Search NASA⌕ Search

SEARCH · Search NASA

Results for “interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,747 records · Page 97

Cryogenic EM Across Length Scales for Li Metal Anode Batteries

An interfacial understanding is necessary for developing strategies to commercialize high-energy density rechargeable lithium metal anode batteries, as currently, the lithium anode/electrolyte interface is unstable with prolonged cycling. We have used several strategies to improve the cycling performance of lithium metal anodes, including reducing the parasitic reactions between lithium metal and the electrolyte, and improving the electrodeposited lithium metal morphology. These strategies have generated unconclusive electrochemical data, that has required the need for nanoscale interfacial characterization of these solid-liquid interfaces. Our team has used the cryogenic transfer workflow developed by Leica in collaboration with cryo-SEM/FIB tools by Thermo Fisher Scientific to cross-section lithium metal anodes and intact coin cell batteries to observe the interfacial structures, lithium morphology, and failure mechanisms relative to changes in electrode contract pressure and electrolyte chemistry. Cross-sectional SEM images and EDS maps of the lithium metal anodes have provided a better understanding of the electrodeposited lithium morphology, quantity of 'dead' lithium metal, and quantity of solid electrolyte interphase material that has formed alongside the lithium metal. In understanding lithium metal battery failure at the system level, we used a cryogenic stage in a laser plasma FIB to cross-section through the coin cell's cap for imaging/mapping the entire battery stack under cryogenic conditions. The tools, methods, and results of these studies will be detailed in this presentation.

characterization↗

Anode Upcycling via Tailored Solvent Treatment

To achieve a truly closed-loop direct recycling process for lithium-ion batteries, all component materials must be recovered. To date, direct recycling method development has primarily focused on the high-value transition-metal cathode materials, while the inherently lower-value graphite has been challenging to recover in a cost-effective manner. However, end-of-life graphite contains a unique engineered value due to the presence of the solid electrolyte interphase (SEI). Growth of the SEI during the cell's active lifetime stabilizes the electronically reactive graphite surface through an irreversible consumption of Li, and thus necessitates both excess lithiation of the cathode and a costly and time-intensive formation procedure during manufacturing. An optimized pre-formed SEI that capitalizes on existing SEI components from end-of-life batteries has the potential to significantly reduce cathode lithiation requirements and eliminate the critical bottleneck of formation cycling during cell remanufacturing. Further, retaining Li at the anode obviates the need for a separate Li leaching and recovery step, improving the overall efficiency of the direct recycling line. In this work, we present a novel approach to "upcycling" spent graphite through use of tailored chemical treatment to remove adverse (i.e., highly resistive and/or poorly passivating) SEI species while retaining beneficially passivating components. We have explored a rational set of solvents spanning a range of polarity, proticity, and molecular size to evaluate structure-property-performance relationships between applied solvent(s), removed and remaining SEI species, and electrochemical response of the resulting graphite product. Further, we have developed and optimized a robust and holistic analysis procedure that couples symmetric-cell electrochemical testing, multi-modal materials characterization, and advanced electrochemical modeling. These analysis results inform a set of correlative metrics for graphite performance relative to both solvent properties and upcycled SEI composition. We demonstrate effective tunability in the residual SEI composition by varying solvent identity and concentration, and report on several promising solvent systems that achieve comparable or performance to pristine graphite.

anode recycling↗

Understanding LIB Battery Electrodes Through Classical Electrochemical Interface Theory

Classical models of the electrochemical interface can be applied to complex and dynamic electrodes to understand important mechanisms that are relevant to device-level phenomena like calendar aging or cycle life. Here, we show that negative alloy electrodes with wide electrochemical windows cannot be assumed to have static interfaces throughout all states of charge. Under high states of charge, the interface -including the solid electrolyte interphase - has characteristics that resemble a highly polarized electrode far from the point of zero charge. Under these conditions, the interface can be understood through the Helmholtz model. At lower states of charge, the interface capacitance decreases and the space charge layer length increases. This transformation resembles a metal electrode approaching the point of zero charge which is understood through the Gouy-Chapman-Stern-Grahame model of the electrochemical interface. This transformation happens at both silicon and carbon-coated silicon interfaces. From voltage-limited cycling experiments, in the limit of the diffuse double layer, the silicon electrode impedance rises significantly in the first few cycles. This rise is related to the continuous electrochemical reduction of electrolyte components from an interface that is not electronically screened from the electrolyte. In other words, an electrode interface for batteries should resemble a 'Helmholtz-like' structure.

