Search NASA⌕ Search

SEARCH · Search NASA

Results for “Microstructures”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,747 records · Page 97

Electron Backscattered Diffraction Study of Microstructural Evolution During Isothermal Deformation of High-N Mn18Cr18 Alloy

In order to understand the dynamic recrystallization (DRX) mechanism of Mn18Cr18N austenitic stainless steel during hot deformation, the investigation of microstructure evolution is significant. Isothermal compression tests were conducted on a Gleeble-3500 thermomechanical simulator in the temperature range of 950 °C to 1150 °C and strain rate range between 0.001 and 1 s{sup −1}. Optical microscopy (OM) and electron backscattered diffraction (EBSD) were employed to study the resultant microstructures. More grain boundary information of hot-deformed specimens was provided by EBSD. It was found that the fraction of low-angle grain boundaries (LAGBs) increases with the decrease of deformation temperature or the increase of strain rate and can be expressed as a function of the Zener–Hollomon parameter. DRX easily occurs at the high deformation temperature and low strain rate. From the flow stress curves, the occurrence of single peak behavior and multiple transient steady-state (MTSS) behavior illustrated the existence of different DRX mechanisms. The EBSD analysis indicated that both continuous dynamic recrystallization (CDRX) and discontinuous dynamic recrystallization (DDRX) existed during hot deformation. For the low fraction of 10 to 15 deg misorientation, CDRX is the minor DRX mechanism while DDRX is the major DRX mechanism for the studied steel.

36 MATERIALS SCIENCE↗

Fluid Dynamics Effects on Microstructure Prediction in Single-Laser Tracks for Additive Manufacturing of IN625

Single-track laser fusion were simulated using a heat-transfer-solidification-only (HTS) model and its extension with fluid dynamics (HTS_FD) model using a parallel open-source code, which included laminar fluid dynamics, flat-free surface of the molten alloy, heat transfer, phase-change, evaporation, and surface tension phenomena. The results illustrate that the fluid dynamics affects the solidification and ensuing microstructure. For the HTS_FD simulations, thermal gradient, G was found to exhibit a maximum at the extremity of the solidified pool ( i.e. , at the free surface), while for HTS simulations, G exhibited a maximum around the entire edge of the solidified pool. HTS_FD simulations predicted a wider range of cooling rates than the HTS simulations, exhibited an increased spread in the solidification speed, V variation within the melt-pool with respect to the HTS model results. Primary dendrite arm spacing (PDAS) were evaluated based on power law correlations and marginal stability theory models using the ( G , V ) from HTS and HTS_FD simulations to quantify the effect of the fluid dynamics on the microstructure. At low-laser powers and low-scan speeds, the PDAS obtained with the fluid dynamics model (HTS_FD) was larger by more than 30 pct with respect to the PDAS calculated with the simple HTS model. A new PDAS correlation, i.e. , \( \lambda_{1} \left[ {\mu {\text{m}}} \right] = 832\;G\left[ {\text{K/m}} \right]^{ - 0.5} V\left[ {\text{m/s}} \right]^{ - 0.25} \) , which uses the ( G , V ) results from the HTS_FD model was developed and validated against experimental results.

36 MATERIALS SCIENCE↗

Microstructure and Sn crystal orientation evolution in Sn-3.5Ag lead-free solders in high temperature packaging applications

Understanding the reliability of eutectic Sn-3.5Ag lead-free solders in high temperature packaging applications is of significant interest in power electronics for the next generation electric grid. Large area (2.5mm 2.5mm) Sn-3.5Ag solder joints between silicon dies and direct bonded copper substrates were thermally cycled between 5 C and 200 C. Sn crystal orientation and microstructure evolution during thermal cycling were characterized by electron backscatter diffraction (EBSD) in scanning electron microscope (SEM). Comparisons are made between observed initial texture and microstructure and its evolution during thermal cycling. Gradual lattice rotation and grain boundary misorientation evolution suggested the continuous recrystallization mechanism. Recrystallization behavior was correlated with dislocation slip activities.

high temperature packaging↗

Probing Phase Transformations and Microstructural Evolutions at the Small Scales: Synchrotron X-ray Microdiffraction for Advanced Applications in [Phase 3 Memory,] 3D IC (Integrated Circuits) and Solar PV (Photovoltaic) Devices

Synchrotron x-ray microdiffraction (μXRD) allows characterization of a crystalline material in small, localized volumes. Phase composition, crystal orientation and strain can all be probed in few-second time scales. Crystalline changes over a large areas can be also probed in a reasonable amount of time with submicron spatial resolution. However, despite all the listed capabilities, μXRD is mostly used to study pure materials but its application in actual device characterization is rather limited. This article will explore the recent developments of the μXRD technique illustrated with its advanced applications in microelectronic devices and solar photovoltaic systems. Application of μXRD in microelectronics will be illustrated by studying stress and microstructure evolution in Cu TSV (through silicon via) during and after annealing. Here, the approach allowing study of the microstructural evolution in the solder joint of crystalline Si solar cells due to thermal cycling will be also demonstrated.

