Search NASA⌕ Search

SEARCH · Search NASA

Results for “PRESSING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,747 records · Page 97

Quantitative description of microstructure defects in hexagonal boron nitrides using X-ray diffraction analysis

A routine for simultaneous quantification of turbostratic disorder, amount of puckering and the dislocation and stacking fault density in hexagonal materials was proposed and tested on boron nitride powder samples that were synthesised using different methods. The routine allows the individual microstructure defects to be recognised according to their effect on the anisotropy of the X-ray diffraction line broadening. For quantification of the microstructure defects, the total line broadening is regarded as a linear combination of the contributions from the particular defects. The total line broadening is obtained from the line profile fitting. As testing material, graphitic boron nitride (h-BN) was employed in the form of hot-isostatically pressed h-BN, pyrolytic h-BN or a h-BN, which was chemically vapour deposited at a low temperature. The kind of the dominant microstructure defects determined from the broadening of the X-ray diffraction lines was verified by high resolution transmission electron microscopy. Their amount was attempted to be verified by alternative methods. - Highlights: • Reliable method for quantification of microstructure defects in BN was suggested. • The method is based on the analysis of anisotropic XRD line broadening. • This XRD line broadening is unique and characteristic of the respective defect. • Thus, the quantification of coexistent microstructure defects is possible. • The method was tested on hexagonal BN, which was produced by different techniques.

36 MATERIALS SCIENCE↗

Influence of powder metallurgy route on precipitation processes in MgTbNd alloy

Solution treated MgTb3Nd2 alloy (nominal composition in wt.%) (ST) and the alloy prepared by hot extrusion of isostatically pressed powder (PM) were isochronally heat treated and studied by electrical resistivity and hardness measurements and by differential scanning calorimetry. Microstructure development was investigated in transmission electron microscopy. Successive precipitation of transient phases in the sequence β″ (D0{sub 19} plates) → β′(cbco) → β{sub 1} (Mg{sub 3}Gd type, fcc) → β (Mg{sub 5}Gd type, fcc) known from the ST alloy was identified also in the PM alloy. The early precipitation stage (D0{sub 19} clusters) revealed in the ST alloy as well as precipitation of equilibrium β{sub e} phase Mg{sub 41}(Tb,Nd){sub 5} manifest themselves only slightly in the PM alloy. Powder metallurgy route does not change the values of activation energies but shifts the temperature ranges of these processes. Vickers hardness of the as prepared state is higher in the PM alloy and is very resistant against the heat treatment up to 510 °C. Contrary to the ST alloy precipitation due to isochronal annealing does not lead to pronounced hardness changes in the PM alloy. - Highlights: • Powder metallurgy (PM) does not change precipitation sequence in MgTbNd alloy. • Temperature ranges of transient phase precipitations are shifted in PM alloy. • Hardness is resistant against isochronal heat treatment up to 510 °C in the PM alloy. • PM procedure does not change activation energies of precipitation.

36 MATERIALS SCIENCE↗

Investigation of nanostructured Al-10 wt.% Zr material prepared by ball milling for high temperature applications

Ground chips of as-cast Al-10 wt.% Zr alloy were subjected to mechanical alloying (MA) with 5 vol.% of nanodiamond addition in a high energy planetary ball-mill. The aim of this work was to investigate the microstructure, phase transformation and mechanical properties of the material both after MA and after subsequent annealing. Optical and transmission electron microscopes were used for morphological and microstructural analysis. The effect of milling time on powder microhardness, Al lattice parameter, lattice microstrain and crystallite size was determined. It was shown that mechanical alloying of as-cast Al-10wt.%Zr alloy during 20 h leads to a complete dissolution of the primary tetragonal Al{sub 3}Zr crystals in aluminum. At the same time, the powder microhardness increases to 370 HV. Metastable cubic Al{sub 3}Zr phase nanoparticles precipitate from the Al solution due to its decomposition after annealing, however, the Al solid solution remains supersaturated and nanocrystalline. Compression tests at room temperature and at 300 °C showed that the strength values of the hot-pressed samples reach 822 MPa and 344 MPa, respectively. - Highlights: •As-cast Al-10 wt.% Zr alloy was mechanically alloyed with 5 vol.% nanodiamond. •The primary tetragonal Al{sub 3}Zr crystals were completely dissolved in Al after 20 h. •Cubic Al{sub 3}Zr phase nanoparticles precipitated from Al solution after aging. •The aged bulk material showed a high strength at room and elevated temperatures.