anode↗

Surface heterogeneity propagation and homogenization for pouch cell-scale Li metal anodes

Li metal anode is a promising candidate for next-generation energy storage systems and is widely explored in Li-ion and solid-state batteries. Despite its potential, Li metal anodes face instabilities during long-term cycling, especially when paired with NMC or sulfur-based cathodes, where Li is cycled at high capacities of 6-8 mAh/cm2, equivalent to a thickness of 30-40 µm. During such extensive utilization, degradation mechanisms such as excessive solid electrolyte interphase (SEI), dendrites, and dead Li emerge, and ultimately lead to sudden failure and reduced cycle life. The origin of the degradation mechanisms stem from surface heterogeneities introduced during Li foil manufacturing and storage [1, 2]. As cycling progresses, the local heterogeneities propagate, resulting in uneven Li utilization and degradation-prone regions across the electrode [3], which consequently induce performance variations at the cell level. This heterogeneity propagation is particularly pronounced in large-format pouch cells in practical applications, where the surface effects are magnified. Without a clear understanding of the multi-scale heterogeneities and the development of surface homogenization methods, the performance consistency will be compromised, hindering the commercialization of Li metal batteries. In this presentation, we investigate the evolution of surface heterogeneity propagation on commercially available Li foils. We discover that inhomogeneous Li utilization appears as early as the first half-cycle of formation, manifesting as localized clusters and pits. In pouch cell configurations, these features exhibit areal density variations across the electrode on a scale of millimeters. To improve Li utilization homogeneity, a scalable mechanical brushing method is introduced to remove the chemically heterogeneous surface passivation layer. Furtherore, the influence of utilization homogeneity on cell-to-cell consistency is evaluated using 32 Li-NMC811 pouch cells divided into as-received and brushed Li groups. On the brushed Li, clusters and pits are no longer observable, and the cells exhibit significantly improved consistency in discharge capacity trajectories and cycle lifetime. Overall, this study highlights the role of Li surface utilization homogeneity on long-term cycling performance. Our research provides a pathway for improving large-area electrode uniformity and establishing evaluation methods for cell-to-cell consistency, both are key steps toward the commercialization of Li metal batteries and beyond. [1] Otto, Svenja-K., et al. "In-depth characterization of lithium-metal surfaces with XPS and ToF-SIMS: toward better understanding of the passivation layer." Chemistry of Materials 33.3 (2021): 859-867. [2] Hatzell, Kelsey, et al. "Aligning lithium metal battery research and development across academia and industry." Joule (2024). [3] Kim, Sangwook, et al. "Calendar life of lithium metal batteries: Accelerated aging and failure analysis." Energy Storage Materials 65 (2024): 103147.

25 - ENERGY STORAGE↗

TRANSMISSION ELECTRON MICROSCOPY STUDY OF HELIUM BEARING FUSION WELDS

A transmission electron microscopy (TEM) study was conducted to characterize the helium bubble distributions in tritium-charged-and-aged 304L and 21Cr-6Ni-9Mn stainless steel fusion welds containing approximately 150 appm helium-3. TEM foils were prepared from C-shaped fracture toughness test specimens containing {delta} ferrite levels ranging from 4 to 33 volume percent. The weld microstructures in the low ferrite welds consisted mostly of austenite and discontinuous, skeletal {delta} ferrite. In welds with higher levels of {delta} ferrite, the ferrite was more continuous and, in some areas of the 33 volume percent sample, was the matrix/majority phase. The helium bubble microstructures observed were similar in all samples. Bubbles were found in the austenite but not in the {delta} ferrite. In the austenite, bubbles had nucleated homogeneously in the grain interiors and heterogeneously on dislocations. Bubbles were not found on any austenite/austenite grain boundaries or at the austenite/{delta} ferrite interphase interfaces. Bubbles were not observed in the {delta} ferrite because of the combined effects of the low solubility and rapid diffusion of tritium through the {delta} ferrite which limited the amount of helium present to form visible bubbles.

