At least 1,711 records · Page 95

Photoemission electron microscopy of localized surface plasmons in silver nanostructures at telecommunication wavelengths

We image the field enhancement at Ag nanostructures using femtosecond laser pulses with a center wavelength of 1.55 μm. Imaging is based on non-linear photoemission observed in a photoemission electron microscope (PEEM). The images are directly compared to ultra violet PEEM and scanning electron microscopy (SEM) imaging of the same structures. Further, we have carried out atomic scale scanning tunneling microscopy on the same type of Ag nanostructures and on the Au substrate. Measuring the photoelectron spectrum from individual Ag particles shows a larger contribution from higher order photoemission processes above the work function threshold than would be predicted by a fully perturbative model, consistent with recent results using shorter wavelengths. Investigating a wide selection of both Ag nanoparticles and nanowires, field enhancement is observed from 30% of the Ag nanoparticles and from none of the nanowires. No laser-induced damage is observed of the nanostructures neither during the PEEM experiments nor in subsequent SEM analysis. By direct comparison of SEM and PEEM images of the same nanostructures, we can conclude that the field enhancement is independent of the average nanostructure size and shape. Instead, we propose that the variations in observed field enhancement could originate from the wedge interface between the substrate and particles electrically connected to the substrate.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Investigation of microstructure, surface morphology, and hardness properties of PtIr films by magnetron sputtering

Pt{sub 1-x}Ir{sub x} films with x varying from 22.76 to 63.25 at. % are deposited on (100) Si wafer substrates at 400 deg. C by magnetron sputtering deposition. The effects of the Ir concentration on the microstructure, morphology, and hardness of PtIr films are investigated by field emission scanning electron microscopy, x-ray diffraction, atomic force microscopy, and nanoindentation system. The columnar structures are observed by field emission scanning electron microscopy. X-ray diffraction analysis reveals that PtIr films have preferred orientation along Pt(111) when the Ir concentration is below 50.84 at. %. When the Ir content is more than 50.84 at. %, the PtIr film shifts to another preferred orientation, Ir(111). The surface morphology is analyzed by atomic force microscopy. The roughness of the PtIr films decreases with increasing Ir content. The hardness of all the PtIr films is below 20 GPa. The maximum hardness of the PtIr films is about 14.9 GPa when the Ir concentration is 57.9 at. %.

36 MATERIALS SCIENCE↗

Synthesis, structure and electrochemical properties of polyaniline/MoO{sub 3} nanobelt composite for lithium battery

Graphical abstract: Hydrothermal method was introduced for the synthesis of MoO{sub 3} nanobelts and polyaniline (PANI)/MoO{sub 3} nanobelt composites. The structure and morphology of the samples were studied by X-ray diffraction (XRD), Fourier transform infrared radiation (FTIR), scanning electron microscopy (SEM) and transmission electron microscopy (TEM) analysis. We can see the presence of polyaniline on the MoO{sub 3} nanobelts surface in the TEM pictures as shown in Fig. (a). The pure MoO{sub 3} nanobelts exhibit the initial specific capacity 276 mAhg{sup −1}, whereas PANI/MoO{sub 3} nanobelt composite shows little low initially 228 mAhg{sup −1} after that it has more stabilized specific capacity with increasing cycle numbers as shown in Fig. (b). The cyclic voltammograms of the PANI/MoO{sub 3} nanobelt composite show better cyclic performance compared to pure MoO{sub 3} nanobelts. The electrochemical impedance spectres were studied for both the pure and PANI/MoO{sub 3} samples at 2.0 and 3.5 potentials. The role of the PANI polymeric component of the composite material seems to be the stabilization of the specific capacity due to probable homogeneous distribution of the induced stress during cycling. Display Omitted Highlights: ► Hydrothermal synthesis of MoO{sub 3}, PANI/MoO{sub 3} nanobelts. ► Samples were characterised by XRD, FTIR, DSC, SEM, TEM, CV and impedance. ► MoO{sub 3} nanobelts cathode battery shows initial specific capacity 276 mAhg{sup −1}. ► PANI/MoO{sub 3} nanobelts show initial specific capacity 228 mAhg{sup −1} but high stability. ► PANI/MoO{sub 3} sample studies by impedance at the potentials of 2.0 and 3.5 V. -- Abstract: The MoO{sub 3} nanobelts and polyaniline (PANI)/MoO{sub 3} nanobelt composite were synthesized using hydrothermal method. The crystal structure and morphology of the samples were studied by X-ray diffraction (XRD), Fourier transform infrared radiation (FTIR), scanning electron microscopy (SEM) and transmission electron microscopy (TEM). Differential scanning calorimetric (DSC) and thermo gravimetric (TG) measurements were carried out for PANI/MoO{sub 3} nanobelt composite. The pure MoO{sub 3} nanobelts exhibit the initial specific capacity 276 mAhg{sup −1}, whereas PANI/MoO{sub 3} nanobelt composite showed little low initially 228 mAhg{sup −1} after that it has more stabilized specific capacity with increasing cycle numbers at constant current density of 30.7 mAg{sup −1} in the potential range 1.0–4.0 V vs. Li/Li{sup +}. The electrochemical impedance profiles were also studied. The cyclic voltammograms of the PANI/MoO{sub 3} nanobelt composite showed better cyclic performance as compared with pure MoO{sub 3} nanobelts, this is due to the role of PANI polymeric component stabilization of the specific capacity by homogeneous distribution within nanobelts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Surface modification of cellulose acetate membrane using thermal annealing to enhance produced water treatment