36 MATERIALS SCIENCE↗

Microstructure and Thermal Stability of A357 Alloy With and Without the Addition of Zr

The principal purpose of this research was to evaluate the effects of Zr on the microstructure and thermal stability of an A357 alloy that has been subjected to an aging treatment (T6) and thermal exposure (250 °C). The results show that the addition of Zr had a significant influence on the refinement of the grain size, which enhanced the hardness and tensile strength of the A357 alloy under the T6 condition. During thermal exposure at 250 °C, the rodlike metastable β’-Mg{sub 2}Si precipitates transformed into coarse equilibrium phase β-Mg{sub 2}Si precipitates, resulting in a significant drop in the hardness and tensile strength of the T6 heat-treated A357 alloy. However, after thermal exposure, coherent, finely dispersed Al{sub 3}Zr precipitates were found to be formed in the T6 heat-treated A357 alloy. The addition of 0.1% Zr played a critical role in improving the high-temperature strength. Consequently, the A357 alloy with the addition of Zr demonstrated better mechanical properties at room temperature and high temperature than the alloy without Zr, in terms of both microstructure and thermal stability.

36 MATERIALS SCIENCE↗

Effect of Post-deformation Annealing Treatment on the Microstructural Evolution of a Cold-Worked Corrosion-Resistant Superalloy (CRSA) Steel

The post-deformation annealing treatments of a commercial cold-worked corrosion-resistant superalloy steel (Sanicro 28 steel) were carried out at different temperatures in the range of 900-1100 °C for different holding durations of 5, 10, and 15 min. The effects of post-deformation annealing time and temperature on the microstructural evolution and subsequent mechanical properties of the processed Sanicro 28 steel were investigated. The observations indicated that twin–twin hardening in cold deformation condition mainly correlates with abundant nucleation of mechanical twins in multiple directions resulting in considerable strain hardening behavior. Microstructural investigations showed that the static recrystallization takes place after isothermal holding at 900 °C for 5 min. Increasing the annealing temperature from 900 to 1050 °C leads to recrystallization development and grain refinement in the as-recrystallized state. In addition, an increase in annealing duration from 5 to 15 min leads to subgrain coarsening and subsequently larger recrystallized grains size. The occurrence of large proportion of the grain refinement, which is achieved in the first annealing stage at 1050 °C after 5 min, is considered as the main factor for the maximum elongation at this stage.

36 MATERIALS SCIENCE↗

Effect of Quenching Process on Microstructures and Mechanical Properties of Fe-0.9Mn-0.5Cr-2.4Ni-0.5Mo-C Steel

To develop an appropriate quenching process to produce Fe-0.9Mn-0.5Cr-2.4Ni-0.5Mo-C steel, the microstructures and mechanical properties of this steel were investigated under the direct quenching and tempering (DQT) and the direct quenching, reheated quenching and tempering (DQQT) heat treatment processes. The microstructure of the DQQT specimen was basically tempered sorbite with spherical precipitates, while quite a bit of tempered martensite was in the DQT specimen with dispersive nanoscaled precipitates. The yield strengths of the DQT and DQQT specimens were 1154 and 955 MPa, respectively. The yield strength of the DQT specimen was higher than that of the DQQT specimen because of its finer grain size, higher density of dislocations and dispersed precipitates. The DQQT specimen had spherical precipitates, which hindered the propagation of the crack. Moreover, the high-angle grain boundaries in the DQQT specimen took a higher proportion. Therefore, the Charpy impact values of DQT and DQQT specimens at − 60 °C were 38 and 75 J, respectively. Consequently, the mechanical properties of the Fe-0.9Mn-0.5Cr-2.4Ni-0.5Mo-C steel, which met the standard of 1000 MPa grade steel plate for hydropower station, were acquired by the DQQT process.

