Search NASA⌕ Search

SEARCH · Search NASA

Results for “Microprobe”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,693 records · Page 94

Delta-doping of boron atoms by photoexcited chemical vapor deposition

Boron delta-doped structures in Si crystals were fabricated by means of photoexcited chemical vapor deposition (CVD). Core electronic excitation with high-energy photons ranging from vacuum ultraviolet to soft x rays decomposes B{sub 2}H{sub 6} molecules into fragments. Combined with in situ monitoring by spectroscopic ellipsometry, limited number of boron hydrides can be delivered onto a Si(100) surface by using the incubation period before the formation of a solid boron film. The boron-covered surface is subsequently embedded in a Si cap layer by Si{sub 2}H{sub 6} photo-excited CVD. The crystallinity of the Si cap layer depended on its thickness and the substrate temperature. The evaluation of the boron depth profile by secondary ion mass spectroscopy revealed that boron atoms were confined within the delta-doped layer at a concentration of 2.5 x 10{sup 20} cm{sup -3} with a full width at half maximum of less than 9 nm, while the epitaxial growth of a 130-nm-thick Si cap layer was sustained at 420 deg. C.

36 MATERIALS SCIENCE↗

Optimizing charge neutralization for a magnetic sector SIMS instrument in negative mode

Successful self-adjusted charge compensation was demonstrated for a CAMECA magnetic-sector secondary ion mass spectrometer applied in negative mode. Operation with the normal-incidence electron gun (NEG) potential positively biased relative to a sample potential enables substantial broadening of the Cs primary-ion-current density range available for analysis of insulators. The decrease of the negative NEG potential by 30 V allows the highest value of primary current density used for the analysis of a silica sample to increase by a factor of more than 6. By applying the improved charge neutralization technique, accurate Na depth profiles for SiO{sub 2} samples were obtained within detection limits of {approx}3 Multiplication-Sign 10{sup 15} atoms/cm{sup 3}.

42 ENGINEERING↗

Surface characterization of Zr/Ti/Nb tri-layered films deposited by magnetron sputtering on Si(111) and stainless steel substrates

Among metallic materials, commercially pure titanium and titanium alloys are very often used as biomaterials for implants. Among these alloys, titanium-aluminum-vanadium alloy Ti-6 A-4 V is one of the most commonly used due to its excellent biocompatibility and ability to allow bone-implant integration. A new class of Ti alloys employs Zr for solid-solution hardening and Nb as {beta}-phase stabilizer. Metals such as Ti, Nb, and Zr-known as valve metals-usually have their surfaces covered by a thin oxide film that forms spontaneously in air. This oxide film constitutes a barrier between the metal and the medium. The Ti-Nb-Zr alloys have mechanical and corrosion resistance characteristics which make them suitable for use as implants. Tri-layered films of Ti-Nb-Zr were deposited on both Si(111) and stainless steel (SS) substrates using dc magnetron sputtering equipment, under an argon atmosphere according to the following methodology: a 100 nm thick layer of Nb was deposited on the substrate, followed by a 200 nm thick layer of Ti, and finally a 50 nm thick layer of Zr, on top of the multilayer stack. The morphology and chemical composition of the films were analyzed by atomic force microscopy (AFM), x-ray photoelectron spectroscopy (XPS), and time-of-flight secondary ion mass spectrometry (ToF-SIMS). AFM images showed that the Zr/Ti/Nb tri-layer films presented nanostructured grains and low roughness. The ToF-SIMS depth profiles confirmed the formation of a three-layered film on Si(111) with well-defined and sharp interfaces between the layers, while the deposition on the stainless steel substrate caused slight intermixing at the different alloy/Nb, Nb/Ti and Ti/Zr interfaces, reflecting the greater roughness of the raw substrate. The XPS results for the Zr/Ti/Nb layers deposited on Si(111) and SS confirmed that the outermost layer consisted of Zr only, with a predominance of ZrO{sub 2}, as the metal layer is passivated in air. An oxidation treatment of 1000 Degree-Sign C in air for 1 h for the multilayer stacks caused some dewetting with Si(111) films, and alloying in the layers. The latter effect was more pronounced for the stainless steel substrate.

36 MATERIALS SCIENCE↗

Comparison of beryllium oxide and pyrolytic graphite crucibles for boron doped silicon epitaxy

This article reports on the comparison of beryllium oxide and pyrolytic graphite as crucible liners in a high-temperature effusion cell used for boron doping in silicon grown by molecular beam epitaxy. Secondary ion mass spectroscopy analysis indicates decomposition of the beryllium oxide liner, leading to significant incorporation of beryllium and oxygen in the grown films. The resulting films are of poor crystal quality with rough surfaces and broad x-ray diffraction peaks. Alternatively, the use of pyrolytic graphite crucible liners results in higher quality films.