08 HYDROGEN↗

Effect of Gallium Focused Ion Beam Milling on Preparation of Aluminum Thin Foils

Focus Ion Beam (FIB) milling has greatly extended the utility of atom probe and TEM because it enables sample preparation with a level of dimensional control never before possible. Using FIB it is possible to extract the samples from desired and very specific locations. The artifacts associated with this sample preparation method must also be fully understood. In this work issues specifically relevant to the FIB milling of aluminum alloys are presented. After using the FIB as a sample preparation technique it is evident that gallium will concentrate in three areas of the sample: on the surface, on grain boundaries and at interphase boundaries. This work also shows that low energy Ar ion nanomilling is potentially quite effective for removing gallium implantation layers and gallium from the internal surfaces of aluminum thin foils.

36 MATERIALS SCIENCE↗

Effects of Imide–Orthoborate Dual-Salt Mixtures in Organic Carbonate Electrolytes on the Stability of Lithium Metal Batteries

The effects of lithium imide and lithium orthoborate dual-salt electrolytes of different salt chemistries in carbonate solvents on the cycling stability of Li metal batteries were systematically and comparatively investigated. Two imide salts (LiTFSI and LiFSI) and two orthoborate salts (LiBOB and LiDFOB) were chosen for this study and compared with the conventional LiPF6 salt. The cycling stability of the Li metal cells with the electrolytes follows the order from good to poor as LiTFSI-LiBOB > LiTFSI-LiDFOB > LiPF6 > LiFSI-LiBOB > LiFSI-LiDFOB, indicating that LiTFSI behaves better than LiFSI and LiBOB over LiDFOB in these four dual-salt mixtures. The LiTFSI-LiBOB can effectively protect the Al substrate and form a more robust surface film on Li metal anode, while the LiFSI-LiBOB results in serious corrosion to the stainless steel cell case and a thicker and looser surface film on Li anode. Computational calculations indicate that the chemical and electrochemical stabilities also follow the order of LiTFSI-LiBOB > LiTFSI-LiDFOB > LiFSI-LiBOB > LiFSI-LiDFOB. The key findings of this work emphasize that the salt chemistry is critically important for enhancing the interfacial stability of Li metal anode and should be carefully manipulated in the development of high performance Li metal batteries.

Li metal batteries, dual-salt electrolyte, solid e↗

Prospective Application, Mechanism, and Deficiency of Lithium Bis(oxalate)Borate as the Electrolyte Additive for Lithium-Batteries

Lithium bis(oxalate)borate (LiBOB) is one of the most common film-forming electrolyte additives used in lithium ion batteries (LIBs), since it can form a dense boron-containing polymer as a solid electrolyte interlayer (or cathode electrolyte interlayer) in order to isolate the electrode material from the electrolyte and prevent side reactions. LiBOB can serve as HF scavenger to maintain the structural integrity of electrodes via avoiding the transition metal dissolution caused by HF attack. Additionally, LiBOB also can react with LiPF 6 to generate lithium difluoro (oxalate)borate (LiDFOB) that can be further used as a clean-up agent for reactive oxygen radicals. This article lists the application of LiBOB in high capacity and high voltage cathode materials, and also reviews the working mechanisms of LiBOB used in these materials to improve the performance of LIBs. Finally, it presents the current shortcomings of LiBOB and strategies to overcome these. This article is expected to provide useful insights for employing LiBOB as a feasible method of dealing with the difficulty of running high capacity LIBs stably under high voltage.

