Search NASA⌕ Search

SEARCH · Search NASA

Results for “substrate”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,639 records · Page 91

High quality InAsSb grown on InP substrates using AlSb/AlAsSb buffer layers

High quality InAsSb grown on semi-insulating InP substrates by molecular beam epitaxy was achieved using AlSb/AlAsSb structure as the buffer layer. A 1000 A InAsSb layer grown on top of 1 {mu}m AlSb/AlAsSb buffer layer showed a room temperature electron mobility of {approx}12 000 cm{sup 2}/V s. High structural quality and low misfit defect density were also demonstrated in the InAsSb layer. This novel AlSb/AlAsSb buffer layer structure with the AlAsSb layer lattice matched to InP substrates could enhance the performance of optoelectronic devices utilizing 6.1 A family of compound semiconductor alloys.

36 MATERIALS SCIENCE↗

Aligned three-dimensional prismlike magnesium nanostructures realized onto silicon substrate

A simple approach is proposed to realize three-dimensional (3D) prismlike Mg nanostructures, which has several advantages over previous investigations such as suitable for mass production, reduced impurities, tailored dimensions, and easier integration into microsystem. 3D Mg nanostructures are realized onto silicon substrate using a conventional thermal evaporator, where the incident angle of Mg vapor flux with respect to the substrate surface normal is fixed at 88 deg. The as-prepared 3D Mg nanostructures are characterized by scanning electron microscopy, x-ray diffraction, energy dispersive x-ray analysis, transmission electron microscopy, high-resolution transmission electron microscopy, and surface area measurement.

36 MATERIALS SCIENCE↗

High-phase-purity zinc-blende InN on r-plane sapphire substrate with controlled nitridation pretreatment

High-phase-purity zinc-blende (zb) InN thin film has been grown by plasma-assisted molecular-beam epitaxy on r-plane sapphire substrate pretreated with nitridation. X-ray diffraction analysis shows that the phase of the InN films changes from wurtzite (w) InN to a mixture of w-InN and zb-InN, to zb-InN with increasing nitridation time. High-resolution transmission electron microscopy reveals an ultrathin crystallized interlayer produced by substrate nitridation, which plays an important role in controlling the InN phase. Photoluminescence emission of zb-InN measured at 20 K shows a peak at a very low energy, 0.636 eV, and an absorption edge at {approx}0.62 eV is observed at 2 K, which is the lowest bandgap reported to date among the III-nitride semiconductors.

36 MATERIALS SCIENCE↗

Features of formation and propagation of 60 deg. and 90 deg. misfit dislocations in Ge{sub x}Si{sub 1-x}/Si (x{approx}0.4-0.5) films caused by Si substrate misorientation from (001)

We have studied the dislocation structure at the initial stage of relaxation of Ge{sub x}Si{sub 1-x} films (x{approx}0.4-0.5) grown on Si substrates tilted 6 deg. about the <011> axis. It is demonstrated that edge misfit dislocations (MDs) in the miscut direction arise in the form of short segments on intersections of 60 deg. MDs. Substrate misorientation from the singular plane made it possible to discover the MD configurations consisting of a short segment of an edge MD and only two 60 deg. MDs diverging from this segment in the miscut direction.

36 MATERIALS SCIENCE↗

Measuring the Ion Flux to the Deposition Substrate in the Hollow Cathode Plasma Jet

Measurements of positive ion flux to a negatively biased substrate for deposition of TiO{sub x} thin films by the hollow cathode plasma jet system are presented. Different methods of obtaining the bias of substrate and measuring the resulting ion flux were used for different bias frequencies. Pulsed DC bias, middle frequency 500 kHz bias, and 13.56 MHz RF bias were compared. For 13.56 MHz two different methods of ion flux determination were used. These measurements were performed for different bias voltage and discharge conditions.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Tilt generation in step-graded In{sub x}Ga{sub 1-x}As metamorphic pseudosubstrate on a singular GaAs substrate using a low-temperature grown InGaP interlayer

