At least 1,711 records · Page 95

Effect of Solutionizing Time on Improving the Microstructure and Mechanical Properties of Aged AZ80 Mg Alloy

The effects of solutionizing soak time and aging on the microstructure and mechanical properties of cast AZ80 Mg alloy were investigated. Optical microscopy, scanning electron microscopy and x-ray diffraction revealed the dissolution of β-Mg{sub 17}Al{sub 12} phase in the solution-treated samples which was later detected in the aged condition. Solution treatments at 420 °C for 4-16 h with water quenching followed by aging at 200 °C for 10 h were carried out, causing discontinuous precipitates to be formed with different precipitate morphologies at the various soak times. The discontinuous precipitates were observed to transform from the interdendritic segregation to parallel lamellae with increasing soak time to 8-10 h. As the soak time increased to 16 h, parallel lamellae transformed into tree-like precipitate morphology. The results showed significant changes in the interlamellar spacing at different soak times, and such precipitate morphology could influence the microstructure and mechanical properties after the aging process. A good combination of strength and ductility was obtained when the cast AZ80 Mg alloy was solution-treated at 420 °C for 10 h and aged at 200 °C for 10 h. Compared to the as-cast condition, a significant increase in ultimate tensile strength (50%), yield strength (47%) and elongation (43%) were observed.

36 MATERIALS SCIENCE↗

Cryo diffraction microscopy: Ice conditions and finite supports

Using a signal-to-noise ratio estimation based on correlations between multiple simulated images, we compare the dose efficiency of two soft x-ray imaging systems: incoherent brightfield imaging using zone plate optics in a transmission x-ray microscope (TXM), and x-ray diffraction microscopy (XDM) where an image is reconstructed from the far-field coherent diffraction pattern. In XDM one must computationally phase weak diffraction signals; in TXM one suffers signal losses due to the finite numerical aperture and efficiency of the optics. In simulations with objects representing isolated cells such as yeast, we find that XDM has the potential for delivering equivalent resolution images using fewer photons. This can be an important advantage for studying radiation-sensitive biological and soft matter specimens.

36 MATERIALS SCIENCE↗

Study on mechanism of photocatalytic performance of La-doped TiO{sub 2}/Ti photoelectrodes by theoretical and experimental methods

TiO{sub 2} photoelectrodes with various nanostructures have been successfully prepared by the anodization method. The morphology, microstructure and optical properties of as-prepared photoelectrodes were studied by scanning electron microscopy (SEM), X-ray diffraction (XRD), ultraviolet/visible light diffuse reflectance spectra (UV/vis/DRS), surface photovoltage spectroscopy (SPS) and photocurrent. The electronic structure and optical properties of La doped/undoped TiO{sub 2} photoelectrodes with different crystal structures were calculated by the density function theory. The photocatalytic and photoelectrocatalytic activities of as-prepared photoelectrodes were evaluated. The results showed that the anodization potentials played a crucial role in the surface morphology and microstructure. Both results of theoretical calculations and experimental tests demonstrated that La-doped photoelectrodes were more sensitive to light than undoped one. The difference of photoelectrodes performance was ascribed to the crystal configuration, impurity energy levels and long-range orientation moving of photogenerated carriers. - Graphical abstract: Photophysical chemistry processes in as-prepared TiO{sub 2} photoelectrodes. Overall scheme of TiO{sub 2} photoelectrodes: (A) movement of photoelectrons and holes without bias potentials; (B) movement of photoelectrons and holes at applied bias potentials; (a) and (b) were the transmission of photogenerated electrons and holes of local enlargement of (A) (black open circle): (a) photoelectrons movement in P-TiO{sub 2} photoelectrodes and La-TiO{sub 2} photoelectrodes, the red dot line denotes the top of valence band (VB) and the bottom of conduction band (CB) of pure photoelectrodes; (b) photoelectrons movement in P-160 and La-160 TiO{sub 2} photoelectrodes (mixed crystal phase). The number refers to as follows: (1) transmission process of photoelectrons and holes; (2) recombination process of photoelectrons and holes. Arrows represent the moving direction of photoelectrons. Highlights: Black-Right-Pointing-Pointer Morphology and structure of La-doped photoelectrodes. Black-Right-Pointing-Pointer Band gap and electric structure of La-doped and undoped photoelectrodes. Black-Right-Pointing-Pointer Optical, PECH, PC and PEC properties of La-TiO{sub 2} photoelectrodes. Black-Right-Pointing-Pointer Transmission process of photoelectron-hole pairs in La-TiO{sub 2} photoelectrodes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Spatial Light Modulators as Optical Crossbar Switches

