Effect of Annealing on the Microstructure and Properties of Electron Beam Welded 4J34 Kovar Alloy

Electron beam welding of 4J34 Kovar alloy was conducted, and the microstructure and mechanical properties of the joints in as-welded and postweld annealing treatment (PWAT) states were investigated. The martensitic transformation occurred and led to the generation of α lath martensite due to the rapid cooling in the as-welded condition. After annealing treatment, part of the α martensite transformed to γ austenite and subsequently developed the bulk γ phase and α/γ lamellar microstructures in the fusion zone (FZ) of the postwelded joint. Grains in the heat-affected zone (HAZ) clearly developed and penetrated into the FZ, causing the disappearance of the fusion line between the FZ and the HAZ. All the joints in both the as-welded and PWAT conditions exhibited ductile fracture. The maximum tensile strength of 505 MPa was obtained in the as-welded joint with the welding speed of 150 mm/min. The linear expansion coefficients of the joint and base metal decreased with the increase in temperature. However, the decreasing rate of PWAT joints was lower than that of the as-welded joints.

36 MATERIALS SCIENCE↗

Microstructural Properties of Heat-Treated LENS In Situ Additively Manufactured Titanium Aluminide

This study reports on the microstructure, phase identification and hardness property of the LENS-manufactured binary Ti-Al alloy which was achieved via laser in situ alloying. The in situ alloying method, using laser beam as an energy source, indicated that it is possible to achieve a binary gamma phase microstructure from elemental powders of Ti and Al. The as-produced sample, however, was characterized of having different microstructure at the top, middle and bottom regions. The middle and top layers had similar hardness which was lower than that of the bottom region. The as heat-treated sample was characterized of lamellar grain microstructure at the top and just grains at the bottom and the middle. The observed grains were different in size, phase and hardness. This study indicated that in addition to the pores and the precipitation of α{sub 2} phase or aluminum segregation on the grain boundary veins intermetallics lead to severe cracking. Overall, the hardness values of the as-produced and heat-treated samples were similar, and due to extensive cracking, it was inferred that both samples will lack ductility.

36 MATERIALS SCIENCE↗

Role of Si in the Surface Damage Mechanism of RB-SiC/Si Under Mechanical Loading

Indentation test (Nanoindentation and Vickers indentation), diamond scratching and high spindle speed grinding are conducted to investigate the role of silicon (Si) in the surface damage behavior of reaction-bonded SiC/Si composites (RB-SiC/Si). Even though the addition of Si contributes to densifying the bulk materials and improving the toughness, the indentation and diamond scratching results firstly indicate that the cracks initiate at the SiC/Si interfaces due to the non-uniform deformation caused by the existence of Si, and the phase transformation of Si also leads to the pop-out effect during the nanoindentation and the diamond scratching test. The ground surface of RB-SiC/Si is characterized by scratching grooves and brittle fracture, indicating the ductile material removal mode and brittle material removal mode for RB-SiC/Si, respectively, and the surface reliefs form on the ground surface due to the different hardness between Si and SiC phases. Moreover, the phase transformation of Si contributes to the easy fracture of phase boundaries under the mechanical loading, and the accompanied volume change also results in the dislodgement of hard particles and the generation of surface burs on the ground surface.

36 MATERIALS SCIENCE↗

Nonuniformity in Mechanical Properties of Linear Friction Welded Mild Steel Joint

Mild steel was successfully joined by linear friction welding. Grain size at peripheral region was coarser than that at the other zones of the weld interface, which had no significant effect on microhardness. The local tensile properties were considerably decreased when oxides or lack of bonding appeared at the interface. Ductile fracture dominated the fracture mode for all joints. Variation in local tensile properties could be relieved under a medium friction pressure, a relatively high amplitude with a sufficient friction time. It was attributed to the facts that plastic metal layer of joint became uniform to some extent and interfacial defects were eliminated. The standard deviation of plastic metal layer thickness (χ{sub p}) could be used to describe the combined effects of welding parameters on joint integral performance. It was found that the standard deviation of plastic metal layer thickness showed a strong inverse correlation with the joint integral performance. Well-formed and defect-free joints exhibiting 90% of the base metal tensile strength could be produced when processing at a frequency of 20 Hz with a friction pressure of 103 MPa or 155 MPa, an amplitude of 2.5 mm and a friction time of at least 4 s.

