High Resolution Mapping of Orientation and Strain Gradients in Metals by Synchrotron 3D X-ray Laue Microdiffraction

Synchrotron 3D X-ray Laue microdiffraction, available at beamline 34-ID-E at Advanced Photon Source in Argonne National Laboratory, is a powerful tool for 3D non-destructive mapping of local orientations and strains at sub-micron scale in the bulk. With this technique, it is possible to study local residual stresses developed during manufacturing or while in service due to interactions between, for example, different phases and/or grains with different orientations in materials containing multiple or single phase(s). Such information is essential for understanding mechanical properties and designing advanced materials, but is largely non-existent in the current generation of materials models. In the present paper, the principle and experimental set-up of the 3D microdiffraction are introduced, followed by a description of a method for quantification of the local plastic deformation based on high-angular-resolution orientation maps. The quantification of local residual stresses in two model materials, ductile cast iron (two phases) and partially recrystallized pure nickel (single phase), using 3D microdiffraction will then be presented. The results show that 3D microdiffraction is important for understanding the origin of local residual stresses and to relate them to the microstructural evolution. Finally, the limitations of the 3D microdiffraction on the current generation synchrotron source and new possibilities after the synchrotron upgrade are discussed.

36 MATERIALS SCIENCE↗

Heterogeneous fatigue damage in a nickel-based single-crystal superalloy unraveled using correlative 3D X-ray technology

Nickel-based single-crystal (Ni-SX) superalloys under cyclic stress are susceptible to cracking at stress-concentration sites, eventually leading to low-cycle fatigue (LCF) failure. LCF cracks typically originate from intrinsic defects (e.g., voids and carbides) within solidified dendrites. However, systematic quantitative experimental analyses of defect-mediated local damage remain limited. To thoroughly understand the microscopic origins and evolution of LCF damage, correlated 3D mapping of dendrites across various regions is essential. Here, in this study, macroscale micro-computed tomography (μ-CT) was initially used to capture internal interdendritic secondary cracks within bulk DD413 superalloy after LCF testing at 760 °C. Subsequently, a multimodal methodology combining synchrotron 3D microdiffraction (3D-μXRD), high-resolution μ-CT, and electron microscopy was established. This approach allowed precise localization of internal damage zones near interdendritic secondary cracks and detailed mapping of the 3D correlated distributions of dendrites, defects, and residual stress/strain fields within these zones at submicron spatial resolution. Finally, the same approach was applied to specimens subjected to interrupted loading at approximately 40 % of the fatigue life to uncover the early damage states of dendrites. The dendrite cores (DCs) and interdendritic regions (IDs) exhibit microscale heterogeneous mechanical responses: nearly defect-free DCs accumulate local irreversible slip along specific slip systems to generate slip bands, while the IDs containing various defects accommodate local microplasticity through the activation of multiple slip systems around these defects. The local tensile stress near defects in the IDs exceeds that in the DC slip band regions by more than threefold, leading to the generation of local damage zones within the IDs. Chain-like defect distributions facilitate the interconnection of these local zones into a continuous damage region, further elevating the overall tensile stress in the IDs. Additionally, geometrically necessary dislocations alone are insufficient as indicators of LCF damage; both the internal stress state and its magnitude must be considered. These experimental results provide critical data and insights for the development of multi-physics fatigue models.

Localized deformation↗

3D-microdiffraction: A facility for the Australian synchrotron

Phenomena occurring at the mesoscale, 0.1--10 {mu}m, e.g. polycrystallinity, crystal defects, grain boundaries, orientation and strain, can play a profound role in the bulk behaviour of materials. These properties have been extremely difficult to measure in the spatially resolved in situ real time mode critical to obtaining true understanding. The microdiffraction fluorescence probe, an end-station facility selected for the Australian synchrotron, will enable these properties to be measured, in 3D at submicron scale, correlated to composition (X-ray fluorescence) as well as local elemental coordination (X-ray absorption spectroscopy). This facility will have wide spread fundamental and applied application across the earth and material science communities.

