At least 1,639 records · Page 91

Effect of zeolite type, temperature, and pH on Stage III glass alteration behavior for two nuclear waste glasses

We report long-term laboratory scale static alteration tests (up to 1500 d) were conducted on two low-activity waste glasses (LAWA44 and IDF18-A161) at S/V = 2000 m –1 . Tests were seeded with either analcime, clinoptilolite, zeolite P1, or zeolite P2 to induce Stage III glass alteration behavior. The effect of several parameters on glass Stage III behavior was studied with consideration of several variables, including temperature (22 °C – 90 °C) and pH (floating or initially set using KOH at values from 9.5 to 11.5). Temporal solution data and solids characterization at the end of the experiments are reported. Solution data demonstrated the occurrence of a sustained rate acceleration at temperatures down to 40 °C and the activation energy for these Stage III rates was determined for both glasses. Three major secondary phases were identified at the end of the experiments for both glasses: zeolite P1, zeolite P2, and/or analcime (along with minor phases: zeolites, clays, carbonates). The identification of the crystalline phases at the end of the experiment often differed from the zeolite seed phase. In addition, the use of the Avrami equation showed unimpeded zeolite growth (3-dimensional) in certain conditions, suggesting that in certain conditions the glass dissolution rate is controlled by zeolite formation kinetics whereas in other conditions the glass corrosion process impeded zeolite formation kinetics. The morphological evolution of the samples revealed the growth of the zeolites which completely fill the intergranular space in the powder bed. These results are discussed with regards to previous seeded and unseeded Stage III dissolution rate experiments performed on low- and high-activity nuclear waste glasses.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Corrosion of 316L & 316H stainless steel in molten LiF-NaF-KF (FLiNaK)

The corrosion behavior of 316L and 316H stainless steels (low and high carbon, respectively) in molten LiF-NaF-KF (FLiNaK) salt at 700 °C for 500 h has been investigated. Tests were performed in 316L stainless steel, pyrolytic boron nitride, and glassy carbon capsule materials. The capsule material had a notable effect on the corrosion behavior of the two stainless steels. Further, the modes of corrosion for the two types of stainless steel in various capsule materials were classified into three categories, namely, uniform surface recession, selective grain boundary Cr dissolution, and the dissolution of Cr in the bulk grains. By most metrics, the 316H stainless steel exhibited slightly superior corrosion resistance, while by others the two stainless steels were comparable. These differences in corrosion behavior are attributed to the differences in grain size and the degree of sensitization.

36 MATERIALS SCIENCE↗

Interfacial study of the role of SiO 2 on Si anodes using electrochemical quartz crystal microbalance

One of the challenges associated with silicon as an anode material for Li-ion batteries is the formation of an unstable solid-electrolyte interphase which, forms continuously while consuming lithium and other components; and consequently contributes to irreversible capacity. To elucidate some of the details of the formation and subsequent dissolution of species formed during lithiation of silicon anodes we have produced thin film silicon electrodes and analyzed them during lithiation and delithiation using an electrochemical quartz microbalance with in-situ dissipation (EQCM-D). Measurements were conducted on electrodes with silicon alone and silicon with a silicon dioxide coating, and in EC:EMC and EC:DEC:FEC based electrolytes. Mass loss during lithiation was observed in both solvents systems when an oxide layer was present on the surface of the electrode. Solid state and solution NMR measurements indicate that the formation and dissolution of Li2O is the most likely cause of mass loss.

Anodes↗

Elucidating mechanisms of oxide growth and surface passivation on zinc thin film electrodes in alkaline solutions using the electrochemical quartz crystal microbalance

For this study, we utilized electrochemical quartz crystal microbalance to understand electrochemical passivation of the zinc electrode in alkaline media and subsequent oxide growth and stripping. The formation of native zinc oxide on a near pristine Zn surface upon contact with 1 M KOH electrolyte was observed. The surface was seen to roughen with time. During Zn dissolution, the measured mass-charge ratio corresponded to the removal of ZnO and not merely Zn. The mechanism of passivation was determined to be caused by electrochemical etching to form pores. The etching leads to a build-up of solid ZnO and Zn(OH) 2 due to electrochemical reactions on the surfaces of the pores. These reactions functionally close the pores off from the bulk. The cycle of Zn deposition and dissolution develops a porous network, which may be the origin of mossy Zn deposits that plague reversible Zn metal batteries.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Inorganic polymers from alkali activation of metakaolin: Effect of setting and curing on structure

