Room temperature tensile behavior of 100 oriented tungsten single crystals with rhenium in dilute solid solution
Room temperature behavior of oriented tungsten single crystals with rhenium in dilute solid solution
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Room temperature behavior of oriented tungsten single crystals with rhenium in dilute solid solution
Room-temperature tensile behavior of tungsten and tungsten-rhenium single crystals
Axial ratios and major-axis orientations determined from image processing of Palomar and SRC Sky Survey material are tabulated for a sample of 100 Galactic globular clusters. From a subsample of 99 clusters, the mean axial ratio is found to be 0.93 + or - 0.01. Given that only 32 percent are flatter than b/a less than 0.9, and 5 percent flatter than 0.8, the clusters are found to be quite spherical. As predicted by King (1961 and 1966), tidal interactions by the Galaxy on the cluster are not the means by which the observed ellipticities are produced. Rather, Galactic absorption effects may have a moderate but not dominant effect on the clusters' observed ellipticities, as suggested by van den Bergh (1984). The alternate mechanisms of cluster rotation or anisotropic internal velocity distributions, or both, are considered to be more likely. The observed distribution of axial ratios is statistically indistinguishable from that of a similar-size sample of rotationally flattened clusters, which have axial-ratio values lying in the range of 0.75 less than b/a less than 0.83, and the major axes of which are oriented randomly in space.
Fatigue crack propagation in the near-threshold region has been studied in coarse grain Al 7029 alloy. Over eighty percent of the crack surfaces are planar areas parallel to either 100-oriented or 111-oriented planes. The 100-plane crack surfaces show 'pine tree' morphological features formed by slip on two sets of intersecting planes. The 111-plane crack surfaces were planar and shiny. They were formed primarily by slip on a single dominant 111-oriented slip plane with sparse and very light secondary slip markings. Crack growth rates were measured and correlated with Delta-K.
In response to a NASA request, the National Space Propulsion Synergy Team (SPST) team agreed to provide technical and programmatic support to NASA in formulating a Spaceliner 100 Technology Program. The SPST offered a broad cross-section of expertise and experience. Its membership consists of senior level, volunteer representatives from across government, industry, and academia. The purpose of this paper is to provide a summary of the SPST support of SL100, which culminated in a propulsion technologies assessment and prioritization workshop conducted at MSFC. The results of this workshop and the follow-up analysis are part of this report. Also included, is a review of some "lessons learned" that were solicited from the workshop participants.
A diamond film made of (100)-oriented diamond crystallites has relatively flat surfaces in parallel with the silicon surface. This is desirable because it provides a smoother surface of the diamond film. The difficulty in retaining the (100)-oriented diamond crystallites is strongly influenced by the growth temperature. This paper reports the results from a study on the surface morphologies of diamond films deposited in a hot filament reactor at reduced substrate temperature compared to that deposited at higher temperature.
The objective of this presentation is to provide an understanding of the products of the technology assessment and prioritization workshop, increase knowledge of the assessment process utilized, and stimulate interest in applying this process to many other space endeavors.
We report here the crystal morphologies of MV-1 and ALH84001 magnetites as calculated by back-projection using electron tomography. In the present study, we used a 300 keV TEM with a field emission gun (Tecnai F-30 from FEI Inc.), equipped with a 2048 x 2048 pixel CCD camera from Gatan Inc. to image magnetite crystals over tilt ranges of approx. +/- 72 deg in 2 deg tilt intervals. The images were aligned for back-projection, either manually, or through the use of fiducial 5 nm Au spheres affixed to the specimen prior to microscopy. Three-dimensional (3-D) reconstructions were computed using weighted back-projection of the tilted views. The tomograms were viewed and analyzed as a series of slices 1.0 nm thick, taken parallel to the specimen-supporting grid, using the IMOD software package. The shape of each magnetite crystal was determined by defining the external contour of a given magnetite in each slice and assembling a stack of these contours in 3-D. To aid in visualization, the stacked contour array was reduced to an optimal mesh by Delaunay triangulation. The surface normal to each of the triangles in the mesh was calculated and the triangle faces colored according to the orientation of that surface normal relative to the principal crystallographic axis of magnetite. Green surfaces correspond to {111} orientations, blue surfaces to {100} orientations, and red surfaces to {110} orientations. Triangles whose surface normal did not correspond to one of the principal axes were colored gray. Within the experimental and numerical uncertainties of the deconvolution, the tomographic reconstruction of both MV-1 and ALH84001 magnetites are equivalent and correspond to a truncated hexa-octahedral morphology.