Metamorphic pseudosubstrates of In{sub 0.42}Ga{sub 0.58}As were grown by molecular beam epitaxy using step-graded In{sub x}Ga{sub 1-x}As buffer layers grown either directly on a (001) GaAs substrate or on a GaAs substrate overgrown with a layer of low-temperature grown In{sub 0.51}Ga{sub 0.49}P (LT-InGaP). The structures were examined using x-ray reciprocal space mapping to determine the characteristics of the pseudosubstrates and buffer layers. For the sample grown on the LT-InGaP layer, the pseudosubstrate exhibited an asymmetric tilt around [110] toward the [110] direction. Weak-beam dark-field electron imaging shows an imbalance of misfit dislocations with opposite sign Burgers vector. An explanation for this tilt is given and it is suggested that it may be responsible for the improved quality of epitaxial layers grown on such pseudosubstrates.

36 MATERIALS SCIENCE↗

Vacancy engineering by optimized laser irradiation in boron-implanted, preamorphized silicon substrate

In this letter, the effect of vacancies generated by preirradiated laser on dopant diffusion and activation in preamorphized silicon substrate has been studied. Laser-induced melting in silicon was used to generate excess vacancies near the maximum melt depth before silicon substrate amorphization and subsequent boron implantation. We demonstrate that by matching the preirradiated laser melt depth with the implant amorphize depth, it can effectively reduce the silicon self-interstitials released from the end-of-range defect band. The results show great suppression in boron transient enhanced diffusion and significant removal of end-of-range defects. This is attributed to the recombination of laser-generated excess vacancies with preamorphizing induced free silicon interstitials at the end-of-range region.

36 MATERIALS SCIENCE↗

Texture of NiSi Films on Si(001), (111), and (110) Substrates

Synchrotron radiation was used to study the texture of poly-crystalline NiSi films that were formed by a solid state reaction between a 30 nm Ni film and Si(001), (111), and (110) substrates. All films were strongly textured, and the different texture components were identified. Apart from the spots and/or circles characteristic of epitaxy or fiber texture, the pole figures contained symmetrical, though complex, patterns of lines. These lines are characteristic of axiotaxy, whereby NiSi grains preferentially align their (211)- or (202)-type planes parallel to Si(110)-type planes in each of the substrates. Since the spacing between NiSi(211) or NiSi(202) planes is almost identical to the spacing of 1.920?Angstroms between Si(220) planes, the alignment of these planes results in a boundary structure that is periodic along a single direction in the plane of the interface. Intensity variations along the lines on the pole figures are also explained by the degree of periodicity of the interface. The brightest spots on the lines correspond to interface structures for which periodicity is achieved along two independent directions within the plane of the interface.

43 PARTICLE ACCELERATORS↗

Integration of thin layers of single-crystalline InP with flexible substrates

Transfer of thin semiconductor layers onto flexible substrates using a combination of ion cutting, adhesive bonding, and laser ablation was investigated. An {approx}1.3 {mu}m thick InP layer was first transferred onto sapphire using adhesive bonding and hydrogen-induced layer exfoliation at {approx}180 deg. C. The resulting structure was then adhesively bonded onto flexible polyethylene naphthalate substrate, followed by UV laser ablation of the first adhesive to separate the initial bond. Additional transfer steps were inserted into the process to enable thermal annealing and electrical recovery. The transferred films were electrically characterized and the potential use in high-speed, flexible electronics is discussed.

