Search NASA⌕ Search

SEARCH · Search NASA

Results for “DUCTILITY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,765 records · Page 98

The Temperature Effect on the Compressive Behavior of Closed-Cell Aluminum-Alloy Foams

In this research, the mechanical behavior of closed-cell aluminum (Al)-alloy foams was investigated at different temperatures in the range of 25-450 °C. The main mechanical properties of porous Al-alloy foams are affected by the testing temperature, and they decrease with the increase in the temperature during uniaxial compression. From both the constant/serrated character of stress–strain curves and macro/microstructural morphology of deformed cellular structure, it was found that Al foams present a transition temperature from brittle to ductile behavior around 192 °C. Due to the softening of the cellular structure at higher temperatures, linear correlations of the stress amplitude and that of the absorbed energy with the temperature were proposed. Also, it was observed that the presence of inherent defects like micropores in the foam cell walls induced further local stress concentration which weakens the cellular structure’s strength and crack propagation and cell-wall plastic deformation are the dominant collapse mechanisms. Finally, an energy absorption study was performed and an optimum temperature was proposed.

36 MATERIALS SCIENCE↗

Workability Limits of Magnesium Alloy AZ31B Subjected to Equal Channel Angular Pressing

Equal channel angular pressing (ECAP) is an important severe plastic deformation process to produce ultrafine grained microstructures in metals and alloys. Magnesium and its alloys generally possess poor workability at temperatures below 250 °C. This investigation examines the influence of different passes and processing routes of ECAP on improving the workability of Mg alloy AZ31B. ECAP was carried out for three passes using a die of angle 120° using processing routes Bc and C. The operating temperature was 523 K for the first pass and 423 K for the subsequent two passes. The resultant microstructure and mechanical properties were determined. Workability of the alloy at 423 K (150 °C) was determined using upsetting experiments on cylindrical specimens machined from the annealed and ECAPed samples. Workability limit diagrams have been constructed for the various processed conditions. The workability data generated were also analyzed using five different workability criteria (also referred to as ductile fracture models) and the material constants for these five models were evaluated. Specimens processed by two passes through route C (pass 2C) exhibits better workability compared to other passes since the workability limit line after this pass shows maximum safe working area and lies above the other workability lines. Among the five different workability criteria investigated, the Freudenthal workability criterion is more suitable for prediction of failure in this alloy.

36 MATERIALS SCIENCE↗

Effect of Al-Si Coating on Weld Microstructure and Properties of 22MnB5 Steel Joints for Hot Stamping

22MnB5 hot stamping steels are gradually being used in tailor-welded blank applications. In this experiment, 1-mm-thick Al-Si coated and de-coated 22MnB5 steels were laser-welded and then hot-stamped. The chemical compositions, solidification process, microstructure and mechanical properties were investigated to reveal the effect of Al-Si coating and heat treatment. In the welded condition, the coated joints had an Al content of approximately 2.5 wt.% in the fusion zone and the de-coated joints had 0.5 wt.% Al. The aluminum promoted the δ-ferrite formation as the skeletal structure during solidification. In the high-aluminum weld, the microstructure consisted of martensite and long and band-like δ-ferrite. Meanwhile, the low-aluminum weld was full of lath martensite. After the hot stamping process, the δ-ferrite fraction increased from 10 to 24% in the coated joints and the lath martensite became finer in the de-coated joints. The tensile strengths of the coated joints or de-coated joints were similar to that before hot stamping, but the strength of the coated joints was reduced heavily after hot stamping compared to the de-coated joints and base material. The effect of δ-ferrite on the tensile properties became stronger when the fusion zone was soft and deformed first in the hot-stamped specimens. The coated weld showed a brittle fracture surface with many cleavage planes, and the de-coated weld showed a ductile fracture surface with many dimples in hot-stamped conditions.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Stainless Steel/Brass Joints Brazed by Sn-Electroplated Ag Brazing Filler Metals

To develop a high-Sn-content AgCuZnSn brazing filler metal, the BAg50CuZn was used as the base filler metal and a Sn layer was electroplated upon it. Then, the 304 stainless steel and the H62 brass were induction-brazed with the Sn-plated brazing filler metals. The microstructures of the joints were examined with an optical microscope, a scanning electron microscope and an x-ray diffractometer. The corresponding mechanical properties were obtained with a universal tensile testing machine. The results indicated that the induction brazed joints consisted of the Ag phase, the Cu phase and the CuZn phase. When the content of Sn in the Sn-plated Ag brazing filler metal was 6.0 or 7.2 wt.%, the Cu{sub 5}Zn{sub 8}, the Cu{sub 41}Sn{sub 11} and the Ag{sub 3}Sn phases appeared in the brazed joint. The tensile strength of the joints brazed with the Sn-plated filler metal was higher compared to the joints with the base filler metal. When the content of Sn was 6.0 wt.%, the highest tensile strength of the joint reached to 395 MPa. The joint fractures presented a brittle mode, mixed with a low amount of ductile fracture, when the content of Sn exceeded 6.0 wt.%.

