QXF Cold Mass Friction Test

The purpose of this test is to determine the longitudinal force on the stainless steel shell that is required to break the friction between the stainless steel shell and the aluminum shell underneath. This is achieved by suspending the short magnet between two backing plates on the eight grade 8 threaded rods which replace the 8 stainless steel toke tie rods in the magnet assembly. Eight hydraulic cylinders are mounted to each backing plate. Six, 22" sections of the stainless steel shell are welded in place on the magnet, each of which has a slightly different developed length, starting from the baseline design, and becoming progressively looser. A pushing flange is mounted to the stainless steel shells via small tack welds. Four load cells are then attached to the flange at designated points, while additional tooling is attached to each of the cylinders to facilitate the transfer of force from the cylinders to the stainless steel shell During the test, the cylinders will be slowly energized to no more than 7000 psi, with a resultant, longitudinal force on the flange of no more than 125,400 lbf. For each set of shells, the test ends when the load cell monitoring software detects a sharp decrease in force. This will indicate that the friction has broken. The cullenders will then be de-energized and the cycle will repeat for the next test. Welding operations outlined in the procedure (US-HiLumi-doc-4200) are outside the scope of the HA as the work is occurring under a previously-issued burn permit by qualified welders.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Surface Tagging of Al 6061-T6 using Photoluminescent Oxides

The goal of tagging nuclear fuels (or related materials, such as fuel cladding) is to provide a persistent marker, traceable to the fuel manufacturer, that can be detected after some length of time, likely after the fuel has been lost, rerouted, or partially destroyed. Ideally, the tag is complicated enough to encode data pertaining to the provenance (manufacturer, date or time, constituents, etc.) and robust enough to survive in-pile exposure and/or further destruction. The taggant should not change the behavior or performance of the fuel in any meaningful way. Photoluminescent tagging was an attractive solution to many of these challenges, as it is undetectable under normal lighting conditions, visible to the naked eye under specific lighting conditions, does not require a significant quantity of material to be photoluminescent, observable with simple commercial detection tools, and is versatile and robust in application. In FY23, the team focused on embedding photoluminescent taggants onto the replicate fuel cladding surface using welding. From a welding standpoint, photoluminescent taggants, in the form of oxides, are a viable option for tagging because the taggants have high melting points, and thus likely to survive welding temperatures (i.e., remain as a secondary phase particle and maintain luminescent properties). Additionally, these taggants have the potential to act as a metal matrix composite which may increase the strength-to-weight ratio, stiffness, and ductility of the base material, all beneficial to cladding and fuel performance.

98 NUCLEAR DISARMAMENT, SAFEGUARDS, AND PHYSICAL P↗

Rolling Behavior of Surface Tagged Aluminum 6061 using Photoluminescent Oxides

Physical tagging of nuclear fuel is potentially one way of tracking throughout the fuel lifecycle. The process of tagging can take many forms, but one promising method is to embed a small amount of photoluminescent particles in the surface of a material which are not detectable under normal illumination but are readily visible under excitation by ultraviolet light. The goal of this project was to explore the potential to tag simulated nuclear fuel cladding with small ceramic particles, via laser beam welding or gas tungsten arc welding, and measure the photoluminescent response. Surface tagging using this method has demonstrated viability and detectability throughout this project; work in FY24 focused on the survivability of these tags through subsequent deformation processing similar to what taggants in a fuel manufacturing environment would be subjected to. This work demonstrated that particles are readily visible in the as-welded state (i.e., before subsequent rolling treatment to represent mechanical processing of a fuel material), but visibility is reduced as the deformation is induced. Despite the reduction in photoluminescence, the taggants are still visible after rolling processes are performed, making this surface tagging technique a promising candidate for nuclear fuel cladding tagging. This work demonstrated, though, that targeted optimization work would be necessary to develop a robust taggant depending on the fidelity and luminescent properties required.