Under a NASA-ESA collaborative research project, three Al-7-weight-percentage Si samples (MICAST-6, MICAST-7 and MICAST 2-12) were directionally solidified aboard the International Space Station to determine the effect of mitigating convection on the primary dendrite array. The samples were approximately 25 centimeters in length with a diameter of 7.8 millimeter-diameter cylinders that were machined from [100] oriented terrestrially grown dendritic Al-7Si samples and inserted into alumina ampoules within the Sample Cartridge Assembly (SCA) inserts of the Low Gradient Furnace (LGF). The feed rods were partially remelted in space and directionally solidified to effect the [100] dendrite-orientation. MICAST-6 was grown at 5 microns per second for 3.75 centimeters and then at 50 microns per second for its remaining 11.2 centimeters of its length. MICAST-7 was grown at 20 microns per second for 8.5 centimeters and then at 10 microns per second for 9 centimeters of its remaining length. MICAST2-12 was grown at 40 microns per second for 11 centimeters. The thermal gradient at the liquidus temperature varied from 22 to 14 degrees Kelvin per centimeter during growth of MICAST-6, from 26 to 24 degrees Kelvin per centimeter for MICAST-7 and from 33 to 31 degrees Kelvin per centimeter for MICAST2-12. Microstructures on the transverse sections along the sample length were analyzed to determine nearest-neighbor spacing of the primary dendrite arms and trunk diameters of the primary dendrite-arrays. This was done along the lengths where steady-state growth prevailed and also during the transients associated with the speed-changes. The observed nearest-neighbor spacings during steady-state growth of the MICAST samples show a very good agreement with predictions from the Hunt-Lu primary spacing model for diffusion controlled growth. The observed primary dendrite trunk diameters during steady-state growth of these samples also agree with predictions from a coarsening-based model. The radial macrosegregation and "steepling" caused by thermosolutal convection during terrestrial growth of the Al-7Si was not observed in the space-grown MICAST samples.
The fracture behavior and deformation of He-charged (at 22 C) single crystals of PWA 1480E Ni-base superalloy were investigated using SEM and TEM techniques to observe the behavior of tensile fractures in notched single crystals with seven different crystal growth orientations: 100-line, 110-line, 111-line, 013-line, 112-line, 123-line, and 223-line. To identify the cleavage plane orientation, a stereoscopic technique, combined with the use of planar gamma-prime morphologies, was applied. It was found that gamma-prime particles were orderly and closely aligned with edges along the 100-line, 010-line, and 001-line-oriented directions of the gamma matrix. Different crystal growth orientations were found not to affect the morphology of gamma-prime particles. The accumulation of dislocations around gamma/gamma-prime interfaces formed strong barriers to subsequent dislocation movement and was the primary strengthening mechanism at room temperature.
Studies are being carried out to determine the feasibility of using ZnSe as a buffer layer for GaAs solar cells grown on silicon. This study was motivated by reports in the literature indicating ZnSe films had been grown by metallorganic chemical vapor deposition (MOCVD) onto silicon with EPD values of 2 x 10(exp 5) cm(sup -2), even though the lattice mismatch between silicon and ZnSe is 4.16 percent. These results combined with the fact that ZnSe and GaAs are lattice matched to within 0.24 percent suggest that the prospects for growing high efficiency GaAs solar cells onto ZnSe-coated silicon are very good. Work to date has emphasized development of procedures for MOCVD growth of (100) ZnSe onto (100) silicon wafers, and subsequent growth of GaAs films on ZnSe/Si substrates. In order to grow high quality single crystal GaAs with a (100) orientation, which is desirable for solar cells, one must grow single crystal (100) ZnSe onto silicon substrates. A process for growth of (100) ZnSe was developed involving a two-step growth procedure at 450 C. Single crystal, (100) GaAs films were grown onto the (100) ZnSe/Si substrates at 610 C that are adherent and specular. Minority carrier diffusion lengths for the GaAs films grown on ZnSe/Si substrates were determined from photoresponse properties of Al/GaAs Schottky barriers. Diffusion lengths for n-type GaAs films are currently on the order of 0.3 microns compared to 2.0 microns for films grown simultaneously by homoepitaxy.
We report on the development and performance of deep-junction (approximately 0.25 micron), graded-emitter-doped, n(sup +)-p InP solar cells grown by metallorganic chemical vapor deposition (MOCVD). A novel, diffusion-transport process for obtaining lightly-doped p-type base regions of the solar cell is described. The I-V data and external quantum-efficiency response of these cells are presented. The best active-area AMO efficiency for these deep-junction cells on (100)-oriented InP substrates is 16.8 percent, with a J(sub SC) of 31.8 mA/sq cm, a V(sub OC) of 0.843 V, and a fill-factor of 0.85. By comparison, the best cell efficiency on the (111)B-oriented InP substrates was 15.0 percent. These efficiency values for deep-junction cells are encouraging and compare favorably with performance of thin-emitter (0.03 micron) epitaxial cells as well as that of deep-emitter diffused cells. The cell performance and breakdown voltage characteristics of a batch of 20 cells on each of the orientations are presented, indicating the superior breakdown voltage properties and other characteristics of InP cells on the (111)B orientation. Spectral response, dark I-V data, and photoluminescence (PL) measurements on the InP cells are presented with an analysis on the variation in J(sub SC) and V(sub OC) of the cells. It is observed, under open-circuit conditions, that lower-V(sub OC) cells exhibit higher band-edge PL intensity for both the (100) and (111)B orientations. This anomalous behavior suggests that radiative recombination in the heavily-doped n(sup +)-InP emitter may be detrimental to achieving higher V(sub OC) in n(sup +)-p InP solar cells.