A proposed method of implementing cross connections in an optical communication network is based on the use of a spatial light modulator (SLM) to form controlled diffraction patterns that connect inputs (light sources) and outputs (light sinks). Sources would typically include optical fibers and/or light-emitting diodes; sinks would typically include optical fibers and/or photodetectors. The sources and/or sinks could be distributed in two dimensions; that is, on planes. Alternatively or in addition, sources and/or sinks could be distributed in three dimensions -- for example, on curved surfaces or in more complex (including random) three-dimensional patterns.

Juday, Richard↗

Thin film growth of boron nitride on {alpha}-Al{sub 2}O{sub 3} (0 0 1) substrates by reactive sputtering

Highlights: Black-Right-Pointing-Pointer A BN film grown on {alpha}-Al{sub 2}O{sub 3} (0 0 1) had a structure in which h-BN sheet stacking continued through almost the whole film thickness. Black-Right-Pointing-Pointer The structure was characterized by X-ray diffraction, ATR-IR, and XPS. Black-Right-Pointing-Pointer Tauc plots suggested the film had direct band gap and the optical band gap was close to that of bulk h-BN. -- Abstract: Boron nitride thin films were grown on {alpha}-Al{sub 2}O{sub 3} (0 0 1) substrates by reactive magnetron sputtering. Infrared attenuated total reflection (ATR) spectra of the films gave an intense signal associated with in-plane B-N stretching TO mode of short range ordered structure of BN hexagonal sheets. X-ray diffraction for the film prepared at a low working pressure (ca. 1 Multiplication-Sign 10{sup -3} Torr) gave a diffraction peak at slightly lower angle than that corresponding to crystal plane h-BN (0 0 2). It is notable that crystal thickness calculated from X-ray peak linewidth (45 nm) was close to film thickness (53 nm), revealing well developed sheet stacking along the direction perpendicular to the substrate surface. When the substrates of MgO (0 0 1) and Si (0 0 1) were used, the short-range ordered structure of h-BN sheet was formed but the films gave no X-ray diffraction. The film showed optical band gap of 5.9 eV, being close to that for bulk crystalline h-BN.

36 MATERIALS SCIENCE↗

Measuring Shock Stage of ltokawa Regolith Grains by Electron Back-Scattered Diffraction and Synchrotron X-Ray Diffraction

We have been analyzing Itokawa samples in order to definitively establish the degree of shock experienced by the regolith of asteroid Itokawa, and to devise a bridge between shock determinations by standard light optical petrography, crystal structures as determined by electron and X-ray diffraction techniques. We are making measurements of olivine crystal structures and using these to elucidate critical regolith impact processes. We use electron back-scattered diffraction (EBSD) and synchrotron X-ray diffraction (SXRD). We are comparing the Itokawa samples to L and LL chondrite meteorites chosen to span the shock scale experienced by Itokawa, specifically Chainpur (LL3.4, Shock Stage 1), Semarkona (LL3.00, S2), Kilabo (LL6, S3), NWA100 (L6, S4) and Chelyabinsk (LL5, S4). In SXRD we measure the line broadening of olivine reflections as a measure of shock stage. In this presentation we concentrate on the EBSD work. We employed JSC's Supra 55 variable pressure FEG-SEM and Bruker EBSD system. We are not seeking actual strain values, but rather indirect strain-related measurements such as extent of intra-grain lattice rotation, and determining whether shock state "standards" (meteorite samples of accepted shock state, and appropriate small grain size) show strain measurements that may be statistically differentiated, using a sampling of particles (number and size range) typical of asteroid regoliths. Using our system we determined that a column pressure of 9 Pa and no C-coating on the sample was optimal. We varied camera exposure time and gain to optimize mapping performance, concluding that 320x240 pattern pixilation, frame averaging of 3, 15 kV, and low extractor voltage yielded an acceptable balance of hit rate (>90%), speed (11 fps) and map quality using an exposure time of 30 ms (gain 650). We found that there was no strong effect of step size on Grain Orientation Spread (GOS) and Grain Reference Orientation Deviation angle (GROD-a) distribution; there was some effect on grain average Kernel Average Misorientation (KAM) (reduced with smaller step size for the same grain), as expected. We monitored GOS, Maximum Orientation Spread (MOS) and GROD-a differences between whole olivine grains and sub-sampled areas, and found that there were significant differences between the whole grain dataset and subsets, as well as between subsets, likely due to sampling-related "noise". Also, in general (and logically) whole grains exhibit greater degrees of cumulative lattice rotation. Sampling size affects the apparent strain character of the grain, at least as measured by GOS, MOS and GROD-a. There were differences in the distribution frequencies of GOS and MOS between shock stages, and in plots of MOS and GOS vs. grain diameter. These results are generally consistent with those reported this year. However, it is unknown whether the differences between samples of different shock states exceeds the clustering of these values to the extent that shock stage determinations can still be made with confidence. We are investigating this by examination of meteorites with higher shock stage 4 to 5. Our research will improve our understanding of how small, primitive solar system bodies formed and evolved, and improve understanding of the processes that determine the history and future of habitability of environments on other solar system bodies. The results will directly enrich the ongoing asteroid and comet exploration missions by NASA and JAXA, and broaden our understanding of the origin and evolution of small bodies in the early solar system, and elucidate the nature of asteroid and comet regolith.