36 MATERIALS SCIENCE↗

Understanding the Thermal Physics and Metallurgy of Metal Big Area Additive Manufacturing

The research goal of this EPSCoR-DOE partnership is to mitigate defects in parts made using a new type of additive manufacturing (AM) process called metal Big Area Additive Manufacturing (m-BAAM). To realize this goal, the PIs will detect and correct defects in the part as it is being printed by combining fundamental knowledge of the thermal physics and metallurgy of m-BAAM with in-process sensor data. Developed at the DOE-funded Manufacturing Demonstration Facility at Oak Ridge National Laboratory, the m-BAAM process involves one or more robots working together to produce a part by fusing metal wire layer-by-layer using arc welding. The process can print large metal parts such as turbine blades, which is not possible using other AM processes. In addition, m-BAAM production rates are more than ten times faster than other AM processes while requiring one-tenth of the material cost. Despite their potential to become a critical force multiplier in the energy generation industry, m-BAAM parts may fail to print accurately due to retention of heat and uneven cooling. Overheating and anomalous cooling rates in turn can cause inconsistencies in the microstructure, leading to sudden failure when used in safety-critical applications. In other words, flaw formation in m-BAAM parts is governed by the thermal history – intensity and spatial distribution of heat inside the part during printing. The thermal history is a complex function of the part shape and process settings such as welding energy, path taken by the welding torch for deposition (tool path), wire feed rate, among others.

36 MATERIALS SCIENCE↗

RESULTS OF EXPERIMENT TO DETERMINE CORROSION RATES FOR 304L IN HB-LINE DISSOLVER VESSEL VENTILATION SYSTEM

Radioactive material being processed as part of the DE3013 program for HB-Line will result in the presence of chlorides, and in some cases fluorides, in the dissolver. Material Science and Technology developed an experimental plan to evaluate the impact of chloride on corrosion of the dissolver vessel ventilation system. The plan set test variables from the proposed operating parameters, previous test results, and a desired maximum chloride concentration for processing. The test variables included concentrations of nitric acid, fluorides and chlorides, and the presence of a welded and stressed metal coupon. Table 1 contains expected general corrosion rates in the HB-Line vessel vent system from dissolution of 3013 contents of varying nitric acid and chloride content. These general corrosion rates were measured upstream of the condenser in the experiment's offgas system near the entrance to the dissolver. However, they could apply elsewhere in the offgas system, depending on factors not simulated in the testing, including offgas system temperatures and airflow. Localized corrosion was significant in Tests One, Two, and Three. This corrosion is significant because it will probably be the first mode of penetration of the 304L steel in several places in the system. See Table 2. For Tests One and Three, the penetration rate of localized corrosion was much higher than that for general corrosion. It was approximately four times higher in Test One and at least 45 times higher in Test Three, penetrating an entire coupon thickness of 54 mils in 186 hours or less. There was no significant difference in corrosion between welded areas and un-welded areas on coupons. There was also no significant attack on stressed portions of coupons. It is probable that the lack of corrosion was because the stressed areas were facing downwards and offered no place for condensation or deposits to form. Had deposits formed, pitting may have occurred and led to stress corrosion cracking. The significant localized corrosion observed was usually associated with deposits. General corrosion on the offgas coupons was extremely high for the test containing 10,000 ppm chloride in the dissolver solution. Localized corrosion caused deep penetration of coupon surfaces with a solution of 2000 ppm chloride, both at 12 M and 8 M nitric acid. We recommend that when processing chloride-containing solutions, the pre-condenser side of the vessel vent system be inspected at a frequency calculated from acceptable material losses and expected general corrosion rate. The presence of deposits and heavy condensation during inspection should be taken as indicators of possibly severe localized corrosion.