36 MATERIALS SCIENCE↗

Effect of Y/Ti atomic ratio on microstructure of oxide dispersion strengthened alloys

Highlights: • Controlling nano oxide distributions in ODS alloys by tuning Y/Ti ratio. • Advanced characterization techniques have been conducted to comprehensively study the various nano oxides. • A recipe with a Y/Ti ratio of 0.4 was found and the intrinsic oxide formation mechanism was explained. - Abstract: Oxide dispersion strengthened (ODS) alloys are the leading candidate materials for advanced fission and fusion reactor components because of their excellent high temperature creep strength and radiation tolerance. The promising performance of ODS alloys relies on a high-density population of nano oxides. Here, four 9Cr-ODS alloys with varying initial Y/Ti atomic ratio were processed using a combined route of mechanical alloying (MA) and hot isostatic pressing (HIP). Microstructural characterizations of the consolidated alloys were examined by advanced transmission electron microscopy (TEM). Great differences in oxide distribution behavior were observed. 9Cr-ODS alloy with a Y/Ti ratio of 0.4 presented the finest and the highest number density of nano oxides among the four alloys. The effects of Y/Ti ratio on oxide formation were explored, and the precipitated mechanisms of the nano oxides were interpreted.

36 MATERIALS SCIENCE↗

Dynamic restoration of severely predeformed, ultrafine-grained pure Cu at 373 K observed in situ

Highlights: • Discontinuous grain coarsening during tension at 373 K generated new grains exceeding significantly grain size of UFG Cu. • The coarsening was preferentially located at shear bands. • There are indications that the grain coarsening occurs by recrystallization. - Abstract: Microstructure changes of ultrafine-grained pure copper prepared by equal-channel angular pressing were investigated during in situ tensile testing inside a scanning electron microscope at constant total strain rate of 10{sup −4} s{sup −1} at 373 K (~ 0.28 T{sub m}). After fast work hardening the flow stress saturated at an inelastic strain of 0.06. Significant local coarsening of grains was observed to start at about 2/3 of the maximum flow stress. However, these localized events did not significantly change the mean grain size up to an inelastic strain of 0.09. Surface observations showed that the coarsening was preferentially located at shear bands.

36 MATERIALS SCIENCE↗

A comprehensive investigation of the strengthening effects of dislocations, texture and low and high angle grain boundaries in ultrafine grained AA6063 aluminum alloy

Highlights: • Evolution of microstructure and mechanical properties of AA6063 after severe plastic deformation was investigated. • Average cell size shows a more solid relationship with mechanical properties rather than the average grain size. • This indicates that in addition to high angle boundaries, cell boundaries play a strengthening role. - Abstract: The effect of equal channel angular pressing (ECAP) on the microstructure and mechanical properties of AA6063 aluminum alloy was investigated. For this purpose, samples of AA6063 aluminum alloy were deformed up to 10 passes using ECAP and the evolution of microstructure, texture and dislocation density was investigated. It was found that the dislocation density increased and cells mostly surrounded by low angle boundaries (LABs) formed after 2 passes ECAP. Increasing the dislocation density continued with further processing and reached a maximum at the 4th ECAP pass. With further deformation to 6 passes, the dislocation density reduced, the fraction of high angle boundaries (HABs) increased and the averages of cell size and grain size reduced, significantly, which indicated the occurrence of grain refinement. However, a slight increase in dislocation density, average cell size (ACS) and average grain size (AGS), indicating coarsening, occurred when 10 passes of ECAP are imposed. Hardness, yield (YS) and ultimate tensile strength (UTS) increased continuously although the most significant enhancement occurred after 2 passes of ECAP. Investigating the correlation between the microstructure and mechanical properties indicated that Hall-Petch relationship was valid for ultrafine grained AA6063 before the coarsening started provided that the property of interest was correlated to average cell size but not the average grain size.

