it is produced. The concentration of oxide ion is kept low by a buffering effect of the silicate, the exact level being dependent on the silicate composition. Data on the kinetics of reaction of the dissociation of molecular oxygen and on the buffering reactions are provided. It is demonstrated that the data on oxygen in these silicate melts are consistent with those for solid buffers.

Semkow, K. W.↗

Addition polymers from 1,4,5,8-tetrahydro-1,4;5,8-diepoxyanthracene and Bis-dienes: Processable resins for high temperature application

1,4,5,8-Tetrahydro-1,4;5,8-diepoxyanthracene reacts with various anthracene endcapped polyimide oligomers to form Diels-Alder cycloaddition copolymers. The polymers are soluble in common organic solvents, and have molecular weights of approximately 21,000 to 32,000. Interestingly, these resins appear to be more stable in air then in nitrogen. This is shown to be due to a unique dehydration (loss of water ranges from 2 to 5 percent) at temperatures of 390 to 400 C to give thermo-oxidatively stable pentiptycene units along the polymer backbone. Because of their high softening points and good thermo-oxidative stability, the polymers have potential as processible, matrix resins for high temperature composite applications.

Meador, Mary Ann B.↗

Polymer membrane based electrolytic cell and process for the direct generation of hydrogen peroxide in liquid streams

An electrolytic cell for generating hydrogen peroxide is provided including a cathode containing a catalyst for the reduction of oxygen, and an anode containing a catalyst for the oxidation of water. A polymer membrane, semipermeable to either protons or hydroxide ions is also included and has a first face interfacing to the cathode and a second face interfacing to the anode so that when a stream of water containing dissolved oxygen or oxygen bubbles is passed over the cathode and a stream of water is passed over the anode, and an electric current is passed between the anode and the cathode, hydrogen peroxide is generated at the cathode and oxygen is generated at the anode.

White, James H.↗

Use of Atomic Oxygen for the Determination of Document Alteration

Atomic oxygen, which normally is found only the near Earth space environment, causes oxidation and erosion of polymers on spacecraft. The development of technology to prevent this degradation has required NASA to develop ground laboratory facilities that generate atomic oxygen. Atomic oxygen has also been found to be able to oxidize most types of ink from a variety of types of pens. The use of atomic oxygen to identify alteration of documents has been investigated and is reported. Results of testing indicates that for many types of ink, pen, and paper, identification of document alteration of pen and ink numbers and evidence of alteration can be made visible by exposing the questionable writing to atomic oxygen. Atomic oxygen provides discrimination because different inks may oxidize at different rates, the amount of time between delayed alteration may add to ink thickness at crossings, and the end of pen strokes tend to have much thicker ink deposits than the rest of the character. Examples and techniques of using atomic oxygen to identify document alteration indicate that the technology can, in many but not all cases, provide discrimination between original and altered documents.

Banks, Bruce A.↗

Reducing the Cation Exchange Capacity of Lithium Clay to Form Better Dispersed Polymer-Clay Nanocomposites

Polymer-clay nanocomposites have exhibited superior strength and thermo- oxidative properties as compared to pure polymers for use in air and space craft; however, there has often been difficulty completely dispersing the clay within the matrices of the polymer. In order to improve this process, the cation exchange capacity of lithium clay is first lowered using twenty-four hour heat treatments of no heat, 130 C, 150 C, or 170 C to fixate the lithium ions within the clay layers so that they are unexchangeable. Generally, higher temperatures have generated lower cation exchange capacities. An ion exchange involving dodecylamine, octadecylamine, or dimethyl benzidine (DMBZ) is then employed to actually expand the clay galleries. X-ray diffraction and transmission electron microscopy can be used to determine whether the clay has been successfully exfoliated. Finally, resins of DMBZ with clay are then pressed into disks for characterization using dynamic mechanical analyzer and oven- aging techniques in order to evaluate their glass transition, modulus strength, and thermal-oxidative stability in comparison to neat DMBZ. In the future, they may also be tested as composites for flexural and laminar shear strength.