Geopolymers, obtained by chemical reaction between aluminosilicate oxides and silicates under highly alkaline conditions, are studied in this paper. The proposed mechanism of geopolymer setting and hardening or curing consists of a dissolution, a transportation or an orientation, as well as a polycondensation step. The aim of this paper is to investigate the influence of the curing time and temperature, the relative humidity and the reagents temperature on the geopolymerization process in order to obtain a resistant matrix usable for inertization of hazardous wastes. The evolution of the process from the precursors dissolution to final geopolymer matrix hardening has been followed by FTIR spectroscopy, X-ray diffractometry, SEM/EDS and leaching tests. The results show the significant influence of both curing temperature in the curing stage and of the mould materials on the matrix stability. The easy-to-run preparation procedure for a chemically stable metakaolin geopolymer individuated can be summarized as reagents setting and curing at room temperature and material mould which permits moisture level around 40%. - Graphical abstract: Chemical stability as a function of curing conditions. Highlights: ► Metakaolin in highly alkaline solutions produced solid materials at room temperature. ► Curing time and temperature, relative humidity, reagents temperature were optimized. ► Leaching tests were used to confirm final hardening. ► FTIR spectroscopy, SEM analysis and X-ray diffractometry were used to interpret matrix stability.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Calcium carbonate formation on mica supported extracellular polymeric substance produced by Rhodococcus opacus

Extracellular polymeric substance (EPS) extracted from Rhodococcus opacus bacterial strain was used as a matrix for calcium carbonate precipitation using the vapour diffusion method. The total exopolymer and water-soluble exopolymer fraction of different concentrations were spread on the mica surface by the spin-coating method. The obtained layers were characterized using the atomic force microscopy measurement and XPS analysis. The effects of polymer concentration, initial pH of calcium chloride solution and precipitation time on the obtained crystals properties were investigated. Raman spectroscopy and scanning electron microscopy were used to characterize the precipitated minerals. It was found that the type of precipitated CaCO{sub 3} polymorph and the crystal size depend on the kind of EPS fraction. The obtained results indicates that the water soluble fraction favours vaterite dissolution and calcite growth, whereas the total EPS stabilizes vaterite and this effect is stronger at basic pH. It seems to be due to different contents of the functional group of EPS fractions. - Highlights: • CaCO{sub 3} crystal size and polymorph can be controlled by EPS substance obtained from R. opacus. • The water soluble fraction favours vaterite dissolution and calcite growth. • The total EPS stabilizes vaterite. • This effect is stronger at basic pH.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effects of carbon dioxide sequestration on California margin deep-sea foraminiferal assemblages