36 MATERIALS SCIENCE↗

Simultaneously improving mechanical properties and corrosion resistance of pure Ti by continuous ECAP plus short-duration annealing

Highlights: • Additional short-time annealing led to enhanced strength of UFG Ti due to texture strengthening. • UFG Ti showed improved corrosion resistance in artificial seawater compared with initial CG Ti. • Short-duration annealing enhanced corrosion resistance of UFG Ti due to stronger basal texture. - Abstract: This work investigated the effect of short-duration annealing on mechanical properties and corrosion behavior of bulk ultrafine-grained (UFG) pure Ti (grade 2) produced by high-efficiency equal-channel angular pressing (ECAP), serving the fast developing of marine industries. The initial coarse-grained (CG) Ti achieved higher strength after continuous ECAP at 420 °C for 4 passes, while additional short-duration annealing at 300 °C for 15 min of UFG Ti further led to extraordinary improvement of strength, which was associated with texture strengthening. The yield strength was increased from 362 MPa in as-received state to 561 MPa in post-ECAP annealed condition, and ultimate tensile strength from 450 MPa to 663 MPa. The ECAP-processed UFG Ti had better corrosion resistance in artificial seawater than the initial CG Ti. Short-duration annealing further improved the corrosion resistance of UFG Ti, which was related to stronger basal texture. The corrosion current density decreased from 68.37 nA cm{sup −2} for CG Ti in as-received condition to 41.77 nA cm{sup −2} for UFG Ti processed by ECAP plus short-duration annealing. The fraction of TiO{sub 2} within the surface oxide film for the post-ECAP annealed sample was increased. The bulk UFG Ti after post-ECAP short-duration annealing revealed an excellent combination of high strength, good ductility and superior corrosion resistance for marine applications.

36 MATERIALS SCIENCE↗

Microstructure of titanium on complex deformation paths: Comparison of ECAP, KOBO and HE techniques

Highlights: • Method for producing CP titanium rods for medical implants is searched. • Three processing methods producing ultra-fine grain titanium are compared. • Microstructure and textures are examined and analysed. • Mechanical characteristics are determined based on microhardness and tensile tests. • Hydrostatic extrusion (HE) leads to the best properties of titanium rods for medical implants. - Abstract: In this work samples of commercial purity grade 2 titanium were severely deformed by three different extrusion techniques: equal-channel angular pressing (ECAP), extrusion through oscillating die (KOBO), and hydrostatic extrusion (HE). Resulting microstructures and mechanical properties of processed titanium samples are studied and compared with regard to potential application as a material for dental implants. The obtained results demonstrate the effect of different strain paths, involved by three applied deformation methods, on microstructure refinement, mechanical properties and textures of the studied material. Heterogeneous microstructures with bimodal grain size distributions are observed for all deformation techniques in the examined material, however differences in their internal structures and grain boundary distributions point to different grain refinement mechanisms. The fraction of ultra-fine grains is the highest in titanium deformed by HE. Also the internal grain fragmentation is the most important after HE deformation. This leads to the best mechanical and microstructural properties obtained in this type of deformation. Consequently, the HE process seems to be very interesting for production of material for medical implants.

36 MATERIALS SCIENCE↗

Effect of temperature on microstructure and mechanical properties of ECAPed (TiB + La2O3)/Ti-6Al-4V composites

Highlights: • Dynamic recrystallization resulted in ultrafine grains near TiB interface region. • Tensile strength of ECAPed composites increased by up to 18%. • The average aspect ratio of TiB reduced with increasing ECAP temperature. • Interface debonding of TiB led to crack propagation and low ductility. TiB short fibers and La{sub 2}O{sub 3} particles reinforced titanium matrix composites (TMCs) were successfully equal-channel angular pressed (ECAPed) at 600 °C–900 °C. The effect of ECAP temperature on the microstructure and mechanical properties of the TMCs was investigated. The results indicated that dislocation tangling formed cell structures in matrix at lower ECAP temperature. In contrast, continuous dynamic recrystallization occurred at higher ECAP temperature, and promoted the formation of numerous new ultrafine grains. The average aspect ratio of TiB short fibers decreased with increasing ECAP temperature, which induced interfacial debonding. The tensile strength of TMCs ECAPed at 800 °C was up to 1128 MPa, which was 18% higher than the as-received composites. Interfacial debonding led TiB short fibers in low aspect ratios disabled to bear load, while the formation of ultrafine grains increased the strength of TMCs. The coupling of these two factors resulted in little effect of ECAP temperature on the tensile strength. However, the elongation of ECAPed TMCs generally decreased due to the loss of strain hardening capacity. Stress concentration tended to occur around the tips of TiB short fibers due to the interfacial debonding and cause crack propagation. It led to the premature fracture and low ductility.

