Search NASA⌕ Search

SEARCH · Search NASA

Results for “tensile behavior”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Tensile Creep and Stress-rupture Behavior of Polymer Derived Sic Fibers

Tensile creep and stress-rupture studies were conducted on polymer derived Nicalon, Hi-Nicalon, and SiC/BN-coated Nicalon SiC fibers. Test conditions were temperatures from 1200 to 1400 C, stresses from 100 to 1600 MPa, stress application times up to 200 hours, and air, argon, and vacuum test environments. For all fibers, creep occurred predominantly in the primary stage. Hi-Nicalon had much higher 0.2 and 1 percent creep strengths than as-produced as well as-coated Nicalon fibers. The stress-rupture strength of Hi-Nicalon up to 100 hours was also higher than that of the coated and as-produced Nicalon fibers. SiC/BN coating on Nicalon increased only the short-term low-temperature rupture strength. Limited testing in argon and vacuum suggests that for all fiber types, creep and rupture resistances are reduced in comparison to the results in air. Possible mechanisms for the observed behavior are discussed.

Yun, H. M.↗

Tensile and creep rupture behavior of P/M processed Nb-base alloy, WC-3009

Due to its high strength at temperatures up to 1600 K, fabrication of niobium base alloy WC-3009 (Nb30Hf9W) by traditional methods is difficult. Powder metallurgy (P/M) processing offers an attractive fabrication alternative for this high strength alloy. Spherical powders of WC-3009 produced by electron beam atomizing (EBA) process were successfully consolidated into a one inch diameter rod by vacuum hot pressing and swaging techniques. Tensile strength of the fully dense P/M material at 300-1590 K were similar to the arc-melted material. Creep rupture tests in vacuum indicated that WC-3009 exhibits a class 1 solid solution (glide controlled) creep behavior in the 1480 to 1590 K temperature range and stress range of 14 to 70 MPa. The creep behavior was correlated with temperature and stress using a power law relationship. The calculated stress exponent n, was about 3.2 and the apparent activation energy, Q, was about 270 kJ/mol. The large creep ductility exhibited by WC-3009 was attributed to its high strain rate sensitivity.

Hebsur, Mohan G.↗

Effect of Specimen Thickness on Mechanical Behavior of SiC/SiC Composites

Potential composite applications in aerospace and transportation application systems have different thickness requirements. For example, space applications such as nozzle ramps or heat exchangers use very thin (less than 1 mm) structures whereas turbine blades need very thick parts greater than or equal to cm). There has been little investigation into the effect of thickness on stress-strain behavior or elevated temperature tensile properties controlled by oxidation. In this study, composites consisting of woven Hi-NicalonTM fibers, a carbon interphase, and CVI Sic matrix were fabricated with different numbers of plies to provide variable thickness. The composites ranged from a single ply (approximately 0.4 mm) to thirty-six plies (approximately 1 cm). Tensile tests were performed at room temperature with acoustic emission used to monitor matrix crack behavior. Elevated temperature tensile stress-rupture tests were performed in air. Considerably different room and elevated temperature tensile behavior was observed that will be discussed with respect to the effect of thickness on matrix crack formation, matrix crack growth and oxidation diffusion kinetics.

Morscher, Gregory N.↗

Deformation and fracture behavior of a laser powder bed fusion processed stainless steel: In situ synchrotron x-ray computed microtomography study

Tensile plastic deformation and fracture behavior of a laser powder bed fusion processed 316L stainless steel alloy was investigated in situ using high-resolution synchrotron x-ray computed microtomography (sXCT). Three different cases were studied: (1) specimen A1, near full-density with initial porosity of 0.04%, (2) specimen B1, initial lack-of-fusion (LOF) porosity of about 3% with the major axis of defects aligned nearly perpendicular to the tensile loading direction (LD), and (3) specimen B, similar to B1 but with the major axis of LOF defects aligned nearly parallel to LD. The effects of type, density, and orientation of defects in as-printed samples on plastic deformation and failure modes were studied by analyzing sXCT image sequences and quantitative defect properties. Specifically, the evolutions of porosity, size, aspect ratio, and angle of gas pores and LOF defects were characterized as a function of applied strain. Moreover, interactions between as-printed defects and deformation-induced crack propagation were investigated. The tensile behavior of specimen A1 was comparable to that of a commercial wrought plate. Furthermore, the quantitative in-situ sXCT results showed a void-growth phenomenon in A1 but without noticeable coalescence, resulting in a ductile cup-cone failure. Specimen B1 showed damage-driven brittle failure with limited plasticity due to early and rapid propagation of open voids. On the other hand, specimen B, with a similar amount of LOF defects as B1, showed deceivingly strong and ductile tensile behavior similar to A1 without any major crack propagations due to the favorable orientation relationship between LOF defects and the LD.