This study is performed primarily to investigate the effect of surface modification of cellulose acetate using thermal annealing on the enhancement of membrane performance for produced water treatment. In this study, Cellulose Acetate membranes were casted using dry/wet phase inversion technique. The effect of additive and post-treatment using thermal annealing on the membrane surface were examined for produced water treatment. Therma annealing was subjected to membrane surface at 60 and 70 °C for 5, 10 and 15 second, respectively. Membrane characterizations were done using membrane flux and rejection with produced water as a feed, Scanning Electron Microscopy (SEM) and Fourier Transform Infra Red (FTIR) analysis. Experimental results showed that asymmetric cellulose acetate membrane can be made by dry/wet phase inversion technique. The results from the Scanning Electron Microscopy (FESEM) analysis was also confirmed that polyethylene glycol as additivie in dope solution and thermal annealing was affected the morphology and membrane performance for produced water treatment, respectively. Scanning electron microscopy micrographs showed that the selective layer and the substructure of membrane became denser and more compact after the thermal annealing processes. Therefore, membrane rejection was significantly increased while the flux was slighty decreased, respectively. The best membrane performance is obtained on the composition of 18 wt % cellulose acetate, poly ethylene glycol 5 wt% with thermal annealing at 70° C for 15 second.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Fabrication of lead-free (Na{sub 0.82}K{sub 0.18}){sub 0.5}Bi{sub 0.5}TiO{sub 3} piezoelectric nanofiber by electrospinning

(Na{sub 0.82}K{sub 0.18}){sub 0.5}Bi{sub 0.5}TiO{sub 3} nanofibers were synthesized by sol-gel process and electrospinning. Scanning electron microscopy was used to verify that the diameters and lengths are in the range of 150-600 nm and several hundreds of micrometer. Perovskite structure and grain size (20-70 nm) were verified by X-ray diffraction and transmission electron microscopy. The high effective piezoelectric coefficient d{sub 33} (96 pm/V) was measured by scanning force microscopy. It may be attributed to easily tilting the polar vector of domain for an electric field and the increase in the number of possible spontaneous polarization direction near the rhombohedral-tetragonal morphotropic phase boundary. The research shows that there are potentional applications for (Na{sub 0.82}K{sub 0.18}){sub 0.5}Bi{sub 0.5}TiO{sub 3} nanofiber in nanoscale lead-free piezoelectric devices.