43 PARTICLE ACCELERATORS↗

Probing Phase Transformations and Microstructural Evolutions at the Small Scales: Synchrotron X-ray Microdiffraction for Advanced Applications in [Phase 3 Memory,] 3D IC (Integrated Circuits) and Solar PV (Photovoltaic) Devices

Synchrotron x-ray microdiffraction (μXRD) allows characterization of a crystalline material in small, localized volumes. Phase composition, crystal orientation and strain can all be probed in few-second time scales. Crystalline changes over a large areas can be also probed in a reasonable amount of time with submicron spatial resolution. However, despite all the listed capabilities, μXRD is mostly used to study pure materials but its application in actual device characterization is rather limited. This article will explore the recent developments of the μXRD technique illustrated with its advanced applications in microelectronic devices and solar photovoltaic systems. Application of μXRD in microelectronics will be illustrated by studying stress and microstructure evolution in Cu TSV (through silicon via) during and after annealing. Here, the approach allowing study of the microstructural evolution in the solder joint of crystalline Si solar cells due to thermal cycling will be also demonstrated.

36 MATERIALS SCIENCE↗

Real-time microstructure imaging by Laue microdiffraction: A sample application in laser 3D printed Ni-based superalloys

Synchrotron-based Laue microdiffraction has been widely applied to characterize the local crystal structure, orientation, and defects of inhomogeneous polycrystalline solids by raster scanning them under a micro/nano focused polychromatic X-ray probe. In a typical experiment, a large number of Laue diffraction patterns are collected, requiring novel data reduction and analysis approaches, especially for researchers who do not have access to fast parallel computing capabilities. In this article, a novel approach is developed by plotting the distributions of the average recorded intensity and the average filtered intensity of the Laue patterns. Visualization of the characteristic microstructural features is realized in real time during data collection. As an example, this method is applied to image key features such as microcracks, carbides, heat affected zone, and dendrites in a laser assisted 3D printed Ni-based superalloy, at a speed much faster than data collection. Such analytical approach remains valid for a wide range of crystalline solids, and therefore extends the application range of the Laue microdiffraction technique to problems where real-time decision-making during experiment is crucial (for instance time-resolved non-reversible experiments).

36 MATERIALS SCIENCE↗

Microstructure and residual elastic strain at graphite nodules in ductile cast iron analyzed by synchrotron X-ray microdiffraction

The microstructure and residual elastic strain at graphite nodules (GNs) in ductile cast iron produced using either a fast or slow cooling rate have been characterized using synchrotron 3D X-ray Laue microdiffraction. The results demonstrate that thermal stress is introduced during cooling and that part of this stress is relaxed by plastic deformation of the polycrystalline ferrite matrix. It is observed that the plastic deformation is accommodated by the formation of dislocations and dislocation boundaries, which are organized in a cell structure. The dislocation density quantified based on the microstructure is most pronounced at the GN/matrix interface around small GNs in the fast cooled sample. Residual elastic strain is also present, which is mainly compressive with a maximum of 6.0–9.9 × 10 -4 near the GNs. Gradients of plastic deformation and elastic strain field around the GNs are observed. The results document for the first time that both the elastic strain field and the plastic strain field averaged over the grains around the GNs is approximately scaling with GN size and not affected by the cooling rate. The experimental data are compared with simulations by a finite element method, and agreement and disagreement are considered in detail.

36 MATERIALS SCIENCE↗

A synchrotron study of defect and strain inhomogeneity in laser-assisted three-dimensionally-printed Ni-based superalloy

Synchrotron X-ray microdiffraction was employed to investigate the inhomogeneous distribution of defect and residual strain in the transitional region between the dendritic and stray grains in a laser-assisted 3D printed Ni-based superalloy. The dendritic region was found to be under tensile strain transversely to the primary dendrite arm directions. The dendrite edges, where high level of strains and geometrically necessary dislocations were detected, were discerned as low angle grain boundaries. Lastly, high angle grain boundaries were observed in the stray grain region, and the orientation of the strain tensor in this region varied dramatically at the micron scale, in contrast with the more or less homogeneous distribution in the dendritic region.

