The role of N-Si-O bonding configurations in tunable photoluminescence of oxygenated amorphous silicon nitride films
Last year, we have reported that the internal quantum efficiency of photoluminescence (PL) from amorphous silicon oxynitride (a-SiN{sub x}O{sub y}) films has been achieved as high as 60%. The present work intensively investigated the mechanisms for tunable PL in the 2.05–2.95 eV range from our a-SiN{sub x}:O films, by using a combination of optical characterizations, X-ray photoelectron spectroscopy (XPS) and electron paramagnetic resonance (EPR) measurements. The results of XPS, EPR, and photoluminescence excited measurements indicated that the incorporation of oxygen atoms into silicon nitride (a-SiN{sub x}) networks not only reduced the band tail structure disorder (Urbach tail width E{sub U}) but also created N-Si-O (N{sub x}) defect states in the band gap. We have discovered the distinctive PL characteristics from a-SiN{sub x}:O films with various NH{sub 3/}SiH{sub 4} ratios. The PL peak energy (E{sub PL}) is independent of the excitation energy (E{sub exc}) and the PL intensity (I{sub PL}) is regardless of the optical band gap (E{sub opt}) but is proportional to the N{sub x} defects concentration, both of which are completely different from the PL characteristics by band tail states recombination mechanism, in which the E{sub PL} is proportional to E{sub exc} (when E{sub exc} ≤ E{sub opt}) and the I{sub PL} is dependent on the relative position of E{sub exc} and E{sub opt}. Based on the N-Si-O bonding configurations and the distinctive PL characteristics, the radiative recombination mechanism through the N-Si-O defect states has been proposed, by which the performance of stimulated emission may be realized in this kind of a-SiN{sub x}:O films.