Search NASA⌕ Search

SEARCH · Search NASA

Results for “tungsten”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Dual-Band Electrochromism in Hydrous Tungsten Oxide

The independent modulation of visible and near-infrared light by a single material, termed dualband electrochromism, is highly desirable for smart windows to enhance the energy efficiency of buildings. Tungsten oxides are commercially important electrochromic materials, exhibiting reversible visible and near-infrared absorption when electrochemically reduced in an electrolyte containing small cations or protons. The presence of structural water in tungsten oxides has been associated with faster electrochromic switching speeds. Here, we find that WO 3 ·H 2 O, a crystalline hydrate, exhibits dual-band electrochromism unlike the anhydrous WO 3 providing a heretofore unexplored route to tune the electrochromic response of tungsten oxides. Absorption of near-infrared light is achieved at low Li + /e - injection, followed by the absorption of visible light at higher Li + /e - injection as a result of an electrochemically-induced phase transition. We propose that this dual-band modulation is possible due to the more open structure of WO 3 ·H 2 O as compared to WO 3 . This facilitates a more extended solid solution Li + insertion regime that benefits the modulation of near-infrared radiation via plasmon absorption. Higher degrees of Li + /e - insertion lead to polaronic absorption associated with localized charge storage. Furthermore, these results inform how structural factors influence the electrochemically induced spectral response of transition metal oxides and the important role of structural water beyond optical switching speed.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Tungsten-dioxo single-site heterogeneous catalyst on carbon: synthesis, structure, and catalysis

This study investigates the application of a novel third-row metal, tungsten, to carbon-supported single-site metal-oxo heterogeneous catalysis. Tungsten is a green and earth-abundant metal, but an unexplored candidate in this role. The carbon (AC = activated carbon)-supported tungsten dioxo complex, AC/WO 2 was prepared via grafting of (DME)WO 2 Cl 2 (DME = 1,2-dimethoxyethane) onto high-surface-area activated carbon. AC/WO 2 was fully characterized by ICP-OES, XPS, EXAFS, XANES, SMART-EM, and DFT. W 4d 7/2 XPS and W L III -Edge XANES assign the oxidation state as W(VI), while EXAFS reveals two W=O double and two W–O single bonds at distances of 1.73 and 1.92 Å, respectively. These data align well with DFT computational results, supporting the structure as Carbon(–μ-O–) 2 M(=O) 2 . SMART-EM verifies that single W(VI) catalytic sites are bonded in an out-of-plane manner. The catalytic performance of air- and water-stable AC/WO 2 is compared to that of AC/MoO 2 . AC/WO 2 is more active and selective than the molybdenum analog in mediating alcohol dehydration of various substrates, and is recyclable. Notably, AC/WO 2 is an effective and recyclable catalyst for primary aliphatic alcohol dehydration and forms no dehydrogenation side products in contrast to AC/MoO 2 . However, AC/WO 2 is less effective in epoxidation and PET depolymerization. Overall, this work demonstrates the potential of carbon-supported third row metals for future studies.

02 PETROLEUM↗

Non-dilute helium-related defect interactions in the near-surface region of plasma-exposed tungsten

We report a systematic energetic analysis of helium-related defect interactions that mediate helium (He) segregation on surfaces of plasma-exposed tungsten at different levels of He ion implantation. We focus on high He fluences that increase the He content in the plasma-exposed material well beyond the dilute limit of He concentration and employ atomic configurations generated by large-scale molecular dynamics simulations of He-implanted tungsten. We perform systematic molecular statics computations of cluster– defect interaction energetics in the highly defect-rich near-surface region of plasma-exposed tungsten for small mobile helium clusters as a function of the cluster distance from the surface. In this region, mobile clusters are also subjected to the stress fields generated by defects such as helium bubbles and other clusters, which govern cluster–defect interactions in addition to the cluster–surface interaction. Based on systematic investigation of individual cluster–defect interactions, we develop a mathematical framework to describe the interaction energy landscapes consisting of elastic interaction potential perturbations to finite-width square-well potentials, where the potential well accounts for cluster trapping by the defect at close range and subsequent coalescence and the perturbation potential is parameterized according to elastic inclusion theory. Superposition of all the relevant interaction potentials provides a comprehensive description of the interaction energy landscape that would be experienced by a small mobile cluster along its migration path toward the plasma-exposed surface at high He fluence. Such descriptions are particularly important for developing atomistically-informed, hierarchical multi-scale models of helium cluster dynamics in plasma-facing materials.