36 MATERIALS SCIENCE↗

High-coercivity SmCo{sub 5} thin films deposited on glass substrates

Structural and magnetic properties of SmCo{sub 5} thin films grown on glass substrates with a Cr underlayer were investigated. The nanocrystalline SmCo{sub 5} film with a (1120) texture exhibited high in-plane intrinsic coercivity up to 26.5 kOe and a large in-plane magnetic anisotropy. The crystallinity of the SmCo{sub 5} layer plays an important role, which is strongly dependent on the texture and the morphology of the Cr underlayer. A smooth Cr underlayer with a (200) texture and a good crystallinity is desired for the SmCo{sub 5} film with a good magnetic performance. This work demonstrates a process to achieve high intrinsic coercivity and large in-plane magnetic anisotropy SmCo{sub 5} films on glass substrates deposited at a relatively low temperature (400 deg. C)

36 MATERIALS SCIENCE↗

Influence of Si/Fe ratio in multilayer structures on crystalline growth of {beta}-FeSi{sub 2} thin film on Si substrate

The deposited Si/Fe ratio has been found to have a significant influence on crystalline growth of {beta}-FeSi{sub 2} film on Si substrate. Stoichiometry is always satisfied by interdiffusion of Si, under both Si-lean and Si-rich conditions. However, Si diffusion from the substrate into the deposited layer, which compensates for deficient Si, induces an undulated interface, as well as Fe and Si vacancies. On the other hand, excess Si is driven to the {beta}-FeSi{sub 2}/Si interface, which results in a lamellar structure with a large number of small grains. Fe and Si vacancies are significantly reduced by excess Si. These results suggest that precise control of the Si/Fe ratio is essential for good crystallinity and fewer vacancies.

36 MATERIALS SCIENCE↗

Multiple substrate microwave plasma-assisted chemical vapor deposition single crystal diamond synthesis

A multiple substrate, microwave plasma-assisted chemical vapor deposition synthesis process for single crystal diamond (SCD) is demonstrated using a 915 MHz reactor. Diamond synthesis was performed using input chemistries of 6-8% of CH{sub 4}/H{sub 2}, microwave input powers of 10-11.5 kW, substrate temperatures of 1100-1200 deg. C, and pressures of 110-135 Torr. The simultaneous synthesis of SCD over 70 diamond seeds yielded good quality SCD with deposition rates of 14-21 {mu}m/h. Multiple deposition runs totaling 145 h of deposition time added 1.8-2.5 mm of diamond material to each of the 70 seed crystals.

36 MATERIALS SCIENCE↗

Ion composition produced by high power impulse magnetron sputtering discharges near the substrate

Plasma composition near the substrate was investigated in a high power impulse magnetron sputtering (HIPIMS) discharge using Langmuir probe analysis, mass spectroscopy, and atomic absorption spectroscopy. The HIPIMS discharge was operated in nonreactive Ar atmosphere at a pressure of 2.66 Pa and the magnetron cathode was furnished with Ti target. Plasma density, metal ion-to-neutral ratio, and gas ion-to-metal ion ratio were studied as a function of discharge current. At peak discharge current densities of {approx}1 A cm{sup -2}, the results show that a dense plasma (n{sub e}{approx}10{sup 18} m{sup -3}) expanded from the target toward the substrate and lasted more than 330 {mu}s after the supplied power was turned off. The shape of the time-averaged ion energy distribution function of sputtered material exhibited a transition from Thompson to Maxwellian distribution, indicating efficient energy transfer in the discharge. The metal content in the plasma monotonically increased with discharge current and the metal ion-to-neutral ratio reached approximately 1:1 in the postdischarge plasma at peak current density of 5 A cm{sup -2}.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Substrate misorientation induced strong increase in the hole concentration in Mg doped GaN grown by metalorganic vapor phase epitaxy

