Search NASA⌕ Search

SEARCH · Search NASA

Results for “substrate amorphization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Growth of nanostructured molybdenum disulfide (MoS 2 ) thin films on a nanohole-patterned substrate using plasma-enhanced atomic layer deposition (ALD)

Nanostructured molybdenum disulfide (MoS 2 ) thin films were grown on a nanohole-patterned silicon substrate using plasma-enhanced atomic layer deposition. A nanoscale hole-patterned silicon substrate was fabricated for the growth of MoS 2 film using the self-assembly-based nanofabrication method. The nanoscale holes can significantly increase the surface area of the substrate while the formation and growth of nanostructures normally start at the surface of the substrate. Hydrogen sulfide (H 2 S) gas was used as the S source in the growth of molybdenum disulfide (MoS 2 ) while molybdenum (V) chloride (MoCl 5 ) powder was used as the Mo source. The MoS 2 film had a stoichiometric ratio of 1 (Mo) to 2 (S), and had peaks of E 1 2g and A 1g , which represent the in-plane and out-plane vibration modes of the Mo–S bond, respectively. It was found that the MoS 2 film grown in the nanoscale hole, especially at the wall of the hole, has more hexagonal-like structures due to the effects of nanoscale space confinement and the nanoscale interface although the film shows an amorphous structure. Post-growth high-temperature annealing ranging from 800 to 900 °C produced local crystalline structures in the film, which are compatible with those reported by other researchers.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Optical properties of Mo and amorphous MoOx, and application to antireflection coatings for metals

To form antireflection (AR) coatings to hide metal architecture in display technologies, we deposited thin films of metal Mo and oxide MoOx by sputtering targets of various compositions using pure Ar sputter gas. The optical constants [n,k] of these samples were measured by the direct numerical solution of reflectance and transmittance at each wavelength point measured. We find that 50 nm films are uniform in the growth direction, but for thicker 100 nm samples, evidence exists for nonuniform growth, where the top 20 nm appears to be metal rich. From these [n,k], negative Tauc bandgap energies show these oxides are semi-metals. We then identified the specific composition (x) that optimizes the AR response for a host of metals (Al, Cu, Ag, Au). Finally, two methods were used to understand why these MoOx materials function well as AR media, including (i) using phasor rays and (ii) developing a universal expression for the AR condition that applies to both dielectric and metal substrates. In (i), we find two characteristics for AR of metals: (a) its optical thickness should be roughly π3, not the π2 for dielectrics, since for MoOx, their [r^ij,t^ij] Fresnel phases differ from the usual [180°, 0°] of dielectrics; and (b) the medium incorporates a k-dominant strategy whose function is to absorb the energy that is reflected at the AR/metal interface. In (ii), the universal AR condition is found to be r^01+r^12z^=0. For dielectrics, this reduces to the well-known nAR=nairnsub condition. However, for metals, a concise analytic expression is lacking since this expression is highly nonlinear but is easily solved by numerical methods.

Tsu, David V. (ORCID:0000000295903418)↗

Failure modes of protection layers produced by atomic layer deposition of amorphous TiO 2 on GaAs anodes

Amorphous titanium dioxide (a-TiO 2 ) films formed by atomic layer deposition can serve as protective coatings for semiconducting photoanodes in water-splitting cells using strongly alkaline aqueous electrolytes. Herein, we experimentally examine the mechanisms of failure for p + -GaAs anodes coated with a-TiO 2 films (GaAs/a-TiO 2 ). Galvanic displacement of exposed GaAs by Au allowed imaging of pinholes in the a-TiO 2 coatings, and enabled collection of quantitative and statistical data associated with pinhole defects. A combination of imaging, electrochemical measurements, and quantitative analyses of corrosion products indicated that extrinsic pinholes were present in the a-TiO 2 films before electrochemical operation. During electrochemical operation these pinholes led to pitting corrosion of the underlying GaAs substrate. The dominant source of pinholes was the presence of atmospheric particulate matter on the GaAs surface during deposition of the a-TiO 2 layer. The pinhole density decreased substantially when the thickness of the a-TiO 2 coating increased beyond 45 nm, and approached zero when the thickness of the film exceeded 112 nm. The density of pinholes in films thinner than 45 nm decreased when the a-TiO 2 coating was deposited in an environmentally controlled cleanroom. Pinhole-free GaAs/a-TiO 2 devices were also tested via chronoamperometry to quantify the rate of pinhole formation during electrochemistry. The time-to-failure increased with thickness, suggesting that the failure mechanism may involve diffusion or migration through the film. However, other mechanisms may also contribute to the degradation of thicker films (>112 nm). Nevertheless, as previously hypothesized, extrinsic pinhole defects formed during deposition and testing control the short-term protective performance of the a-TiO 2 film for GaAs anodes evolving O 2 from water.