36 MATERIALS SCIENCE↗

Microstructural Evolution and the Precipitation Behavior in X90 Linepipe Steel During Isothermal Processing

Thermomechanical controlled processing of 560-MPa (X90) linepipe steel was simulated in the laboratory using a thermomechanical simulator to study the microstructural evolution and precipitation behavior during isothermal holding. The results indicated that martensite was obtained when the steels were isothermally held for 5 s at 700 °C. Subsequently, granular bainite and acicular ferrite transformation occurred with increased holding time. Different amount of polygonal ferrite formed after isothermally holding for 600-3600 s. Pearlite nucleated after isothermally holding for 3600 s. Precipitation occurred after isothermal holding for 5 s and continuous precipitation occurred at grain boundaries after isothermally holding for 600 s. After isothermally holding for 3600 s, large Nb/Ti carbide precipitated. The presence of MX-type precipitates was confirmed by diffraction pattern. The interphase precipitation (IP) occurred between 5 and 30 s. Maximum hardness was obtained after isothermally holding for 600 s when IP occurred and rapidly decreased to a low value, mainly because polygonal ferrite dominated the microstructure after isothermally holding for 3600 s.

36 MATERIALS SCIENCE↗

Effect of Al-Si Coating on Weld Microstructure and Properties of 22MnB5 Steel Joints for Hot Stamping

22MnB5 hot stamping steels are gradually being used in tailor-welded blank applications. In this experiment, 1-mm-thick Al-Si coated and de-coated 22MnB5 steels were laser-welded and then hot-stamped. The chemical compositions, solidification process, microstructure and mechanical properties were investigated to reveal the effect of Al-Si coating and heat treatment. In the welded condition, the coated joints had an Al content of approximately 2.5 wt.% in the fusion zone and the de-coated joints had 0.5 wt.% Al. The aluminum promoted the δ-ferrite formation as the skeletal structure during solidification. In the high-aluminum weld, the microstructure consisted of martensite and long and band-like δ-ferrite. Meanwhile, the low-aluminum weld was full of lath martensite. After the hot stamping process, the δ-ferrite fraction increased from 10 to 24% in the coated joints and the lath martensite became finer in the de-coated joints. The tensile strengths of the coated joints or de-coated joints were similar to that before hot stamping, but the strength of the coated joints was reduced heavily after hot stamping compared to the de-coated joints and base material. The effect of δ-ferrite on the tensile properties became stronger when the fusion zone was soft and deformed first in the hot-stamped specimens. The coated weld showed a brittle fracture surface with many cleavage planes, and the de-coated weld showed a ductile fracture surface with many dimples in hot-stamped conditions.

36 MATERIALS SCIENCE↗

Effect of Rolling Temperature on the Microstructure and Tensile Properties of 47Zr-45Ti-5Al-3V Alloy

The 47Zr-45Ti-5Al-3V (wt.%) alloy was solution-treated at 850 and 780 °C for 30 min and then rolled at different temperatures. The effect of rolling temperature on microstructure and tensile properties was investigated. The results showed that the microstructure contained a large amount of α phase at a rolling temperature of 600 °C. As the rolling temperature increased, the amount of α phase decreased, whereas the amount of β phase increased. When the rolling temperature was higher than 700 °C, the alloy was composed of a single β phase. The tensile properties of the alloy depended strongly on rolling temperature. The yield strength and tensile strength decreased with increasing rolling temperature, whereas the elongation increased. At a given rolling temperature, low solution treatment temperature resulted in higher strength and lower elongation than high solution treatment temperature. The fracture mode changed from cleavage fracture and quasi-cleavage fracture to dimple fracture with increasing rolling temperature.

36 MATERIALS SCIENCE↗

Effect of Retrogression Heat Treatment Time on Microstructure and Mechanical Properties of AA7010

The effect of retrogression time during retrogression and re-aging (RRA) treatment of AA7010 is evaluated by performing tensile tests and characterizing the microchemistry of the grain boundary precipitates (GBPs) using transmission electron microscope coupled with the energy-dispersive spectroscopy. Retrogression time is evaluated so that the ultimate tensile strength of the RRA-treated sample is equal to that of the T6-treated sample and the grain boundary microstructure similar to that of the over-aged (T7451) condition. The investigation reveals that the sample retrogressed at 200 °C for 20 min has UTS of 586 MPa which is equivalent to that of the T6 sample and 11.5% higher than that of the T7451 condition. The fracture toughness of the RRA-treated sample was 41 MPa√m. Microstructure of the RRA-treated sample is similar to T7451, along the grain boundaries and in the grain interior similar to that of the T6-treated sample. Energy-dispersive spectroscopy confirmed the increment of Cu content on the GBP’s with increase in the retrogression time, which is expected to improve the stress corrosion cracking resistance of the alloy.