36 MATERIALS SCIENCE↗

Investigation of Mechanical and Electromagnetic Interference Shielding Properties of Nickel–CFRP Textile Composites

The most common materials used for electromagnetic interference shielding are metals and their alloys. However, those materials are heavy and highly reflective. In order to eliminate or reduce the intensity of wave radiation in their working environment, lightweight materials that have interference shielding properties are needed. In this paper, nickel wire mesh yarns (warps) were woven into carbon fibers-reinforced plastic yarns (wefts) to produce metal–carbon textile composite materials. The plain weave and 2/2 twill weave techniques were used, and the woven fabrics were laminated to manufacture experimental test samples. The nickel, which has high magnetic permeability and good electric conductivity, and carbon fibers, which have good electrical, thermal and mechanical properties, were used together to achieve the desired properties. The shielding effectiveness of each sample was investigated using a network analyzer connected with coaxial transmission line test in accordance with ASTM 4935-99 standard, with the frequencies ranging from 500 MHz to 1.5 GHz. Here, the plain weave structure showed higher shielding effectiveness than twill weave. The absorption losses for both materials were relatively greater than reflection losses. In reference to the orientation of wire mesh yarns about the loading axis, the tensile strengths in the transversal direction were 19.04 and 16.34% higher than the tensile strengths in longitudinal direction for plain weave and twill weave, respectively. The fractography analysis with SEM showed a ductile fracture of wire mesh and brittle fracture of epoxy matrix and carbon fibers.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment on the Properties of CoCrMo Alloy Manufactured by Selective Laser Melting

To obtain medical implants with better mechanical properties, it is necessary to conduct studies on the heat treatment process of the selective laser melting (SLM) manufacturing parts. The differential scanning calorimetry method was used to study the heat treatment process of the phase transition of SLM CoCrMo alloy parts. The tensile properties were tested with a tensile test machine, the quantity of carbide precipitated after heat treatment was measured by energy-dispersive x-ray spectroscopy, and the tensile fracture morphology of the parts was investigated using SEM. The obtained results were: Mechanical properties in terms of elongation and tensile strength of CoCrMo alloy manufactured by SLM that had been heat-treated at 1200 °C for 2 h followed by cooling with water were not only higher than the national standard but also higher than the experimental results of the same batch of castings. The mechanism of fracture of parts manufactured by SLM without heat treatment was brittle fracture, whereas parts which had been heat-treated at 1200 °C for 2 h combined with water cooling and at 1200 °C for 1 h with furnace cooling suffered ductile fracture. This study provides the basis for defining the applications for which CoCrMo alloys manufactured by SLM are suitable within the field of medical implants.

36 MATERIALS SCIENCE↗

Analysis of Microstructure and Sliding Wear Behavior of Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} High-Entropy Alloy

Α Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} high-entropy alloy (HEA) of the well-known family of CoCrFeNiTi has been designed using empirical parameters. The aim of this design was the production of a HEA with fcc structure that gives ductile behavior and also high strength because of the solid solution effect. The VEC calculations (8.1) supported the fcc structure while the δ factor calculations (4.97) not being out of the limit values, advised a significant lattice distortion. From the other hand, the ΔΗ{sub mix} calculations (− 9.64 kJ/mol) gave strong indications that no intermetallic would be formed. In order to investigate its potential application, the Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} HEA was prepared by vacuum arc melting and a primary assessment of its surface degradation response was conducted by means of sliding wear testing using different counterbody systems for a total sliding distance of 1000 m. An effort to correlate the alloy’s wear response with the microstructural characteristics was attempted. Finally, the wear behavior of the Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} HEA was compared with that of two commercially used wear-resistant alloys. The results obtained provided some first signs of the high-entropy alloys’ better wear performance when tested under sliding conditions against a steel ball.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Three-Layer TIG-Welded 2219 Aluminum Alloys with Dissimilar Heat Treatments