25 ENERGY STORAGE↗

In Situ Observations of Barium Sulfate Nucleation in Nanopores

In this work, the nucleation and growth of barium sulfate in nanoporous silica was investigated using in situ small-angle X-ray scattering and X-ray pair distribution function analysis, together with ex situ transmission and scanning transmission electron microscopy (TEM and STEM) imaging. We found that crystalline barite formation in micropores is likely preceded by a nonbulk barite phase in the nanopores, indicating a possible nonclassical nucleation pathway for barium sulfate under confinement. The nucleation of barium sulfate inside the nanopores stopped at ~12% of the pores filled and was seemingly limited by the formation of crystals near the exterior of the silica particles, which likely blocked subsequent solute transport into the interior of the nanopores. The growth rate of barium sulfate was fit using the Johnson–Mehl–Avrami–Kolmogorov equation and constrained using a growth rate of barite of ~1.0 × 10 –7 mol/m 2 /s, obtained from previous studies, but is consistent with TEM and STEM observations made here. The inferred nucleation rate of barium sulfate inside nanopores is estimated to be on the order of 1.0 × 10 9 nuclei/m 2 /s, which is 2 orders of magnitude higher than previous measurements on a planar silica substrate (~1.0 × 10 7 nuclei/m 2 /s). This implies that the ability of silica nanopores to promote barium sulfate nucleation is sufficiently high as to create a potentially self-limiting condition, where the nucleation reaction is shut down prematurely because rapid growth blocks reactant transport.

36 MATERIALS SCIENCE↗

XANES reflects coordination change and underlying surface disorder of zinc adsorbed to silica

In this work, zinc K -edge X-ray absorption near-edge structure (XANES) spectroscopy of Zn adsorbed to silica and Zn-bearing minerals, salts and solutions was conducted to explore how XANES spectra reflect coordination environment and disorder in the surface to which a metal ion is sorbed. Specifically, XANES spectra for five distinct Zn adsorption complexes (Zn ads ) on quartz and amorphous silica [SiO 2(am) ] are presented from the Zn–water–silica surface system: outer-sphere octahedral Zn ads on quartz, inner-sphere octahedral Zn ads on quartz, inner-sphere tetrahedral Zn ads on quartz, inner-sphere octahedral Zn ads on SiO 2(am) and inner-sphere tetrahedral Zn ads on SiO 2(am) . XANES spectral analysis of these complexes on quartz versus SiO 2(am) reveals that normalized peak absorbance and K -edge energy position generally decrease with increasing surface disorder and decreasing Zn–O coordination. On quartz, the absorption-edge energy of Zn ads ranges from 9663.0 to 9664.1 eV for samples dominated by tetrahedrally versus octahedrally coordinated species, respectively. On SiO 2(am) , the absorption-edge energy of Zn ads ranges from 9662.3 to 9663.4 eV for samples dominated by tetrahedrally versus octahedrally coordinated species, respectively. On both silica substrates, octahedral Zn ads presents a single K -edge peak feature, whereas tetrahedral Zn ads presents two absorbance features. The energy space between the two absorbance peak features of the XANES K -edge of tetrahedral Zn ads is 2.4 eV for Zn on quartz and 3.2 eV for Zn on SiO 2(am) . Linear combination fitting of samples with a mixture of Zn ads complex types demonstrates that the XANES spectra of octahedral and tetrahedral Zn ads on silica are distinct enough for quantitative identification. These results suggest caution when deciphering Zn speciation in natural samples via linear combination approaches using a single Zn ads standard to represent sorption on a particular mineral surface. Correlation between XANES spectral features and prior extended X-ray absorption fine structure (EXAFS) derived coordination environments for these Zn ads on silica samples provides insight into Zn speciation in natural systems with XANES compatible Zn concentrations too low for EXAFS analysis.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Zinc‐Imidazolate Films as an All‐Dry Resist Technology