36 MATERIALS SCIENCE↗

Nanoscale compositional analysis of NiTi shape memory alloy films deposited by DC magnetron sputtering

The formation of surface oxide layer as well as compositional changes along the thickness for NiTi shape memory alloy thin films deposited by direct current magnetron sputtering at substrate temperature of 300 °C in the as-deposited condition as well as in the postannealed (at 600 °C) condition have been thoroughly studied by using secondary ion mass spectroscopy, x-ray photoelectron spectroscopy, and scanning transmission electron microscopy-energy dispersive x-ray spectroscopy techniques. Formation of titanium oxide (predominantly titanium dioxide) layer was observed in both as-deposited and postannealed NiTi films, although the oxide layer was much thinner (8 nm) in as-deposited condition. The depletion of Ti and enrichment of Ni below the oxide layer in postannealed films also resulted in the formation of a graded microstructure consisting of titanium oxide, Ni{sub 3}Ti, and B2 NiTi. A uniform composition of B2 NiTi was obtained in the postannealed film only below a depth of 200–250 nm from the surface. Postannealed film also exhibited formation of a ternary silicide (Ni{sub x}Ti{sub y}Si) at the film–substrate interface, whereas no silicide was seen in the as-deposited film. The formation of silicide also caused a depletion of Ni in the film in a region ∼250–300 nm just above the film substrate interface.

36 MATERIALS SCIENCE↗

SIMS of organics—Advances in 2D and 3D imaging and future outlook

Secondary ion mass spectrometry (SIMS) has become a powerful technique for the label-free analysis of organics from cells to electronic devices. The development of cluster ion sources has revolutionized the field, increasing the sensitivity for organics by two or three orders of magnitude and for large clusters, such as C{sub 60} and argon clusters, allowing depth profiling of organics. The latter has provided the capability to generate stunning three dimensional images with depth resolutions of around 5 nm, simply unavailable by other techniques. Current state-of-the-art allows molecular images with a spatial resolution of around 500 nm to be achieved and future developments are likely to progress into the sub-100 nm regime. This review is intended to bring those with some familiarity with SIMS up-to-date with the latest developments for organics, the fundamental principles that underpin this and define the future progress. State-of-the-art examples are showcased and signposts to more in-depth reviews about specific topics given for the specialist.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Surface characterization of nanomaterials and nanoparticles: Important needs and challenging opportunities

This review examines characterization challenges inherently associated with understanding nanomaterials and the roles surface and interface characterization methods can play in meeting some of the challenges. In parts of the research community, there is growing recognition that studies and published reports on the properties and behaviors of nanomaterials often have reported inadequate or incomplete characterization. As a consequence, the true value of the data in these reports is, at best, uncertain. With the increasing importance of nanomaterials in fundamental research and technological applications, it is desirable that researchers from the wide variety of disciplines involved recognize the nature of these often unexpected challenges associated with reproducible synthesis and characterization of nanomaterials, including the difficulties of maintaining desired materials properties during handling and processing due to their dynamic nature. It is equally valuable for researchers to understand how characterization approaches (surface and otherwise) can help to minimize synthesis surprises and to determine how (and how quickly) materials and properties change in different environments. Appropriate application of traditional surface sensitive analysis methods (including x-ray photoelectron and Auger electron spectroscopies, scanning probe microscopy, and secondary ion mass spectroscopy) can provide information that helps address several of the analysis needs. In many circumstances, extensions of traditional data analysis can provide considerably more information than normally obtained from the data collected. Less common or evolving methods with surface selectivity (e.g., some variations of nuclear magnetic resonance, sum frequency generation, and low and medium energy ion scattering) can provide information about surfaces or interfaces in working environments (operando or in situ) or information not provided by more traditional methods. Although these methods may require instrumentation or expertise not generally available, they can be particularly useful in addressing specific questions, and examples of their use in nanomaterial research are presented.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Properties of zinc oxide films grown on sapphire substrates using high-temperature H{sub 2}O generated by a catalytic reaction on platinum nanoparticles