36 MATERIALS SCIENCE↗

Evolution of microstructure and microtexture during hot deformation in an advanced P/M nickel base superalloy

Highlights: • Microstructural evolution of PM superalloy sensitive to temperature and strain rate. • Highest DRX with finer grained structure at higher temperatures and strain rates. • Dominance of DDRX showed by serrated grain boundaries and misorientation gradient. • Weak microtextural evolution inclined towards [110] fiber compression texture seen. In the present study, the effect of hot deformation parameters on the microstructural evolution is investigated for an experimental powder metallurgy nickel superalloy. The hot isostatically pressed (HIPed) alloy is isothermally hot compressed at constant true strain rate over wide temperatures (1000 °C, 1050 °C, 1100 °C, 1150 °C) and strain rates (0.001 s{sup −1}, 0.01 s{sup −1}, 0.1 s{sup −1}, 1 s{sup −1}) regimes. Electron Back-Scattered Diffraction (EBSD) characterization of the hot deformed samples is carried out to evaluate the microstructural evolution, grain boundary characteristics, and microtextural behaviour. The strong dependence of dynamic recrystallization characteristics on the hot deformation conditions is divulged through EBSD derived colour inverse pole figure maps endorsed by grain/twin boundary characteristics and misorientation gradient. Dynamic recrystallization (DRX) is maximized at higher deformation temperatures, whereas limited DRX is observed at lower deformation temperatures, especially at higher strain rates. The dominance of discontinuous dynamic recrystallization (DDRX) is manifested through bulged/serrated grain boundaries resulting in the formation of necklace microstructure corroborated by grain boundary cumulative misorientation gradient. Although random microtexture is revealed in both deformed and recrystallized microstructures, the tendency towards the formation of 110 fiber compression texture is apparently evident.

36 MATERIALS SCIENCE↗

High strength W/TiNi micro-laminated composite with transformation-mediated ductility

A laminated W/TiNi composite is fabricated by hot pressing under vacuum and subsequent forging. The W and TiNi constituents are about 250 μm and 80 μm respectively in thicknesses and their interfaces are chemically sharp with negligible intermixing. The material exhibits two yielding plateaus and excellent strength-ductility combination during compression tests. In situ X-ray technique is employed to demonstrate that the unusual yielding phenomenon is related to the reversible thermoelastic phase transformation of TiNi layers. Furthermore, such mechanisms also contribute to the damage tolerance of the materials by inhibiting crack propagation in W.

36 MATERIALS SCIENCE↗

Evolution of the mechanical properties of a cobalt-based alloy under thermal shocks

A cobalt-base alloy manufactured by hot isostatic pressing sintering (HIP) was investigated in the present work. A series of quenching thermal-shock experiments were carried out to study the effects of thermal-cycle shocks on this new cobalt-based alloy. Scanning Electron Microscope (SEM) and Energy Dispersion Spectrum (EDS) were employed to observe the evolution of microstructures under thermal-shock cycles. Results show that some floccus Co 3 W 3 C precipitated around the WC particles after several thermal-shock cycles. These precipitates and the carbide particles correspond to the locations with the high-stress concentration. The mechanical properties evolution under thermal-shock cycles was analyzed by Nanoindentation tests. The nanohardness presents no noticeable change with thermal-shock cycles. However, the reduced modulus demonstrates a decreasing trend with the thermal-shock cycles. The variation of the mechanical properties has an unestimated relationship with the residual stress and densities of dislocations caused by thermal shocks. Furthermore, the present work pointed out that the precipitates around the carbides are the places where the thermal fatigue crack initiated. How to deal with the precipitates will be the optimized way for this material.