36 MATERIALS SCIENCE↗

Decoupling indirect topographic cross-talk in band excitation piezoresponse force microscopy imaging and spectroscopy

Here, all scanning probe microscopies are subjected to topographic cross-talk, meaning the topography-related contrast in functional images. Here, we investigate the signatures of indirect topographic cross-talk in piezoresponse force microscopy (PFM) imaging and spectroscopy and its decoupling using band excitation (BE) method in ferroelectric BaTiO 3 deposited on the Si substrates with free standing nanopillars of diameter 50 nm. Comparison between the single-frequency PFM and BE-PFM results shows that the measured signal can be significantly distorted by topography-induced shifts in the contact resonance frequency and cantilever transfer function. However, with proper correction, such shifts do not affect PFM imaging and hysteresis loop measurements. This suggests the necessity of an advanced approach, such as BE-PFM, for detection of intrinsic sample piezoresponse on the topographically non-uniform surfaces.

36 MATERIALS SCIENCE↗

Resolution theory and static- and frequency dependent cross-talk in piezoresponse force microscopy

Probing materials functionality locally by scanning probe microscopy requires reliable framework for identifying the target signal and separating it from the effects of surface morphology and instrument non-idealities, i.e. instrumental and topographical cross-talk. Here we develop the linear resolution theory framework to describe the cross-talk effects, and apply it for elucidation of frequency dependent cross-talk mechanisms in the Piezoresponse Force Microscopy. The use of band excitation method allows electromechanical/electrical and mechanical/topographic signals to be unambiguously separated. The applicability of functional fit approach and multivariate statistical analysis methods for data identification in band excitation SPM is explored.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Cathodoluminescence of stacking fault bound excitons for local probing of the exciton diffusion length in single GaN nanowires

We perform correlated studies of individual GaN nanowires in scanning electron microscopy combined to low temperature cathodoluminescence, microphotoluminescence, and scanning transmission electron microscopy. We show that some nanowires exhibit well localized regions emitting light at the energy of a stacking fault bound exciton (3.42 eV) and are able to observe the presence of a single stacking fault in these regions. Precise measurements of the cathodoluminescence signal in the vicinity of the stacking fault give access to the exciton diffusion length near this location.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Shape controlled synthesis of CaMoO{sub 4} thin films and their photoluminescence property

CaMoO{sub 4} (CMO) disordered and ordered thin films were prepared by the complex polymerization method (CPM). The films were annealed at different temperatures and time in a conventional resistive furnace (RF) and in a microwave (MW) oven. The microstructure and surface morphology of the structure were monitored by atomic force microscopy (AFM) and high-resolution scanning electron microscopy (HRSEM). Order and disorder were characterized by X-ray diffraction (XRD) and optical reflectance. A strong photoluminescence (PL) emission was observed in the disordered thin films and was attributed to complex cluster vacancies. The experimental results were compared with density functional and Hartree-Fock calculations. - Graphical abstract: CaMoO{sub 4} thin films were prepared by the complex polymerization method (CPM). The films were annealed at different temperatures and time in a conventional resistive furnace and in a microwave oven. A strong photoluminescence emission was observed in the disordered thin films and was attributed to complex cluster vacancies. The experimental results were confirmed by high level first principle calculations.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Morphology and strain of self-assembled semipolar GaN quantum dots in (1122) AlN

GaN quantum dots (QDs) grown in semipolar (1122) AlN by plasma-assisted molecular-beam epitaxy were studied by transmission electron microscopy (TEM) and scanning transmission electron microscopy techniques. The embedded (1122)-grown QDs exhibited pyramidal or truncated-pyramidal morphology consistent with the symmetry of the nucleating plane, and were delimited by nonpolar and semipolar nanofacets. It was also found that, in addition to the (1122) surface, QDs nucleated at depressions comprising (1011) facets. This was justified by ab initio density functional theory calculations showing that such GaN/AlN facets are of lower energy compared to (1122). Based on quantitative high-resolution TEM strain measurements, the three-dimensional QD strain state was analyzed using finite-element simulations. The internal electrostatic field was then estimated, showing small potential drop along the growth direction, and limited localization at most QD interfaces.