Enhanced Hall-effect mobilities have been measured in epitaxial (100)-oriented multilayer n-type Si/Si(1-x)Ge(x) films grown on single-crystal Si substrates by chemical vapor deposition. Mobilities from 20 to 40% higher than that of epitaxial Si layers and about 100% higher than that of epitaxial SiGe layers on Si were measured for the doping range 8 x 10 to the 15th to 10 to the 17th/cu cm. No mobility enhancement was observed in multilayer p-type (100) films and n-type (111)-oriented films. Experimental studies included the effects upon film properties of layer composition, total film thickness, doping concentrations, layer thickness, and growth temperature.
The deposition of Tl-Ba-Ca-Cu-O thick films by spray pyrolyzing a Ba-Ca-Cu-O precursor film and diffusing thallium into the film to form the superconducting phase is examined. This approach was taken to reduce exposure to thallium and its health and safety hazards. The Tl-Ba-Ca-Cu-O system was selected because it has very attractive features which make it appealing to device and manufacturing engineering. Tl-Ba-Ca-Cu-O will accommodate a number of superconducting phases. This attribute makes it very forgiving to stoichiometric fluctuations in the bulk and film. It has excellent thermal and chemical stability, and appears to be relatively insensitive to chemical impurities. Oxygen is tightly bound into the systems, consequently there is no orthorhombic (conductor) to tetragonal (insulator) transition which would affect a component's lifetime. More significantly, the thallium based superconductors appear to have harder magnetic properties than the other high-Tc oxide ceramics. Estimates using magnetoresistance measurements indicate that at 77 K Tl2Ba2CaCu2O10 will have an upper critical field, H(sub c2) fo 26 Tesla for applied fields parallel to the c-axis and approximately 1000 Tesla for fields oriented in the a-b plane. Results to date have shown that superconducting films can be reproducibly deposited on 100 oriented MgO substrates. One film had a zero resistance temperature of 111.5 K. Furthermore, x ray diffraction analysis of the films showed preferential c-axis orientation parallel to the plane of the substrate. These results have now made it possible to consider the manufacture of a superconducting tape wire which can be configured into a topology useful for high-field magnet designs. The research which leads to the preparation of these films and plans for further development are reviewed.
A finite element program analysis was used to model the stress distribution of two monocrystalline silicon diaphragm pressure sensors. One configuration consists of an anisotropically backside etched diaphragm into a 250 micron thick, (100) oriented, silicon wafer. The diaphragm and total chip dimensions are given. The device is rigidly clamped on the back to a support substrate. Another configuration consists of a monocrystalline, (100), microdiaphragm which is formed on top of the wafer and whose area is reduced by a factor of 25 over the first configuration. The diaphragm is rigidly clamped to the silicon wafer. The stresses were calculated at a gauge pressure of 300 mm Hg and used to estimate the piezoresistive responses of resistor elements which were placed parallel and perpendicular near the diaphragm edges.
Electrical characteristics of Au contacts on beta-SiC films, grown epitaxially on both nominal and off-axis (100) silicon substrates, are reported. An analysis of the logarithmic I-V plots of the Au/beta-SiC diodes revealed information pertaining to the deep states present in the materials. It was found that while the beta-SiC films grown on nominally (100) oriented substrates show the presence of two deep levels located between 0.26 and 0.38 eV below the conduction bandedge, the beta-SiC films deposited on off-axis substrates have only one deep level, located about 0.49 eV below the conduction bandedge for the 2-deg off (100) substrates and 0.57 eV for the 4-deg off (100) substrates. The presence of the shallower deep states in the beta-SiC films grown on nominal (100) substrates is attributed to the electrical activity of antiphase domain boundaries.
Friction experiments were conducted in air with polytetrafluoroethylene (PTFE) sliding on aluminum single crystals. Mechanical scoring of the crystals with (110) and (100) orientations was observed with a single pass of the PTFE slider. No scoring was observed on the (111). The degree of scoring of the crystals is related to the hardness, with the hardest surface (111) showing no damage and the softest surface (110) showing the most severe scoring. Scoring is caused by work-hardened pieces of aluminum which, as a consequence of the adhesion between PTFE and aluminum, were pulled out of the bulk and became embedded in the PTFE polymer.
A test vehicle with a low work function collector which can be incorporated in a thermionic converter was constructed from standard vacuum components including an ultrahigh vacuum ion pump. The collector assembly was fabricated by diffusion bonding a (100) oriented silicon single crystal to a molybdenum block. The silicon surface was treated with cesium and oxygen to produce an NEA-type condition and the results were tested by photoemission and work function measurements. An n-type silicon collector was successfully activated to a work function of 1.0 eV, which was verified by photoemission spectral yield measurements. The stability test of an activated surface at elevated temperatures was conducted in the range from room temperature to 619 K, which was slightly lower than the designed collector temperature of 700 K. The work function measurements clearly demonstrated that the behavior of cesium replenishment on the activated Si surface was similar in nature to that of a metallic surface; that is, the loss of cesium by thermal desorption could be compensated by maintaining an adequate vapor pressure of cesium.