36 MATERIALS SCIENCE↗

A STRUCTURAL IMPACT ASSESSMENT OF FLAWS DETECTED DURING ULTRASONIC EXAMINATION OF TANK 15

Ultrasonic (UT) inspection of Tank 15 was conducted between April and July 2007 in accordance with the Tank 15 UT inspection plan. This was a planned re-inspection of this tank, the previous one was performed in 2002. Ten cracks were characterized in the previous examination. The re-inspection was performed to verify the present models and understanding for stress corrosion cracking. During this re-examination, one indication that was initially reported as a 'possible perpendicular crack <25% through wall' in 2002, was clearly shown not to be a crack. Additionally, examination of a new area immediately adjacent to other cracks along a vertical weld revealed three new cracks. It is not known when these new cracks formed as they could very well have been present in 2002 as well. Therefore, a total of twelve cracks were evaluated during the re-examination. A critical review of the information describing stress corrosion crack behavior for the SRS waste tanks, as well as a summary review of the service history of Tank 15, was performed. Each crack was then evaluated for service exposure history, consistency of the crack behavior with the current understanding of stress corrosion cracking, and present and future impact to the structural integrity of the tank. Crack instability calculations were performed on each crack for a bounding waste removal loading condition in Tank 15. In all cases, the crack behavior was determined to be consistent with the previous understanding of stress corrosion cracking in the SRS waste tank environment. The length of the cracks was limited due to the short-range nature of the residual stresses near seam, repair and attachment welds. Of the twelve cracks, nine were located in the vapor space above the sludge layer, including the three new cracks. Comparison of the crack lengths measured in 2002 and 2007 revealed that crack growth had occurred in four of the six previously measured vapor space cracks. However, the growth remained within the residual stress zone. None of the three cracks beneath the sludge showed evidence of growth. The impact of the cracks that grew on the future service of Tank 15 was also assessed. Tank 15 is expected to undergo closure activities including sludge waste removal. A bounding loading condition for waste removal of the sludge at the bottom of Tank 15 was considered for this analysis. The analysis showed that the combination of hydrostatic, seismic, pump and weld residual stresses are not expected to drive any of the cracks identified during the Tank 15 UT inspection to instability. Wall thickness mapping for general thinning and pitting was also performed. No significant wall thinning was observed. The average wall thickness values were well above nominal. Two isolated pit-like indications were observed. Both were approximately 30 mils deep. However, the remaining wall thickness was still greater than nominal specified for the original construction plate material. It was recommended that a third examination of selected cracks in Tank 15 be performed in 2014. This examination would provide information to determine whether any additional detectable degradation is occurring in Tank 15 and to supplement the basis for characterization of conditions that are non-aggressive to tank corrosion damage. The in-service inspection program is re-evaluated on a three year periodicity. The Type I and II tanks are not active receipt tanks at present, and are therefore not a part of the In-Service Inspection Program for the Type III Tanks [1]. Changes to the mission for Tank 15 and other Type I and II tanks may be considered by the In-Service Inspection Review Committee (ISIRC) and the program adjusted accordingly.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Development of PWHT-Free, Reduced Activation Creep-Strength Enhanced Bainitic Ferritic Steel for Large-Scale Fusion Reactor Components

A compositional modification has been proposed to validate an alloy design which potentially eliminates the requirement of post-weld heat treatment (PWHT) while preserving the advantage of mechanical properties in a reduced activation bainitic ferritic steel based on Fe-3Cr-3W-0.2V- 0.1Ta-Mn-Si-C, in weight percent, developed at Oak Ridge National Laboratory in 2007. The alloy design includes reducing the hardness in the as-welded condition for improving toughness, while increasing the hardenability for preserving the high-temperature mechanical performance such as creep-rupture resistance in the original steel. To achieve such a design, a composition range with a reduced C content combining with an increased Mn content has been proposed and investigated. Newly proposed “modified” steel successfully achieved an improved impact toughness in the as- welded condition, while the creep-rupture performance across the weldments without PWHT demonstrated ~50% improvement of the creep strength compared to that of the original steel weldment after PWHT. The obtained results strongly support the validity of the proposed alloy design.

Yamamoto, Yukinori↗

Altering the Supply of Shielding Gases to Fabricate Distinct Geometry in GMA Additive Manufacturing

Wire arc additive manufacturing (WAAM) is the process by which large, metallic structures are built, layer-by-layer, using a welding arc to melt wire feedstock. In this process, the proper selection of the shielding gas plays a vital role in the achievement of structurally acceptable part geometries and quality surface finishes. In this study, the authors used either a ternary mix (He, Ar and CO 2 ) or a binary mix (Ar and CO 2 ) of shielding gases to deposit wall geometries using an open loop-controlled WAAM system developed at Oak Ridge National Laboratory’s Manufacturing Demonstration Facility. The binary blend produced a wider and shorter geometry, while the ternary blend resulted in a narrower build that was more equivalent to the CAD geometry. The data indicated that the binary blend provided a higher oxygen concentration in the weld as compared to that of the ternary blend. The results imply that the arc characteristics and heat input had a significantly higher impact on the weld penetration than the surface tension effect of surface active elements. This was further verified by developing and applying a high-fidelity computational fluid dynamics (CFD) model of the thermophysical properties of gas mixtures. The results from the model showed that, while the influence of increased oxygen concentration on the surface tension for the binary blend led to a deeper penetration, the ternary blend gave rise to heat flux to the workpiece.