2219-C10S and 2219-CYS aluminum alloys are 2219 aluminum alloys with different heat treatment processes, and they have been widely used in the aerospace industry. In the present study, 2219-C10S and 2219-CYS aluminum alloys were butt-welded by three-layer tungsten inert gas arc welding (with the welding center of the third layer shifted toward the CYS side), and the microstructure characteristics and mechanical properties of the welded joint were investigated. The lamellar θ′ phases, the bulk or rod θ phases, and the coarse rod-shaped or pancake-shaped Al-Cu-Fe-Mn phases coexisted in the two aluminum alloys. The Cu content of the α-Al matrix and the distribution of eutectic structures of different welding layers in the weld zone (WZ) were varied, implying that the segregation degrees of the Cu element were different due to the different welding thermal cycles in different welding layers. The microhardness values of the CYS side were much higher than those of the C10S side in each region on both sides of the joint. The tensile test deformation was concentrated mainly in the regions of WZ and the over aged zone (OAZ), where the microhardness values were relatively low. The main deformation concentrated region was transferred from the CYS side to the C10S side with the increase in the tensile load during the tensile test. The fracture behavior of the tensile test showed that the macroscopic crack initiated near the front weld toe had gone through the crack blunt region, the shear fracture region of the partially melted zone (PMZ), and the shear fracture region of OAZ. Meanwhile, the fracture characteristics gradually evolved from brittle to ductile. The concentrated stress and the dense eutectic structure in the region near the front weld toe of the C10S side contributed to the fracture of the joint. The shift of the welding center of the third layer to the CYS side resulted in two effects: (i) the microhardness values from the middle layer to the top layer in the PMZ of the CYS side were the most significantly increased and (ii) the distance between the front weld toe and the fusion line of the CYS side was significantly larger.

36 MATERIALS SCIENCE↗

Effect of Strengthening Mechanism on Strain-Rate Related Tensile Properties of Low-Carbon Sheet Steels for Automotive Application

In order to ensure crash resistance of the steels used in automotive components, the ensile deformation behavior needs to be studied and predicted not only under quasi-static condition, but also under dynamic loading rates. In the present study, tensile tests have been performed on four different automobile grade sheet steels, namely interstitial free steel, dual-phase 600 and 800, and a carbon manganese steel over the strain rate regime of 0.001-800/s. Apart from the variation in strength (which always increased with strain rate), the effect of strengthening mechanism on strain rate sensitivity and strain hardening behavior has been evaluated. Strain rate sensitivity was found to increase at high-strain rate regime for all the steels. Contribution of solid solution hardening on strain rate sensitivity at lower plastic strains was found to be higher compared to dislocation strengthening and second-phase hardening. However, precipitation hardening coupled with solid solution hardening produced the highest strain rate sensitivity, in C-Mn-440 steel at high strain rates. Different strain-rate-sensitive models which take into account the change in yield stress and strain hardening behavior with strain rate for ductile materials were used to predict the flow behavior of these sheet steels at strain rates up to 800/s.

36 MATERIALS SCIENCE↗

Investigation of the Tribological Properties of AlxSi-1.2Fe(Mn) (x = 5-13 wt.%) Alloys

The effect of Fe-impurity and Mn modification on the sliding wear behavior of Al-xSi-1.2Fe(Mn) (x = 5-13 wt.%) alloys was investigated in dry sliding against AISI 52100 steel. According to the results, in the Si range of 5-9 wt.%, Fe-impurity promotes the formation of finely distributed β-Al{sub 5}FeSi intermetallics in the matrix increasing its hardness and potential to support the tribolayer leading to the improved wear characteristics. The presence of Fe in the composition of Al-(9-13)Si alloys, however, leads to the formation of primary β-platelets that their sizes and volume fractions increase with Si concentration. The formation of primary compounds increases the hardness, but makes the alloys less ductile and more vulnerable to microcracking and wear. Manganese modification converts the β-Fe platelets to the α-Al{sub 15}(Fe,Mn){sub 3}Si{sub 2} compounds with different morphologies. The substitution of fine β-platelets by α-Chinese scripts in Al-(5-9)Si-1.2FeMn alloys reduces the wear resistance, but the formation of primary α-compounds with star-like or polyhedral morphologies in Al-(9-13)Si-1.2FeMn alloys improves their wear characteristics. Moreover, it was found that the formation of Fe(Mn)-rich compounds affects the friction coefficient which is likely due to the fracture of particles in the subsurface region, their interaction with contacting surfaces, and their effect on the stability of the tribolayer.