Here, motivated by the drawbacks of solution phase processing, an all‐dry resist formation process is presented that utilizes amorphous zinc‐imidazolate (aZnMIm) films deposited by atomic/molecular layer deposition (ALD/MLD), patterned with electron beam lithography (EBL), and developed by novel low temperature (120 °C) gas phase etching using 1,1,1,5,5,5‐hexafluoroacetylacetone (hfacH) to achieve well‐resolved 22 nm lines with a pitch of 30 nm. The effects of electron beam irradiation on the chemical structure and hfacH etch resistance of aZnMIm films are investigated, and it is found that electron irradiation degrades the 2‐methylimidazolate ligands and transforms aZnMIm into a more dense material that is resistant to etching by hfacH and has a C:N:Zn ratio effectively identical to that of unmodified aZnMIm. These findings showcase the potential for aZnMIm films to function in a dry resist technology. Sensitivity, contrast, and critical dimensions of the patterns are determined to be 37 mC cm −2 , 0.87, and 29 nm, respectively, for aZnMIm deposited on silicon substrates and patterned at 30 keV. This work introduces a new direction for solvent‐free resist processing, offering the prospect of scalable, high‐resolution patterning techniques for advanced semiconductor fabrication processes.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Electrocatalytic cleavage of lignin model dimers using ruthenium supported on activated carbon cloth

Biomass lignin is the largest natural source of renewable aromatic compounds, creating an opportunity for its use as a feedstock provided that deconstruction and upgrading methods become available. Valorization of lignin is challenging because its complex structure is naturally recalcitrant to biological degradation. Deconstruction of this amorphous cross-linked polymer requires cleavage of aryl ether bonds, which account for more than half of the linkages between lignin's phenylpropanoid building blocks. High temperature cracking of lignin is possible via pyrolysis, but linkages such as 4-O-5 bonds are resistant to thermal degradation. Electrocatalytic hydrogenation offers a mild alternative; operated at low temperature and atmospheric pressure, it cleaves ether bonds while saturating aromatic rings with in situ generated hydrogen. To investigate the use of catalytic ruthenium supported on activated carbon cloth to cleave 4-O-5 bonds, model compounds that exhibit this linkage were selected, including 3-phenoxyphenol, 4-phenoxyphenol, 3-phenoxyanisole, and 3-phenoxytoluene. The two phenols, 3-phenoxyphenol and 4-phenoxyphenol, were cleaved and hydrogenated to form cyclohexanol. 3-Phenoxyanisole and 3-phenoxytoluene were also cleaved but with lower conversion rates and cyclohexanol yields. Alkaline electrolyte solutions showed the highest cyclohexanol yields for both substrates. Increasing substrate concentrations from 10 mM to 40 mM increased faradaic efficiency to 25%, while decreasing current density from 100 mA (33.33 mA cm -2 ) to 20 mA (6.67 mA cm -2 ) greatly improved the faradaic efficiency to 96%.

09 BIOMASS FUELS↗

Boride-Carbon Hybrid Technology to Produce Ultra-Wear and Corrosion Resistant Surfaces for Applications in Harsh Conditions (Final Technical Report)