36 MATERIALS SCIENCE↗

Analysis of Favorable Process Conditions for the Manufacturing of Thin-Wall Pieces of Mild Steel Obtained by Wire and Arc Additive Manufacturing (WAAM)

Here, one of the challenges in additive manufacturing (AM) of metallic materials is to obtain workpieces free of defects with excellent physical, mechanical, and metallurgical properties. In wire and arc additive manufacturing (WAAM) the influences of process conditions on thermal history, microstructure and resultant mechanical and surface properties of parts must be analyzed. In this work, 3D metallic parts of mild steel wire (American Welding Society-AWS ER70S-6) are built with a WAAM process by depositing layers of material on a substrate of a S235 JR steel sheet of 3 mm thickness under different process conditions, using as welding process the gas metal arc welding (GMAW) with cold metal transfer (CMT) technology, combined with a positioning system such as a computer numerical controlled (CNC) milling machine. Considering the hardness profiles, the estimated ultimate tensile strengths (UTS) derived from the hardness measurements and the microstructure findings, it can be concluded that the most favorable process conditions are the ones provided by CMT, with homogeneous hardness profiles, good mechanical strengths in accordance to conditions defined by standard, and without formation of a decohesionated external layer; CMT Continuous is the optimal option as the mechanical properties are better than single CMT.

36 MATERIALS SCIENCE↗

Benchmarking a 9Cr-2WVTa Reduced Activation Ferritic Martensitic Steel Fabricated via Additive Manufacturing

Reduced activation ferritic (RAF) martensitic steels are promising candidates for the first wall of fusion reactors. However, current manufacturing capabilities call for these components to be made by welding wrought plates. This limits design freedom and necessitates the use of post-weld heat treatments (PWHT) in accordance with the boiler and pressure vessel code. Additive manufacturing (AM) can offer a unique solution to solve this challenge by leveraging the layer-wise deposition strategy to come up with temper bead deposition techniques to eliminate post-processing heat treatments (PPHT). However, it is necessary to benchmark the properties of RAF steels fabricated by AM with their wrought counterparts to identify the process-structure-property correlation, which is the goal of this study. The study demonstrates that while tensile properties at room temperature and high temperatures are satisfactory, the as fabricated and samples after PPHT have significant heterogeneity in tensile elongation. This has been attributed to the presence of discontinuities in the build. The as-fabricated samples have an average tensile strength of 1190 + 12 MPa and an average elongation of 15 + 5% at room temperature and 658 ± 20 MPa ultimate tensile strength (UTS) and 14 ± 7% at 600 °C. After the post-weld heat treatment, mechanical properties decrease to around 600–650 MPa and an elongation between 20–25% at room temperature to 300 MPa UTS and 25–28% elongation at 600 °C. The characterization of microstructures at various length scales demonstrates that the as-fabricated structure has a significant fraction of delta ferrite in a lath martensitic matrix. No precipitates could be identified in the as-fabricated structure. PPHT led to a decrease in the area fraction of delta ferrite and precipitation of M 23 C 6 and MX. Detailed characterization clearly demonstrates that the lack of precipitates in the as-fabricated structure could be due to the slow tempering response of the alloy. Finally, the needs to develop new alloys to achieve the objectives stated above are articulated.

36 MATERIALS SCIENCE↗

Physical and Visual Evaluation of Filters for Direct Observation of the Sun and the International Standard ISO 12312-2:2015

We investigated the compliance of 43 commercially available solar filters (eclipse glasses) with the ISO 12312-2:2015 standard by measuring their spectral transmittances (280–2000 nm) and calculating their luminous, solar ultraviolet A, ultraviolet B, and infrared (IR) transmittances. We also evaluated the filters for usability by observing the full midday Sun and rating the view on a seven-point balanced scale, from “far too dark, details seen only with great difficulty” to “far too light, uncomfortable to view the Sun.” The mean ratings of two observers, one experienced and one inexperienced in solar observing, differed by 0.28 (95% confidence interval of the mean = 0.26). The inexperienced observer tended to be less accepting of high transmittances. All 43 solar filters complied with the UV and IR requirements. Eighteen filters passed the luminous transmittance requirements, and 24 were borderline too light or too dark. Seven of the 15 solar filters with a luminous transmittance darker than the requirement were rated as acceptable. One filter that passed and another that was borderline too light were rated as too light or far too light. The ISO 12312-2 limits derive from welding filter standards and do not represent an appropriate evidence base for direct solar viewing. This work provides the evidence base for a maximum 0.0012% and a minimum 0.00004% luminous transmittance for solar filters. The results of this study also support the use of welding filters between shades 12 and 16. Lighter welding filters are more acceptable than solar filters of the same luminous transmittance.

