Search NASA⌕ Search

SEARCH · Search NASA

Results for “Amorphous”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,621 records · Page 90

Ultralow equivalent oxide thickness obtained for thin amorphous LaAlO{sub 3} layers grown on Si(001)

Electron beam evaporation in a molecular beam epitaxy reactor was used to deposit, at 400 deg. C, amorphous LaAlO{sub 3} high-{kappa} oxide films on p-type Si(001). X-ray photoelectron spectroscopy and transmission electron microscopy showed that the interface with Si is free of SiO{sub 2} or silicates. Electrical measurements performed on as-deposited samples reveal an equivalent oxide thickness as low as 5 A for a film having a physical thickness of 41 A, a leakage current of 5.6x10{sup -2} A/cm{sup 2} at |V{sub g}-V{sub FB}|=1 V, and no flatband voltage shift.

36 MATERIALS SCIENCE↗

Characterization of hydrogenated amorphous germanium compounds obtained by x-ray chemical vapor deposition of germane: Effect of the irradiation dose on optical parameters and structural order

Hydrogenated nonstoichiometric germanium materials have been produced by x-ray activated-chemical vapor deposition from germane. The reactions pattern leading to the solid products has been investigated. The dose effect on the composition, the local bonding configuration, and structural characteristics of the deposited solids has been studied using infrared absorption and Raman spectroscopy and has been discussed. Optical parameters have been also determined from ultraviolet-visible spectrophotometry data. The results show that the solids are formed by a random bound network of germanium and hydrogen atoms with a-Ge zones dispersed in the matrix. The Raman results and optical parameters indicate that the structural order, both short-range and intermediate-range, decreases with increasing irradiation time. This behavior suggests that the solid is involved in the reactions leading to the final product and indicates that the formation of amorphous germanium zones is stimulated by postdeposition irradiation, which induces compositional and structural modifications.

36 MATERIALS SCIENCE↗

Influence of the deposition-induced stress on the magnetic properties of magnetostrictive amorphous (Fe{sub 80}Co{sub 20}){sub 80}B{sub 20} multilayers with orthogonal anisotropy

In this work, we experimentally justify that the control of the mechanical stress induced during the deposition of sputtered amorphous magnetostrictive (Fe{sub 80}Co{sub 20}){sub 80}B{sub 20} allows a custom design of its magnetic properties. FeCoB multilayers have been sputtered on thermal oxide Si substrates with different buffer materials. The crystalline quality and the thermomechanical properties of the buffer layer influence both the coercive and the anisotropy field. Those buffer layers with both high rigidity and poor thermal conductivity do not allow the dissipation of energy of the incoming sputtered material. Therefore, the mechanical stresses related to the deposition process cannot be released, leading to magnetic layers with high easy-axis coercive field and low anisotropy field. This shows that the mechanical stresses accumulated during deposition are a key parameter for the control of coercivity.

36 MATERIALS SCIENCE↗

Magnetic properties and microstructure of Fe/Pt multilayer films capped with SiO{sub 2} amorphous layer for magnetic recording use

Fe/Pt multilayer films capped with an amorphous SiO{sub 2} layer have been fabricated in order to study the microstructure and magnetic properties via a molecular beam epitaxy technique at 400 deg. C. The formation of granularlike FePt films was obtained with this process due to the interpenetration of SiO{sub 2} which has a lower surface energy. Studies of angular dependent coercivity show a tendency of a domain-wall motion weaken toward rotation of reverse-domain type upon thickness of SiO{sub 2} capping layer atop the Fe/Pt multilayer films. The intergrain interaction was confirmed from the Kelly-Henkel plot that indicated the exchange coupling between neighboring grains in the uncapped FePt films. On the other hand, negative {delta}M value was obtained when the FePt films capped with SiO{sub 2} layer, indicating that the SiO{sub 2} capping layer can lead to the reduction of intergrain exchange coupling in SiO{sub 2}/FePt films.