Engineered functional surfaces play an important role to enable new products and manufacturing processes that can endure harsh service conditions such as high impact and contact loads, highly abrasive wear, extreme temperatures, and corrosive environments. Engineered surfaces can also be instrumental to improving the efficient use of energy by reducing frictional losses and extending service life. The main objective of this project was to develop a hybrid surface engineering technology that combines the advantages of a novel ultrafast boriding process with the next generation of superhard carbon coatings. The hypothesis was that this hybrid process will offer an unprecedented combination of wear and corrosion resistance, low frictional losses and affordability for treated parts so that it can be utilized in many applications. During this project, a duplex process was developed that combines the advantages of ultra-fast electrochemical boriding with those of hard tetrahedral amorphous carbon coatings. Both technologies can be combined to form a hybrid technology that is characterized by low friction and wear properties combined with corrosion and fatigue resistance. Good adhesion of both layers to each other was one main goal of this project, that has been achieved with HF1 adhesion through the Rockwell-C adhesion test. In this project, the mechanical properties of the hybrid coating were modeled through a finite-element analysis approach. We can conclude that the FEA model resembles the actual samples and be utilized to predict mechanical behavior under impacts. Based on this model, application-oriented load conditions can be simulated for optimal layer design regarding thickness and mechanical properties. To exemplify, one conclusion that can be drawn from the nanoindentation model is a boride layer thickness of 50 µm is sufficient to effectively support the carbon coating on the identified AISI 1045 low carbon steel substrate material. The duplex treatment yields wear rates as low as 6 x 10 -8 mm 3 N -1 m -1 and a coefficient of friction of 0.14 when tested against a steel counter face in a ball-on-disk test setup. On the other hand, the wear rate of the only-borided AISI 1045 steel was 5 x 10 -5 mm 3 N -1 m -1 , about three orders of magnitude higher than the duplex coating. At the same time, duplex treated samples experience corrosion resistance, which could not be achieved with single-layer carbon coatings. The developed surface treatment withstands a 3-hour exposure to 15% HCl, while the only carbon coated counter sample shows severe delamination of the coating due to pin hole corrosion. The boride layer is chemically stable and pin hole free because it is formed through an electrochemical process under high current densities (700 mA/cm 2 ) and high temperature. Additionally, the hybrid coating led to at least 3x increase in fatigue strength of the steel substrate, which exceeds the target performance of 30% improvement. There are numerous potential applications for the duplex coatings. A representative application is bearing ball coatings for off-shore windmills. Compared to currently employed surface technologies in this field, the initial costs of applying our technology might be higher due to more process steps but the performance benefits lead to an increased life time of treated parts, which will lower the maintenance and replacement costs in the long-term. To validate the technology for this specific application, the team is currently investigating the process of white etching crack initiation of the duplex coating in collaboration with ANL. Overall, this project successfully validated that the boride-carbon hybrid technology can withstand harsh conditions. One possible approach to commercialization under consideration is to transfer the technology to a startup or an existing coatings company.

36 MATERIALS SCIENCE↗

Nucleation and growth of molybdenum disulfide grown by thermal atomic layer deposition on metal oxides

To enable greater control over thermal atomic layer deposition (ALD) of molybdenum disulfide (MoS 2 ), here we report studies of the reactions of molybdenum hexafluoride (MoF 6 ) and hydrogen sulfide (H 2 S) with metal oxide substrates from nucleation to few-layer films. In situ quartz crystal microbalance experiments performed at 150, 200, and 250 °C revealed temperature-dependent nucleation behavior of the MoF 6 precursor, which is attributed to variations in surface hydroxyl concentration with temperature. In situ Fourier transform infrared spectroscopy coupled with ex situ x-ray photoelectron spectroscopy (XPS) indicated the presence of molybdenum oxide and molybdenum oxyfluoride species during nucleation. Density functional theory calculations additionally support the formation of these species as well as predicted metal oxide to fluoride conversion. Residual gas analysis revealed reaction by-products, and the combined experimental and computational results provided insights into proposed nucleation surface reactions. With additional ALD cycles, Fourier transform infrared spectroscopy indicated steady film growth after ~13 cycles at 200 °C. XPS revealed that higher deposition temperatures resulted in a higher fraction of MoS 2 within the films. Deposition temperature was found to play an important role in film morphology with amorphous films obtained at 200 °C and below, while layered films with vertical platelets were observed at 250 °C. Finally, these results provide an improved understanding of MoS 2 nucleation, which can guide surface preparation for the deposition of few-layer films and advance MoS 2 toward integration into device manufacturing.