Liang, Maggie↗

Tunable Nanoscale Structure via Divalent Ion Identity in Charged-Neutral Polymer Blends

Charged-neutral polymer blends, wherein an ioncontaining polymer is blended with a neutral polymer, are potential candidates for battery electrolytes due to their improved ion transport properties and electrochemical stability. Though electrostatic interactions in charged polymer blends can theoretically stabilize ordered nanostructures analogous to those observed in neutral block copolymers, direct experimental evidence remains limited. Here, we investigate the effects of divalent cation identity on the nanoscale morphology of charged-neutral polymer blends composed of poly(ethylene oxide) (PEO) and Mg 2+ or Ca 2+ ioncontaining polymers, poly[3-(methylacryloxy)propylsulfonyl-1-(trifluoromethanesulfonylimide)] (P(Mg(MTFSI) 2 ) or P(Ca- (MTFSI) 2 ). By tuning the size of the divalent counterion, we are able to precisely tune the ion solvation between the free cation and PEO, which acts as a solvent in this system. Differential scanning calorimetry (DSC) and small-angle X-ray scattering (SAXS) measurements reveal that Mg 2+ and Ca 2+ ions induce distinct structural behavior. In both systems, the blends become more miscible as the concentration of ion-containing polymer is increased indicated by increased suppression of PEO crystallinity. At the highest concentrations of P(Mg(MTFSI) 2 ), the blends undergo microphase separation and generate nanostructures with shortranged ordering. In contrast, calcium ions, which are more readily solvated by PEO, produce more homogeneous blends characterized by a single glass-transition temperature and featureless SAXS data. The results demonstrate the novel experimental confirmation that charged-neutral polymer blends can undergo microphase separation and show that counterion identity can be exploited as a design parameter to control nanoscale morphology.

Ions↗

Evaluation of flammability for cable-like polymers

A new test method is developed for the flammability of insulated electric cables as well as polymers formed in the cables. The rate of downward flame spread along the polymer surface is measured by a technique in which the flame is stopped at a particular position by winding up the cable at the same speed as the flame spreading rate, with external preheating by an electric furnace having oxidative gas flow. The polymer burns continuously without change of flame condition and the rate is obtained from the winding speed of the cable. A flame spread equation relates the flame spreading rate (V) of the cable-like polymer to O concentration (Yo) and the atmosphere, the preheating temperature, and the pyrolysis temperature for polymer burning. Plotting log V vs. log Yo for experimental results allows evaluation of the flammability of polymers, with discrimination between the effects of O concentration, heating temperature, and specimen shape. Results with various types of PVC electrical cable indicated the validity of the method. Application of the method to the cables in groups showed a flame retardation behavior different from the case of a single cable, in a atmosphere of high O concentration.

Mikado, Tuneo↗

Polyimides Containing Fluorine and Phosphorus for Potential Space Applications

As part of an effort to develop low color, ultraviolet (UV) radiation and atomic oxygen resistant polyimides for potential space applications, a novel diamine containing fluorine and phosphorus was synthesized and used to prepare polyimides. The approach was to combine attributes from colorless, UV resistant polyimides and atomic oxygen (AO) resistant polymers into a single material. Preparation of colorless polyimides has focused on minimization of charge transfer complex formation by incorporation of bulky substituents and disrupting conjugation by using meta-catenated monomers. AO resistant polymer technology development has focused on placing phenylphosphine oxide groups into the backbone of aromatic polymers. However, polyimides prepared utilizing this approach thus far have all exhibited significant color. Thus in an attempt to combine these features in a polyimide a new diamine, bis(3-aminophenyl)-3,5-di(trifluoromethyl)phenylphosphine oxide (TFMDA) was synthesized and used to prepare polyimides. The polyimides were cast into films and characterized for physical and mechanical properties, optical transmission and AO and UV resistance.