36 MATERIALS SCIENCE↗

P-Induced Nanocrystallite Dispersion in Amorphous-Nanocrystalline Mixed-Phase Si:H Thin Films

The effects of P doping on the nanocrystalline formation in mixed-phase Si:H thin films were investigated using secondary-ion mass spectrometry, Raman spectroscopy, atomic force microscopy, cross-sectional transmission electron microscopy, and scanning Kelvin probe microscopy. We found that Si nanocrystallites in the intrinsic and weakly P-doped materials aggregate to form cone-shaped structures. The local work function of the nanocrystalline aggregation areas is larger than the surrounding amorphous areas. Increasing the P-doping level requires an increased hydrogen dilution to reach the similar Raman crystallinity. The nanocrystalline aggregation disappears in the heavily P-doped materials, but isolated nanocrystallites appear. The effect of P-doping on the nanostructure is explained with the coverage of P-related radicals on the existing nanocrystalline surface during the deposition and the P segregation in grain boundaries, which prevent new nucleation on the surface of existing nanocrystallites.

14 SOLAR ENERGY↗

Dark current in multilayer amorphous selenium x-ray imaging detectors

A theoretical model for describing the bias-dependent transient behavior of dark current in multilayer (n-i-p) amorphous selenium (a-Se) detectors has been developed. The transient dark currents in these detectors are measured and are compared to the proposed dark current model. It has been found that the dark current is mainly controlled by Schottky emission of holes from the metal/a-Se contact. The initial and steady state dark currents are mainly controlled by the barrier height and the trap centers in the n layer, respectively.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Release of hydrogen molecules from the photodissociation of amorphous solid water and polycrystalline ice at 157 and 193 nm

The production of H{sub 2} in highly excited vibrational and rotational states (v=0-5, J=0-17) from the 157 nm photodissociation of amorphous solid water ice films at 100 K was observed directly using resonance-enhanced multiphoton ionization. Weaker signals from H{sub 2}(v=2,3 and 4) were obtained from 157 nm photolysis of polycrystalline ice, but H{sub 2}(v=0 and 1) populations in this case were below the detection limit. The H{sub 2} products show two distinct formation mechanisms. Endothermic abstraction of a hydrogen atom from H{sub 2}O by a photolytically produced H atom yields vibrationally cold H{sub 2} products, whereas exothermic recombination of two H-atom photoproducts yields H{sub 2} molecules with a highly excited vibrational distribution and non-Boltzmann rotational population distributions as has been predicted previously by both quantum-mechanical and molecular dynamics calculations.

74 ATOMIC AND MOLECULAR PHYSICS↗

Influence of film thickness on the crystallization of Ni-doped amorphous silicon samples

This work reports on the crystallization of amorphous silicon (a-Si) films doped with 1 at. % of nickel. The films, with thicknesses ranging from 10 to 3000 nm, were deposited using the cosputtering method onto crystalline quartz substrates. In order to investigate the crystallization mechanism in detail, a series of undoped a-Si films prepared under the same deposition conditions were also studied. After deposition, all a-Si films were submitted to isochronal thermal annealing treatments up to 1000 deg. C and analyzed by Raman scattering spectroscopy. Based on the present experimental results, it is possible to state that (a) when compared to the undoped a-Si films, those containing 1 at. % of Ni crystallize at temperatures {approx}100 deg. C lower, and that (b) the film thickness influences the temperature of crystallization that, in principle, tends to be lower in films thinner than 1000 nm. The possible reasons associated to these experimental observations are presented and discussed in view of some experimental and thermodynamic aspects involved in the formation of ordered Si-Si bonds and in the development of Ni-silicide phases.

36 MATERIALS SCIENCE↗

High-performance amorphous gallium indium zinc oxide thin-film transistors through N{sub 2}O plasma passivation

Amorphous-gallium-indium-zinc-oxide (a-GIZO) thin filmtransistors (TFTs) are fabricated without annealing, using processes and equipment for conventional a-Si:H TFTs. It has been very difficult to obtain sound TFT characteristics, because the a-GIZO active layer becomes conductive after dry etching the Mo source/drain electrode and depositing the a-SiO{sub 2} passivation layer. To prevent such damages, N{sub 2}O plasma is applied to the back surface of the a-GIZO channel layer before a-SiO{sub 2} deposition. N{sub 2}O plasma-treated a-GIZO TFTs exhibit excellent electrical properties: a field effect mobility of 37 cm{sup 2}/V s, a threshold voltage of 0.1 V, a subthreshold swing of 0.25 V/decade, and an I{sub on/off} ratio of 7.