36 MATERIALS SCIENCE↗

Fusion Blanket and Fuel Cycle Research at PNNL: FY22 Year-end Report

During the reporting period, research at PNNL focused on two tasks within the DOE Fusion Blanket and Fuel Cycle Program. Research on Task 1, Tritium Extraction from Pb-Li and He Using a Vacuum Permeator, focused on atomistic modeling to better understand tritium transport in Pd-coated V vacuum permeators. As a lower cost alternative to Pd permeators, thin coatings of Pd (or other noble metals) can be deposited over a substrate like V. However, the permeation performance of composite metal membranes degrades over time, due to the formation of intermetallics at the coating-substrate interface. Computational studies were performed to better understand tritium transport through these Pd-V intermetallics. The results of the FY22 Pd-V modeling study were recently submitted for publication in Computational Materials Science and presented at the Technology of Fusion Energy conference. Future work in this area will focus on interdiffusion barriers to prevent intermetallic formation that is deleterious to tritium transport. There are opportunities for collaboration with researchers at the Colorado School of Mines, who are manufacturing and testing candidate interdiffusion barriers. Research on Task 3, Solid Breeder Materials, included ion irradiation and post-irradiation characterization of lithium orthosilicate (Li 4 SiO 4 ) and lithium metasilicate (Li 2 SiO 3 ) to improve fundamental understanding of irradiation effects, in combination with atomistic modeling focused on the energetics of He clustering in these two ceramic phases. The results of the study suggested that the Li 4 SiO 4 phase, which is more desirable as a solid breeder due to its higher Li density, was amorphized during ion irradiation while the Li 2 SiO 3 phase appeared to be more resistant to irradiation damage. It is possible that Li loss contributed to the poor irradiation performance of the Li 4 SiO 4 , and some thoughts are provided regarding coatings that could be applied to solid breeders like this to prevent Li loss at elevated temperature while not hindering tritium diffusion. The results of the FY22 ion irradiation study were recently submitted for publication in Journal of Nuclear Materials and presented at the 22nd International Conference on Ion Beam Modification of Materials. Future work in this area will focus on Li-rich ceramics such as Li 5 AlO 4 and Li 8 ZrO 6 that have high Li density and should provide rapid tritium release based on previous work with less Li-rich ceramics.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Controlling Structure and Properties of Vapor-Deposited Glasses of Organic Semiconductors: Recent Advances and Challenges

The past decade has seen great progress in manipulating the structure of vapor-deposited glasses of organic semiconductors. Upon varying the substrate temperature during deposition, glasses with a wide range of density and molecular orientation can be prepared from a given molecule. Here, we review recent studies that show the structure of vapor-deposited glasses can be tuned to significantly improve the external quantum efficiency and lifetime of organic light-emitting diodes (OLEDs). We highlight the ability of molecular simulations to reproduce experimentally observed structures, setting the stage for in silico design of vapor-deposited glasses in the coming decade. Finally, we identify research opportunities for improving the properties of organic semiconductors by controlling the structure of vapor-deposited glasses.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Exploiting Saturation Regimes and Surface Effects to Tune Composite Design: Single Platelet Nanocomposites of Peptoid Nanosheets and CaCO 3

Mineral-polymer composites found in nature exhibit exceptional structural properties essential to their function, and transferring these attributes to the synthetic design of functional materials holds promise across various sectors. Biomimetic fabrication of nanocomposites introduces new pathways for advanced material design and explores biomineralization strategies. This study presents a novel approach for producing single platelet nanocomposites composed of CaCO 3 and biomimetic peptoid (N-substituted glycines) polymers, akin to the bricks found in the brick-and-mortar structure of nacre, the inner layer of certain mollusc shells. The significant aspect of the proposed strategy is the use of organic peptoid nanosheets as the scaffolds for brick formation, along with their controlled mineralization in solution. Here, we employ the B28 peptoid nanosheet as a scaffold, which readily forms free-floating zwitterionic bilayers in aqueous solution. The peptoid nanosheets were mineralized under consistent initial conditions (σ calcite = 1.2, pH 9.00), with variations in mixing conditions and supersaturation profiles over time aimed at controlling the final product. Nanosheets were mineralized in both feedback control experiments, where supersaturation was continuously replenished by titrant addition and in batch experiments without a feedback loop. Complete coverage of the nanosheet surface by amorphous calcium carbonate was achieved under specific conditions with feedback control mineralization, whereas vaterite was the primary CaCO 3 phase observed after batch experiments. Thermodynamic calculations suggest that time-dependent supersaturation profiles as well as the spatial distribution of supersaturation are effective controls for tuning the mineralization extent and product. We anticipate that the control strategies outlined in this work can serve as a foundation for the advanced and scalable fabrication of nanocomposites as building blocks for nacre-mimetic and functional materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ferroelectric Al1 − xBxN thin films integrated on Si