36 MATERIALS SCIENCE↗

The effect of hydrogen on the deformation behavior of a single crystal nickel-base superalloy

The effect of hydrogen on the tensile deformation behavior of PWA 1480 is presented. Tensile tests were interrupted at different plastic strain levels to observe the development of the dislocation structure. Transmission electron microscopy (TEM) foils were cut perpendicular to the tensile axis to allow the deformation of both phases to be simultaneously observed as well as parallel to zone axes (III) to show the superdislocations on their slip planes. Similar to other nickel-base superalloys, hydrogen was detrimental to the room temperature tensile properties of PWA 1480. There was little effect on strength, however the material was severely embrittled. Even without hydrogen, the elongation-to-failure was only approximately 3 percent. The tensile fracture surface was made up primarily of ductile voids with regions of cleavage fracture. These cleavage facets are the eutectic (gamma') in the microstructure. It was shown by quantitative fractography that hydrogen embrittles the eutectic (gamma') and causes the crack path to seek out and fracture through the eutectic (gamma'). There was two to three times the amount of cleavage on the fracture surface of the hydrogen-charged samples than on the surface of the uncharged samples. The effect of hydrogen can also be seen in the dislocation structure. There is a marked tendency for dislocation trapping in the gamma matrix with and without hydrogen at all plastic strain levels. Without hydrogen there is a high dislocation density in the gamma matrix leading to strain exhaustion in this region and failure through the matrix. The dislocation structure at failure with hydrogen is slightly different. The TEM foils cut parallel to zone axes (III) showed dislocations wrapping around gamma precipitates. Zone axes (001) foils show that there is a lower dislocation density in the gamma matrix which can be linked to the effects of hydrogen on the fracture behavior. The primary activity in the gamma precipitates is in the form of superlattice intrinsic stacking faults (SISFs). These faults have also been reported in other ordered alloys and superalloys.

Walston, W. S.↗

Effect of tensile mean stress on fatigue behavior of single-crystal and directionally solidified superalloys

Two nickel base superalloys, single crystal PWA 1480 and directionally solidified MAR-M 246 + Hf, were studied in view of the potential usage of the former and usage of the latter as blade materials for the turbomachinery of the Space Shuttle main engine. The baseline zero mean stress (ZMS) fatigue life (FL) behavior of these superalloys was established, and then the effect of tensile mean stress (TMS) on their FL behavior was characterized. A stress range based FL prediction approach was used to characterize both the ZMS and TMS fatigue data. In the past, several researchers have developed methods to account for the detrimental effect of tensile mean stress on the FL for polycrystalline engineering alloys. These methods were applied to characterize the TMS fatigue data of single crystal PWA 1480 and directionally solidified MAR-M 246 + Hf and were found to be unsatisfactory. Therefore, a method of accounting for the TMS effect on FL, that is based on a technique proposed by Heidmann and Manson was developed to characterize the TMS fatigue data of these superalloys. Details of this method and its relationship to the conventionally used mean stress methods in FL prediction are discussed.

Kalluri, Sreeramesh↗

Effect of tensile mean stress on fatigue behavior of single-crystal and directionally solidified superalloys

Two nickel base superalloys, single crystal PWA 1480 and directionally solidified MAR-M 246 + Hf, were studied in view of the potential usage of the former and usage of the latter as blade materials for the turbomachinery of the space shuttle main engine. The baseline zero mean stress (ZMS) fatigue life (FL) behavior of these superalloys was established, and then the effect of tensile mean stress (TMS) on their FL behavior was characterized. At room temperature these superalloys have lower ductilities and higher strengths than most polycrystalline engineering alloys. The cycle stress-strain response was thus nominally elastic in most of the fatigue tests. Therefore, a stress range based FL prediction approach was used to characterize both the ZMS and TMS fatigue data. In the past, several researchers have developed methods to account for the detrimental effect of tensile mean stress on the FL for polycrystalline engineering alloys. However, the applicability of these methods to single crystal and directionally solidified superalloys has not been established. In this study, these methods were applied to characterize the TMS fatigue data of single crystal PWA 1480 and directionally solidified MAR-M 246 + Hf and were found to be unsatisfactory. Therefore, a method of accounting for the TMS effect on FL, that is based on a technique proposed by Heidmann and Manson was developed to characterize the TMS fatigue data of these superalloys. Details of this method and its relationship to the conventionally used mean stress methods in FL prediction are discussed.