The authors investigated the characteristics of ZnO films grown on a-plane (11-20) sapphire substrates at 773–873 K using a reaction between dimethylzinc and high-temperature H{sub 2}O generated by a catalytic reaction on Pt nanoparticles. The growth rate was 0.02–0.07 μm min{sup −1}. The largest electron mobility and the smallest residual carrier concentration for the ZnO films were 169 cm{sup 2} V{sup −1} s{sup −1} and 1.6 × 10{sup 17} cm{sup −3}, respectively. X-ray diffraction patterns for the ZnO films exhibited intense (0002) and (0004) peaks associated with ZnO (0001) planes. The minimum full width at half maximum of the ω-rocking curve for ZnO (0002) was less than 0.1°. In a ZnO film with a high electron mobility, no rotational domains were identified using a ZnO (10-10) ϕ scan. From secondary ion mass spectroscopy, a hydrogen concentration of 3 × 10{sup 18} cm{sup −3} and a boron concentration of 2–5 × 10{sup 17} cm{sup −3} were determined. These were identified as extrinsic donor impurities.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Mechanical and transparent conductive properties of ZnO and Ga-doped ZnO films sputtered using electron-cyclotron-resonance plasma on polyethylene naphtalate substrates

Transparent conductive ZnO and Ga-doped ZnO (GZO) films were deposited on polyethylene naphtalate (PEN) sheet substrates using electron cyclotron resonance plasma sputtering. Both ZnO and GZO films were highly adhesive to the PEN substrates without inserting an intermediate layer in the interface. When compared at the same thickness, the transparent conductive properties of GZO films on PEN substrates were only slightly inferior to those on glass substrates. However, the carrier concentration of ZnO films on PEN substrates was 1.5 times that of those on glass substrates, whereas their Hall mobility was only 60% at a thickness of 300 nm. The depth profile of elements measured by secondary ion mass spectroscopy revealed the diffusion of hydrocarbons out of the PEN substrate into the ZnO film. Hence, doped carbons may act as donors to enhance carrier concentration, and the intermixing of elements at the interface may deteriorate the crystallinity, resulting in the lower Hall mobility. When the ZnO films were thicker than 400 nm, cracks became prevalent because of the lattice mismatch strain between the film and the substrate, whereas GZO films were free of cracks. The authors investigated how rolling the films around a cylindrical pipe surface affected their conductive properties. Degraded conductivity occurred at a threshold pipe radius of 10 mm when tensile stress was applied to the film, but it occurred at a pipe radius of 5 mm when compressive stress was applied. These values are guidelines for bending actual devices fabricated on PEN substrates.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Atomic layer deposition of molybdenum oxide using bis(tert-butylimido)bis(dimethylamido) molybdenum

Molybdenum trioxide films have been deposited using thermal atomic layer deposition techniques with bis(tert-butylimido)bis(dimethylamido)molybdenum. Films were deposited at temperatures from 100 to 300 °C using ozone as the oxidant for the process. The Mo precursor was evaluated for thermal stability and volatility using thermogravimetric analysis and static vapor pressure measurements. Film properties were evaluated with ellipsometry, x-ray photoelectron spectroscopy, secondary ion mass spectroscopy, and secondary electron microscopy. The growth rate per cycle was determined to extend from 0.3 to 2.4 Å/cycle with <4% nonuniformity (1-sigma) with-in-wafer across a 150 mm wafer for the investigated temperature range.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

TOF SIMS analysis and generation of white photoluminescence from strontium silicate codoped with europium and terbium

White light emitting terbium (Tb{sup 3+}) and europium (Eu{sup 3+}) codoped strontium silicate (Sr{sub 2}SiO{sub 4}) phosphors were prepared by a solid state reaction process. The structure, particle morphology, chemical composition, ion distribution, photoluminescence (PL), and decay characteristics of the phosphors were analyzed by x-ray diffraction (XRD), scanning electron microscopy (SEM), time-of-flight secondary ion mass spectrometry (TOF-SIMS), and PL spectroscopy, respectively. The XRD data showed that our Sr{sub 2}SiO{sub 4} composed of two phases, namely, β-Sr{sub 2}SiO{sub 4} and α′-Sr{sub 2}SiO{sub 4}, and the α′-Sr{sub 2}SiO{sub 4} phase was more prominent than the β-Sr{sub 2}SiO{sub 4} phase. The SEM micrographs showed that the particles were agglomerated together and they did not have definite shapes. All ions (i.e., negative and positive) present in our materials were identified by TOF-SIMS. In addition, the chemical imaging performed with the TOF-SIMS demonstrated how the individual ions including the dopants (Eu{sup 3+} and Tb{sup 3+}) were distributed in the host lattice. White photoluminescence was observed when the Sr{sub 2}SiO{sub 4}:Tb{sup 3+}, Eu{sup 3+} phosphor was excited at 239 nm using a monochromatized xenon lamp as the excitation source. The phosphor exhibited fast decay lifetimes implying that it is not a good candidate for long afterglow applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Low sheet resistance titanium nitride films by low-temperature plasma-enhanced atomic layer deposition using design of experiments methodology