25 ENERGY STORAGE↗

Ternary Potassium‐Bismuth‐Telluride Intermetallic Support Promotes Electrochemical Stability in Potassium Metal Anodes

We employed accumulative roll bonding to fabricate self‐standing metallurgical composite of in situ formed alkaline potassium‐bismuth‐telluride intermetallic K 2 (Bi 2/6 Te 3/6 Vac 1/6 ) embedded in potassium metal. This newly discovered thermodynamically stable potassiophilic crystal, termed “KBT”, is fcc antifluorite with K 2 Te archetype. Symmetric cells achieve 880 h of cycling at 0.5 mA cm −2 and 0.5 mAh cm −2 . Potassium metal battery (KMB) with Prussian blue (PB) cathode in carbonate electrolyte retains 80% capacity after 200 cycles at 1C. In ether‐based electrolyte with organic cathode, it achieves 80% retention after 900 cycles at 2C. Combined synchrotron X‐ray nano‐tomography, cryogenic‐focused ion beam microscopy (Cryo‐FIB) and sputter‐down X‐ray photoelectron spectroscopy (XPS) demonstrate uniform electrodeposits, versus baseline of potassium filaments intermixed with pores and coarse SEI. Binary K 3 Bi‐K and K 2 Te‐K intermetallic supports also provide improved electrochemical performance, albeit to lesser extent. Multiscale simulation provides insight into role of support structure in adatom energetics, film nucleation, early‐stage SEI morphology and interfacial stability.

36 MATERIALS SCIENCE↗

Lithicone‐Protected Lithium Metal Anodes for Lithium Metal Batteries with Nickel‐Rich Cathode Materials

The high energy density advantage of lithium (Li) metal batteries (LMBs) makes them increasingly desirable; however, problems such as strong reactivity and dendrite growth of Li metal anode limit their practical uses. In this work, a novel Li‐containing glycerol (LiGL) or lithicone protection layer on a 50 μm thick Li metal anode is employed for improving the performance of LMBs. This LiGL layer was accurately deposited via a molecular layer deposition (MLD) process at 150 °C, using lithium tert‐butoxide and glycerol as precursors. The as‐formed LiGL coating layer is highly tunable in its thickness by simply adjusting MLD cycles and shows a good stability and outstanding ionic transport properties. The LiGL layer is found to effectively mitigate side reactions and enhance cycling stability in both symmetric cells and full cells. Specifically, the LMBs with LiGL@Li anode of 400 MLD cycles and LiNi 0.6 Mn 0.2 Co 0.2 O 2 cathode enable a capacity retention of ≈87%, much higher than ≈35% of the cells with bare Li after 200 cycles at a charge/discharge current density of 2.1 mA cm −2 . This work paves a feasible way for practical LMBs with improved capacity and stability through applying an innovative protection layer on Li metal anodes.

25 ENERGY STORAGE↗

Calendar life of lithium metal batteries: Accelerated aging and failure analysis

Lithium metal batteries (LMBs) are prime candidates for next-generation energy storage devices characterized by their remarkable energy storage capabilities. Despite the importance of understating the calendar aging impacts in LMBs, cycle life and calendar life have received inconsistent attention across various research and development stages. For acceptance into an application, especially electric vehicles, batteries are required to have sufficient calendar life to ensure performance over the life of vehicles which often experience extended periods of inactivity. In this study, an in-depth exploration into the calendar aging of LMB (Li/ Li[Ni 0.8 Mn 0.1 Co 0.1 ]O 2 in pouch cell format) is conducted. Specifically, the impact of calendar aging factors, state-of-charge (SOC), temperature, pressure, and operating conditions (open-circuit voltage, OCV and constant voltage, CV) on the surface morphology and thickness change rate in lithium metal anode is investigated. Notably, the results show that storing LMB pouch cells at an OCV, 80 % SOC, 25 °C, and 10 psi external pressure leads to a <1% reduction in capacity over 18 months. The results also suggest routes which can be utilized in the future for accelerated aging without altering the primary degradation modes. The results also show an accelerated calendar aging at high temperatures (45 °C), 100 % SOC, and CV suggesting they may serve as key accelerated aging methods for future studies. During calendar aging, pressure mitigates dendrite growth and extends calendar life. In conclusion, the insights from this study reinforce the viability of LMBs as a compelling solution for addressing increased energy storage needs in real-world applications.