Ferroelectric Al0.93B0.07N thin films are prepared (100) Si substrates. The necessary c-axis out-of-plane orientation to observe macroscopic ferroelectric switching was achieved by implementing an initial Ar/N2 plasma treatment, followed by a thin layer of AlN to initiate the desired texture and a 150 nm W layer. The plasma treatment facilitates crystallinity enhancement of the AlN template layer, allowing for subsequent growth of highly oriented W and Al0.93B0.07N layers. The W layer exhibits random in-plane orientation and exclusive (110) out-of-plane orientation with a rocking curve width of 1.4°. When grown on these W surfaces, 175 nm thick Al0.93B0.07N films exhibit random in-plane orientation and exclusive (001) texture with rocking curve full-width-half-max values of 1.6° and RMS roughness values less than 1 nm. Polarization hysteresis measurements show robust hysteresis with coercive field values of 5.4 MV/cm and remanent polarization values of 136 μC/cm2. XPS depth profile analysis suggests that the plasma treatment converts the existing native oxide to a nitrogen rich oxynitride with approximate composition Si3O0.5N3.67. Cross-sectional TEM reveals that the oxynitride interlayer is amorphous and ∼3.4 nm thick, more than double the native oxide thickness measured by multiwavelength ellipsometry, implying that (oxy)nitride growth continues after conversion of the native oxide. This new family of ferroelectric wurtzites is interesting from an integration perspective given their chemical compatibility with mainstream semiconductors. Developing synthesis routes that promote needed texture while preserving compatible processing windows is an important step toward practical integration.

Physics↗

Investigating Single-Molecule Fluorescence Spectral Heterogeneity of Rhodamines Using High-Throughput Single-Molecule Spectroscopy

We experimentally investigated several intra-molecular coordinate and environmental changes as potential causes of single-molecule fluorescence spectral heterogeneities (smFSH). Here, we developed a high-throughput single-molecule spectroscopy technique to analyze more than 5,000 single-molecule emission spectra from each of nine commonly used fluorophores with different structural rigidities deposited on substrates with different polarities. We observed an unexpected high smFSH from structurally rigid Rhodamine B compared with a structurally flexible Cyanine dye - Alexa Fluor 647. Based on experimentally measured smFSH, we ruled out the system’s noise uncertainty, single-molecule spectral diffusion, and environmental polarity as the primary causes of the high smFSH. We found that the rotational flexibility of N, N-dialkylated groups contributed to the smFSH. With the high smFSH observed in structurally more rigid model fluorophores, we speculated that other intra-molecular coordinate and environmental changes might also contribute to the high smFSH in Rhodamines.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ultrathin silicon oxide prepared by in-line plasma-assisted N 2 O oxidation (PANO) and the application for n-type polysilicon passivated contact

We develop a plasma-assisted nitrous-oxide (N 2 O) gas oxidation (PANO) method to prepare the ultrathin silicon oxide (SiO x ) for polysilicon (poly-Si) passivated contact. The effects of preparation conditions, including the substrate temperature, processing time, and plasma power, are studied. Afterwards, we integrate the PANO SiO x into the polysilicon passivated contact and optimize the passivation and contact performances. Excellent surface passivation with the n-type poly-Si and PANO SiO x on the n-type c-Si wafer is achieved by 880 °C annealing, which shows competitive passivation quality to the one with NASO SiO x . Champion implied open-circuit voltage (iV oc ) and single-sided recombination saturated current (J 0 ) reach 730 mV and 4.3 fA/cm 2 after crystallization; and they are further improved to 747 mV and 2.0 fA/cm 2 (3 × 10 15 cm -3 ) after subsequent AlO x /SiN x hydrogenation. Using transmission electron microscopy (TEM), we find that the thickness of PANO SiO x ranges 1.1–2.4 nm and the controlled nitric acid oxidized SiO x (NAOS) ranges 1.3–1.8 nm. The contact resistivity (ρ c ) is typically <10 mΩ cm 2 with the annealing temperature of >820 °C. Also, the crystallinity, phosphorous in-diffusion profile, and current-leaking density of the passivated contacts are investigated. In general, the PANO SiO x and in-situ doping amorphous silicon precursor can be fabricated in one PECVD system without additional equipment or transfer procedures, which is favorable for the high-efficiency, low-cost industrial manufacture.