36 MATERIALS SCIENCE↗

Thin film ceria–bismuth bilayer electrolytes for intermediate temperature solid oxide fuel cells with La0.85Sr0.15MnO3-δ–Y0.25Bi0.75O1.5 cathodes

Thin film electrolytes of bilayer bismuth oxide/ceria are developed for intermediate temperature solid oxide fuel cells. Y0.25Bi0.75O1.5 is deposited via Direct Current magnetron sputtering technique on an Sm0.2Ce0.8O1.90 electrolyte film which is prepared by a dry-pressing process on an NiO–Sm0.2Ce0.8O1.90 substrate. La0.85Sr0.15MnO3-δ–Y0.25Bi0.75O1.5 composite is applied onto the Y0.25Bi0.75O1.5 film as the cathode to form a single cell. Cells with 6-μm-thick Y0.25Bi0.75O1.5 and 26-μm-thick Sm0.2Ce0.8O1.90 bilayer electrolytes exhibit improved open circuit voltages and power density compared with those obtained with only Sm0.2Ce0.8O1.90 electrolytes. The open circuit voltages are comparable and power densities are higher than those previously reported for solid oxide fuel cells with thick bilayer electrolytes using noble metals such as Pt as the electrodes. Impedance spectra show that the change of electrolyte resistance is negligible while the cathodic interfacial polarization resistance decreased significantly when the Y0.25Bi0.75O1.5 layer is added to form the Sm0.2Ce0.8O1.90/Y0.25Bi0.75O1.5 bilayer electrolytes.

36 MATERIALS SCIENCE↗

Microstructure control on thermoelectric properties of Ca{sub 0.96}Sm{sub 0.04}MnO{sub 3} synthesised by co-precipitation technique

Nanopowder of Ca{sub 0.96}Sm{sub 0.04}MnO{sub 3} (CSM) perovskite was prepared by chemical co-precipitation technique. It was characterized and studied by X-ray diffraction and Transmission Electron Microscopy. Nano-crystalline CSM phase having grain size of 60-70 nm can be prepared by calcination at 1073 K for 6 h in air. The obtained nanopowder was pressed, sintered at 1373 K for 24 h to obtain a dense sample. In comparison, CSM samples prepared from normal powder need sintering temperature of 1623 K to reach a similar microstructure, showing the efficiency of nanopowder to decrease the sintering temperature. The thermoelectric properties of samples prepared with two different processes were studied. The Seebeck coefficient and the thermal conductivity slightly decrease by using the nanopowder while the value of the electrical resistivity does not change. This results in the same figures of merit for the two materials.

36 MATERIALS SCIENCE↗

Multiferroic properties of Pb{sub 2}Fe{sub 2}O{sub 5} ceramics

Research highlights: {yields} Simultaneous occurrence of ferromagnetism and ferroelectricity in Pb{sub 2}Fe{sub 2}O{sub 5} ceramics. {yields} The off-centers of shifted Pb{sup 2+} ions as well as the FeO{sub 6} octahedra in the 'Pb{sub 2}Fe{sub 2}O{sub 5}' lead to a ferroelectric polarization. {yields} Pb{sub 2}Fe{sub 2}O{sub 5} ceramic demonstrates ferromagnetic order state due to the spin arrangement in the double chains of FeO{sub 5} tetrahedral pyramids. -- Abstract: Pb{sub 2}Fe{sub 2}O{sub 5} (PFO) powders in monoclinic structure have been synthesized using lead acetate in glycerin and ferric acetylacetonate as the precursor. The powders were pressed into pellets, which were sintered into ceramics at 800 {sup o}C for 1 h. The morphology and structure have been determined by X-ray diffraction (XRD) and field emission scanning electron microscopy (FESEM). Polarization was observed in Pb{sub 2}Fe{sub 2}O{sub 5} ceramics at room temperature, exhibiting a clear ferroelectric hysteresis loop. The remanent polarization of Pb{sub 2}Fe{sub 2}O{sub 5} ceramic is estimated to be Pr {approx} 0.22 {mu}C/cm{sup 2}. The origin of the polarization may be attributed to the off-centers of shifted Pb{sup 2+} ions as well as the FeO{sub 6} octahedra in the perovskite-based structure of Pb{sub 2}Fe{sub 2}O{sub 5}. Magnetic hysteresis loop was also observed at room temperature. The Pb{sub 2}Fe{sub 2}O{sub 5} ceramic shows coexistence of ferroelectricity and ferromagnetism. It provides a new field of research for complex oxides with multiferroic properties.