36 MATERIALS SCIENCE↗

Diagnosis of PV Cell Passivation Degradation Resulting from Hot-Humid, High Voltage Potential Aging

Corrosion of the antireflective coating on the cell ("AR c corrosion") was previously observed in studies using hot-humid test conditions with external high voltage (HV) bias. Because AR c corrosion is not well understood, mini-modules (MiMos) were examined in a comparative experiment using PERC and PERT as well as legacy Al-BSF cells. For separate MiMos with the cell circuit electrical at +1500 V, -1500 V, or unbiased "V oc", test conditions in the comparative study included 60degrees C/60% RH for 96 h, as in IEC TS 62804-1; 70degrees C/70%RH for 200 h; and 85degrees C/85% RH for 200 h. Characterizations at each read point included: camera and electroluminescence (EL) imaging, colorimetry, and I-V curve tracing. Characterizations at the final read point included: SunsVoc; spatially mapping external quantum efficiency (EQE); high resolution: photoluminescence (PL), EL, and dark lock-in thermographic (DLIT) imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS) and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos (stepped HV aging) and full-sized modules (outdoor aging) from previous studies. AR c corrosion was specifically observed for the glass/encapsulant/cell side of +1500 V (HV+) stressed MiMos, where appearance, color, and reflectance were the characteristics most distinguished relative to simultaneously occurring degradation modes. SEM/EDS and SAM identified conversion of silicon nitride to silicon oxide or hydrous silica, preferentially occurring at the edges and tips of the pyramidal textured cell surface.

aging↗

Characterization of low alloy ferritic steel–Ni base alloy dissimilar metal weld interface by SPM techniques, SEM/EDS, TEM/EDS and SVET

The interface region of welded A508–Alloy 52 M is characterized by scanning probe microscope (SPM) techniques, scanning electron microscopy (SEM)/energy dispersive spectroscopy (EDS), transmission electron microscopy (TEM)/Energy Dispersive Spectroscopy (EDS) and scanning vibrate electrode technique (SVET). The regions along the welded A508–Alloy 52 M interface can be categorized into two types according to their different microstructures. In the type-I interface region, A508 and Alloy 52 M are separated by the fusion boundary, while in the type-II interface region, A508 and Alloy 52 M are separated by a martensite zone. A508, martensite zone and grain boundaries in Alloy 52 M are ferromagnetic while the Alloy 52 M matrix is paramagnetic. The Volta potentials measured by scanning Kelvin probe force microscopy (SKPFM) of A508, martensite zone and Alloy 52 M follow the order: V{sub 52} {sub M} > V{sub A508} > V{sub martensite}. The corrosion behavior of A508–Alloy 52 M interface region is galvanic corrosion, in which Alloy 52 M is cathode while A508 is anode. The martensite dissolves faster than Alloy 52 M, but slower than A508 in the test solution. - Highlights: • The A508–Alloy 52 M interface regions can be categorized into two types. • The chromium depleted region is observed along the Alloy 52 M grain boundary. • The Alloy 52 M grain boundaries which are close to the interface are ferromagnetic. • Martensite zone has lower Volta potential but higher corrosion resistance than A508.

36 MATERIALS SCIENCE↗

Scanning thermo-ionic microscopy for probing local electrochemistry at the nanoscale

Conventional electrochemical characterization techniques based on voltage and current measurements only probe faradaic and capacitive rates in aggregate. In this work we develop a scanning thermo-ionic microscopy (STIM) to probe local electrochemistry at the nanoscale, based on imaging of Vegard strain induced by thermal oscillation. It is demonstrated from both theoretical analysis and experimental validation that the second harmonic response of thermally induced cantilever vibration, associated with thermal expansion, is present in all solids, whereas the fourth harmonic response, caused by local transport of mobile species, is only present in ionic materials. The origin of STIM response is further confirmed by its reduced amplitude with respect to increased contact force, due to the coupling of stress to concentration of ionic species and/or electronic defects. The technique has been applied to probe Sm-doped Ceria and LiFePO{sub 4}, both of which exhibit higher concentrations of mobile species near grain boundaries. The STIM gives us a powerful method to study local electrochemistry with high sensitivity and spatial resolution for a wide range of ionic systems, as well as ability to map local thermomechanical response.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Chemical beam epitaxy growth of III–V semiconductor nanowires