14 SOLAR ENERGY↗

Surface Equilibration Mechanism Controls the Stability of a Model Codeposited Glass Mixture of Organic Semiconductors

While previous work has identified the conditions for preparing ultrastable single-component organic glasses by physical vapor deposition (PVD), little is known about the stability of codeposited mixtures. Here, we prepared binary PVD glasses of organic semiconductors, TPD (N,N'-Bis(3-methylphenyl)-N,N'-diphenylbenzidine) and m-MTDATA (4,4',4"-Tris[phenyl(m-tolyl)amino]triphenylamine), with a 50:50 mass concentration over a wide range of substrate temperatures (T sub ). The enthalpy and kinetic stability are evaluated with differential scanning calorimetry and spectroscopic ellipsometry. Binary organic semiconductor glasses with exceptional thermodynamic and kinetic stability comparable to the most stable single-component organic glasses are obtained when deposited at T sub = 0.78–0.90T g (where T g is the conventional glass transition temperature). When deposited at 0.94T g , the enthalpy of the m-MTDATA/TPD glass equals that expected for the equilibrium liquid at that temperature. Thus, the surface equilibration mechanism previously advanced for single-component PVD glasses is also applicable for these codeposited glasses. Furthermore, these results provide an avenue for designing high-performance organic electronic devices.

36 MATERIALS SCIENCE↗

High-Throughput In-Line Deposition of Silicon Oxide for Polycrystalline Silicon Passivating Contacts

Polycrystalline silicon passivating contacts rely on an ultrathin (1–2 nm) silicon oxide layer to minimize recombination at the wafer/oxide interface and regulate dopant diffusion. Traditionally formed by thermal or chemical oxidation, this oxide is herein replaced by silicon oxide deposited via aerosol impact-driven assembly (AIDA), enabling high wafer-per-hour throughput and precise thickness control. In this study, we show that AIDA coatings conformally cover planar or textured substrates and achieve a SiO x /poly-Si(n) structure with an implied open-circuit voltage (iV oc = 726 mV) and contact saturation current density (J 0 = 8.8 fA/cm 2 ). Furthermore, annealing AIDA SiO x films at elevated temperatures desorbs hydroxyl groups while the stoichiometry transitions toward SiO 2 , improving passivation quality. Together, these results highlight AIDA’s potential for scalable, high-throughput manufacturing of advanced passivating contacts, offering a cost-effective alternative to conventional low-pressure chemical vapor deposition and plasma-enhanced chemical vapor deposition-based silicon and oxide processes.

TOPcon↗

Discovery of a Hybrid System for Photocatalytic CO 2 Reduction via Attachment of a Molecular Cobalt-Quaterpyridine Complex to a Crystalline Carbon Nitride

While recent reports have demonstrated the attachment of molecular catalysts to amorphous, graphitic carbon nitrides (g-CN) for light-driven CO 2 reduction, approaches to the utilization of crystalline carbon nitrides have remained undiscovered. Herein, a functional hybrid photocatalyst system has been found using a crystalline carbon nitride semiconductor, poly(triazine imide) lithium chloride (PTI-LiCl), with a surface-attached CoCl 2 (qpy-Ph-COOH) catalyst for CO 2 reduction. The molecular catalyst attaches to PTI-LiCl at concentrations from 0.10 to 4.30 wt % and exhibits ∼96% selectivity for CO production in a CO 2 -saturated, aqueous 0.5 M KHCO 3 solution. Optimal loadings were found to be within 0.42–1.04 wt % with rates between 1,400 and 1,550 μmol CO/g·h at an irradiance of 172 mW/cm 2 (λ = 390 nm) and apparent quantum yields of ∼2%. This optimized loading is postulated to represent a balance between maximal turnover frequency (TOF; 300+ h –1 ) and excess catalyst that can limit excited-electron lifetimes, as probed via transient absorption spectroscopy. An increase in the incident irradiance yields a concomitant increase in the TOFs and CO rates only for the higher catalyst loadings, reaching up to 2,149 μmol CO/g·h with a more efficient use of the catalyst surface capacity. The lower catalyst loadings, by comparison, already function at maximal TOFs. Higher surface loadings are also found to help mitigate deactivation of the molecular catalysts during extended catalytic testing (>24 h) owing to the greater net surface capacity for CO 2 reduction, thus representing an effective strategy to extend lifetime. The hybrid particles can be deposited onto an FTO substrate to yield ∼60% Faradaic efficiency for photoelectrochemical CO production at −1.2 V vs Ag/AgCl bias. In conclusion, these results demonstrate the synergistic combination of a crystalline carbon nitride with a molecular catalyst that achieves among the highest known rates in carbon-nitride systems for the light-driven CO 2 reduction to CO in aqueous solution with >95% selectivity.

CO2 reduction↗