36 MATERIALS SCIENCE↗

Unraveling submicron-scale mechanical heterogeneity by three-dimensional X-ray microdiffraction

Shear banding is a ubiquitous phenomenon of severe plastic deformation, and damage accumulation in shear bands often results in the catastrophic failure of a material. Despite extensive studies, the microscopic mechanisms of strain localization and deformation damage in shear bands remain elusive due to their spatial-temporal complexities embedded in bulk materials. Here we conducted synchrotron-based X-ray microdiffraction (μXRD) experiments to map out the 3D lattice strain field with a submicron resolution around fatigue shear bands in a stainless steel. Both in situ and postmortem μXRD results revealed large lattice strain gradients at intersections of the primary and secondary shear bands. Such strain gradients resulted in severe mechanical heterogeneities across the fatigue shear bands, leading to reduced fatigue limits in the high-cycle regime. The ability to spatially quantify the localized strain gradients with submicron resolution through μXRD opens opportunities for understanding the microscopic mechanisms of damage and failure in bulk materials.

36 MATERIALS SCIENCE↗

Quantitative Scanning Laue Diffraction Microscopy: Application to the Study of 3D Printed Nickel-Based Superalloys

Progress in computing speed and algorithm efficiency together with advances in area detector and X-ray optics technologies have transformed the technique of synchrotron radiation-based scanning Laue X-ray microdiffraction. It has now evolved into a near real-time quantitative imaging tool for material structure and deformation at the micrometer and nanometer scales. We will review the achievements of this technique at the Advanced Light Source (Berkeley, CA, USA), and demonstrate its application in the thorough microstructural investigations of laser-assisted 3D printed nickel-based superalloys.

36 MATERIALS SCIENCE↗

Statistical study of ductility-dip cracking induced plastic deformation in polycrystalline laser 3D printed Ni-based superalloy

Ductility-dip cracking in Ni-based superalloy, resulting from heat treatment, is known to cause disastrous failure, but its mechanism is still not completely clear. A statistical study of the cracking behavior as a function of crystal orientation in a laser 3D-printed DL125L Ni-based superalloy polycrystal is investigated here using the synchrotron X-ray microdiffraction. The dislocation slip system in each of the forty crystal grains adjacent to the 300 μm long crack has been analyzed through Laue diffraction peak shapes. In all these grains, edge-type geometrically necessary dislocations (GNDs) dominate, and their dislocation line directions are almost parallel to the crack plane. Based on Schmid's law, the equivalent uniaxial tensile force direction is revealed normal to the trace of the crack. A qualitative mechanism is thus proposed. Thermal tensile stress perpendicular to the laser scanning direction is elevated due to a significant temperature gradient, and thus locations in the materials where the thermal stress exceeds the yield stress undergo plastic deformation mediated by GND activations. As the dislocations slip inside the crystal grains and pile up at the grain boundaries, local strain/stress keeps increasing, until the materials in these regions fail to sustain further deformation, leading to voids formation and cracks propagation.

36 MATERIALS SCIENCE↗

Mechanism of heat affected zone cracking in Ni-based superalloy DZ125L fabricated by laser 3D printing technique

Laser 3D printing is a promising technique to repair damaged Ni-based superalloy components. However, the occurrence of heat affected zone (HAZ) cracking severely limits its applicability. In this paper, we unravel the cracking mechanism by studying the element, phase, defect, and strain distribution around an intergranular crack that initiated from the primary HAZ. Using synchrotron X-ray Laue microdiffraction, we measured high tensile strain/stress transverse to the building direction in both the primary HAZ and the cladding layers, as well as high-density dislocations, which resulted from the thermal contraction and rapid precipitation of γ' phase. The crack initiated because the transverse tensile strain/stress tore up the liquid film formed by the low-melting point preexisting phases in the primary HAZ, such as γ/γ' eutectics and coarse γ' precipitates. The incoherent carbide particles were frequently observed near the crack root as local strain concentrators. In the cladding layers, micro-segregation could not be completely avoided, thus the hot crack continued to propagate over several layers with the assistance of the transverse tensile stress. Finally, our investigations provide a useful guideline for the optimization of the 3D printing process to repair Ni-based superalloys with high susceptibility to hot cracking.