79 ASTRONOMY AND ASTROPHYSICS↗

Initial measurements of BN-350 spent fuel in dry storage casks using the dual slab verification detonator

The Dual Slab Verification Detector (DSVD) has been developed, built, and characterized by Los Alamos National Laboratory in cooperation with the International Atomic Energy Agency (IAEA) as part of the dry storage safeguards system for the spent fuel from the BN-350 fast reactor. The detector consists of two rows of 3He tubes embedded in a slab of polyethylene which has been designed to be placed on the outer surface of the dry storage cask. By performing DSVD measurements at several different locations around the outer surface of the DUC, a signature 'fingerprint' can be established for each DUC based on the neutron flux emanating from inside the dry storage cask. The neutron fingerprint for each individual DUC will be dependent upon the spatial distribution of nuclear material within the cask, thus making it sensitive to the removal of a certain amount of material from the cask. An initial set of DSVD measurements have been performed on the first set of dry storage casks that have been loaded with canisters of spent fuel and moved onto the dry storage pad to both establish an initial fingerprint for these casks as well as to quantify systematic uncertainties associated with these measurements. The results from these measurements will be presented and compared with the expected results that were determined based on MCNPX simulations of the dry storage facility. The ability to safeguard spent nuclear fuel is strongly dependent on the technical capabilities of establishing and maintaining continuity of knowledge (COK) of the spent fuel as it is released from the reactor core and either reprocessed or packaged and stored at a storage facility. While the maintenance of COK is often done using continuous containment and surveillance (C/S) on the spent fuel, it is important that the measurement capabilities exist to re-establish the COK in the event of a significant gap in the continuous CIS by performing measurements that independently confirm the presence and content of Plutonium (Pu) in the spent fuel. The types of non-destructive assay (NDA) measurements that can be performed on the spent fuel are strongly dependent on the type of spent fuel that is being safeguarded as well as the location in which the spent fuel is being stored. The BN-350 Spent Fuel Disposition Project was initiated to improve the safeguards and security of the spent nuclear fuel from the BN-350 fast-breeder reactor and was developed cooperatively to meet the requirements of the International Atomic Energy Agency (IAEA) as well as the terms of the 1993 CTR and MPC&A Implementing Agreements. The unique characteristics of fuel from the BN-350 fast-breeder reactor have allowed for the development of an integrated safeguards measurement program to inventory, monitor, and if necessary, re-verify Pu content of the spent fuel throughout the lifetime of the project. This approach includes the development of a safeguards measurement program to establish and maintain the COK on the spent fuel during the repackaging and eventual relocation of the spent-fuel assemblies to a long-term storage site. As part of the safeguards measurement program, the Pu content of every spent-fuel assembly from the BN-350 reactor was directly measured and characterized while the spent-fuel assemblies were being stored in the spent-fuel pond at the BN-350 facility using the Spent Fuel Coincidence Counter (SFCC). Upon completion of the initial inventory of the Pu content of the individual spent-fuel assemblies, the assemblies were repackaged into welded steel canisters that were filled with inert argon gas and held either four or six individual spent-fuel assemblies depending on the type of assembly that was being packaged. This repackaging of the spent-fuel assemblies was performed in order to improve the stability of the spent-fuel assemblies for long-term storage and increase the proliferation resistance of the spent fuel. To maintain the capability of verifying the presence of the spent-fuel assemblies inside the welded steel canisters, measurements were performed on the canisters using the Spent Fuel Attribute Monitor (SPAM), which was a neutron coincidence counter very similar in design to the SFCC, but with a larger operational volume to accommodate the canisters. The analysis of the neutron coincidence data from the measurements of the welded steel canisters using SP AM yielded a Canister Attribute (CA) that was shown to be proportional to the total amount of Pu mass that was present inside the canister and comparable to the CA values that were calculated based on the previous SFCC measurements. The next step in securing the spent fuel from the BN-350 reactor is the packaging of the steel canisters into Dual-Use Casks (DUCs) and the transportation of the DUCs to a remote dry storage site.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Corrosion resistant neutron absorbing coatings

A method of forming a corrosion resistant neutron absorbing coating comprising the steps of spray or deposition or sputtering or welding processing to form a composite material made of a spray or deposition or sputtering or welding material, and a neutron absorbing material. Also a corrosion resistant neutron absorbing coating comprising a composite material made of a spray or deposition or sputtering or welding material, and a neutron absorbing material.