25 ENERGY STORAGE↗

Hybrid polymer network cathode-enabled soluble-polysulfide-free lithium–sulfur batteries

Among the emerging 'beyond lithium-ion' technologies for maximized sustainability, lithium-sulfur (Li-S) is a favoured chemistry because of its exceptional energy density from the conversion of sulfur, an element in abundant supply. However, the dissolution of several intermediate polysulfides formed during conversion leads to rapid performance degradation over cycling. Here, in this study, we address this issue by sulfurizing a hybrid polymer network with polyphosphazene and carbon as a cathode for Li-S batteries. With rich sites to re-bond and adsorb dissociative sulfur species, this hybrid polymer network circumvents the formation of soluble polysulfides and enables a unique, reversible inserting conversion reaction. Thus, our cathode delivers both high capacity (~900 mAh g -1 cathode ) and excellent cycling stability in Li-S coin cells, with a pouch cell demonstration of projected energy density of ~300 Wh kg -1 and 84.9% capacity retention after 150 cycles. The strategy can be extended to other cost-effective, recyclable polymers, advancing sulfur-based batteries towards practical energy storage application.

25 ENERGY STORAGE↗

Unveiling Nickel Chemistry in Stabilizing High-Voltage Cobalt-Rich Cathodes for Lithium-Ion Batteries

We present a practical solution to increase the stability of 4.45 V LiCoO 2 via high-temperature Ni doping, without adding any extra synthesis step or cost. We identify how a putative uniform bulk doping with highly soluble elements can profoundly modify the surface chemistry and structural stability from systematic chemistry and microstructure analysis. This modification has an electronic origin, where surface-oxygen-loss induced Co reduction that favors tetrahedral site and causes damaging spinel phase formation is replaced by Ni reduction that favors octahedral site and creates a better cation-mixed structure. Furthermore, our findings point to many unknown surface effects on the electrochemical performance of battery electrode materials hidden behind extensively practiced bulk doping strategy. The new understanding of complex surface chemistry is expected to help develop higher-energy-density cathode materials for battery applications.

25 ENERGY STORAGE↗

Degradation Pathways of Cobalt–Free LiNiO 2 Cathode in Lithium Batteries

Electrode-electrolyte reactivity (EER) and particle cracking (PC) are considered two main causes of capacity fade in high-nickel layered oxide cathodes in lithium-based batteries. However, whether EER or PC is more critical remains debatable. Herein, the fundamental correlation between EER and PC is systematically investigated with LiNiO 2 (LNO), the ultimate cobalt-free lithium layered oxide cathode. Specifically, EER is found more critical than secondary particle cracking (SPC) in determining the cycling stability of LNO; EER leads to primary particle cracking, but mitigates SPC due to the inhibition of H2-H3 phase transformation. Two surface degradation pathways are identified for cycled LNO under low and high EERs. A common blocking surface reconstruction layer (SRL) containing electrochemically-inactive Ni 3 O 4 spinel and NiO rock-salt phases is formed on LNO in an electrolyte with a high EER; in contrast, an electrochemically-active SRL featuring regions of electron- and lithium-ion-conductive LiNi 2 O 4 spinel phase is formed on LNO in an electrolyte with a low EER. These findings unveil the intrinsic degradation pathways of LNO cathode and are foreseen to provide new insights into the development of lithium-based batteries with a minimized EER and a maximized service life.