36 MATERIALS SCIENCE↗

Investigation of plastic yielding in near-micrometer grain size aluminum using synchrotron microdiffraction

The onset of plastic yielding has been studied in samples of aluminum with nearmicrometer average grain size using in situ tensile loading combined with synchrotron radiation. A white-beam Laue 3D micro-diffraction technique was used allowing the collection of diffraction signal from a volume with a resolution of 1 μm in all three dimensions. The orientation data obtained from the micro-diffraction are used to estimate the local variation in geometrically necessary dislocation density, and correction factors are suggested for voxels where neighbors are missing in either one or two dimensions. The results demonstrate a considerable heterogeneity in deformation in the early stages of plastic deformation.

Zhang, C L↗

Hardness and microstructural inhomogeneity at the epitaxial interface of laser 3D-printed Ni-based superalloy

Here in this letter, microstructural and mechanical inhomogeneities, a great concern for single crystal Ni-based superalloys repaired by laser assisted 3D printing, have been probed near the epitaxial interface. Nanoindentation tests show the hardness to be uniformly lower in the bulk of the substrate and constantly higher in the epitaxial cladding layer. A gradient of hardness through the heat affected zone is also observed, resulting from an increase in dislocation density, as indicated by the broadening of the synchrotron X-ray Laue microdiffraction reflections. Lastly, the hardening mechanism of the claddin g region, on the other hand, is shown to originate not only from high dislocation density but also and more importantly from the fine γ/γ' microstructure.

36 MATERIALS SCIENCE↗

Residual strain orientation in rolled titanium determined with synchrotron X-ray Laue microdiffraction

Previously, synchrotron X-ray Laue microdiffraction has been used to measure the magnitudes of residual strain in materials. Recently the method was advanced to determine the orientation of the strain ellipsoid and applied to naturally deformed quartzites; however, the deformation history of these quartzites is ambiguous due to their natural origin. Here, in this study, synchrotron X-ray Laue microdiffraction (µXRD) is used to measure the residual strain for the first time in a sample with known stress history, rolled titanium. A deviatoric strain tensor is calculated from each Laue diffraction image collected with two µXRD scans of a rolled titanium sheet in different sample orientations. The principal strain axes are calculated using an eigen decomposition of the deviatoric strain tensors. The results show that the principal axis of compression is aligned with the normal direction of the titanium sheet, and the principal axis of extension is aligned with the rolling direction. Pole figures are used to represent the 3D distribution of residual strain axes.

36 MATERIALS SCIENCE↗

A peak position comparison method for high-speed quantitative Laue microdiffraction data processing

Indexing Laue patterns of a synchrotron microdiffraction scan can take as much as ten times longer than collecting the data, impeding efficient structural analysis using this technique. Here in this paper, a novel strategy is developed. By comparing the peak positions of adjacent Laue patterns and checking the intensity sequence, grain and phase boundaries are identified, requiring only a limited number of indexing steps for each individual grain. Using this protocol, the Laue patterns can be indexed on the fly as they are taken. The validation of this method is demonstrated by analyzing the microstructure of a laser 3D printed multi-phase/multi-grain Ni-based superalloy.

36 MATERIALS SCIENCE↗

Synchrotron X-Ray Microdiffraction Investigation of Scaling Effects on Reliability for Through-Silicon Vias for 3-D Integration

Synchrotron x-ray microdiffraction has been applied to TSV characterization in various studies for nondestructive inspection with submicron resolution due to its high beam intensity and penetration depth. Here, the application of this technique to TSV investigations is examined and the correlation of the plastic deformation to the microstructure and extrusion behavior along with the effect of TSV dimensional scaling is examined. It is shown that the variability of the copper microstructure and resulting TSV behavior requires a larger number of samples in order to report statistically significant observations. The role of the microstructure in creating statistical scatter is demonstrated through microdiffraction measurements of grain orientation correlated with the observed peak widening, which shows that degraded TSV reliability is largely due to the high elastic anisotropy of copper. After taking the statistical variations into account, the scaling effect was clearly observed, with larger plastic deformation in 2μm diameter TSVs than in 5μm diameter TSVs consistent with microstructure variations. This is confirmed by TSV extrusion measurements, which show that the magnitude and statistical spread of the via extrusion for the 2μm diameter TSVs is higher than that of the 5μm diameter TSVs. These findings, confirmed by thermomechanical simulation, demonstrate first that large sample sizes are required in copper TSV investigations due to high variability, which is not improved with scaling.

36 MATERIALS SCIENCE↗