36 MATERIALS SCIENCE↗

Implantation conditions for diamond nanocrystal formation in amorphous silica

We present a study of carbon ion implantation in amorphous silica, which, followed by annealing in a hydrogen-rich environment, leads to preferential formation of carbon nanocrystals with cubic diamond (c-diamond), face-centered cubic (n-diamond), or simple cubic (i-carbon) carbon crystal lattices. Two different annealing treatments were used: furnace annealing for 1 h and rapid thermal annealing for a brief period, which enables monitoring of early nucleation events. The influence of implanted dose and annealing type on carbon and hydrogen concentrations, clustering, and bonding were investigated. Rutherford backscattering, elastic recoil detection analysis, infrared spectroscopy, transmission electron microscopy, selected area electron diffraction, ultraviolet-visible absorption measurements, and Raman spectroscopy were used to study these carbon formations. These results, combined with the results of previous investigations on similar systems, show that preferential formation of different carbon phases (diamond, n-diamond, or i-carbon) depends on implantation energy, implantation dose, and annealing conditions. Diamond nanocrystals formed at a relatively low carbon volume density are achieved by deeper implantation and/or lower implanted dose. Higher volume densities led to n-diamond and finally to i-carbon crystal formation. This observed behavior is related to damage sites induced by implantation. The optical properties of different carbon nanocrystal phases were significantly different.

36 MATERIALS SCIENCE↗

The evolution of the structure and mechanical properties of fullerenelike hydrogenated amorphous carbon films upon annealing

Hydrogenated amorphous carbon films were deposited on Si (100) substrates using dc-pulse plasma chemical vapor deposition. Structurally, the as-deposited carbon films could be considered as nanocomposite thin films with fullerenelike microstructure in diamondlike carbon matrix based on our previous result [Q. Wang et al., Appl. Phys. Lett. 91, 141902 (2007)]. In this paper, the evolution of the structure and the mechanical properties of hydrogenated carbon films with fullerenelike microstructure on the annealing in vacuum was investigated. The fullerenelike hydrogenated carbon films annealed at 500 deg. C showed higher hardness (16.9% harder) and higher elastic recovery (11.2% higher) than the as-deposited films. The friction coefficient of fullerenelike hydrogenated carbon films in air with 40% relative humidity remained constant at about 0.037 when annealed at 600 deg. C. The wear rate of the films decreased sharply when annealed at 200 or 300 deg. C. Structural analysis shows that annealing at 300 deg. C improved tribological properties originated from the volume increase in the fullerenelike microstructure, and further annealing at 600 deg. C improved mechanical properties originated from the transformation of nanosized curved sp{sup 2} to sp{sup 3} clusters.

36 MATERIALS SCIENCE↗

On the growth mechanism of plasma deposited amorphous silicon thin films

We propose a comprehensive mechanism of amorphous silicon thin film growth by plasma deposition based on results of kinetic Monte Carlo simulations according to a database constructed by first-principles density functional theory calculations. The growth mechanism consists of various surface kinetic events including radical-surface and adsorbed radical-radical interactions, radical-surface diffusion, and surface hydride dissociation reactions. Of particular importance is the radical dissociative adsorption mediated by Si over-coordination defects along the reaction pathway. The proposed mechanism explains fully the experimentally measured surface composition of plasma deposited films under conditions that make the silyl radical the dominant deposition precursor.

36 MATERIALS SCIENCE↗

Performance enhancement of n-channel inversion type In{sub x}Ga{sub 1-x}As metal-oxide-semiconductor field effect transistor using ex situ deposited thin amorphous silicon layer

Significant enhancement in metal-oxide-semiconductor field effect transistor (MOSFET) transport characteristics is achieved with In{sub x}Ga{sub 1-x}As (x=0.53, x=0.20) channel material using ex situ plasma enhanced chemical vapor deposited amorphous Si layer. In{sub x}Ga{sub 1-x}As MOSFETs (L=2 {mu}m, V{sub gs}-V{sub t}=2.0 V) with Si interlayer show a maximum drain current of 290 mA/mm (x=0.53) and 2 {mu}A/mm (x=0.20), which are much higher compared to devices without a Si interlayer. However, charge pumping measurements show a lower average interface state density near the intrinsic Fermi level for devices without the silicon interlayer indicating that a reduction in the midgap interface state density is not responsible for the improved transport characteristics.