36 MATERIALS SCIENCE↗

Divertor detachment and heat exhaust mitigation control in KSTAR with tungsten divertor

KSTAR has recently undergone an upgrade to use a new tungsten divertor to run experiments in ITER-relevant scenarios. Even with a high melting point of tungsten, it is important to control the heat flux impinging on tungsten divertor targets to minimize sputtering and contamination of the core plasma. Heat flux on the divertor is often controlled by increasing the degree of detachment of scrape-off layer plasma from the target plates. In this work, we have demonstrated successful divertor detachment and heat exhaust dissipation control experiments using two different methods. The first method uses attachment fraction as a control variable which is estimated using ion saturation current measurements from embedded Langmuir probes in the divertor. The second method uses a novel machine-learning-based surrogate model of 2D UEDGE simulation database, DivControlNN. We demonstrated running inference operation of DivControlNN in realtime to estimate heat flux at the divertor and use it as the control variable in a feedback loop with impurity gas flow. We present interesting insights from these experiments including a systematic approach to tuning controllers and discuss future improvements in the control infrastructure and control variables for future burning plasma experiments.

KSTAR tungsten divertor operations↗

A First-Principles Study of the Structural and Thermo-Mechanical Properties of Tungsten-Based Plasma-Facing Materials

Tungsten (W) and tungsten alloys are being considered as leading candidates for structural and functional materials in future fusion energy devices. The most attractive properties of tungsten for the design of magnetic and inertial fusion energy reactors are its high melting point, high thermal conductivity, low sputtering yield, and low long-term disposal radioactive footprint. Despite these relevant features, there is a lack of understanding of how the structural and mechanical properties of W-based alloys are affected by the temperature in fusion power plants. In this work, we present a study on the thermo-mechanical properties of five W-based plasma-facing materials. First-principles density functional theory (DFT) calculations are combined with the quasi-harmonic approximation (QHA) theory to investigate the electronic, structural, mechanical, and thermal properties of these W-based alloys as a function of temperature. The coefficient of thermal expansion, temperature-dependent elastic constants, and several elastic parameters, including bulk and Young’s modulus, are calculated. Our work advances the understanding of the structural and thermo-mechanical behavior of W-based materials, thus providing insights into the design and selection of candidate plasma-facing materials in fusion energy devices.

42 ENGINEERING↗

Evidence for a High Temperature Whisker Growth Mechanism Active in Tungsten during In Situ Nanopillar Compression

A series of nanopillar compression tests were performed on tungsten as a function of temperature using in situ transmission electron microscopy with localized laser heating. Surface oxidation was observed to form on the pillars and grow in thickness with increasing temperature. Deformation between 850 °C and 1120 °C is facilitated by long-range diffusional transport from the tungsten pillar onto adjacent regions of the Y2O3-stabilized ZrO2 indenter. The constraint imposed by the surface oxidation is hypothesized to underly this mechanism for localized plasticity, which is generally the so-called whisker growth mechanism. The results are discussed in context of the tungsten fuzz growth mechanism in He plasma-facing environments. The two processes exhibit similar morphological features and the conditions under which fuzz evolves appear to satisfy the conditions necessary to induce whisker growth.

36 MATERIALS SCIENCE↗

Characterization of boundary precipitation in a heavy ion irradiated tungsten heavy alloy under the simulated fusion environment

In the concerted effort to identify materials capable of surviving the adverse environment of a fusion reactor interior, tungsten heavy alloys have been put forth as leading candidates. Experimental trials and behavioral studies have yielded positive results for their adoption by taking advantage of the alloy’s unique balance of inherently high fracture toughness and low sputter yields; yet due to their relative novelty in the fusion community, there remains a lack of understanding on the response of these materials to the extended high temperature irradiation environment of the reactor interior. Further, to alleviate this issue and provide the necessary data on the behavior of tungsten heavy alloys to the simulated fusion environment, a 90W-7Ni-3Fe alloy has been subjected to elevated temperature sequential Ni + and He + ion irradiations to mimic the expected displacement damage and gas production expected after five years of service as a plasma facing material component. Atomic-scale structural analyses and nanoscale chemical mapping have identified the formation of two distinct precipitation structures, a surface localized η-carbide and an a-W 2 C type tungsten carbide, both of which appear to originate at the bi-phase interface between W and the ductile phase. This irradiation assisted and induced precipitate formation respectively is anticipated to adversely affect these materials by selective embrittlement at bi-phase interfaces leading to a reduction in the material’s overall fracture toughness during prolonged high temperature irradiation. It is asserted that any potential exposure to C during fusion reactor operational service should be minimized as to prevent the formation of these phases.

