Search NASA⌕ Search

SEARCH · Search NASA

Results for “Modulus”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,639 records · Page 91

Nanocomposites of Waterborne Polyurethane Reinforced with Cellulose Nanocrystals from Sisal Fibres

Cellulose nanocrystals (CNC) were isolated from sisal fibres and were incorporated in the form of an aqueous suspension to a waterborne polyurethane (WBPU) synthesized from components derived from natural sources using an aliphatic diisocyanate. Transparent nanocomposite films with different CNC contents were prepared using a casting method. The morphology, thermal behaviour and mechanical properties of the nanocomposite films were characterized. Homogeneous distribution of CNC in the WBPU, even at high CNC contents was observed, resulting in an increase of 100% in modulus for systems with 5 and 10 wt% of CNC, with high elongations around 650%.

36 MATERIALS SCIENCE↗

An Investigation on Transparency and Mechano-Acoustic Properties of Poly Methyl Methacrylate/Polycarbonate Based Nanocomposites

The main goal of this paper was to investigate transparency and mechano-acoustic properties of poly methyl methacrylate (PMMA)/polycarbonate (PC) based nanocomposites, reinforced with silica (SiO{sub 2}), zinc dioxide (ZnO), and titanium dioxide (TiO{sub 2}) nanoparticles. For this purpose, morphological, transparency, acoustical and mechanical tests were carried out on the specimens, prepared by melt-compounding method in a twin-screw extruder. The morphological test results confirmed uniform dispersion of the nanoparticles in the polymer matrix. The results also revealed that transparency of the PC and PMMA nanocomposites, characterized by the degree of light transmittance, was decreased by adding 0.3 wt% of the nanoparticles. Also, tensile modulus of the nanocomposite specimens was higher than that of neat PC and PMMA. Unlike the neat PC specimens, tensile strength showed a decrease in PMMA specimens. The presence of nanoparticles in the composites decreased mobility of polymer chains and consequently, reduced elongation at break in the specimens. After surface roughening process, noise absorption coefficient in PC/PMMA nanocomposite specimens (PCSI3-R, PMSI3-R, and PMZN3-R) showed a higher absorption coefficient than the other specimens in the dominant frequency of traffic noise (500 Hz). As conclusion, roughening the surface of materials would be one of the most important factors enhancing the absorption coefficient of some of the nanocomposites in the middle frequency. The rough surface of particles in the base matrix increases the absorption coefficient of the materials, especially in the frequency of 500 Hz, as the dominant frequency of noise traffic. The suggested materials are predestinated to be appropriate in building industry, particularly in the structure of noise barriers.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Biodegradability and Thermal Properties of Novel Natural Rubber/Linear Low Density Polyethylene/Thermoplastic Starch Ternary Blends

This work aimed to prepare biodegradable thermoplastic elastomers based on NR/LLDPE/TPS ternary simple blends to achieve some exclusive properties, i.e., good biodegradability in terms of water absorption and weight loss after burial, together with reasonable mechanical and thermal properties. A comparative study on biodegradability and other related properties of NR/LLDPE binary and NR/LLDPE/TPS ternary blends was performed. It was found that increasing the TPS proportion decreased storage modulus and complex viscosity. In addition, the size of dispersed TPS domains in the NR/LLDPE co-continuous matrix increased with TPS proportion, while the mechanical properties in terms of 100% moduli, tensile strength, elongation at break, and hardness decreased. This might be attributed to decreased interfacial adhesion with increasing size of TPS domains. Furthermore, increasing the TPS loading in the blend reduced the temperatures for 5 or 50% mass loss (T{sub 5} or T{sub 50}) and the degradation temperature (T{sub d}). However, the biodegradability improved, in terms of increased water absorption and weight loss after burial in soil, with the loading level of TPS.