Zolensky, Michael↗

Measuring the Shock Stage of Asteroid Regolith Grains by Electron Back-Scattered Diffraction

We have been analyzing Itokawa samples in order to definitively establish the degree of shock experienced by the regolith of asteroid Itokawa, and to devise a bridge between shock determinations by standard light optical petrography, crystal structures as determined by electron and X-ray diffraction. These techniques would then be available for samples returned from other asteroid regoliths.

Zolensky, Michael↗

The Ammonia-Hydrogen System under Pressure

Binary mixtures of hydrogen and ammonia were compressed in diamond anvil cells to 15 GPa at room temperature over a range of compositions. The phase behavior was characterized using optical microscopy, Raman spectroscopy, and synchrotron X-ray diffraction. Below 1.2 GPa we observed two-phase coexistence between liquid ammonia and fluid hydrogen phases with limited solubility of hydrogen within the ammonia-rich phase. Complete immiscibility was observed subsequent to the freezing of ammonia phase III at 1.2 GPa, although hydrogen may become metastably trapped within the disordered face-centered-cubic lattice upon rapid solidification. For all compositions studied, the phase III to phase IV transition of ammonia occurred at ~3.8 GPa and hydrogen solidified at ~5.5 GPa, transition pressures equivalent to those observed for the pure components. A P-x phase diagram for the NH 3 -H 2 system is proposed on the basis of these observations with implications for planetary ices, molecular compound formation, and possible hydrogen storage materials.

08 HYDROGEN↗

Mononuclear to Polynuclear U(IV) Structural Units: Effects of Reaction Conditions on U-Furoate Phase Formation

In this work, Uranium(IV) complexation by 2-furoic acid was examined to better understand the effects of ligand identity and reaction conditions on species formation and stability. Five compounds were isolated: [UCl 2 (2-FA) 2 (H 2 O) 2 ] n (1), [U 4 Cl 10 O 2 (THF) 6 (2-FA) 2 ]•2(THF) (2), [U 6 O 4 (OH) 4 (H 2 O) 3 (2-FA) 12 ]•7(THF)•(H 2 O) (3), [U 6 O 4 (OH) 4 (H 2 O) 2 (2-FA) 12 ]•8.76(H 2 O) (4), and [U 38 Cl 42 O 54 (OH) 2 (H 2 O) 20 ]•m(H 2 O)•n(THF) (5). The structures were determined by single crystal X-ray diffraction and further characterized by Raman, IR, and optical absorption spectroscopy. The thermal stability and magnetic behavior of the compounds were also examined. Variations in the synthetic conditions led to notable differences in the structural units observed in the solid state. At low H 2 O/THF ratios, a tetranuclear oxo bridged [U 4 O 2 ] core was isolated. Aging of this solution resulted in the formation a U 38 oxo cluster capped by chloro and water ligands. However, at increasing water concentrations only hexanuclear units were observed. In all cases, at temperatures of 100-120 °C, UO 2 nanoparticles formed.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Characterization and Rationalization of Microstructural Evolution in GRCop-84 Processed by Laser-Powder Bed Fusion (L-PBF)