36 MATERIALS SCIENCE↗

Uniaxial Ratcheting Behavior of Dual-Phase Steel Sheet

Uniaxial ratcheting behavior of an automotive-grade dual-phase steel sheet of 1.6 mm thickness has been investigated through engineering stress-controlled asymmetric cyclic loading experiments in the elastoplastic regime at ambient temperature (~ 28°C). Experiments have been performed keeping mean stress, stress amplitude or maximum stress constant. The effect of stress combinations on ratcheting deformation has been rationalized in terms of plastic strain amplitudes, both in loading and in unloading directions. It is found that for all stress combinations the steady-state ratcheting rate follows a perfect power relationship. Scanning electron fractography reveals that failure under asymmetric cyclic loading conditions occurs in a ductile manner through the formation of voids as it happens under tensile loading.

36 MATERIALS SCIENCE↗

Notch Sensitivity and Failure Behavior of TiAl and K418 Alloys

The notch sensitivity of tensile specimens of TiAl and K418 alloys has been investigated, and the notch strength has been quantitatively analyzed. The fracture surface of the specimens has also been observed and analyzed by scanning electron microscopy (JEOL-6700F). By comparing notch rod tensile specimens and special notch rod tensile specimens, it was found that the basic nature, fracture driving force, and fracture criteria of the brittle TiAl alloy and the ductile K418 alloy are different. The final fracture of the K418 alloy is controlled by strain and not by stress, and the specimens do not exhibit notch sensitivity. However, the final fracture of the TiAl alloy is controlled by stress, and the specimens exhibit small notch sensitivity. For the special notch rod tensile specimens, the K418 specimens do not exhibit notch sensitivity. However, for the TiAl alloy, when the notch depth reaches 10% of the specimen diameter, the tensile strength decreases, and when the notch depth reaches 20% of the specimen diameters, the tensile strength sharply decreases.

36 MATERIALS SCIENCE↗

Cryorolling-Induced Texture, Mechanical Properties and Fracture Behavior of Al-Mg-Si Alloys During Cold Deformation

This study investigated the texture, mechanical properties, and fracture behavior during cold working of cryorolled (CR) Al-Mg-Si alloys. An x-ray texture goniometer was used to examine the crystallographic texture, and tensile tests were performed to understand the deformation behavior in more detail. SEM/EBSD/TEM was used to observe the microstructures and fracture morphology of the alloy during cryorolling. The microstructures indicated that a large number of ultrafine grains and dislocations formed after cryorolled. The recrystallization was prohibited due to low temperature during deformation. The ultrafine grains and dislocation strength improved the tensile strength from 279.38 MPa for the room-rolled alloy to 313.98 MPa for the cryorolled alloy; better plasticity (4.6%) was observed in the CR sheet. Ductile and intergranular fractures were observed in the CR sheet deformation from 20 to 90%.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Rapidly Cooled Friction Stir Welded Ti-6Al-4V Alloys

Two mm-thick Ti-6Al-4V alloy plates were friction stir butt welded under natural- and rapid-cooling conditions. The microstructures and mechanical properties of joints were investigated and compared. The rapid cooling via spraying cooling liquid nitrogen on the plate top surface was beneficial to obtaining a narrower cross section and finer and more uniform grains in the stir zone than those obtained by natural cooling. Joint tensile strength of 1021 MPa and elongation of 1.88% under the rapid-cooling condition respectively reached 102.7 and 150.4% of those under the natural-cooling condition, respectively. The uniform-and-compact equiaxed grains led to equiaxed dimples on the fracture surface, which demonstrated a ductile fracture of the welding joints.

36 MATERIALS SCIENCE↗

The Effect of Heat Treatment Process Parameters on Mechanical Properties, Precipitation, Fatigue Life, and Fracture Mode of an Austenitic Mn Hadfield Steel

In this study, the effect of cooling rate after heat treatment on mechanical properties, fatigue life, precipitation and fracture mode of an austenitic Mn Hadfield steel was investigated. Cast samples of the Hadfield steel were heat treated at 1100 C for 2 h. The samples were subsequently quenched in pure water and also in 3 wt.% NaCl salt bath. Optical microscope (OM) and scanning electron microscope (SEM) were used to analyze microstructure and fracture surfaces. Transmission electron microscope (TEM) was used to assess the precipitates. X-ray diffraction (XRD) was used to determine the phases formed. Mechanical properties and fatigue life were determined by uniaxial tensile test, bending fatigue and hardness measurements. Results showed that the sample quenched in salt bath had lower Mn{sub 3}C precipitates, hardness, yield and tensile strengths. Instead, this situation resulted in a more ductile fracture mode and higher formability. Finally, the fatigue life of the sample quenched in salt bath was longer than the one quenched in pure water.