Kalluri, Sreeramesh↗

Tensile stress-strain behavior of hybrid composite laminates

A study was made of the stress-strain response of several hybrid laminates, and the damage was correlated with nonlinear stress-strain response and ultimate strength. The fibers used in the laminates were graphite, S-glass, and Kevlar. Some laminates with graphite fibers had perforated Mylar film between plies, which lowered the interlaminar bond strength. The laminate configurations were chosen to be like those of buffer strips in large panels and fracture coupons. Longitudinal and transverse specimens were loaded in tension to failure. Some specimens were radiographed to reveal damage due to edge effects. Stress-strain response is discussed in terms of damage shown by the radiographs. Ultimate strengths are compared with simple failure criteria, one of which account for damage.

Kennedy, J. M.↗

Effects of Thermal Treatment on Tensile Creep and Stress-Rupture Behavior of Hi-Nicalon SiC Fibers

Tensile creep and stress-rupture studies were conducted on Hi-Nicalon SiC fibers at 1200 and 1400 C in argon and air. Examined were as-received fibers as well as fibers annealed from 1400 to 1800 C for 1 hour in argon before testing. The creep and rupture results for these annealed fibers were compared to those of the as-received fibers to determine the effects of annealing temperature, test temperature, and test environment. Argon anneals up to 1500 C degrade room temperature strength of Hi-Nicalon fibers, but improve fiber creep resistance in argon or air by as much as 100% with no significant degradation in rupture strength. Argon anneals above 1500 C continue to improve fiber creep resistance when tested in argon, but significantly degrade creep resistance and rupture strength when tested in air. Decrease in creep resistance in air is greater at 1200 C than at 1400 C. Mechanisms are suggested for the observed behavior.

Yun, H. M.↗

Tensile and stress-rupture behavior of hafnium carbide dispersed molybdenum and tungsten base alloy wires

The tensile strain rate sensitivity and the stress-rupture strength of Mo-base and W-base alloy wires, 380 microns in diameter, were determined over the temperature range from 1200 K to 1600 K. Three molybdenum alloy wires; Mo + 1.1w/o hafnium carbide (MoHfC), Mo + 25w/o W + 1.1w/o hafnium carbide (MoHfC+25W) and Mo + 45w/o W + 1.1w/o hafnium carbide (MoHfC+45W), and a W + 0.4w/o hafnium carbide (WHfC) tungsten alloy wire were evaluated. The tensile strength of all wires studied was found to have a positive strain rate sensitivity. The strain rate dependency increased with increasing temperature and is associated with grain broadening of the initial fibrous structures. The hafnium carbide dispersed W-base and Mo-base alloys have superior tensile and stress-rupture properties than those without HfC. On a density compensated basis the MoHfC wires exhibit superior tensile and stress-rupture strengths to the WHfC wires up to approximately 1400 K. Addition of tungsten in the Mo-alloy wires was found to increase the long-term stress rupture strength at temperatures above 1400 K. Theoretical calculations indicate that the strength and ductility advantage of the HfC dispersed alloy wires is due to the resistance to recrystallization imparted by the dispersoid.

Yun, Hee Mann↗

Recrystallization driven softening and heating rate dependencies of FeCrAl nuclear fuel cladding during accident transients