In this study, prismatic geometries of GRCop-84 [Cu-8Cr-4Nb (at. pct)] were built with laser-powder bed fusion (L-PBF) process. The samples were sectioned parallel or perpendicular to the build direction and characterized in the as-built and after post-processing with a hot-isostatically pressing (HIP) treatment. The microstructure and phase evolutions were evaluated with optical microscopy, scanning electron microscopy (SEM), electron backscattered diffraction (EBSD), and high-temperature X-ray diffraction (HTXRD) up to 1223 K. The samples in the as-built conditions exhibited predominantly columnar epitaxial and misoriented Cu-FCC grains. The microstructure evolutions are discussed based on locations within the overall build geometry, the dynamics of small melt pool shape and sectioning effects. The above grain structure did not change significantly during post-process HIP treatment. The stability of this FCC grain structure is attributed to the formation of primary stable Cr 2 Nb (Laves phase) during L-PBF, even before the emergence of FCC grains from liquid. The stability of Cr 2 Nb in both as-built and HIPed samples were evaluated using high-temperature X-ray diffraction measurements and compared with that of gas-atomized powder. The significance of these results is discussed with reference to aerospace applications.

36 MATERIALS SCIENCE↗

Effect of Hot Rolling on the Microstructure and Mechanical Properties of Nitrogen Alloyed Austenitic Stainless Steel

In the present investigation, the effect of multi-pass hot rolling in the temperature range of 700–1000 °C on the microstructure and mechanical properties of nitrogen alloyed austenitic stainless steel was studied with the aid of optical microscopy, tensile testing and x-ray diffraction measurements. The microstructural changes that occurred in the hot rolled specimens were elongation of grains in rolling direction, nucleation of new grains at the grain boundaries of elongated grains and growth of nucleated grains to form fully recrystallized grains. Elongated grains formed at lower rolling temperature (700–800 °C) due to inadequate strain/temperature for the initiation of dynamic recrystallization. At higher rolling temperature (900–1000 °C), fine grains formed due to dynamic recrystallization. Tensile properties showed strong dependency on the rolling temperature. Tensile strength increased with the decrease in the rolling temperature at the cost of ductility. Maximum strength was observed in samples hot rolled at 700 °C with yield strength of 917 MPa and ductility of 25%. This variation in the tensile properties with the rolling temperature is attributed to changes in the dislocation density and grain structure. The estimated yield strength from the dislocation density, solid solution and grain boundary strengthening closely matched with experimentally determined yield strength confirming the role of dislocation density and grain size in the strengthening.

36 MATERIALS SCIENCE↗

Effect of high temperature preoxidation treatment on the oxidation behavior of MoSi 2 - and WSi 2 –Al 2 O 3 composites

Composites of 30 vol% MoSi 2 -70 vol% Al 2 O 3 and 30 vol% WSi 2 -70 vol% Al 2 O 3 were prepared via sintering at 1600 °C in argon. The high-temperature preoxidation treatments were applied at 1000°-1200 °C for 10–120 min in air. The non-isothermal oxidation tests were conducted in air at temperatures ranging between 50° and 870 °C to study and understand the influence of the alumina phase and preoxidation process on the low-temperature oxidation behavior. The optical and scanning electron microscopy, X-ray diffraction, X-ray photoelectron and Raman spectroscopy were used to characterize the surface layers formed. The oxidation-induced mass gains were substantially reduced by 82.1–99.8%, implying their enhanced oxidation resistance. This was due to the formation of highly dense, protective surface layers with a sufficient thickness (3.1–14.2 μm). The structural and surface analyses revealed their complex chemistries, since the ternary (Mo–Si–Al, W–Si–Al) intermetallic, mullite, alumina and silica phases with high oxidation resistances were identified within these surface features. In addition, the high-temperature electrical properties of the composites were highly preserved after the preoxidation treatment, and their electrical conductivities were measured as 45.1–78.6 S/cm at 800 °C and 40.1–69.1 S/cm at 900 °C.