36 MATERIALS SCIENCE↗

Multiple Reprocessing Cycles of Corn Starch-Based Biocomposites Reinforced with Curauá Fiber

Biocomposites with a corn starch-based biodegradable polymer as matrix and 10 wt% vegetable curauá fiber were processed by injection molding and were submitted to reprocessing up to ten cycles with or without 3 wt% of maleic anhydride grafted polypropylene as coupling agent. The effect of reprocessing on hardness, impact and tensile properties as well as on the morphology, thermal properties, chemical structure and soil degradation behaviour of the matrix and biocomposites was evaluated. Curauá fibers have increased hardness, impact and tensile strengths as well as increased tensile modulus and decreased elongation at break of the biocomposites with respect to starch-based matrix and these properties slightly decreased or no considerable changes were observed with the reprocessing cycle increase. The addition of coupling agent promoted an increase in all properties and they remained almost constant with the reprocessing cycle increase. Thus, the incorporation of curauá fiber within starch-based matrix can improve the mechanical properties of the biocomposites which showed potential to be recycled despite the weight loss in soil degradation tests reached around 10 wt% after 230 days for biocomposites reprocessed ten cycles.

36 MATERIALS SCIENCE↗

Urea Formaldehyde and Cellulose Nanocrystals Adhesive: Studies Applied to Sugarcane Bagasse Particleboards

The aim of this research was to investigate the behavior of urea formaldehyde (UF) adhesive based particleboards using sugarcane bagasse (SCB), with and without the addition of cellulose nanocrystals (NCC). In the first step of this research study, the interaction between UF and the NCC was evaluated. The NCC were dispersed in the UF, in different proportions (0, 0.5, 1, 2, 3 and 5%). Subsequent to this, the mixtures were dried, milled, and put in molds, to produce flexural specimens. The second step involved evaluation of the interaction between the NCC, UF, and SCB. After sonication, the NCC and UF were applied on the SCB particles to produce particleboards. They were evaluated according to the modulus of elasticity and rupture, water absorption (WA), and thickness swelling. The viscosity of the mixture of NCC and UF increased according to the NCC increase load. At 5% of NCC load, the viscosity increased greatly, which prevented adhesive dispersion in the particleboard. The thermogravimetric analysis of UF showed that better conditions of processing were at 160 °C for 8 min, so these parameters were used to produce the specimens. SCB is a promising raw material for particleboard, and its potential to produce SCB particleboards with relatively good performance was demonstrated. For the particleboards specimens, the best performance was observed with 1% of NCC. Particleboards did not show improvement compared with UF specimens, probably because bond links were not sufficient. Addition of NCC in UF increased the liquid suspension viscosity, and the specimens showed a better mechanical performance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Novel Biocomposites Based on Sunflower Oil and Alfa Fibers as Renewable Resources

The aim of this work is to develop biocomposites based on modified sunflower oil as resin and short natural fibers from Alfa plants (Stipa tenacissima) as reinforcement. Epoxidized sunflower oil (ESFO) was chemically modified via acrylation reaction to obtain acrylated epoxidized sunflower oil resin (AESFO). The AESFO resin was then copolymerized with styrene as co-monomer in the presence of boron trifluoride (BF{sub 3}) as cationic initiator and cobalt octoate (Co) as catalyst. Experimental conditions of this modification were optimized by varying styrene, Co and BF{sub 3} wt%. The styrene was varied from 30, 40 to 50 wt% while the catalyst (Co) was varied from 0, 0.01, 0.02 to 0.03 wt%. Two different percents of BF{sub 3} were considered: 0.5 and 1 wt%. The prepared samples were evaluated according to their appearance and then characterized in terms of tensile properties (stress at break, Young’s modulus and elongation at break) to determine the best ratio of styrene/BF{sub 3}/Co. Alfa fibers, used as bio-reinforcement, were treated with a 5% NaOH solution and characterized by Fourier transform infrared (FTIR) spectroscopy, scanning electron microscopy (SEM) and thermo gravimetric analysis (TGA). Biocomposites were prepared by using untreated (UAF) and treated Alfa fibers (TAF) at a ratio of 5 wt% and characterized in terms of tensile properties and morphology by SEM. The best results were obtained with TAF. Then, the ratio of TAF was varied (5, 7.5 and 10 wt%) and the tensile and thermal properties of the biocomposites were characterized. The results showed that the best results were obtained with the ratio of 7.5 wt%.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Poly(lactic acid)/Cellulose Composites Obtained from Modified Cotton Fibers by Successive Acid Hydrolysis