36 MATERIALS SCIENCE↗

Sulfide Stress Corrosion Cracking Behavior of G105 and S135 High-Strength Drill Pipe Steels in H{sub 2}S Environment

Slow strain rate testing was employed to investigate the sulfide stress corrosion cracking (SSCC) behavior of low-carbon high-strength drill pipe steels (G105 and S135) in the simulated drilling environment containing H{sub 2}S. Results reveal that both G105 and S135 steels have a high SSCC susceptibility in the simulated drilling environment containing H{sub 2}S. In the range of experimental slow strain rate, the SSCC sensitivity of drill pipe steel increases with the decrease in slow strain rate, and the ductility and fracture properties of drill pipe steels also decrease obviously. With the increase in the steel strength, the SSCC sensitivity of the drill pipe steel increases, and the S135 drill pipe steel has higher SSCC sensitivity than G105. There is no obvious plastic deformation on the fracture surface of G105 and S135 steels in H{sub 2}S solution. The cracks of fracture sprout on the surface of the specimen, the instantaneous fracture zone is in the middle, and the fracture can be divided into the cracking and the final fracture zone. The SSCC mechanisms of two drill pipe steels are hydrogen embrittlement. The hydrogen enters the steel and reduces the binding force of the iron atom, resulting in cleavage fracture.

36 MATERIALS SCIENCE↗

Thermally Assisted Adhesion Enhancement in High-Phosphorous Electroless Nickel Plating

High-phosphorus electroless nickel is a widely recognized protective plating for oilfield metallic parts subject to corrosion and wear. In the present investigation, thermally activated diffusion treatment was applied to enhance electroless nickel (10-13 wt.% P) plating adhesion on low-alloy steel (UNS G41400) and reduce the risks of spalling. High-phosphorus electroless nickel (10-13 wt.% P) was applied to a variety of UNS G41400 low-alloy steel test samples as per ASTM B733 that were subsequently heat-treated in air for four distinct temperatures, i.e., 510, 540, 570, and 600 °C for 2-10 h. Following post-plating diffusion heat treatments, the initial amorphous electroless nickel was replaced by Ni{sub 3}P precipitates dispersed in a crystalline nickel-rich phase, with an average hardness improvement from 500 to 700 HK. An increased atomic interdiffusion (from 400 to 3.5 µm) was observed at plating–substrate interfaces, resulting in enhanced adhesion and reduced susceptibility toward spalling. This improvement in adhesion was measured repeatedly through post-bending crack analyses and subsequently validated by interface microindentation. Along with diffusion across plating–substrate interface, nickel oxide formation on surface by oxidation was observed to grow at quasi-parabolic rate with no detrimental impact on spalling. In all cases, plating adhesion was improved by heat treatments due to the diffusion-controlled formation of a seemingly ductile layer.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of a Multiphase FeCrCuMnNi High-Entropy Alloy

A FeCrCuMnNi high-entropy alloy was produced using vacuum induction melting, starting from high-purity raw materials. The microstructure and mechanical properties of the as-cast FeCrCuMnNi alloy were studied, considering x-ray diffraction (XRD), scanning electron microscopy, and hardness and tensile tests. XRD results revealed the existence of two FCC phases and one BCC phase. Microstructural evaluation illustrated that the as-cast alloy has a typical cast dendritic structure, where dendrite regions (BCC) were enriched in Cr and Fe. Interdendritic regions were saturated with Cu and Ni and revealed G/B(T) {110} 〈111〉 and Brass {110} 〈112〉 as the major texture components. The produced alloy revealed an excellent compromise in mechanical properties due to the mixture of solid solution phases with different structures: 300 HV hardness, 950 MPa ultimate tensile strength and 14% elongation. Microhardness test results also revealed that the BCC phase was the hardest phase. The fracture surface evidenced a typical ductile failure. Furthermore, heat treatment results revealed that phase composition remained stable after annealing up to 650 °C. Phase transformation occurred at higher temperatures in order to form more stable phases; therefore, FCC2 phase grew at the expense of the BCC phase.

36 MATERIALS SCIENCE↗

The Effects of Sc Addition on the Microstructure and Mechanical Properties of Be-Al Alloy Fabricated by Induction Melting