36 MATERIALS SCIENCE↗

Effect of Final Cooling Temperature on Microstructure and Mechanical Properties of a Cr-Ni-Mo-V Bainite Steel

The microstructural evolution and mechanical properties of a low-carbon high-strength bainitic steel under different final cooling temperatures were studied. The microstructures of the experimental steel at different final cooling temperatures were composed of acicular ferrite and granular bainite. A decrease in final cooling temperature resulted in an increase in volume fraction of granular bainite and a decrease in volume fraction of acicular ferrite. The specimen with the lowest final cooling temperature (459 °C) exhibited the highest yield strength, tensile strength, and yield ratio, and a lower total elongation than the specimens with the highest final cooling temperatures (501 and 535 °C) because of the higher volume fraction of granular bainite and finer bainitic ferrite lath. The specimen with the lowest final cooling temperature had a lower absorbed energy than that of the highest final cooling temperature, because the strip-like martensite–austenite (M-A) constituents that existed between the bainitic ferrite or in prior austenite grain boundaries reduced its toughness. At an intermediate final cooling temperature of 501 °C, the experimental steel exhibited excellent mechanical properties with a yield strength, tensile strength, and absorbed energy of 825 MPa, 1232 MPa, and 102 J, respectively.

36 MATERIALS SCIENCE↗

Annealing Effects on Microstructure and Mechanical Properties of Ultrafine-Grained Al Composites Reinforced with Nano-Al{sub 2}O{sub 3} by Rotary Swaging

Microstructure evolution and variations in mechanical properties of Al-Al{sub 2}O{sub 3} nanocomposite produced by powder metallurgy were investigated and compared with commercially pure aluminum (Al-1050) after furnace annealing. Fine gas-atomized Al powder compacts were first sintered in flowing nitrogen, subsequently consolidated into wires by rotary swaging and eventually annealed at 300 and 500 °C for 24 h each. Scanning and transmission electron microscopy with energy-dispersive spectroscopy was utilized to document the microstructure evolution. Rotary swaging was proven to lead to a marked decrease in grain size. After heavy swaging to true deformation degree of φ = 6 and annealing at 500 °C, obvious recrystallization was observed at Al-1050’s existing grain boundaries and the crystals began to grow perpendicular to the flow direction. In the Al-Al{sub 2}O{sub 3} nanocomposite, fabricated from d{sub 50} = 6 μm Al powder, recrystallization partially occurred, while grains were still extremely fine. Due to the dual role of fine-grained Al{sub 2}O{sub 3} dispersion strengthening, the nanocomposite showed improved mechanical performance in terms of tensile strength, approximately twice higher than Al-1050 after annealing at 500 °C.

36 MATERIALS SCIENCE↗

Effect of Hot Rolling on the Microstructure and Mechanical Properties of Nitrogen Alloyed Austenitic Stainless Steel

In the present investigation, the effect of multi-pass hot rolling in the temperature range of 700–1000 °C on the microstructure and mechanical properties of nitrogen alloyed austenitic stainless steel was studied with the aid of optical microscopy, tensile testing and x-ray diffraction measurements. The microstructural changes that occurred in the hot rolled specimens were elongation of grains in rolling direction, nucleation of new grains at the grain boundaries of elongated grains and growth of nucleated grains to form fully recrystallized grains. Elongated grains formed at lower rolling temperature (700–800 °C) due to inadequate strain/temperature for the initiation of dynamic recrystallization. At higher rolling temperature (900–1000 °C), fine grains formed due to dynamic recrystallization. Tensile properties showed strong dependency on the rolling temperature. Tensile strength increased with the decrease in the rolling temperature at the cost of ductility. Maximum strength was observed in samples hot rolled at 700 °C with yield strength of 917 MPa and ductility of 25%. This variation in the tensile properties with the rolling temperature is attributed to changes in the dislocation density and grain structure. The estimated yield strength from the dislocation density, solid solution and grain boundary strengthening closely matched with experimentally determined yield strength confirming the role of dislocation density and grain size in the strengthening.