This work is focused on the hydrolysis of cotton fibers from waste textiles to obtain micro and nanofibers to be used as reinforcements in polymer composites. To promote their compatibility with polymeric matrix, hydrolyzed cotton fibers were surface modified with various silane compounds. Thus, these fibers were mixed with commercial poly(lactic acid) (PLA) at 5% w/w loading by melt compounding. Acid treatments caused a decrease of the crystallinity index whereas the thermal stability was significantly improved, especially for cellulose fibers hydrolyzed in two steps. Morphological analysis revealed a reduction of the fibers diameter and a decrease of their length as a consequence of the hydrolysis. NMR analysis confirmed the silanization of the fibers by reaction with the silane agent. Tensile tests revealed that silanization treatments were able to increase the composite Young’s modulus and the stress at break with respect to the neat matrix, indicating that silanization improved the polymer/fiber compatibility interfacial adhesion. The overall results demonstrated that applying suitable surface modification strategies, waste cotton textiles can be effectively recycled as fillers in polymer based composites.

36 MATERIALS SCIENCE↗

Preparation and Characterization of PVC Matrix Composites with Biochemical Sludge

Biochemical sludge (BS), generated in the waste water treatment of paper mills, was pretreated by enzyme hydrolysis. The effect and action mechanism of the enzymatic treatment on the properties of polyvinyl chloride (PVC) matrix composites with BS were discussed. Results showed that when the filler content was 30 wt%, the tensile strength of the PVC composites filled with BS and its modified products which were pretreated by laccase, cellulase and hemicellulase can be increased by 38.64, 67.4, 63.5 and 66.3% than the PVC composite filled with calcium carbonate. When the dosage of filler was 40 wt%, the elastic modulus of PVC composites filled with BS and its above three modified products decreased by 53.3, 52.3, 50.0 and 46.3%, respectively. Meanwhile, the thermal stability of PVC composites can also be improved at the temperature of over 340 °C. It can be concluded that the enzyme pretreatment can improve the application performance of BS usage in PVC matrix composites.

54 ENVIRONMENTAL SCIENCES↗

Effects of MCC Content on the Structure and Performance of PLA/MCC Biocomposites

Green composites of polylactic acid (PLA) with microcrystalline cellulose (MCC) as reinforcement of the polymer matrix were produced by melt blending to improve the brittleness of PLA. The MCC was prepared by hydrolysis of wheat straw cellulose with sulfuric acid to remove amorphous area. The biocomposites were prepared with different MCC contents (2, 4, 6, 8 wt%). Scanning electron microscopy, thermogravimetric analysis, X-ray diffraction, differential scanning calorimetry, Fourier transform infrared and mechanical testing were used to study the structure and properties of MCC and biocomposites. The tensile modulus and the strength of PLA/MCC biocomposites increased from 206 to 262 MPa and from 67.35 to 73.01 MPa, respectively.

36 MATERIALS SCIENCE↗

Fabrication and Characterization of Poly(lactic acid) Biocomposites Reinforced by Calcium Sulfate Whisker

The biodegradable poly(lactic acid) (PLA) composites filled with calcium sulfate whisker (CSW) were fabricated via melt-blending and subsequent injection molding. Surface organification of γ-aminopropyltriethoxysilane (APTES) on CSW was applied to accelerate the wettability of PLA to CSW. The mechanical properties, morphological structures, crystallization behaviors and thermal stabilities of PLA/CSW composites were investigated in detail. Results showed that modification of APTES changed the surface morphologies and element compositions, helping to form the well bonded interfaces. By adding CSW, the elastic modulus of PLA/CSW composites presented a sustained increment, while tensile strength, elongation at break and impact toughness were increased first and then decreased. The presence of CSW impeded the melt-crystallization but accelerated the cold-crystallization process. On the whole, the actual crystallinity for the composites was suppressed except for the case with 20% CSW. The thermal stability was enhanced by CSW as expected, and all the samples showed the exact same reaction order (n = 1) according to Carrasco method. Nevertheless, the activation energies were declined, indicating CSW was in favor of thermal decomposition of PLA phases. Finally, it was interestingly found that CSW could improve the comprehensive properties of PLA without deteriorating the processibility.