36 MATERIALS SCIENCE↗

Phase stability and microstructure of neutron-irradiated substoichiometric yttrium dihydrides

The impact of the neutron-displacement damage on phase stability and microstructure of substoichiometric yttrium dihydrides (YH x , x <2) were investigated to assess their use as solid moderator in high-temperature nuclear reactors. YH x specimens were, thus, subjected to neutron irradiations in the range of 0.1–2 displacements per yttrium atom (dpa-Y) in the temperature range of 536–878°C at the Oak Ridge National Laboratory's (ORNL's) High Flux Isotope Reactor (HFIR). YH x specimens were initially prepared at stoichiometry (H/Y) ratios of 1.69 and 1.83. HFIR-irradiated specimens were characterized by variety of techniques to investigate H retention characteristics including dimensional analysis, optical microscopy, scanning electron microscopy electron back scatter diffraction (EBSD), transmission electron microscopy, thermal desorption spectroscopy (TDS), and high-energy x-ray diffraction (HE-XRD) characterizations. Overall, YH x exhibited notable structural and phase stability under short-term neutron-irradiation, except for the samples with significant silicon carbide (SiC) interaction at high doses and temperatures. Basic dimensional and mass measurements were misleading for accurate assessment of H retention, as confirmed by EBSD phase maps, XRD line profiles, and TDS signals. Thus, it was discussed that a robust H retention metric is needed to assess irradiated hydrides. Further, nanoscale cavities were observed as a result of the neutron irradiation in all samples. Although no clear impact of dose and irradiation temperature was determined, the initial H/Y ratio had an impact on the cavity number density where low H/Y specimens had high-resistance to cavity formation. The Y-vacancy cluster formation at the collision stage of the displacement cascade and their stabilization by H were considered to be the likely underlying mechanisms for the observed cavity microstructure.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Aging behavior and mechanical properties of maraging steels in the presence of submicrocrystalline Laves phase particles

Cold rolling and annealing of homogenized Fe-Ni-Mn-Mo-Ti-Cr maraging steels resulted in the formation of submicrocrystalline Fe{sub 2}(Mo,Ti) Laves phase particles. Optical and scanning electron microscopy, X-ray diffraction, tensile and hardness tests were used to study the microstructure, aging behavior and mechanical properties of the annealed steels. The annealed microstructures showed age hardenability during subsequent isothermal aging at 753 K. Ultrahigh fracture stress but poor tensile ductility was obtained after substantial age hardening in the specimens with 2% and 4% chromium. Increasing chromium addition up to 6% toughened the aged microstructure at the expense of the fracture stress by increasing the volume fraction of retained austenite. The Laves phase particles acted as crack nucleation sites during tensile deformation. - Highlights: {yields} Laves phases dispersed in a BCC iron matrix by annealing of cold rolled samples. {yields} The samples showed age hardenability during subsequent isothermal aging at 753 K. {yields} Ultrahigh fracture stress but poor ductility was obtained after age hardening. {yields} Increasing chromium addition toughened the aged microstructure. {yields} Laves phase particles acting as crack nucleation sites during tensile deformation.

36 MATERIALS SCIENCE↗

Modification of Mg{sub 2}Si in Mg–Si alloys with gadolinium

The modification effect of gadolinium (Gd) on Mg{sub 2}Si in the hypereutectic Mg–3 wt.% Si alloy has been investigated using optical microscope, scanning electron microscope, X-ray diffraction and hardness measurements. The results indicate that the morphology of the primary Mg{sub 2}Si is changed from coarse dendrite into fine polygon with the increasing Gd content. The average size of the primary Mg{sub 2}Si significantly decreases with increasing Gd content up to 1.0 wt.%, and then slowly increases. Interestingly, when the Gd content is increased to 4.0 and 8.0 wt.%, the primary and eutectic Mg{sub 2}Si evidently decrease and even disappear. The modification and refinement of the primary Mg{sub 2}Si is mainly attributed to the poisoning effect. The GdMg{sub 2} phase in the primary Mg{sub 2}Si is obviously coarsened as the Gd content exceeds 2.0 wt.%. While the decrease and disappearance of the primary and eutectic Mg{sub 2}Si are ascribed to the formation of vast GdSi compound. Therefore, it is reasonable to conclude that proper Gd (1.0 wt.%) addition can effectively modify and refine the primary Mg{sub 2}Si. - Highlights: ► Proper Gd (1.0 wt.%) addition can effectively modify and refine the primary Mg{sub 2}Si. ► We studied the reaction feasibility between Mg and Si, Gd and Si in Mg–Gd–Si system. ► We explored the modification mechanism of Gd modifier on Mg{sub 2}Si.