Abstract Deep-sea sequestration of CO2 is being considered as a possible mitigation tool to decrease atmospheric CO2 concentrations and its associated negative effects. This study investigated potential effects of liquid carbon dioxide (CO2) injection on deep-sea foraminiferal assemblages. Foraminifera are ideal for this ecological impact investigation because of differing test composition (calcareous and non-calcareous) and thickness, and diverse epifaunal and infaunal depth preferences. The experiment was conducted on August-September 2003, at 3600 m off the coast of Monterey Bay, California, aboard the R/V Western Flyer using the ROV Tiburon. The pH of the site was monitored throughout the experiment. Sediment push-cores were collected (both from the experimental and control sites) and stained to distinguish live (stained) from dead (unstained) individuals. Effects of CO2 injection on assemblages have been tracked both vertically (to 10 cm depth below sea floor) and horizontally (up to 10 m from CO2 injection sites), as well as between live and dead individuals. Within corrals (containing the injected CO2) and their underlying sediments, severe pH changes (near 4.0 units) were recorded. This compares with a record of small average reductions in ocean pH (-0.05 units) combined with large episodic excursions (-1.7 units) over the experimental area due to the injection of CO2. Exposure to this gradient of low pH caused increased mortality and dissolution of calcareous forms within corrals, as far as 5 m from the injection site, and to at least 10 cm depth in the sediments. This experiment revealed several major effects of CO2 injection on foraminiferal assemblages in surficial sediments: 1) total number of foraminifera in a sample decreases; 2) foraminiferal species richness decreases in both stained and unstained specimens; and 3) relative percentage of stained (live) forms in the remaining tests increases. Down-core trends (to 10 cm below sea floor) have revealed: 1) percent agglutinated forms decline and calcareous forms increase with depth; 2) agglutinated species richness decreases with depth; and 3) experimental core assemblages become increasingly similar with depth to those in control cores not subjected to CO2 injection. These results imply almost complete initial mortality and dissolution in the upper 10 cm throughout the corrals following liquid CO2 injection. Since calcareous foraminifera represent more than 50% of the total assemblages, this clearly indicates that emplacement of CO2 will result in negative effects to diversity and survivorship of the deep-sea benthic meiofauna.

54 ENVIRONMENTAL SCIENCES↗

Deformation characteristics of {delta} phase in the delta-processed Inconel 718 alloy

The hot working characteristics of {delta} phase in the delta-processed Inconel 718 alloy during isothermal compression deformation at temperature of 950 deg. C and strain rate of 0.005 s{sup -1}, were studied by using optical microscope, scanning electron microscope and quantitative X-ray diffraction technique. The results showed that the dissolution of plate-like {delta} phase and the precipitation of spherical {delta} phase particles coexisted during the deformation, and the content of {delta} phase decreased from 7.05 wt.% to 5.14 wt.%. As a result of deformation breakage and dissolution breakage, the plate-like {delta} phase was spheroidized and transferred to spherical {delta} phase particles. In the center with largest strain, the plate-like {delta} phase disappeared and spherical {delta} phase appeared in the interior of grains and grain boundaries.

36 MATERIALS SCIENCE↗

Effect of re-melting on particle distribution and interface formation in SiC reinforced 2124Al matrix composite

The interface between metal matrix and ceramic reinforcement particles plays an important role in improving properties of the metal matrix composites. Hence, it is important to find out the interface structure of composite after re-melting. In the present investigation, the 2124Al matrix with 10 wt.% SiC particle reinforced composite was re-melted at 800 °C and 900 °C for 10 min followed by pouring into a permanent mould. The microstructures reveal that the SiC particles are distributed throughout the Al-matrix. The volume fraction of SiC particles varies from top to bottom of the composite plate and the difference increases with the decrease of re-melting temperature. The interfacial structure of re-melted 2124Al–10 wt.%SiC composite was investigated using scanning electron microscopy, an electron probe micro-analyzer, a scanning transmission electron detector fitted with scanning electron microscopy and an X-ray energy dispersive spectrometer. It is found that a thick layer of reaction product is formed at the interface of composite after re-melting. The experimental results show that the reaction products at the interface are associated with high concentration of Cu, Mg, Si and C. At re-melting temperature, liquid Al reacts with SiC to form Al{sub 4}C{sub 3} and Al–Si eutectic phase or elemental Si at the interface. High concentration of Si at the interface indicates that SiC is dissociated during re-melting. The X-ray energy dispersive spectrometer analyses confirm that Mg- and Cu-enrich phases are formed at the interface region. The Mg is segregated at the interface region and formed MgAl{sub 2}O{sub 4} in the presence of oxygen. The several elements identified at the interface region indicate that different types of interfaces are formed in between Al matrix and SiC particles. The Al–Si eutectic phase is formed around SiC particles during re-melting which restricts the SiC dissolution. - Highlights: • Re-melted composite shows homogeneous particle distribution • Thick reaction products are observed at the interface • Carbide is identified at interface due to SiC dissolution at high temperature • Reaction products are also Si enrich phase • Mg and Cu segregated and formed MgAl{sub 2}O{sub 4}, CuMgAl{sub 2} phase at grain boundary.