25 ENERGY STORAGE↗

Dendrite–Free Potassium Metal Anodes in a Carbonate Electrolyte

Potassium (K) metal anodes suffer from a challenging problem of dendrite growth. In this study, it is demonstrated that a tailored current collector will stabilize the metal plating–stripping behavior even with a conventional KPF 6 –carbonate electrolyte. A 3D copper current collector is functionalized with partially reduced graphene oxide to create a potassiophilic surface, the electrode being denoted as rGO@3D–Cu. Potassiophilic versus potassiophobic experiments demonstrate that molten K fully wets rGO@3D–Cu after 6 s, but does not wet unfunctionalized 3D–Cu. Electrochemically, a unique synergy is achieved that is driven by interfacial tension and geometry: the adherent rGO underlayer promotes 2D layer–by–layer (Frank–van der Merwe) metal film growth at early stages of plating, while the tortuous 3D–Cu electrode reduces the current density and geometrically frustrates dendrites. The rGO@3D–Cu symmetric cells and half–cells achieve state–of–the–art plating and stripping performance. Here, the symmetric rGO@3D–Cu cells exhibit stable cycling at 0.1–2 mA cm –2 , while baseline Cu prematurely fails when the current reaches 0.5 mA cm –2 . The half–cells cells of rGO@3D–Cu (no K reservoir) are stable at 0.5 mA cm –2 for 10 000 min (100 cycles), and at 1 mA cm –2 for 5000 min. The baseline 3D–Cu, planar rGO@Cu, and planar Cu foil fails after 5110, 3012, and 1410 min, respectively.

25 ENERGY STORAGE↗

Unraveling the Stable Cathode Electrolyte Interface in all Solid‐State Thin‐Film Battery Operating at 5 V

Abstract Spinel‐type LiNi 0.5 Mn 1.5 O 4 (LNMO) is one of the most promising 5 V‐class cathode materials for Li‐ion batteries that can achieve high energy density and low production costs. However, in liquid electrolyte cells, the high voltage causes continuous cell degradation through the oxidative decomposition of carbonate‐based liquid electrolytes. In contrast, some solid‐state electrolytes have a wide electrochemical stability range and can withstand the required oxidative potential. In this work, a thin‐film battery consisting of an LNMO cathode with a solid lithium phosphorus oxynitride (LiPON) electrolyte is tested and their interface before and after cycling is characterized. With Li metal as the anode, this system can deliver stable performance for 600 cycles with an average Coulombic efficiency >99%. Neutron depth profiling indicates a slight overlithiated layer at the interface prior to cycling, a result that is consistent with the excess charge capacity measured during the first cycle. Cryogenic electron microscopy further reveals intimate contact between LNMO and LiPON without noticeable structure and chemical composition evolution after extended cycling, demonstrating the superior stability of LiPON against a high voltage cathode. Consequently, design guidelines are proposed for interface engineering that can accelerate the commercialization of a high voltage cell with solid or liquid electrolytes.

25 ENERGY STORAGE↗

Assessing the Intrinsic Roles of Key Dopant Elements in High–Nickel Layered Oxide Cathodes in Lithium–Based Batteries

A rational compositional design is critical for utilizing LiNiO 2 -based cathodes with Ni contents > 90% as promising next-generation cathode materials. Unfortunately, the lack of a fundamental understanding of the intrinsic roles of key elements, such as cobalt, manganese, and aluminum, makes the rational compositional design of high-Ni cathodes with a limited range of dopants (<10%) particularly challenging. Here, with 5% single-element doped cathodes, viz., LiNi 0.95 Co 0.05 O 2 , LiNi 0.95 Mn 0.05 O 2 , and LiNi 0.95 Al 0.05 O 2 , along with undoped LiNiO 2 (LNO), the influences of the dopants are systematically examined through a control of cutoff charge energy density and a common practice of cutoff charge voltage. Comprehensive investigations into the electrochemical properties, combined with in-depth analyses of the structural and interfasial stabilities and electrolyte decomposition pathways through advanced characterizations, unveil the following: i) the intrinsic role of dopants regulates the cathode energy density or state-of-charge and, more critically, the occurrence of H2–H3 phase transition, which essentially dictates cyclability; ii) undoped LNO can be stabilized well with the avoidance of H2–H3 phase transition; and iii) Co provides more merits overall with an optimized electrochemical operating condition. Finally, this work provides guidance for the compositional design of high-energy-density high-Ni cathodes and sheds light on the challenges of removing Co.

25 ENERGY STORAGE↗