A design of experiments methodology was used to optimize the sheet resistance of titanium nitride (TiN) films produced by plasma-enhanced atomic layer deposition (PE-ALD) using a tetrakis(dimethylamino)titanium precursor in a N{sub 2}/H{sub 2} plasma at low temperature (250 °C). At fixed chamber pressure (300 mTorr) and plasma power (300 W), the plasma duration and N{sub 2} flow rate were the most significant factors. The lowest sheet resistance values (163 Ω/sq. for a 20 nm TiN film) were obtained using plasma durations ∼40 s, N{sub 2} flow rates >60 standard cubic centimeters per minute, and purge times ∼60 s. Time of flight secondary ion mass spectroscopy data revealed reduced levels of carbon contaminants in the TiN films with lowest sheet resistance (163 Ω/sq.), compared to films with higher sheet resistance (400–600 Ω/sq.) while transmission electron microscopy data showed a higher density of nanocrystallites in the low-resistance films. Further significant reductions in sheet resistance, from 163 Ω/sq. to 70 Ω/sq. for a 20 nm TiN film (corresponding resistivity ∼145 μΩ·cm), were achieved by addition of a postcycle Ar/N{sub 2} plasma step in the PE-ALD process.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Improved oxidation resistance of organic/inorganic composite atomic layer deposition coated cellulose nanocrystal aerogels

Cellulose nanocrystal (CNC) aerogels are coated with thin conformal layers of Al{sub 2}O{sub 3} using atomic layer deposition to form hybrid organic/inorganic nanocomposites. Electron probe microanalysis and scanning electron microscopy analysis indicated the Al{sub 2}O{sub 3} penetrated more than 1500 μm into the aerogel for extended precursor pulse and exposure/purge times. The measured profile of coated fiber radius versus depth from the aerogel surface agrees well with simulations of precursor penetration depth in modeled aerogel structures. Thermogravimetric analysis shows that Al{sub 2}O{sub 3} coated CNC aerogel nanocomposites do not show significant thermal degradation below 295 °C as compared with 175 °C for uncoated CNC aerogels, an improvement of over 100 °C.

36 MATERIALS SCIENCE↗

Optimization of a plasma immersion ion implantation process for shallow junctions in silicon

A plasma immersion ion implantation (PIII) process has been developed for realizing shallow doping profiles of phosphorus and boron in silicon using an in-house built dual chamber cluster tool. High Si etch rates observed in a 5% PH{sub 3} in H{sub 2} plasma have been ascribed to high concentration of H(α) radicals. Therefore, subsequent work was carried out with 5% PH{sub 3} in He, leading to much smaller etch rates. By optical emission spectroscopy, the radical species H(α), PH*{sub 2}, and PH* have been identified. The concentration of all three species increased with pressure. Also, ion concentrations increased with pressure as evidenced by Langmuir data, with a maximum occurring at 0.12 mbar. The duty cycle of pulsed DC bias has a significant bearing on both the implantation and the etching process as it controls the leakage of positive charge collected at the surface of the silicon wafer during pulse on-time generated primarily due to secondary electron emission. The P implant process was optimized for a duty cycle of 10% or less at a pressure of 0.12 mbar with implant times as low as 30 s. Secondary ion mass spectroscopy showed a P dopant depth of 145 nm after rapid thermal annealing (RTA) at 950 °C for 5 s, resulting in a sheet resistance of 77 Ω/◻. Si n{sup +}/p diodes fabricated with phosphorus implantation using optimized PIII and RTA conditions exhibit J{sub on}/J{sub off} > 10{sup 6} with an ideality factor of nearly 1.2. Using similar conditions, shallow doping profiles of B in silicon have also been realized.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Molecular layer deposition of alucone films using trimethylaluminum and hydroquinone