36 MATERIALS SCIENCE↗

Examining deformation localization of irradiated tungsten under uniaxial compression with crystal plasticity

In this work, the deformation behavior of irradiated tungsten at elevated service temperatures is examined using mechanism-based crystal plasticity finite element framework by considering multiple mechanisms, including thermal softening and irradiation hardening. The previously developed mechanism-based crystal plasticity model is first utilized to assess the yield stress of unirradiated and irradiated tungsten upon low-temperature irradiation. Additionally, the engineering stress-strain response under uniaxial compression is then predicted by considering the effect of irradiation-induced defect clusters on the motion of deformation-induced dislocations, and the predicted results agree well with the experimental measurements. More importantly, the formation and evolution of plastic strain localization zones in the form of shear bands are qualitatively captured, and the maximal principal strain distribution is quantitatively linked to the dose of irradiation damage. Finally, the deformation-induced shear band as a result of plastic instability in the compressed tungsten specimen is discussed.

36 MATERIALS SCIENCE↗

Defect formation and transmutation behaviors in irradiated tungsten under thermal-neutron shielded and mixed spectrum conditions

Here, this study investigates the microstructural evolution of pure tungsten irradiated under thermal-neutron shielded and mixed spectrum conditions in the High Flux Isotope Reactor (HFIR). Four samples were irradiated at temperatures from 570 °C to 1130 °C up to 0.73 dpa. Neutron spectrum significantly influenced the accumulation of transmutation products, with Re+Os content estimated at ∼0.3–0.6% under thermal-neutron shielded conditions and ∼5.2% under the mixed spectrum condition. Irradiation temperature strongly influences tungsten’s microstructure, with dislocation loops and fine voids forming at lower temperatures and only larger voids and Re/Os segregation observed at higher temperature. Under thermal-neutron shielded conditions, dislocation loops and voids were observed at 570 °C and 790 °C. At the highest irradiation temperature (1130 °C), dislocation loops were no longer observed, while larger but less dense voids remained. Re and Os segregation to void surfaces was evident at 790 °C and 1130 °C, though no precipitation was observed. In contrast, under the mixed-spectrum condition, both spherical and needle-like Re/Os-rich precipitates were observed, frequently accompanied by large voids. Dislocation loops were not observed, but loop-like contrast within the precipitates suggests they may have nucleated on pre-existing loops. Irradiation-induced hardening was assessed for the shielded samples at 570 °C and 790 °C. Dispersed barrier hardening (DBH) analysis, based on TEM-resolved defects, revealed that voids were the dominant contributors to hardening, consistent with literature results. A schematic model is proposed to describe defect and precipitate evolution in tungsten under fusion-relevant transmutation-to-dpa conditions.

Dislocation loops↗

Thermal gradient effect on helium and self-interstitial transport in tungsten

First-wall materials in a fusion reactor are expected to withstand harsh conditions, with high heat and particle fluxes that modify the materials microstructure. These fluxes will create strong gradients of temperature and concentration of diverse species. Besides the He ash and the hydrogenic species, neutron particles generated in the fusion reaction will collide with the material creating intrinsic defects, such as vacancies, self-interstitials atoms (SIAs), and clusters of such point defects. These defects and the He atoms will then migrate in the presence of the aforementioned gradients. In this study, we use nonequilibrium molecular dynamics to analyze the transport of He and SIAs in the presence of a thermal gradient in tungsten. We observe that, in all cases, the defects and impurity atoms tend to migrate toward the hot regions of the tungsten sample. The resulting species concentration profiles are exponential distributions, rising toward the hot regions of the sample, in agreement with irreversible thermodynamics analysis. For both He atoms and SIAs, we find that the resulting species flux is directed opposite to the heat flux, indicating that species transport is governed by a Soret effect (thermal-gradient-driven diffusion) characterized by a negative heat of transport that drives species diffusion uphill (from the cooler to the hot regions of the sample). Here, we demonstrate that the steady-state species profiles obtained accounting for the Soret effect vary significantly from those where temperature-gradient-driven transport is not considered and discuss the implications of such a Soret effect on the response to plasma exposure of plasma-facing tungsten.