36 MATERIALS SCIENCE↗

Phase transformations in a Cu−Cr alloy induced by high pressure torsion

Phase transformations induced by high pressure torsion (HPT) at room temperature in two samples of the Cu-0.86 at.% Cr alloy, pre-annealed at 550 °C and 1000 °C, were studied in order to obtain two different initial states for the HPT procedure. Observation of microstructure of the samples before HPT revealed that the sample annealed at 550 °C contained two types of Cr precipitates in the Cu matrix: large particles (size about 500 nm) and small ones (size about 70 nm). The sample annealed at 1000 °C showed only a little fraction of Cr precipitates (size about 2 μm). The subsequent HPT process resulted in the partial dissolution of Cr precipitates in the first sample and dissolution of Cr precipitates with simultaneous decomposition of the supersaturated solid solution in another. However, the resulting microstructure of the samples after HPT was very similar from the standpoint of grain size, phase composition, texture analysis and hardness measurements. - Highlights: • Cu−Cr alloy with two different initial states was deformed by HPT. • Phase transformations in the deformed materials were studied. • SEM, TEM and X-ray diffraction techniques were used for microstructure analysis. • HPT leads to formation the same microstructure independent of the initial state.

36 MATERIALS SCIENCE↗

Characterizing precipitate evolution of an Al–Zn–Mg–Cu-based commercial alloy during artificial aging and non-isothermal heat treatments by in situ electrical resistivity monitoring

In situ electrical resistivity monitoring technique was employed to continuously evaluate the precipitate evolution of an Al–Zn–Mg–Cu-based commercial alloy during typical artificial aging treatments. The effects of artificial aging on the precipitates stability during non-isothermal heat treatments were also explored. Conventional hardness test, transmission electron microscopy and differential scanning calorimetry were also adopted to verify the electrical resistivity results. The results indicated that both the precipitation process and its timely rate could be followed by the monitored electrical resistivity during artificial aging treatments. The electrical resistivity results gave overall information on continuous precipitation and dissolution processes, especially under high heating rates. Samples artificial aging heat treated at 120 °C for 24 h followed by aging at 150 °C for 24 h presented more stable state and coarser precipitates than the samples only artificial aging heat treated at 120 °C for 24 h or triple artificial aging heat treated at 120 °C/24 h + 195 °C/15 min + 120 °/24 h. While the incoherent η precipitates in the samples artificial aging heat treated at 120 °C for 24 h followed by aging at 150 °C for 24 h were more easiness to coarsening and dissolve during non-isothermal heat treatments as well. - Highlights: • In situ electrical resistivity monitoring technique was employed on an Al-Zn-Mg-Cu alloy. • The precipitate evolution during typical artificial aging treatments was studied. • The precipitate stability during non-isothermal heat treatments was explored. • The electrical resistivity wonderfully monitored continuous precipitation and dissolution. • The alloy submitted to a T7 treatment presents a more stable state during heating due to incoherent η precipitates.

36 MATERIALS SCIENCE↗

Investigation of carbon segregation during low temperature tempering in a medium carbon steel

Low temperature tempering is important in improving the mechanical properties of steels. In this study, the thermoelectric power method was employed to investigate carbon segregation during low temperature tempering ranging from 110 °C to 170 °C of a medium carbon alloyed steel, combined with micro-hardness, transmission electron microscopy and atom probe tomography. Evolution of carbon dissolution from martensite and segregation to grain boundaries/interfaces and dislocations were investigated for different tempering conditions. Carbon concentration variation was quantified from 0.33 wt.% in quenching sample to 0.15 wt.% after long time tempering. The kinetic of carbon diffusion during tempering process was discussed through Johnson-Mehl-Avrami equation. - Highlights: • The thermoelectric power (TEP) was employed to investigate the low temperature tempering of a medium carbon alloyed steel. • Evolution of carbon dissolution was investigated for different tempering conditions. • Carbon concentration variation was quantified from 0.33 wt.% in quenching sample to 0.15 wt.% after long time tempering.