This study investigated the alloying effects of 0.4 wt.% Sc on the microstructure, mechanical properties, and fracture behavior of a cast Be-Al alloy prepared by vacuum induction melting. The micromechanics of Sc-containing secondary-phase particles (SPs) were characterized by nanoindentation, and the fracture behavior of the alloy was investigated via tensile fractography and optical metallography. The addition of 0.4 wt.% Sc significantly modified the alloy microstructure by decreasing the secondary dendritic arm spacing (SDAS), weakening the dendritic structure of Be, and producing an equiaxed/cellular alloy microstructure with refined Be grains. Sc alloying increased the Vickers hardness by 36%, elastic modulus by 28%, yield strength by 35%, ultimate strength by 52%, but decreased the elongation from 3.6 to 2.9%. Sc-containing SPs had a higher elastic modulus, yield strength, microhardness, and a lower plasticity index than the Be and Al matrices, resulting in interface separation during the fracture process. SPs located at the Be/Al interfaces did not act as microcrack sources for the matrices, whereas highly faceted SPs within the Be grains induced microcrack formation and decreased the elongation. The failure mode of the cast Be-Al-0.4Sc alloy still involved the brittle cleavage failure of Be regions and ductile dimple failure of Al regions, which was not the case with the cast Be-Al alloy.

36 MATERIALS SCIENCE↗

Experimental Research on Tensile Behavior of Advanced High-Strength Steel DP600 at High Strain Rate

We conducted a series of experimental investigations on the mechanical properties of DP600 dual-phase steel under strain rates from 0.001 to 3000 s{sup −1} at room temperature. A split Hopkinson tensile bar was used to capture a high strain rate response. A comparison of the quasi-static and dynamic experiment results showed that the yield strength and ultimate tensile strength increased significantly under dynamic conditions. Fractographs were analyzed by scanning electron microscopy, which indicated a better ductility at a high strain rate. Based on the experimental results, the Johnson–Cook constitutive model was applied to describe the tensile deformation behavior under various strain rates. A reasonable agreement was observed between the experimental data and the Johnson–Cook model. A metallographic analysis of tensile specimens showed that the average ferritic grain size of the fractured specimens at a high strain rate was smaller than that of the fractured specimens under quasi-static conditions. Ferritic grain refinement proved that high-speed forming could enhance the forming ability of the DP600 steel.

36 MATERIALS SCIENCE↗

Effect of Annealing on the Impact Resistance and Fracture Mechanism of PNC-60 Sinters After Cold Plastic Deformation

Compaction of sintered metal powders by free upsetting at room temperature dangerously reduces their plastic properties, particularly the fracture toughness. The reason for the occurrence of two unfavorable phenomena accompanying this deformation route is sought. The first phenomenon depends on the initial porosity of the preform and the amount of cold work resulting in the destruction of bonds and violation of continuity between sintered powder particles. The second phenomenon is the deformation of the metal matrix, which reduces the plasticity of the sintered product. To correctly assess the effect of changes occurring in the matrix as a result of deformation, it is necessary to use the properly defined sintered matrix hardening parameter discussed in this study. The adverse effects of cold forming can be eliminated by annealing the deformed sinters at a temperature below the sintering point and above the recrystallization temperature. The annealing temperature causes favorable changes in the structure and increases the impact resistance of the deformed sinters depending on the degree of deformation of the sintered matrix and the initial porosity of the preform. Annealing at a properly selected temperature restores the ductility of the metal matrix and improves the integrity of the sintered material impaired by the effect of deformation. Annealing also causes favorable changes in the porosity morphology, removing defects in the form of gaps and resulting in the spheroidization of voids. With an appropriately selected initial porosity and degree of deformation, subsequent annealing of sinters compacted by free cold upsetting provides products with strength properties comparable to sinters with the same density and subjected to single compaction and sintering but with considerably higher fracture toughness.

36 MATERIALS SCIENCE↗

On Mechanical Properties of New Railway Wheel Steels for Desert Environments and Sand Caused Wheel Damage Mechanisms

Worn railway wheels after service in the desert were investigated by means of failure analysis, hardness measurements, tensile tests, fracture toughness tests and low-cycle fatigue (LCF) tests. The results complete both previous small-scale laboratory experiments and FEM simulations performed by the authors on widely used steels and new steel grades allowing to better understand the main damage mechanisms due to the sand. These new steel grades were developed for forged-rolled solid wheels in alternative to AAR Class B/C/D steel grades and were designed to ensure high resistance to wear and rolling contact fatigue in the presence of sand, debris or gravel on the rails. This paper covers the in-depth mechanical characterization of wheels made of the new steels. Hardness measurements, tensile tests, fracture toughness tests and LCF tests were carried out. The results are compared with AAR Class B/C/D steels showing an excellent combination of fracture toughness, cyclic yield strength and ductility.