Connell, John W.↗

Achieving Electrode Smoothing by Controlling the Nucleation Phase of Metal Deposition Through Polymer‐Substrate Binding

Polymer additives [like polyethylene oxide (PEO)] are widely used for smooth electrode deposition in aqueous zinc and many other battery systems. However, the precise mechanism by which they regulate morphology and suppress dendrite formation remains unclear. In this study, the knowledge gap is addressed by using in situ electrochemical atomic force microscopy to directly observe the interfacial evolution during Zn electrodeposition and polymer adsorption on Cu substrates in the presence of varying concentrations of ZnSO 4 and PEO. Contrary to previous literature assumptions, which emphasize the binding to the growing Zn crystal surfaces or Zn 2+ ions, the results demonstrate that PEO smooths Zn films by promoting nucleation of (002)-oriented Zn platelets through interactions with the Cu substrate. Density functional theory simulations support this finding by showing that PEO adsorption on Cu modifies the interfacial energy of Zn/Cu/electrolyte interfaces, favoring the stabilization of Zn (002) on the Cu substrate, as well as confines Zn electrodeposition to a narrow near-surface region. In conclusion, these findings elucidate a novel design principle for electrode smoothing, emphasizing the importance of substrate selection paired with polymer additives that exhibit an attractive interaction with the substrate but minimal interaction with growing crystals, offering a mechanistic perspective for improved battery performance.

Electrodeposition↗

Surface and interfacial properties of carbon fibers

The adhesion strength of AS4 fibers to thermoplastic polymers was determined. The specific polymers were polycarbonate, polyphenylene oxide, polyetherimide, polyphenylene oxide blends with polystyrene, and polycarbonate blends with a polycarbonate-polysiloxan copolymer. Data are also included for polysulfone. It was recognized at the outset that an absolute measure of the fiber matrix adhesion would be difficult. However, it is feasible to determine the fiber bond strengths to the thermoplastics relative to the bond strengths of the same fibers to epoxy polymers. It was anticipated, and in fact realized, that the adhesion of AS4 to the thermoplastic polymers was relatively low. Therefore, further objectives of the study were to identify means of increasing fiber/matrix adhesion and to try to determine why the adhesion of AS4 to thermoplastics is significantly less than to epoxy polymers.

Bascom, Willard D.↗

Synthesis of highly sulfonated 2,6-diphenyl-p-Phenylene oxide: A highly conductive membrane

Highly sulfonated aromatic polymers are desired for the possible highest performance of polymer electrolytes in fuel cells and electrolyzer applications. Here, we reported the method to prepare highly sulfonated 2,6-diphenyl-p-phenylene oxide (SP3O), a commercially available aromatic polymer, with the highest IEC of 4.42 meq/g. Three sulfonation reagents including chlorosulfonic acid (HSO3Cl), concentrated sulfuric acid (conc. H2SO4), and trimethylsilyl chlorosulfonate (TMSCS) were investigated for single and two-step sulfonation reactions. In addition, DMSO-assisted thermal crosslinking method was applied to prepare crosslinked SP3O membranes to improve their mechanical strength and film-forming ability. Proton exchange membrane from crosslinked SP3O displayed a proton conductivity as high as 250 mS/cm at 95 % RH and 60 °C.

Khomein, Piyachai↗

Effect of High Temperature Storage on AC Characteristics of Polymer Tantalum Capacitors

Replacement of MnO2 with conductive polymers as cathode materials in chip tantalum capacitors allows for a substantial reduction of the equivalent series resistance (ESR), improvement of frequency characteristics, and elimination of the possibility of ignition during failures. One of the drawbacks of chip polymer tantalum capacitors (CPTCs) is a relatively poor long-term stability at high temperatures. In this work, variations of capacitance, dissipation factor, and ESR in different types of capacitors including automotive grade parts from three manufacturers have been monitored during storage at temperatures from 100 ºC to 175 ºC for up to 18,000 hours. Results show that ESR is the most and capacitance the least sensitive to degradation parameter. Times to parametric failures have been simulated using a Weibull-Arrhenius model that allowed for assessments of activation energies of the degradation and prediction of times to failure at the use temperature. Degradation of CPTCs was explained by thermo-oxidative processes in conductive polymers that result in exponential increasing of the resistivity with time of ageing. This process starts after a certain incubation period that depends on packaging materials and design and corresponds to the time that is necessary to form delamination between the encapsulating molding compound and lead frame. The effectiveness of the existing qualification procedures to assure stable operation of CPTCs is discussed.