A hybrid organic–inorganic polymer film grown by molecular layer deposition (MLD) is demonstrated here. Sequential exposures of trimethylaluminum [Al(CH{sub 3}){sub 3}] and hydroquinone [C{sub 6}H{sub 4}(OH){sub 2}] are used to deposit the polymeric films, which is a representative of a class of aluminum oxide polymers known as “alucones.” In-situ quartz crystal microbalance (QCM) studies are employed to determine the growth characteristics. An average growth rate of 4.1 Å per cycle at 150 °C is obtained by QCM and subsequently verified with x-ray reflectivity measurements. Surface chemistry during each MLD-half cycle is studied in depth by in-situ Fourier transform infrared (FTIR) vibration spectroscopy. Self limiting nature of the reaction is confirmed from both QCM and FTIR measurements. The conformal nature of the deposit, typical for atomic layer deposition and MLD, is verified with transmission electron microscopy imaging. Secondary ion mass spectroscopy measurements confirm the uniform elemental distribution along the depth of the films.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Atomic layer deposition of aluminum sulfide thin films using trimethylaluminum and hydrogen sulfide

Sequential exposures of trimethylaluminum and hydrogen sulfide are used to deposit aluminum sulfide thin films by atomic layer deposition (ALD) in the temperature ranging from 100 to 200 °C. Growth rate of 1.3 Å per ALD cycle is achieved by in-situ quartz crystal microbalance measurements. It is found that the growth rate per ALD cycle is highly dependent on the purging time between the two precursors. Increased purge time results in higher growth rate. Surface limited chemistry during each ALD half cycle is studied by in-situ Fourier transformed infrared vibration spectroscopy. Time of flight secondary ion-mass spectroscopy measurement is used to confirm elemental composition of the deposited films.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Room temperature atomic layerlike deposition of ZnS on organic thin films: Role of substrate functional groups and precursors

The room temperature atomic layerlike deposition (ALLD) of ZnS on functionalized self-assembled monolayers (SAMs) was investigated, using diethyl zinc (DEZ) and in situ generated H{sub 2}S as reactants. Depositions on SAMs with three different terminal groups, –CH{sub 3,} –OH, and –COOH, were studied. It was found that the reaction of DEZ with the SAM terminal group is critical in determining the film growth rate. Little or no deposition is observed on –CH{sub 3} terminated SAMs because DEZ does not react with the methyl terminal group. ZnS does deposit on both –OH and –COOH terminated SAMs, but the grow rate on –COOH terminated SAMs is ∼10% lower per cycle than on –OH terminated SAMs. DEZ reacts with the hydroxyl group on –OH terminated SAMs, while on –COOH terminated SAMs it reacts with both the hydroxyl and carbonyl bonds of the terminal groups. The carbonyl reaction is found to lead to the formation of ketones rather than deposition of ZnS, lowering the growth rate on –COOH terminated SAMs. SIMS spectra show that both –OH and –COOH terminated SAMs are covered by the deposited ZnS layer after five ALLD cycles. In contrast to ZnO ALLD where the composition of the film differs for the first few layers on –COOH and –OH terminated SAMs, the deposited film composition is the same for both –COOH and –OH terminated SAMs. The deposited film is found to be Zn-rich, suggesting that the reaction of H{sub 2}S with the Zn-surface adduct may be incomplete.

36 MATERIALS SCIENCE↗

Quantitative imaging of trace B in Si and SiO{sub 2} using ToF-SIMS

Changes in the oxidation state of an element can result in significant changes in the ionization efficiency and hence signal intensity during secondary ion mass spectrometry (SIMS) analysis; this is referred to as the SIMS matrix effect [Secondary Ion Mass Spectrometry: A Practical Handbook for Depth Profiling and Bulk Impurity Analysis, edited by R. G. Wilson, F. A. Stevie, and C. W. Magee (Wiley, New York, 1990)]. The SIMS matrix effect complicates quantitative analysis. Quantification of SIMS data requires the determination of relative sensitivity factors (RSFs), which can be used to convert the as measured intensity into concentration units [Secondary Ion Mass Spectrometry: A Practical Handbook for Depth Profiling and Bulk Impurity Analysis, edited by R. G. Wilson, F. A. Stevie, and C. W. Magee (Wiley, New York, 1990)]. In this manuscript, the authors report both: RSFs which were determined for quantification of B in Si and SiO{sub 2} matrices using a dual beam time of flight secondary ion mass spectrometry (ToF-SIMS) instrument and the protocol they are using to provide quantitative ToF-SIMS images and line scan traces. The authors also compare RSF values that were determined using oxygen and Ar ion beams for erosion, discuss the problems that can be encountered when bulk calibration samples are used to determine RSFs, and remind the reader that errors in molecular details of the matrix (density, volume, etc.) that are used to convert from atoms/cm{sup 3} to other concentration units will propagate into errors in the determined concentrations.

42 ENGINEERING↗