36 MATERIALS SCIENCE↗

Microstructural and electrical changes in nickel manganite powder induced by mechanical activation

Highlights: {yields} The influence of mechanical activation on microstructure evolution in the nickel manganite powder was investigated as well as electrical properties of the sintered samples. {yields} Structural refinement obtained by Topas-Academic software based on Rietveld analysis showed that the milling process remarkably changed the powder morphology and microstructure. {yields} SEM studies of sintered samples also revealed the strong influence of milling time on ceramics density (increases with milling time). {yields} The electrical properties of ceramic samples are clearly conditioned by terms of synthesis, in our case the time of mechanical activation. {yields} The highest density and higher values of dielectric constant were achieved at the sample activated for 45 min. -- Abstract: Nickel manganite powder synthesized by calcination of a stoichiometric mixture of manganese and nickel oxide was additionally mechanically activated in a high energy planetary ball mill for 5-60 min in order to obtain a pure NiMn{sub 2}O{sub 4} phase. The as-prepared powders were uniaxially pressed into disc shape pellets and then sintered for 60 min at 1200 {sup o}C. Changes in the particle morphology induced by mechanical activation were monitored using scanning electron microscopy, while changes in powder structural characteristics were followed using X-ray powder diffraction. The ac impedance spectroscopy was performed on sintered nickel manganite samples at 25 {sup o}C, 50 {sup o}C and 80 {sup o}C. It was shown that mechanical activation intensifies transport processes causing a decrease in the average crystallites size, while longer activation times can lead to the formation of aggregates, defects and increase of lattice microstrains. The observed changes in microstructures were correlated with measured electrical properties in order to define optimal processing conditions.

36 MATERIALS SCIENCE↗

In situ formation of sintered cordierite–mullite nano–micro composites by utilizing of waste silica fume

Highlights: ► We succeeded to obtain in situ formed sintered cordierite–mullite nano–macro composites from waste and pure materials at 1400 °C. ► Their sinterability was greatly dependent on both firing temperature and composition. ► XRD patterns showed that the optimum temperature required for formation of sintered cordierite–mullite nano–macro composites was achieved at 1400 °C. ► The batch containing 70 wt.% cordierite and 30 wt.% mullite exhibited the best properties. ► Microstructures of the densified composites were composed of nano–macro cordierite–mullite structures. -- Abstract: This study aims at in situ formation of sintered cordierite–mullite nano–macro composites having high technological properties using waste silica fume, calcined ball clay, calcined alumina, and magnesia as starting materials. The starting materials were mixed in different ratios to obtain different cordierite–mullite composite batches in which the cordierite contents ranged from 50 to 100 wt.%. The batches were uni-axially pressed at 100 MPa and sintered at 1350, 1400 and 1450 °C to select the optimum temperature required for cordierite–mullite nano–macro composites formation. The formed phases were identified by X-ray diffraction (XRD) pattern. The sintering parameters in terms of bulk density (BD) and apparent porosity (AP) were determined. The microstructure of composites has been investigated by scanning electron microscope (SEM). Cold crushing strength (CCS) of the sintered batches was evaluated. The result revealed that the cordierite–mullite nano–macro composites were in-situ formed at 1400 °C. The batch containing 70 wt.% cordierite showed good physical and mechanical properties.

36 MATERIALS SCIENCE↗

Photo-oxidative degradation of TiO{sub 2}/polypropylene films

Graphical abstract: - Highlights: • Photo-oxidative degradation of polypropylene is accelerated by TiO{sub 2} incorporation. • Weight loss, FTIR, SEM and GPC shown high degree of degradation of polypropylene. • A mechanism of the photo-degradation of polypropylene by TiO{sub 2} is proposed. - Abstract: Photo-oxidative degradation of polypropylene films with TiO{sub 2} nanoparticles incorporated was studied in a chamber of weathering with Xenon lamps as irradiation source. TiO{sub 2} powder with crystalline structure of anatase was synthesized by thermal treatments at 400 and 500 °C starting from a precursor material obtained by sol–gel method. Composites of TiO{sub 2}/polypropylene were prepared with 0.1, 0.5 and 1.0 wt% of TiO{sub 2}. The mixture of components was performed using a twin screw extruder, the resulting material was pelletized by mechanical fragmenting and then hot-pressed in order to form polypropylene films with TiO{sub 2} dispersed homogeneously. Photo-oxidative degradation process was followed by visual inspection, weight loss of films, scanning electron microscopy (SEM), infrared spectroscopy with Fourier transformed (FTIR), and gel permeation chromatography (GPC)

36 MATERIALS SCIENCE↗