36 MATERIALS SCIENCE↗

Modeling of small tungsten dust grains in EAST tokamak with NDS-BOUT ++

In order to investigate the transport of small dusts as well as their evolution property along their trajectories, the NDS module is developed under the BOUT++ framework, a highly desirable C++ code package to perform parallel plasma fluid simulations with an arbitrary number of equations in three-dimensional curvilinear coordinates. Due to the severe dust ablation in fusion plasmas, the dust size would decrease from micrometer to nanometer, resulting in impurities. Small dusts in the simulations here are specified as tungsten spheres with the radii on or below the order of submicrometer. The Rayleigh limit is included in the charging process when the dust is ablated to the droplet phase. The simulation results from the NDS module show that a 200 nm radius spherical tungsten dust originated from upper divertor region of EAST Tokamak is ablated completely due to the intense heating from the incoming plasma inside the core region, well consistent with the CCD footage of EAST shot # 81459. Furthermore it is found that the magnetic field dominates the dust transport when the dust radius is below 100 nm during the ablation along the trajectory. Our simulations predict that a 10 nm radius spherical tungsten dust injected from the inner midplane is well constrained by the magnetic field, and it reaches the inner divertor target with a velocity on the order of km/s.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

The effectiveness of D 2 pellet injection in reducing intra-ELM and inter-ELM tungsten divertor erosion rates in DIII-D during the Metal Rings Campaign

Abstract Edge localized modes (ELMs) in H-mode plasmas erode plasma-facing components (PFCs) and lead to impurities in the core, reducing confinement. This study analyzes D 2 pellet injection on the DIII-D fusion experiment used as an ELM mitigation technique applied during the 2016 tungsten Metal Rings Campaign to reduce W erosion during ELMs. The 400.9 nm photon wavelength line emission intensity of tungsten atoms (WI) filterscope channels and Langmuir probes were used to infer the gross erosion rate of tungsten-coated tiles installed in the divertor of DIII-D. D 2 mass injection rates ranging from 34 to 41 arbitrary units (A.U.) and no D 2 injection resulted in a similar total W erosion rate during ELMs (intra-ELM). On average, results show a 29% increase in the total gross W erosion rate with intermediate mass injection rates (∼13–23 A.U.) compared to the no pellets and the highest injection rate cases. On average, the fast D 2 mass injection rate cases had 15% less erosion in the inter-ELM phase than the case with no pellets. Generally, higher D 2 mass injection rates increased the ELM frequency, and the highest injection rates reduced the average erosion per ELM and fractional carbon impurities at the top of the pedestal by nearly 40% when compared to the no-pellet case. As expected, a higher D 2 pellet injection rate led to a higher plasma density and lower plasma temperature in the divertor. Additionally, an increasing divertor inter-ELM plasma electron density directly correlated to more frequent pellet injection and a decrease in both the average gross intra-ELM W erosion and the total gross intra-ELM W erosion rate. Simulations of intra-ELM erosion using the ‘free-streaming plus recycling model’ (FSRM) underestimate W erosion during pellet injection by about 30% on average. The discrepancies between the experimental measurements and the FSRM intra-ELM W erosion predictions are postulated to be due to C/W material mixing. A simple analytic mixed-material model is presented and results in better agreement with the experimental data. These results highlight the importance of incorporating the effects of a mixed-material layer in the analysis of PFC erosion.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Visible spectroscopy of highly charged tungsten ions with the JET charge exchange diagnostic

Since the installation of the ITER-like wall on the JET tokamak, visible emission from a broad range of tungsten charge states has complicated plasma ion temperature and toroidal rotation measurements. A plethora of charge exchange transitions, from ions up to W 56+ , and 21 suspected magnetic dipole transitions have been observed. In particular W 39+ and W 46+ charge exchange emission contaminates the long-established carbon measurement at 529 nm. Fortunately the wavelength and relative intensity of the tungsten charge exchange lines is predictable and their influence can be mitigated when they are included in the spectral fit. Neon based charge exchange measurements at 525 nm are now preferred on JET since the ITER-like wall, however in this case an unidentified tungsten magnetic dipole transition contaminates the spectrum when the electron temperature is low.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Erosion of tungsten marker layers in W7-X

In order to get first insight into net tungsten erosion in W7-X, tungsten (W) marker layers were exposed during the operational phase OP 1.2b at one position of the Test Divertor Unit (TDU), at 21 different positions of the inner heat shield, and at two scraper elements. The maximum tungsten erosion rate at the TDU strike line was 0.13 nm s -1 averaged over the whole campaign. The erosion was inhomogeneous on a microscopic scale, with higher erosion on ridges of the rough surface inclined towards the plasma and deposition of hydrocarbon layers in the recessed areas of the rough surface. The W erosion at the inner heat shield was below the detection limit of 3–6 × 10 12 W-atoms/cm 2 s, and all inner heat shield tiles were covered with a thin B/C/O layer with thickness in the range 2 × 10 17 –10 18 B + C atoms/cm 2 (about 20–100 nm B + C). W-erosion of the marker layers on the scraper elements was also below the detection limit.