36 MATERIALS SCIENCE↗

Tailoring Microstructure and Properties of a Superelastic Ti–Ta Alloy by Incorporating Spark Plasma Sintering with Thermomechanical Processing

A powder metallurgy Ti–35 at.% Ta alloy was produced using a spark plasma sintering process. The sintered alloy exhibited Ta-rich regions at a sintering temperature of 1100 °C. Complete diffusion of elemental powders was achieved via homogenization heat treatment at 1500 °C for 12 h, but the ductility declined drastically. The brittle behavior of the homogenized sample was due to the high-oxygen content, continuous grain boundary α-phase and high-angle grain boundaries. Excellent mechanical properties were achieved when hot forging was used along with preheating the homogenized specimen at 1100 °C. The mechanisms underlying this phenomenon were suppression of the solid grain boundary α-phase, high fraction of low-angle grain boundaries and dynamic recrystallization. Tensile strength improved to the maximum value of 868 MPa. The strain recovery ratio increased to 90% in the first cycle during a cyclic loading–unloading test. Incomplete strain recovery of the first cycle was due to the presence of the martensite phase (α″).

36 MATERIALS SCIENCE↗

Effect of Dual-Phase Heat Treatment on Microstructure and Mechanical Properties of S135 High-Strength Drill Pipe Steel

Effect of dual-phase heat treatment (DPHT) on microstructure and mechanical properties of S135 high-strength drill pipe steel was studied by means of optical microscope, scanning electron microscope and mechanical property testing. The results show that the ferrite–martensite dual-phase microstructures were obtained at 760-800 °C. With increase in DPHT temperature, the volume fraction of martensite increases and the ferrite decreases. When the DPHT temperature is low, martensite is distributed as an island on the ferrite matrix, and ferrite is distributed as an island on the martensite matrix when the DPHT temperature is high. The hardness and strength of the steel increase, the plasticity and toughness decrease, the steel changes from ductile fracture to brittle fracture and the micro-fracture morphology changes from dimple to cleavage with increase in DPHT temperature. The strain hardening exponent of the as-received steel shows one ‘n’ value, but exhibits two ‘n’ values after DPHT. When the DPHT temperature is 750 °C, the relative content of martensite in the duplex structure is 15-20%, and the impact energy of the steel is similar to that of the as-received S135 drill pipe steel, and the strength is increased by about 15%. Micropores and micro-cracks on the subsurface of tensile fracture surface are mainly formed at the martensite/ferrite phase boundary or in the martensite slit.

36 MATERIALS SCIENCE↗

Microstructure Characteristics and Comparative Analysis of Constitutive Models for Flow Stress Prediction of Inconel 718 Alloy

An accurate constitutive model is essential for analyzing deformation behavior of material and reliable numerical simulations in metal forming processes. In this study, hot tensile tests of Inconel 718 alloy have been conducted over a wide range of temperatures (300-973 K at an interval of 100 K), strains (0.01-0.3 at an interval of 0.01) and quasi-static strain rates (0.0001, 0.001, 0.01 s{sup −1}). Flow stress behavior is significantly affected by test temperatures and strain rates. Microstructure characteristics of deformed test specimens have been examined using scanning electron microscope and electron backscatter diffraction (EBSD). The fractography study revealed that fracture is mix-mode type, i.e., ductile and brittle. Subsequently, EBSD analysis shown that dynamic recrystallization mechanism is more pronounced at a higher temperature. Furthermore, four constitutive models, namely modified Cowper–Symonds, modified Johnson Cook, modified Zerillie-Armstrong and integrated Johnson Cook–Zerillie-Armstrong (JC-ZA) models have been investigated for flow stress prediction. Capability of models has been evaluated based on the correlation coefficient (R), average absolute error (Δ) and its standard deviation (δ). Accurate prediction of flow stress behavior is found by integrated JC-ZA model with R = 0.9873, Δ = 2.44 and δ = 4.08%.

36 MATERIALS SCIENCE↗

The Application of Canned Deformation to a Hard-Deformed Spray-Deposited Al-Zn-Mg-Cu Alloy

A wide variety of industrial applications require Al-Zn-Mg-Cu alloys with high strength and ductility. However, Zn-rich Al-Zn-Mg-Cu alloys prepared by rapid solidification methods usually show excellent strength but poor formability, which restricts their wide application in complex forming. In this study, we developed a new deformation method for the spray-deposited Zn-rich Al-Zn-Mg-Cu alloy to avoid crack formation and achieve isotropic properties. The microstructure evolution and crystallographic textures were analyzed and compared with the results of a normal deformation process. Crack-free forgings with the ultimate tensile strength (UTS), yield strength (YS) and elongation of 727 ± 5 MPa, 690 ± 3 MPa, 5.0 ± 0.7% along the radial direction and 735 ± 2 MPa, 693 ± 3 MPa, 6.3 ± 0.2% along the tangential direction were finally obtained. The improvement in the mechanical properties can be attributed to the larger amount of subgrains and substructures generated in the canned deformed alloy. The results of this study show excellent advantages and potential application prospects of the canned deformation to hard-deformed Al-Zn-Mg-Cu alloys.