36 MATERIALS SCIENCE↗

Synthesis of Recycled Poly(ethylene terephthalate)/Polyacrylonitrile/Styrene Composite Nanofibers by Electrospinning and Their Mechanical Properties Evaluation

Consumption of polyethylene terephthalate (PET) products has increased dramatically in recent decades, resulting in the generation of a large amount of PET waste. For that reason, is necessary to find a new application of recycled material. In this article, we report the synthesis and characterization of recycled poly (ethylene terephthalate) (RPET) obtained from the chemical recycling of post-consumer PET bottles by glycolysis method and the formation of composites nanofibers RPET/polyacrylonitrile (PAN)/styrene (ST). The RPET synthesis was studied through infrared spectroscopy (FT-IR) and thermogravimetric analysis (TGA). The viscosity and frequency sweep of the polymeric solutions was evaluated. The composites nanofibers were elaborated by the electrospinning technique and characterized by scanning electron microscopy (SEM), FT-IR, TGA/DSC and nanoindentation. The RPET/PAN/ST composite nanofibers present an average diameter of 456 nm and higher thermal stability compared PAN fibers. The mechanical properties such as hardness and elastic modulus were 4.5 and 7.5 times PAN fibers values, respectively.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Preparation of nanofibrillated cellulose and application in reinforced PLA/starch nanocomposite film

Polylactic acid (PLA), one of the most promising biopolymers with exceptional properties, is being used in a wide variety of applications in diverse fields. However, low degradation rate, relatively high cost and inherently high brittleness of PLA severely hamper its further development, particularly in functional nanocomposites for bio-based packaging. In the present work, green, biodegradable and reinforced PLA-based nanocomposite films were designed and prepared, where starch was incorporated for reducing the overall cost of nanocomposites for large-scale application, and nanofibrillated cellulose (NFC) isolated from microcrystalline cellulose (MCC) via a completely green process was employed as a reinforcing phase. Initially, the morphology structure and dimension of the NFC samples isolated by high-pressure homogenization (HPH) coupled with hot water pretreatment were characterized using SEM, FT-IR, XRD, and laser scattering particle analyzer. Moreover, the effect of NFC loadings on the rheological behavior of the PLA based nanocomposite suspensions and the overall properties of the corresponding nanocomposite films were investigated. Results indicated that increased NFC loadings reduced the shear viscosity and shear stress of the nanocomposite suspensions. Furthermore, the desired PLA/starch/NFC nanocomposite films were found to exhibit improved tensile strength, Young’s modulus and reduced air permeability in comparison to pure PLA/starch films. This work offered an effective route for the preparation of biodegradable and reinforced PLA-based nanocomposite films, which may be promising bio-nanocomposite materials for food packaging applications.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Effect of Rice Husk Derived Nanosilica on the Structure, Properties and Biodegradability of Corn-Starch/LDPE Composites

Development of material with enhanced mechanical properties and biodegradability by the incorporation of synthesized inorganic nanostructured mesoporous silica from rice husk has been investigated. The produced nanosilica (≈ 25 nm and 213.045 m{sup 2}/g surface area) and nanosilica blended LDPE/starch composites were extensively characterised by SEM, FTIR, XRD, XRF, TEM, EDAX and TGA analysis. The low cost of production estimated, ensures its feasibility toward large scale application. The addition of nanosilica into the matrix led to the enhancement of Young’s modulus and stiffness by a value of 535.6 MPa and 32172.81 N/m respectively at 3% nanosilica content, thereby enhancing the initial rigidity and resistivity towards deformation making a better biodegradable substitute in terms of initial application range. The MFI and hardness value also increased with increase of silica content upto 1.5% and 2% respectively to 7.23 g/10 min and 42 (Shor D). Increase in nanofiller content improved the value of degradation rate constant (k) of the weight loss data plot in both vegetable waste and garden soil environment. The addition of 1.5% of nanosilica to a blend of 80% LDPE and 20% starch showed almost the same biodegradation rate as that without nanosilica but with superior mechanical properties and applicability range.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Development of Green Composites Based on Polypropylene and Corncob Agricultural Residue