We demonstrate that relatively small GaN substrate misorientation can strongly change hole carrier concentration in Mg doped GaN layers grown by metalorganic vapor phase epitaxy. In this work intentionally misoriented GaN substrates (up to 2 deg. with respect to ideal <0001> plane) were employed. An increase in the hole carrier concentration to the level above 10{sup 18} cm{sup -3} and a decrease in GaN:Mg resistivity below 1 {omega} cm were achieved. Using secondary ion mass spectroscopy we found that Mg incorporation does not change with varying misorientation angle. This finding suggests that the compensation rate, i.e., a decrease in unintentional donor density, is responsible for the observed increase in the hole concentration. Analysis of the temperature dependence of electrical transport confirms this interpretation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetotransport properties of c-axis oriented La{sub 0.7}Sr{sub 0.3}MnO{sub 3} thin films on MgO-buffered SiO{sub 2}/Si substrates

c-axis oriented La{sub 0.7}Sr{sub 0.3}MnO{sub 3} (LSMO) films on MgO-buffered SiO{sub 2}/Si substrates were prepared, and their texture, microstructure, and magnetotransport properties were studied and compared to epitaxial LSMO/MgO (001) and polycrystalline LSMO/SiO{sub 2}/Si films. c-axis oriented MgO buffer layers were obtained on amorphous SiO{sub 2} layer through rf sputter deposition at low substrate temperature and consequent postannealing processes. In situ pulsed laser deposition-grown LSMO films, deposited on the MgO layer, show strong c-axis texture, but no in-plane texture. The c-axis oriented LSMO films which are magnetically softer than LSMO/SiO{sub 2}/Si films exhibit relatively large low field magnetoresistance (LFMR) and sharper MR drop at lower field. The large LFMR is attributed to a spin-dependent scattering of transport current at the grain boundaries.

36 MATERIALS SCIENCE↗

Effect of substrate roughness on c-oriented AlN thin films

(001)-textured AlN thin films as needed for bulk acoustic wave devices exhibit large mechanical stress variations as a function of growth substrate properties. We studied the relationship between stress and the surface morphology of a thermally oxidized silicon substrate that was modified by a thin amorphous silicon layer. A rms roughness of 0.1-1.1 nm of the latter resulted in an increase in mechanical stress in the subsequently sputtered AlN thin film going from -700 to +200 MPa. At the same time, the x-ray rocking curve width of AlN increased from 1.3 deg. to 2.3 deg. The roughness of the Si interlayer was controlled by the Ar sputter pressure. Interestingly, the maximal roughness is obtained at an intermediate pressure. This is explained by an interplay of nucleation and diffusion phenomena governed by the kinetics of impinging atoms and ions. The Si interlayer was essential to avoid cracking of membranes exhibiting mixed Pt and SiO{sub 2} surfaces below the AlN film.

36 MATERIALS SCIENCE↗

Room-temperature operation of a 2.25 {mu}m electrically pumped laser fabricated on a silicon substrate

We report on a GaSb-based type-I laser structure grown by molecular beam epitaxy on a (001) silicon substrate. A thin AlSb nucleation layer followed by a 1 {mu}m thick GaSb buffer layer was used to accommodate the very large lattice mismatch existing with the silicon substrate. Processed devices with mesa geometry exhibited laser operation in pulsed mode with a duty cycle up to 10% at room temperature.

36 MATERIALS SCIENCE↗

High mobility holes in a strained Ge quantum well grown on a thin and relaxed Si{sub 0.4}Ge{sub 0.6}/LT-Si{sub 0.4}Ge{sub 0.6}/Si(001) virtual substrate

Epitaxial growth of a compressively strained Ge quantum well (QW) on an ultrathin, 345 nm thick, Si{sub 0.4}Ge{sub 0.6}/LT-Si{sub 0.4}Ge{sub 0.6}/Si(001) virtual substrate (VS) has been demonstrated. The VS, grown with a low temperature Si{sub 0.4}Ge{sub 0.6} seed layer on a Si(001) substrate, is found to be fully relaxed and the Ge QW is fully strained. The temperature dependence of Hall mobility and carrier density clearly indicates a two-dimensional hole gas in the Ge QW. At room temperature, which is more relevant for electronic devices applications, the samples show a very high Hall mobility of 1235 cm{sup 2} V{sup -1} s{sup -1} at a carrier density of 2.36x10{sup 12} cm{sup -2}.

36 MATERIALS SCIENCE↗