Indium- Arsenide (InAs) nanowires were grown in a high vacuum chemical beam epitaxy (CBE) unit on InAs(111) wafers substrates at 425–454°C. Two types of nanogold were used as orientation catalyst, 40nm and 80nm. The measurements were performed using scanning electron microscopy showed that uniform nanowires. The nanowires orient vertically in the InAs nanowire scanning electron microscopy of an array 80nm diameter InAs nanowire with length is in the range 0.5–1 μm and of an array 40nm diameter with length is in the range 0.3–0.7μm. The nanowire length with growth time shows that the linear increase of nanowires start to grow as soon as TMIn is available. The growth rate with temperature was studied.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Nanoimaging of Electronic Heterogeneity in Bi 2 Se 3 and Sb 2 Te 3 Nanocrystals

Topological insulators (TIs) are quantum materials with topologically protected surface states surrounding an insulating bulk. However, defect-induced bulk conduction often dominates transport properties in most TI materials, obscuring the Dirac surface states. In order to realize intrinsic topological insulating properties, it is thus of great significance to identify the spatial distribution of defects, understand their formation mechanism, and finally control or eliminate their influence. For this study, the electronic heterogeneity in polyol-synthesized Bi 2 Se 3 and chemical vapor deposition-grown Sb 2 Te 3 nanocrystals is systematically investigated by multimodal atomic-to-mesoscale resolution imaging. In particular, by combining the Drude response sensitivity of infrared scattering-type scanning near-field optical microscopy with the work-function specificity of mirror electron microscopy, characteristic mesoscopic patterns are identified, which are related to carrier concentration modulation originating from the formation of defects during the crystal growth process. This correlative imaging and modeling approach thus provides the desired guidance for optimization of growth parameters, crucial for preparing TI nanomaterials to display their intrinsic exotic Dirac properties.

43 PARTICLE ACCELERATORS↗

Digital processing of SEM images for the assessment of evaluation indexes of cleaning interventions on Pentelic marble surfaces

In this work, digital processing of scanning-electron-microscopy images utilized to assess cleaning interventions applied on the Pentelic marble surfaces of the National Archaeological Museum and National Library in Athens, Greece. Beside mineralogical and chemical characterization that took place by scanning-electron-microscopy with Energy Dispersive X-ray Spectroscopy, the image-analysis program EDGE was applied for estimating three evaluation indexes of the marble micro-structure. The EDGE program was developed by the U.S. Geological Survey for the evaluation of cleaning interventions applied on Philadelphia City Hall. This computer program analyzes scanning-electron-microscopy images of stone specimens cut in cross-section for measuring the fractal dimension of the exposed surfaces, the stone near-surface fracture density, the shape factor (a surface roughness factor) and the friability index which represents the physico-chemical and physico-mechanical stability of the stone surface. The results indicated that the evaluation of the marble surface micro-structure before and after cleaning is achieved by the suggested indexes, while the performance of cleaning interventions on the marble surfaces can be assessed.

36 MATERIALS SCIENCE↗

Early age hydration of calcium sulfoaluminate (synthetic ye'elimite, C{sub 4}A{sub 3}S{sup ¯}) in the presence of gypsum and varying amounts of calcium hydroxide

Suspensions of synthetic ye'elimite (C{sub 4}A{sub 3}S{sup ¯}) in a saturated gypsum (CS{sup ¯}H{sub 2}) and calcium hydroxide (CH) solution were examined in-situ in a wet cell by soft X-ray transmission microscopy and ex-situ by scanning electron microscopy. The most voluminous hydration product observed was ettringite. Ettringite commonly displayed acicular, filiform, reticulated, and stellate crystal habits. Additionally, pastes with C{sub 4}A{sub 3}S{sup ¯}, 15% CS{sup ¯}H{sub 2}, and varying amounts of CH were prepared and examined with X-ray diffraction (XRD) and isothermal calorimetry. The XRD experiments showed that increasing CH content caused more solid solution (SO{sub 4}{sup 2−}/OH{sup −}) AFm phases to form at early ages (< 1 d) and more monosulfate to form at later ages (> 1 d). Calorimetry indicated that the increased production of solid solution AFm was accompanied with an increase in the initial (< 30 min) rate of heat evolution, and increasing CH generally reduced the time till the second maximum rate of heat evolution due to the formation of ettringite and monosulfate.

36 MATERIALS SCIENCE↗