36 MATERIALS SCIENCE↗

Controlling the MC and M2C carbide precipitation in Ferrium® M54® steel to achieve optimum ultimate tensile strength/fracture toughness balance

Highlights: • Small and uniformly distributed undissolved Ti-rich MC carbides control the grain size during the austenitization • High austenitizing temperature (1060°C) allows the full dissolution of the coarse carbides (size > several of 100nm) • Intensive nanometer-sized carbides precipitate during tempering thanks to the high supersaturation of alloying elements • Coarse carbides dissolution and nanometer-size carbides precipitation is necessary to achieve high UTS/K{sub I}C balance - Abstract: Ferrium® M54® exhibits an excellent UTS/K{sub 1C} balance allowing its application in aeronautical structures. This steel belongs to the Co-Ni UHS steels family with M{sub 2}C nanometer-size carbide precipitation during tempering. These steels provide very high strength with a very good fracture toughness thanks to the M{sub 2}C fine precipitation during tempering, but also because coarse particles are dissolved during austenitizing without grain coarsening. The goal of this article is to identify the different carbide populations in M54®. A small addition of Ti in M54® forms a Ti-rich MC carbide precipitation that is stable at high temperature. Consequently, during austenitization at 1060 °C, all other types of coarse carbides are dissolved in the matrix without grain coarsening. As a very small part of the initial carbon content is needed to form MC carbides, efficient and intensive nanometric M{sub 2}C carbide precipitation takes place during tempering, leading to very high final strength. Due to this double precipitation of carbides in M54®, the steel achieves an outstanding UTS/K{sub 1C} balance.

36 MATERIALS SCIENCE↗

Effect of secondary phase particles on thermal stability of ultra-fine grained Mg-4Y-3RE alloy prepared by equal channel angular pressing

Highlights: • UFG structure with grain size of ~340 nm was achieved in WE43 by ECAP. • Fine Mg{sub 5}RE particles are responsible for microstructural stability up to 280 °C. • Segregation of Y and RE solutes in grain boundaries was observed. • Hardening at 200–280 °C was observed due to segregation and precipitation. • Effect of particles dissolution and grain growth on softening was discussed. - Abstract: As-cast magnesium alloy WE43, containing yttrium and rare earth elements, was processed by equal channel angular pressing (ECAP). The processing led to a significant grain refinement together with a massive precipitation of the secondary phase particles. Thermal stability of the ultra-fine grain (UFG) structure together with microstructural changes due to exposure to elevated temperatures were studied by several complementary techniques in the temperature range of 160–500 °C. It was found that UFG structure consisting of grains with size of ~340 nm and high density of Mg{sub 5}RE particles is stable up to 280 °C for 1 h of annealing. Moreover, only negligible change of the microstructure occurred after annealing for 16 h at 250 °C. Excellent thermal stability of UFG structure was caused by fine Mg{sub 5}RE particles, which suppressed the grain growth. Exceeding the limit of thermal stability of these particles above 280 °C resulted in material softening. Moreover, statistically significant hardening of the UFG material occurred in the temperature range of 200–280 °C. Segregation of yttrium and rare earth elements and eventually precipitation at grain boundaries was proved to be responsible for observed hardening by in-situ and ex-situ transmission electron microscope and positron annihilation spectroscopy analysis. Finally, individual effect of particles dissolution and grain growth on the material softening was investigated and discussed.

36 MATERIALS SCIENCE↗

Influence of temperature on the lattice misfit and elastic moduli of a Ni based single crystal superalloy with high volume fraction of γ′ phase