A refined understanding of FeCrAl cladding behavior during rapid transients is critical for its potential deployment in light-water reactors. Current assessments focus on transient burst testing metrics such as balloon geometry, burst temperature, and hoop stress, often used as proxies for simpler conventional tensile properties. However, directly correlating isothermal tensile and creep data with accident transient scenarios remains a challenge, although it is essential for high fidelity model development. Recent modeling based on tensile tests up to 800 °C, conducted with both immediate loading and a 10-minute soak, showed that immediate loading better predicts experimental burst temperatures, indicating a thermal softening effect. Building upon this observation, the current study connects transient performance, microstructural evolution, and high-temperature tensile properties by leveraging results from C26M claddings burst tests performed at heating rates of 1–50 °C/s and hoop stresses from 25 to 100 MPa. At 25 MPa, rupture temperatures varied by only 6 °C, but at 100 MPa, the difference reached 116 °C, with faster heating yielding higher burst temperatures. Microstructural analysis identified recrystallization as the primary cause of heating rate-dependent softening, eliminating prior cold-working. In-situ thermomechanical data linked ballooning onset to localized instabilities, similar to ultimate tensile strength behavior in conventional tensile tests. High heating rates correlated with immediate loading tensile data, while lower rates matched soaked data. Furthermore, by linking burst performance to microstructural evolution and tensile properties, this work provides a foundation for more accurate modeling of FeCrAl claddings and potentially other Fe-based materials under accident conditions.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Tensile creep and creep-recovery behavior of a SiC-fiber-Si3N4-matrix composite

The tensile creep and creep-recovery behavior of a hot-pressed unidirectional SiC-fiber/Si3N4-matrix composite was investigated at 1200 C in air, in order to determine how various sustained and cyclic creep loading histories would influence the creep rate, accumulated creep strain, and the amount of strain recovered upon specimen unloading. The data accumulated indicate that the fundamental damage mode for sustained tensile creep at stresses of 200 and 250 MPa was periodic fiber fracture and that the creep life and the failure mode at 250 MPa were strongly influenced by the rate at which the initial creep stress was applied. Cyclic loading significantly lowered the duration of primary creep and the overall creep-strain accumulation. The implications of the results for microstructural and component design are discussed.

Holmes, John W.↗

Low strain, long life creep fatigue of AF2-1DA and INCO 718

Two aircraft turbine disk alloys, GATORIZED AF2-DA and INCO 718 were evaluated for their low strain long life creep-fatigue behavior. Static (tensile and creep rupture) and cyclic properties of both alloys were characterized. The cntrolled strain LCF tests were conducted at 760 C (1400 F) and 649 C (1200 F) for AF2-1DA and INCO 718, respectively. Hold times were varied for tensile, compressive and tensile/compressive strain dwell (relaxation) tests. Stress (creep) hold behavior of AF2-1DA was also evaluated. Generally, INCO 718 exhibited more pronounced reduction in cyclic life due to hold than AF2-1DA. The percent reduction in life for both alloys for strain dwell tests was greater at low strain ranges (longer life regime). Changing hold time from 0 to 0.5, 2.0 and 15.0 min. resulted in corresponding reductions in life. The continuous cycle and cyclic/dwell initiation failure mechanism was predominantly transgranular for AF2-1DA and intergranular for INCO 718.

Thakker, A. B.↗

Preliminary report on tests of tensile specimens with a part-through surface notch for a filament wound graphite/epoxy material

The behavior of tensile coupons with surface notches of various semi-elliptical shapes were evaluated for specimens obtained from a filament wound graphite/epoxy cylinder. The quasi-static test results, in some instances, are inadequate for defining complete trend curves and the interpretive analysis is considered to be preliminary. Specimens with very shallow notches were observed to be notch insensitive and the unnotched strength from these specimens was determined to be 54.97 Ksi. The failure strain of the laminate was found to be 1.328%. Specimens with deeper notches were sensitive to notch depth, notch aspect ratio, and specimen width. Using the unnotched strength of 54.97 Ksi and Poe's general toughness parameter, the fracture toughness was estimated to be 27.2 Ksi square root of In. Isotropic linear elastic fracture mechanics together with the estimated fracture toughness correctly predicted the influence of notch depth, aspect ratio, and specimen finitewidth.

Harris, C. E.↗

Influence of copper content on the high temperature tensile and low cycle fatigue behavior of cast Al-Cu-Mn-Zr alloys

The relationship between low cycle fatigue (LCF) and monotonic tensile fracture strain was investigated for cast Al-Cu-Mn-Zr alloys containing 6 and 9 wt% Cu at 250 °C. The 9% Cu alloy consisted of larger size and volume fraction of brittle intermetallic grain boundary particles that fractured during tensile tests to reduce the fracture strain by 50% compared to the 6% Cu alloy. We found that LCF life was similar between the two alloys and weakly influenced by the particles. LCF life and fracture strain were poorly correlated due to the dominant influence of particles on monotonic tensile crack but not on fatigue crack.

36 MATERIALS SCIENCE↗