36 MATERIALS SCIENCE↗

Effects of porosity on corrosion resistance of Mg alloy foam produced by powder metallurgy technology

Magnesium alloy foams have the potential to serve as structural material for regular light-weight applications as well as for biodegradable scaffold implants. However, their main disadvantage relates to the high reactivity of magnesium and consequently their natural tendency to corrode in regular service conditions and in physiological environments. The present study aims at evaluating the effect of porosity on the corrosion resistance of MRI 201S magnesium alloy foams in 0.9% NaCl solution and in phosphate buffer saline solution as a simulated physiological electrolyte. The magnesium foams were produced by powder metallurgy technology using space-holding particles to control the porosity content. Machined chips were used as raw material for the production of Mg alloy powder by milling process. The microstructure of the foams was examined using optical and scanning electron microscopy, X-ray diffraction, and X-ray photoelectron spectroscopy analysis. The corrosion behavior was evaluated by immersion test and potentiodynamic polarization analysis. The results obtained clearly demonstrate that the porosity has a significant effect on the corrosion resistance of the tested foams. Foams with 14–19% porosity have a corrosion rate of 4–10 mcd and 7–15 mcd in NaCl and phosphate buffer saline solution, respectively, compared to only 0.10 mcd for the same alloy in as cast conditions. This increased corrosion degradation of the Mg foams by more than one order of magnitude compared to the cast alloy may limit their potential application in regular and physiological environments. - Highlights: • Porosity has a detrimental effect on corrosion resistance of MRI 201S Mg foams. • 14–19% porosity increases the corrosion rate by more than one order of magnitude. • Accelerated corrosion limits the use of foams in regular/physiological environments.

36 MATERIALS SCIENCE↗

Cooling thermal parameters and microstructure features of directionally solidified ternary Sn–Bi–(Cu,Ag) solder alloys

Low temperature soldering technology encompasses Sn–Bi based alloys as reference materials for joints since such alloys may be molten at temperatures less than 180 °C. Despite the relatively high strength of these alloys, segregation problems and low ductility are recognized as potential disadvantages. Thus, for low-temperature applications, Bi–Sn eutectic or near-eutectic compositions with or without additions of alloying elements are considered interesting possibilities. In this context, additions of third elements such as Cu and Ag may be an alternative in order to reach sounder solder joints. The length scale of the phases and their proportions are known to be the most important factors affecting the final wear, mechanical and corrosions properties of ternary Sn–Bi–(Cu,Ag) alloys. In spite of this promising outlook, studies emphasizing interrelations of microstructure features and solidification thermal parameters regarding these multicomponent alloys are rare in the literature. In the present investigation Sn–Bi–(Cu,Ag) alloys were directionally solidified (DS) under transient heat flow conditions. A complete characterization is performed including experimental cooling thermal parameters, segregation (XRF), optical and scanning electron microscopies, X-ray diffraction (XRD) and length scale of the microstructural phases. Experimental growth laws relating dendritic spacings to solidification thermal parameters have been proposed with emphasis on the effects of Ag and Cu. The theoretical predictions of the Rappaz-Boettinger model are shown to be slightly above the experimental scatter of secondary dendritic arm spacings for both ternary Sn–Bi–Cu and Sn–Bi–Ag alloys examined. - Highlights: • Dendritic growth prevailed for the ternary Sn–Bi–Cu and Sn–Bi–Ag solder alloys. • Bi precipitates within Sn-rich dendrites were shown to be unevenly distributed. • Morphology and preferential region for the Ag{sub 3}Sn growth depend on Ag content and Ṫ{sub L}. • Rappaz-Boettinger model reasonably estimated the experimental scatter of λ{sub 2}.

36 MATERIALS SCIENCE↗