Green composites of polypropylene (PP) and corncob (CCB) agricultural residue with CCB content ranging from 5 to 30 wt% were compounded by melt extrusion and their properties investigated by density measurements, thermogravimetric analyses, differential scanning calorimetry, scanning electron microscopy (SEM) and tension, flexural and impact properties. Properties were dependent on CCB content. SEM micrographs showed that PP/CCB composites are composed of all layers of the corncob, but with a higher content of woody ring and pith. Composites with CCB up to 20 wt% presented particles evenly dispersed into PP matrix and density values ranging from 0.929 to 1.026 g/cm{sup 3}. Thermal analyses showed that CCB is thermally stable up to 200 °C, ensuring that no degradation took place during processing, and PP/CCB composites are more crystalline than neat PP. Tensile strength and elongation at break of the composites decreased respectively from 30 to 20 MPa, and 22.7 to 3.7%, and the elastic modulus increased while the impact strength remained practically constant at 14 J/m for the filling contents tested. Elastic and flexural moduli increased respectively from 906 MPa to 1.1 GPa and from to 1.26 to 1.81 GPa with corncob addition.

36 MATERIALS SCIENCE↗

Investigation of Photodegradation Preventing of Polyvinyl Alcohol/Nanoclay Composites

The effects of UV irradiation on chemical, thermal, mechanical, and morphological properties of polyvinyl alcohol (PVOH)/2 wt.% of nanoclay(NC) filler were investigated. PVOH composite films were prepared from PVOH blend with fixed content (2%) of NC via the solution casting method. Pure PVOH and PVOH composites were exposed to 340 nm fluorescent UV lamps and assessed for 50 h, 100 h, and 200 h UV exposue. The experimental results such as Fourier transform infrared (FTIR) confirmed that 2% wt. NC filler is efficient and can resist chemical degradation that is caused by ultraviolet irradiation (UV). The carbonyl and hydroxyl indices were increased with increasing the UV exposure irradiation times of both PVOH and PVOH composite. However, the PVOH nanocomposites exhibited more resistant to increasing the indices after exposure to UV irradiation with a longer exposure time. The thermal results (TGA) indicated that PVOH nanocomposite is exhibited more resistance to thermal degradation after UV irradiation exposure compared to that of pure PVOH sample. From DMA results, the storage of modulus was reduced after exposure to UV irradiation of PVOH and PVOH nanocomposites. The results of T{sub g} of PVOH nanocomposites increased after the incorporation of 2% wt. NC into PVOH after exposure to UV irradiation. PVOH nanocomposite exhibited more resistance to reduce the tensile strength after exposure to 200 h UV irradiation. XRD tests showed that PVOH/2 wt.% NC nanocomposites have more resistant to increase intensity after exposure to 200 h UV irradiation compared to that of PVOH sample. The morphology micrographs showed that no obvious cracks on the PVOH nanocomposite after UV irradiation exposure by comparing to that of pure PVOH.

36 MATERIALS SCIENCE↗

Effect of Talc on Mechanical Characteristics and Fracture Toughness of Poly(lactic acid)/Poly(butylene succinate) Blend

This research investigates the effect of talc additive on physical and mechanical characteristics of poly(lactic acid) (PLA) and poly(butylene succinate) (PBS) polymer blend. In the study, the talc content is varied between 0, 5, 10, and 20 parts per hundred resin (phr) and the PLA/PBS ratio is 80/20 w/w. The results reveal that talc enhances the mechanical properties of PLA/PBS blend. Specifically, tensile strength, Young’s modulus, and impact strength of PLA/PBS/talc composite increase as talc content rises. In addition, fracture toughness increases substantially as talc quantity is raised. The enhanced fracture toughness is attributable to nucleation of talc which promotes crystallization of PLA while hindering PBS crystal growth. Moreover, morphology analysis shows efficient distribution of talc in the polymer matrix.