Highlights: • The variation of the lattice misfit with temperature in a Ni based single-crystal superalloy with high volume fraction of γ' phase was determined by high-temperature X-ray diffraction (HT-XRD) technique at temperatures between 25 °C and 1200 °C. • When the temperature was higher than 1100 °C, the γ' phase obviously dissolved, leading to a lower content of Mo and Re in the γ phase, and then resulted in a smaller absolute value of the lattice misfit. • The contribution of dissolution of γ′ phase to the reduction of the misfit increased with rising temperature and reached 29.5% at 1200 °C. • When the temperature exceeded 1100 °C, the difference of elastic moduli of γ and γ′ phases increased with rising temperature was attributed to the elastic modulus of γ phase decreased significantly. - Abstract: The variation of the lattice parameter with temperature in a Ni based single-crystal superalloy with high volume fraction of γ′ phase IC32 was determined by high-temperature X-ray diffraction (HT-XRD) technique at temperatures between 25 °C and 1200 °C. The effects of the temperature, especially the ultra-high temperature (beyond 1100 °C), on lattice misfit, elastic moduli, γ′ volume fraction and composition of γ, γ′ phases were investigated in this study. The results show that the absolute value of lattice misfit first increased and then decreased with increasing temperature and reached the maximum of 0.53% at 1100 °C. When the temperature was higher than 1100 °C, the γ′ precipitate obviously dissolved, leading to a lower content of Mo and Re in the γ phase, and then resulted in a smaller absolute value of lattice misfit. The contribution of dissolution of γ′ phase to the reduction of the misfit increased with rising temperature and reached 29.5% at 1200 °C. Moreover, when the temperature was above 1100 °C, the elastic moduli of the γ phase and alloy decreased significantly, while this phenomenon was not observed in the γ′ phase.

36 MATERIALS SCIENCE↗

Effect of intermediate annealing time on microstructure, texture and mechanical properties of Al-Mg-Si-Cu alloy

Highlights: • Long intermediate annealing time could be beneficial to the improvement of deep drawability. • Long intermediate annealing time could give rise to more particles with a larger average size. • As intermediate annealing time increases, strength will change and it has no positive correlation with annealing time, • A particle dissolution model is proposed to illustrate the variation of the strengths with intermediate annealing time. - Abstract: The effect of intermediate annealing time on the microstructure, texture and mechanical properties of Al-Mg-Si-Cu alloys was studied by mechanical properties, microstructure and texture characterization in the present study. The results show that the intermediate annealing time has some influence on the microstructure, recrystallization texture, and final mechanical properties. After the pre-aging treatment and natural aging treatment (T4P treatment), in contrast to the sheet with short intermediate annealing time, the sheet with long intermediate annealing time possesses higher plastic strain ratio r value. Strength has no positive correlation with annealing time, and when applying the annealing time of 16 h, the strength is highest. Before solution treatment, the sheet with long intermediate annealing time has more particles with a larger average size, compared with the sheet with short intermediate annealing time. After solution treatment, they possess the similar recrystallization equiaxed grain structure and recrystallization texture. The sheet with short intermediate annealing time is comprised of Cube{sub ND} {001} <310>, Goss {110}<001> and P {011}<122> orientations, while the sheet with long intermediate annealing time possesses weak texture including Cube{sub ND} {001}<310>, Goss {110}<001> and {015}<751> orientations. Finally, a particle dissolution model during solution treatment is proposed to explain the variation of strength with annealing time.

36 MATERIALS SCIENCE↗

Mechanism of chlorine-induced stress corrosion cracking of two 304 SS heats in simulated marine environment through in situ X-ray tomography and diffraction: Role of deformation induced martensite and crack branching

In this work, In-situ synchrotron x-ray tomography and diffraction experiments were conducted on two heats of 304SS undergoing chlorine-induced stress-corrosion-cracking (CISCC) in a simulated marine environment. The role of deformation induced martensite on CISCC was investigated through diffraction analysis where no significant amount of martensite was found to form during CISCC, indicating that it may not play a significant role in affecting the process. Tomography combined with stress-intensity analysis revealed the influence of stress-intensity on branching types with single crack growth, micro-branching, and macro-branching. Post experimental electron microscopy characterization revealed the presence of FeCl 2 , CrCl 2 , and NiCl 2 ·6H 2 O compounds at the crack, which infers a dissolution mechanism during the experiment. A dissolution mechanism highlighting the synergy between stress and corrosion was proposed to explain chlorine-induced stress-corrosion-cracking and crack branching.

36 MATERIALS SCIENCE↗