Mayer, M↗

An atom probe tomography and inventory calculation examination of second phase precipitates in neutron irradiated single crystal tungsten

Tungsten is the prime candidate material for the plasma facing divertor system and first wall armor of future nuclear fusion reactors. However, the understanding of the microstructural and chemical evolution of pure tungsten under neutron irradiation is relatively unknown, in part due to a lack of experimental data on this topic. Here, single crystal tungsten has been irradiated in the High Flux Isotope Reactor (HFIR) at Oak Ridge National Laboratory at a nominal temperature of 700–800 °C to damage levels of 0.1 and 1.8 displacements per atom (dpa). Inventory calculations of the neutron irradiation experiments have been used to track isotope generation and decay to inform atom probe tomography (APT) results in the determination of the transmutation-induced precipitate compositions. Furthermore, APT crystallography has been used to show the relationship between precipitates and matrix. The composition of the precipitates is shown to progress towards that of the σ-phase at the highest dose studied, with those precipitates lying along crystallographic planes similar to those of displacement-induced dislocations. This work also sets the framework for APT studies of materials that contain isotopic ratios far from those observed in the natural state.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Tungsten doped diamond shells for record neutron yield inertial confinement fusion experiments at the National Ignition Facility

We report on fabrication and characterization of layered, tungsten doped, spherical about 2 mm diameter microcrystalline diamond ablator shells for inertial confinement fusion (ICF) experiments at the National Ignition Facility. As previously reported, diamond ICF ablator shells can be fabricated by chemical vapor deposition (CVD) on solid spherical silicon mandrels using an ellipsoidal microwave plasma reactor. In the present work, we further developed these ablator shells by embedding a W -doped diamond layer sandwiched between two undoped diamond regions. W incorporation in diamond was achieved by adding tungsten hexacarbonyl to the CH 4 /H 2 CVD feed gas. We observe that the W doping concentration decreases with increasing deposition rate which, in turn, is controlled by adjusting the total gas pressure. Cross sectional microstructural analysis reveals sharp interfaces between doped and undoped regions of the diamond shell and uniform W distribution with concentrations up to about 0.3 at.%. At higher W concentrations (>0.3 at.%) formation of tungsten carbide precipitates is observed. Using a 3-shock 1.6 MJ laser pulse, the targets described in this work produced the first laser driven implosion to break the 1 × 10 16 neutron yield barrier, followed by experiments (described in future publications) with similar targets and slightly more laser energy producing yields as high as 4 × 10 17 .

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Integrated modeling of RF-induced tungsten erosion at ICRH antenna structures in the WEST tokamak *

This paper introduces STRIPE (Simulated Transport of RF Impurity Production and Emission), an advanced modeling framework developed to analyze material erosion and the global transport of eroded impurities originating from radio-frequency (RF) antenna structures in magnetic confinement fusion devices. STRIPE integrates multiple physics modules: SolEdge3x for scrape-off-layer plasma profiles, COMSOL for 3D RF rectified sheath potentials, RustBCA for erosion yields and surface interactions, and global impurity transport for 3D ion energy-angle distributions and impurity transport. The framework is applied to an ion cyclotron RF-heated L-mode discharge (#57877) in the WEST tokamak, where it predicts a thirty-fold increase in gross tungsten erosion at antenna limiters during the transition from ohmic to ICRH operation. Additionally, under ICRH conditions, a tenfold enhancement in erosion is observed when comparing RF sheath effects to purely thermal sheath conditions. High-charge-state oxygen ions ($\mathrm{O}$ 6+ and above) are identified as the dominant contributors to tungsten sputtering. To validate the model, a synthetic diagnostic tool based on inverse photon efficiency (S/XB coefficients) from the ColRadPy collisional-radiative model enables direct comparison with spectroscopic measurements. Model predictions using a plasma composition of 1% oxygen and 99% deuterium show good agreement with observed W − I (400.9 nm) emission for discharge #57877, supporting the accuracy of the STRIPE framework. This study focuses specifically on gross erosion calculations to demonstrate STRIPE’s capabilities. Future extensions of this work will incorporate net erosion, re-deposition, self-sputtering effects, and whole-device modeling of sputtered tungsten impurity transport. STRIPE is also being applied to other RF-heated linear and toroidal devices, offering valuable insights for antenna design, impurity control, and performance optimization in next-generation fusion reactors.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