36 MATERIALS SCIENCE↗

Failure Analysis of Three-Sheet Stackup Structure Made of Dissimilar High-Strength Steel

A three-sheet stackup structure consisting of B1500HS and B250P1 dissimilar high-strength steel was produced by resistance spot welding. The failure mode and energy absorption ability of two typical samples were investigated in typical loading state such as shear and cross-tension test. Moreover, the fracture characteristics were observed by scanning electron microscopy and the fracture process was analyzed based on the loading state. Results show two samples fracture in interfacial mode or pullout mode in shear test and fracture only in pullout mode in cross-tension test. Despite the different fracture modes, fractured sample shows ductile characteristics during mechanical tests. Compared with the sample fractured in interfacial mode, sample fractured in pullout mode has higher ultimate load and energy absorption ability in shear test. Moreover, sample absorbs more failure energy in cross-tension test than that in shear test because of the deformation of structure in cross-tension test. Both carbon equivalent and welding conditions affect the hardness of the fusion zone—a lower CE value leads to a softer HAZ which helps to promote pullout failure in the cross-tension test.

36 MATERIALS SCIENCE↗

Creep Deformation and Rupture Behavior of P92 Steel Weld Joint Fabricated by NG-TIG Welding Process

The creep deformation and rupture behavior of P92 steel weld joint fabricated by narrow-gap TIG (NG-TIG) welding process have been investigated at 923 K over a stress range of 80-140 MPa. The prior-austenite grain size, M{sub 23}C{sub 6} precipitate size and hardness have been found to vary significantly in the weld joint. The reduction in hardness from weld metal to base metal with a trough at the outer edge of heat-affected zone (HAZ) has been observed. Coarsening of M{sub 23}C{sub 6} precipitate, recovery of martensite lath dislocation structure and formation of subgrain structure led to lower hardness in the intercritical HAZ. The creep rupture life of NG-TIG weld joint was lower than the base metal, the difference in creep rupture life between base metal and weld joint has been increased significantly with decrease in applied stress. The fracture location in the joint changed from base metal at high-stress regime to the fine grain (FG) HAZ (Type IV cracking) under lower stress level. Fracture in the FGHAZ evidenced the significant reduction in ductility, localized deformation and extensive localized cavitation. Extensive Laves phase formation with significant loss of solution strengthening contribution from tungsten and coarsening of M{sub 23}C{sub 6} precipitate with prolonged creep exposure led to reduction in hardness and more extensive cavitation in the FGHAZ resulting in premature Type IV failure of the weld joint. Weld strength reduction factor about 0.59 has been evaluated for 10{sup 5} h at 923 K.

36 MATERIALS SCIENCE↗

Effect of Strain Rate on the Tensile Behavior of CoCrFeNi and CoCrFeMnNi High-Entropy Alloys

High-entropy alloys (HEAs), a novel class of metal alloys, have been receiving increasing attention from the scientific community. HEAs have the potential to be used in critical load-bearing applications in replacement of conventional alloys such as stainless steel and nickel-base superalloys. Tensile experiments at quasi-static to dynamic strain rates (10{sup −4}-10{sup 3} s{sup −1}) were performed on two single-phase face-centered cubic HEAs, CoCrFeNi and CoCrFeMnNi. Electron backscatter diffraction was used to study the microstructure of the samples before the experiments, and transmission electron microscopy was performed postmortem. The dominant deformation mechanisms were dislocation slip at quasi-static strain rates with the addition of deformation nano-twins at dynamic strain rates. Ultimate dynamic tensile strength and ductility improved with the increase in strain rate, which can be attributed to the activation of deformation nano-twins in HEAs. CoCrFeNi and CoCrFeMnNi both have low stacking fault energies, which could promote twinning at high strain rates to accommodate plastic deformation. The strain rate sensitivity of the flow stress increased with increasing strain rate, beginning with negligible strain rate sensitivity in the quasi-static range to high strain rate sensitivity in the dynamic range. CoCrFeMnNi showed greater strain rate sensitivity of flow stress. CoCrFeNi, with less configurational entropy, had higher mechanical properties and strain-hardening rates compared to CoCrFeMnNi, which was attributed to the weakening effect of the addition of Mn on the solid solution hardening.

36 MATERIALS SCIENCE↗