36 MATERIALS SCIENCE↗

Enhanced Strength of 304 SS-Ti6Al4V Laser-Welded Joints Containing Composite Interlayers

This paper investigates the microstructural characterization of the fracture propagation edge during laser beam welding of Ti6Al4V and 304 stainless steel using Cu, V, and Ni interlayers as a single Cu interlayer and composite interlayer structures with different Cu interlayer thicknesses. This study attempts to increase the Ti-SS joint strength through the use of the composite interlayers. X-ray diffraction characterization based on a 0.5-mm-thick Cu interlayer showed that the SS/Cu/Ti joint contained considerable brittle IMCs; however, the fracture surface of the SS/Cu-V/Ti composite interlayer sample did not contain any Fe-Ti IMCs or Cr{sub 2}Ti. EBSD observation indicated that the crack propagated transgranularly from solidified CuTi in the interdendritic regions of the FeTi compounds in the composite interlayer sample; however, the crack propagated intergranularly along Fe{sub 2}Ti grain boundaries in the single interlayer sample. The investigation based on a 1-mm-thick Cu interlayer showed that the SS/Ni-Cu1/Ti sample was stronger than the SS/Cu1/Ti sample due to a lack of CuTi at 3.5 kW. The tensile strength of the SS/Cu1-V/Ti joint was greater than that of the SS/Ni-Cu1/Ti joint due to the formation of ductile NiTi instead of brittle NiTi{sub 2}. The microstructures of the fracture edges after tensile testing illustrated that the eutectic CuTi + CuTi{sub 2} fractured at the SS/Cu1/Ti joint after tensile testing, while CuTi{sub 2} and eutectoid αTi + CuTi{sub 2} compounds fractured during the tensile experiment at the SS/Ni-Cu1/Ti and SS/Cu1-V/Ti joints, respectively. Investigations based on both the 0.5- and 1-mm-thick Cu interlayers showed that the tensile strength and elongation of the composite interlayer joints at a laser power of 3.5 kW were greater than those of the single interlayer joints.

36 MATERIALS SCIENCE↗

Fracture Analysis of ARB-Processed CP-Ti Sheets Under Unidirectional Tensile Loading

The fracture behavior of commercially pure titanium (CP-Ti) processed by accumulative roll bonding (ARB) was investigated in this study. Monolithic and Ti-SiC composite samples were first produced by ARB process and then subjected to uniaxial tensile testing at room temperature. Two different ductile fracture mechanisms including shear dimple rupture and equiaxed dimple rupture were observed in the initial and final ARB cycles, respectively. The difference in the rupture mechanism was attributed to different stress states at the crack tip and different densities of metallurgical defects. A non-uniform distribution of dimple size was obtained for fracture surfaces of the samples processed by a low number of ARB cycles. This was attributed to the heterogeneity of microstructure in the primary ARB cycles. The fracture surface of the samples processed by high ARB cycles represented more uniform dimples. This was attributed to more homogenous microstructure in the final cycles. Moreover, SiC particles showed a major role in fracture of samples, so that they affected the size and depth of the dimples, as well as the number of ARB cycles in which the transmission of the fracture mechanism occurred.

36 MATERIALS SCIENCE↗

Laser Additive Manufacturing of (Ti-6Al-4V)/10 wt.% Ag Composite Using Spherical Powders to Reduce Wear and Friction

In order to extend the service lifetime of Ti-6Al-4V-based components, friction and wear behaviors of Ti-6Al-4V alloys needed to be further improved. Laser additive manufacturing with a moving laser beam was used to prepare (Ti-6Al-4V)/10 wt.% Ag samples, on a three-dimensional RC-SLM400 printer with laser powers of 2-10 kW. (Ti-6Al-4V)/10 wt.% Ag samples were successfully printed using spherical powders prepared by gas atomization process (SPGAP) and combustion reaction (SP-CR). The tribological properties of the as-prepared samples sliding against Si{sub 3}N{sub 4} balls were examined using a ball-on-disk tribometer. The results showed that the tribological behavior of (Ti-6Al-4V)/10 wt.% Ag printed by SP-CR was better than that of the sample printed by SPGAP. The low friction and reduced wear were mainly attributed to the formation of the lubrication layer containing large amounts of silver, which can exhibit an excellent deformation and plastic ductility. It effectively reduced the friction resistance and material loss and provided the good lubrication for 0-80 min, resulting in low friction and reduced wear of the samples prepared by SP-CR.

36 MATERIALS SCIENCE↗