36 MATERIALS SCIENCE↗

Integrated Recycling Test Fuel Fabrication

The Integrated Recycling Test is a collaborative irradiation test that will electrochemically recycle used light water reactor fuel into metallic fuel feedstock. The feedstock will be fabricated into a metallic fast reactor type fuel that will be irradiation tested in a drop in capsule test in the Advanced Test Reactor on the Idaho National Laboratory site. This paper will summarize the fuel fabrication activities and design efforts. Casting development will include developing a casting process and system. The closure welding system will be based on the gas tungsten arc burst welding process. The settler/bonder system has been designed to be a simple system which provides heating and controllable impact energy to ensure wetting between the fuel and cladding. The final major pieces of equipment to be designed are the weld and sodium bond inspection system. Both x-radiography and ultrasonic inspection techniques have been examine experimentally and found to be feasible, however the final remote system has not been designed. Conceptual designs for radiography and an ultrasonic system have been made.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Corrosion resistant neutron absorbing coatings

A method of forming a corrosion resistant neutron absorbing coating comprising the steps of spray or deposition or sputtering or welding processing to form a composite material made of a spray or deposition or sputtering or welding material, and a neutron absorbing material. Also a corrosion resistant neutron absorbing coating comprising a composite material made of a spray or deposition or sputtering or welding material, and a neutron absorbing material.

36 MATERIALS SCIENCE↗

An Empirical Study on Ultrasonic Testing in Lieu of Radiography for Nuclear Power Plants

Research is being conducted for the U.S. Nuclear Regulatory Commission (NRC) at the Pacific Northwest National Laboratory (PNNL) to assess the capability, effectiveness, and reliability of ultrasonic testing (UT) as a replacement method for radiographic testing (RT) for inspecting nuclear power plant (NPP) components. A primary objective of this work is to evaluate UT techniques to assess their ability to detect, locate, size, and characterize fabrication flaws in typical NPP weldments. This particular study focused on the evaluation of four carbon steel pipe-to-pipe welds on specimens that ranged in thicknesses from 19.05 mm (0.75 in.) to 27.8 mm (1.094 in.) and were 355.6 mm (14.0 in.) or 406.4 mm (16.0 in.) in diameter. The pipe welds contained both implanted (intentional) fabrication flaws as well as bonus (unintentional) flaws throughout the entire thickness of the weld and the adjacent base material. The fabrication flaws were a combination of planar and volumetric flaw types, including incomplete fusion, incomplete penetration, cracks, porosity, and slag inclusions. The examinations were conducted using phased-array UT (PA UT) techniques applied primarily for detection and length sizing of the flaws. Radiographic examinations were also conducted on the specimens with RT detection and length sizing results being used to establish true state. This paper will discuss the comparison of UT and RT (true state) detection results conducted to date along with a discussion on the technical gaps that need to be addressed before these methods can be used interchangeably for repair and replacement activities for NPP components.

NDE reliability↗

PERFORMANCE IMPROVEMENT OF CREEP-RESISTANT FERRITIC STEEL WELDMENTS THROUGH THERMO-MECHANICAL TREATMENT AND ALLOY DESIGN

Two different approaches have been proposed for improvement of cross-weld creep properties of the high temperature ferrous structural materials for fossil-fired energy applications. The traditional creep strength-enhanced ferritic (CSEF) steel weldments suffer from Type IV failures which occur at the fine-grained heat affected zone (FGHAZ). In order to minimize the premature failure at FGHAZ in the existing CSEF steels, such as modified 9Cr-1Mo ferritic-martensitic steels (Grade 91), a thermo-mechanical treatment consisting of aus-forging/rolling and subsequent aus-aging is proposed which promotes the formation of stable MX carbonitrides prior to martensitic transformation. Such MX remains undissolved during welding process, even in FGHAZ, which successfully improves the cross-weld creep properties. Another approach is to develop a new fully ferrtic, creep-resistant FeCrAl alloy which is essentially free from Type IV failure issues. Fe-30Cr-3Al base alloys with minor alloying additions were developed which achieved a combination of good oxidation/corrosion resistance and improved tensile and creep performance comparable or superior to Grade 92 steel.

Yamamoto, Yukinori↗