36 MATERIALS SCIENCE↗

Effects of Stress Ratio and Microstructure on Fatigue Failure Behavior of Polycrystalline Nickel Superalloy

The effects of microstructure and stress ratio on high cycle fatigue of nickel superalloy Nimonic 80A were investigated. The stress ratios of 0.1, 0.5 and 0.8 were chosen to perform fatigue tests in a frequency of 110 Hz. Cleavage failure was observed, and three competing failure crack initiation modes were discovered by a scanning electron microscope, which were classified as surface without facets, surface with facets and subsurface with facets. With increasing the stress ratio from 0.1 to 0.8, the occurrence probability of surface and subsurface with facets also increased and reached the maximum value at R = 0.5, meanwhile the probability of surface initiation without facets decreased. The effect of microstructure on the fatigue fracture behavior at different stress ratios was also observed and discussed. Based on the Goodman diagram, it was concluded that the fatigue strength of 50% probability of failure at R = 0.1, 0.5 and 0.8 is lower than the modified Goodman line.

36 MATERIALS SCIENCE↗

Current-Assisted Diffusion Bonding of Extruded Ti-22Al-25Nb Alloy by Spark Plasma Sintering: Interfacial Microstructure and Mechanical Properties

Spark plasma sintering (SPS) technology was used to current-assisted bond extruded Ti-22Al-25Nb alloy. The effects of bonding temperature (920-980 °C) and bonding time (10-30 min) on the microstructure evolution and shear strength of this alloy were investigated systematically. The temperature distribution in the specimen during the current-assisted bonding process was also analyzed by numerical simulation. It is noted that the highest temperature was obtained at the bonding interface. As the bonding temperature and bonding time increased, the voids in the interface shrank increasingly until they vanished. A complete metallurgical bonding interface could be produced at 960 °C/20 min/10 MPa, exhibiting the highest shear strength of 269.3 MPa. In addition, the shear strength of the bonded specimen depended on its interfacial microstructure. With increased bonding temperature, the fracture mode transformed from the intergranular fracture at the bonding interface to the cleavage fracture in the substrate.

36 MATERIALS SCIENCE↗

Study on Microstructures and Mechanical Properties of Foam Titanium Carbide Ceramics Fabricated by Reaction Sintering Process

Foam titanium carbide (TiC) ceramics with a three-dimensional network structure were fabricated by the reaction sintering process, in which polyurethane foam was taken as the template, and TiO{sub 2} and phenolic resin were used as the reactants. Phase, microstructures and fracture morphologies of foam TiC ceramics were characterized by x-ray diffraction (XRD) and scanning electron microscopy (SEM), respectively. The results show that when the mass ratios of phenolic resin and TiO{sub 2} (F/T) are (0.8-1.2): 1, foam TiC ceramics with pure TiC phase can be formed. As the F/T ratios increase, crystal lattice parameters of fabricated foam TiC ceramics become bigger. When the value of F/T decreases from 1.2 to 0.8, grain size of TiC grows larger and microstructures get denser; meanwhile, the compressive strength increases from 0.10 to 1.05 MPa. Additionally, either raising the sintering temperatures or extending holding time can facilitate the completion of the reaction process and increase the compressive strength.

36 MATERIALS SCIENCE↗

Effects of Chromium Additions upon Microstructure and Mechanical Properties of Cold Drawn Pearlitic Steel Wires

Cr-containing pearlitic steel wires were prepared through cold drawing and simulated galvanization process. Effect of chromium microalloying on microstructural and mechanical properties of the steel wires was investigated. Experimental results show that size of pearlitic colonies of the steel rods decreased as Cr content increased from 0.2 to 0.6 wt.%; meanwhile, interlamellar spacing was little affected because of isothermal phase transition in salt bath. The tensile strength of the pearlitic steel rods was increased from 1480 to 1550 MPa. The tensile strength of the Cr-containing cold drawn wires (ε = 1.58) was increased about 33%, and the torsion circle of the wires were about 15 with cleavage fracture. After annealing at 450 °C for 2 min, tensile strength of the wires increased, but torsion circle was decreased to less than 5. As the annealing time increased, the torsion circle of the steel wires with 0.2 wt.% Cr was improved to about 10 with cleavage fracture, while the torsion performance of the wires having high Cr contents remained low because of delamination fracture. The cementite platelets in Cr-containing wires turned into cementite crystal particles during cold drawing. Microstructure observation and thermal analysis have confirmed that thermal stability of cementite was enhanced with the increase of Cr content.

36 MATERIALS SCIENCE↗