Alexander A Teverovsky↗

Effect of High Temperature Storage on AC Characteristics of Polymer Tantalum Capacitors

Replacement of MnO2 with conductive polymers as cathode materials in chip tantalum capacitors allows for a substantial reduction of the equivalent series resistance (ESR), improvement of frequency characteristics, and elimination of the possibility of ignition during failures. One of the drawbacks of chip polymer tantalum capacitors (CPTCs) is a relatively poor long-term stability at high temperatures. In this work, variations of capacitance, dissipation factor, and ESR in different types of capacitors including automotive grade parts from three manufacturers have been monitored during storage at temperatures from 100 ºC to 175 ºC for up to 18,000 hours. Results show that ESR is the most and capacitance the least sensitive to degradation parameter. Times to parametric failures have been simulated using a Weibull-Arrhenius model that allowed for assessments of activation energies of the degradation and prediction of times to failure at the use temperature. Degradation of CPTCs was explained by thermo-oxidative processes in conductive polymers that result in exponential increasing of the resistivity with time of ageing. This process starts after a certain incubation period that depends on packaging materials and design and corresponds to the time that is necessary to form delamination between the encapsulating molding compound and lead frame. The effectiveness of the existing qualification procedures to assure stable operation of CPTCs is discussed.

Aging↗

Effect of High Temperature Storage on AC Characteristics of Polymer Tantalum Capacitors

Replacement of MnO2 with conductive polymers as cathode materials in chip tantalum capacitors allows for a substantial reduction of the equivalent series resistance (ESR), improvement of frequency characteristics, and elimination of the possibility of ignition during failures. One of the drawbacks of chip polymer tantalum capacitors (CPTCs) is a relatively poor long-term stability at high temperatures. In this work, variations of capacitance, dissipation factor, and ESR in different types of capacitors including automotive grade parts from three manufacturers have been monitored during storage at temperatures from 100 ºC to 175 ºC for up to 18,000 hours. Results show that ESR is the most and capacitance the least sensitive to degradation parameter. Times to parametric failures have been simulated using a Weibull-Arrhenius model that allowed for assessments of activation energies of the degradation and prediction of times to failure at the use temperature. Degradation of CPTCs was explained by thermo-oxidative processes in conductive polymers that result in exponential increasing of the resistivity with time of ageing. This process starts after a certain incubation period that depends on packaging materials and design and corresponds to the time that is necessary to form delamination between the encapsulating molding compound and lead frame. The effectiveness of the existing qualification procedures to assure stable operation of CPTCs is discussed.

Aging↗

Effect of High Temperature Storage on AC Characteristics of Polymer Tantalum Capacitors

Replacement of MnO2 with conductive polymers as cathode materials in chip tantalum capacitors allows for a substantial reduction of the equivalent series resistance (ESR), improvement of frequency characteristics, and elimination of the possibility of ignition during failures. One of the drawbacks of chip polymer tantalum capacitors (CPTCs) is a relatively poor long-term stability at high temperatures. In this work, variations of capacitance, dissipation factor, and ESR in different types of capacitors including automotive grade parts from three manufacturers have been monitored during storage at temperatures from 100 ºC to 175 ºC for up to 18,000 hours. Results show that ESR is the most and capacitance the least sensitive parameter to degradation. Times to parametric failures have been simulated using a Weibull-Arrhenius model that allowed for assessments of activation energies of the degradation and prediction of times to failure at the use temperature. Degradation of CPTCs was explained by thermo-oxidative processes in conductive polymers that result in exponential increase of the resistivity with time of aging. This process starts after a certain incubation period that depends on packaging materials and design and corresponds to the time that is necessary to form delamination between the encapsulating molding compound and lead frame. The effectiveness of the existing qualification procedures to assure stable operation of CPTCs is discussed.

high temperature storage (HTS)↗