36 MATERIALS SCIENCE↗

Effective Adsorption of Cr(VI) by High Strength Chitosan/Montmorillonite Composite Hydrogels Involving Spirulina Biomass/Microalgae

The “3-in-1 type” biopolymer composite (chitosan/montmorillonite clay/biosorbent) hydrogels were produced and used as adsorbents for Cr(VI) ion. Na-Montmorillonite (NaMMT) clay was modified with Spirulina (Sp) biosorbent by using lyophilization based “cryoscopic expansion” (C-XP) method. The Sp immobilized MMT (SpMMT) clay containing hydrogels were found to have an open/extended form of Sp structure on their pores’ walls, presenting all possible receptor groups for adsorption of Cr(VI) ions. SpMMT loaded hydrogels showed higher adsorption capacities than NaMMT loaded ones. The physically crosslinked hydrogel including only 1% SpMMT (1SpM-H) clay exhibited 150% higher adsorption capacity as compared to neat chitosan hydrogel even in 50 ppm Cr(VI) solution. The same composite hydrogel was found to adsorp about 780% Cr(VI) with respect to the clay’s weight while individual uses of Sp and MMT can remove only about 4.80 and 0.36% Cr(VI) with respect to their weights. The pseudo-first order model was found to be the most suitable for the kinetic data of NaMMT loaded hydrogels while that of SpMMT containing hydrogels followed the pseudo-second order kinetics. The isotherm data of all the hydrogels exhibited a better fit to the Freundlich and Sips model. The maximum adsorption capacity (3333 mg g{sup −1}) calculated by Sips model was achieved via the hydrogel having 1% SpMMT which is in good agreement with the experimental kinetic data. The highest adsorption with the lowest amount of SpMMT clay could be attributed to its looser Sp network structure whose functional groups are in long-distance, releasing more adsorption sites for the Cr(VI). The highest compression modulus and toughness were also obtained with the 1SpM-H hydrogel which is probably due to increased physical and reversible interactions between chitosan molecules and SpMMT clay layers at optimum clay loading (1%).

60 APPLIED LIFE SCIENCES↗

Toward Greener Polymeric Blends: Study of PBAT/Thermoplastic Whey Protein Isolate/Beeswax Blends

This work evaluated the effects of partial substitution of PBAT by thermoplastic whey protein isolate (WPIT) with addition of beeswax through blends processing and their morphological, mechanical, structural, thermal and rheological properties. Whey protein isolate (WPI) was denatured at 90 °C, using glycerol as plasticizer, to be transformed in a thermoplastic material and subsequently blended with PBAT using a torque rheometer at 130 °C. Addition of 10 and 30% of WPIT in the PBAT matrix was investigated with and without beeswax. Blends were pressed as films with ~ 320 µm of thickness. Scanning electron microscopy (SEM) analysis of PBAT/WPIT blends films revealed the presence of domains. These domains are compounded of whey protein, while at the continuous phase a moderate degree of mixture between PBAT and WPIT was observed by Raman analyses. WPIT did not alter the degree of crystallinity and the glass-transition temperature (T{sub g}) of the PBAT in the blends. Thermogravimetric curves of the blends showed decomposition stages related to WPIT and PBAT phases. Thermal stability of blends decreased in comparison to WPIT, which was associated to the cleavage of disulfide bonds of WPIT during processing and causes other kind of interaction between components. Besides, blends containing WPIT remained non-rigid polymers with Young’s modulus below 70 MPa. The tensile strength and elongation at break decreased due the presence of WPIT. Beeswax did not influence the thermal and mechanical properties explored in this study.

36 MATERIALS SCIENCE↗