36 MATERIALS SCIENCE↗

Dry etching characteristics of amorphous As{sub 2}S{sub 3} film in CHF{sub 3} plasma

The authors describe the dry etching characteristics of amorphous As{sub 2}S{sub 3} films in CHF{sub 3} plasma and the development of an optimized fabrication process for compact waveguides. The observed etching behavior is due to the relative densities of fluorine atoms, polymer precursors, and ions in the plasma which are controlled by the process parameters. In particular, the flow rate of the CHF{sub 3} gas has a significant influence on the etched profile and surface roughness as well as the etch rate of the As{sub 2}S{sub 3}. The profile evolves from isotropic to vertical with the flow rate due to passivation by increasing polymer deposition on the sidewalls. Such passivation also helps achieve smooth sidewalls because it inhibits differential etching between the phases in the inherently phase-separated As{sub 2}S{sub 3} film, which otherwise results in a grainy and rough etched surface. At the highest flow rate, however, excessive polymer deposition occurs and this results in positive-sloped sidewall and grassy etched surface due to micromasking.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Surface evolution of amorphous nanocolumns of Fe-Ni grown by oblique angle deposition

The growth of Fe-Ni based amorphous nanocolumns has been studied using atomic force microscopy. The root mean square roughness of the film surface increased with the deposition time but showed a little change at higher deposition time. It was found that the separation between the nanostructures increased sharply during the initial stages of growth and the change was less pronounced at higher deposition time. During the initial stages of the column growth, a roughening process due to self shadowing is dominant and, as the deposition time increases, a smoothening mechanism takes place due to the surface diffusion of adatoms.

36 MATERIALS SCIENCE↗

Electron-Stimulated Reactions and O-2 Production in Methanol-Covered Amorphous Solid Water Films

The low-energy, electron-stimulated desorption (ESD) of molecular products from amorphous solid water (ASW) films capped with methanol is investigated versus methanol coverage (0 - 4 x 1015 cm-2) at 50 K using 100 eV incident electrons. The major ESD products from a monolayer of methanol on ASW are quite similar to the ESD products from bulk methanol film: H2, CH4, H2O, C2H6, CO, CH2O, and CH3OH. For 40 ML ASW films, the molecular oxygen, hydrogen, and water ESD yields from the ASW are suppressed with increasing methanol coverage, while the CH3OH ESD yield increases proportionally to the methanol coverage. The suppression of the water ESD products by methanol is consistent with the non-thermal reactions occurring preferentially at or near the ASW/vacuum interface and not in the interior of the film. The water and molecular hydrogen ESD yields from the water layer decrease exponentially with the methanol cap coverage with 1/e constants of ~ 0.6 x 1015 cm-2 and 1.6 x 1015 cm-2, respectively. In contrast, the O2 ESD from the water layer is very efficiently quenched by small amounts of methanol (1/e ~ 6.5 x 1013 cm-2). The rapid suppression of O2 production by small amounts of methanol is due to reactions between CH3OH and the precursors for the O2 - mainly OH radicals. A kinetic model for the O2 ESD which semi-quantitatively accounts for the observations is presented.

08 HYDROGEN↗

The change in permeability spectra due to ion irradiation in the Co-based amorphous ribbon

The Ar ion has been irradiated by an ion implanter with energy of 50, 70, and 100 keV and an ion dosage was set to 1.0x10{sup 17} ion/cm{sup 2} at a beam flux of 3.7 {mu}A/cm{sup 2}. The ion irradiation decreased the initial permeability and increased the relaxation frequency, and the behavior of permeability spectra due to ion irradiation was explained with damped harmonic model of domain wall on the general basis of magnetization mechanism. The ion irradiation gives rise to a significant change on the restoring force of domain wall but minor effect on the spin rotation. The enhancement in the permeability of the amorphous ribbon upon ion irradiation leads to a parallel improvement of giant magneto impedance response of the material, which is of practical use for sensing applications.

36 MATERIALS SCIENCE↗