Plastic deformation induced microstructure transition in nano-fibrous Al-Si eutectics
Not Available
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not Available
This study investigates the effect of mechanical cold work (0, 50, and 90% cross-sectional area reduction via swaging) on the creep properties of cast aluminum alloys with high electrical conductivity including high-purity Al (HP-Al), Al-0.15Zr (Al-Zr), and Al-0.27Zr-0.08Sn (Al-Zr-Sn, wt%). The Al-Zr alloy is strengthened by Zr in solid solution while the Al-Zr-Sn alloy is additionally strengthened by Al3Zr nanoprecipitates (8 nm diameter). After 90% cold swaging, the alloys exhibit grains elongated along the swaging direction with their widths ranging between 8 and 152 μm perpendicular to the swaging direction. Creep testing at 200 °C shows that the minimum creep rate of all 90% swaged alloys shows high sensitivity to stress, which can be modeled via a threshold stress σth. Increasing swaging magnitude from 0 to 50 to 90% in Al-Zr-Sn improves the creep resistance without reducing electrical conductivity. The formation of subgrains, increased dislocation density, and columnar grain structure in swaged alloys all enhance creep resistance. HP-Al swaged to 90% exhibits much lower creep resistance (σth = 18 MPa) due to subgrain coarsening and the absence of precipitates compared to Al-Zr (σth = 40 MPa) and Al-Zr-Sn (σth = 40 MPa), which maintain stable subgrain structures and benefit from solid solution strengthening and Al3Zr nanoprecipitates, respectively. Although Al3Zr precipitates are known to stabilize the deformed microstructure by pinning grain-boundaries, this work demonstrates that Zr in solid solution alone can effectively stabilize the deformed microstructure resulting in enhanced creep resistance. This effect of Zr solute on stabilizing grain boundaries for creep performance was not previously well-defined in the literature. Despite similar creep performances of Al-Zr and Al-Zr-Sn, the latter shows 70% higher room-temperature microhardness and slightly improved electrical conductivity (56%IACS (International Annealed Copper Standard) vs. 57%IACS, respectively). This work provides new insights into creep mechanisms of cold-worked Al–Zr alloys that will guide the design of heat-resistant Al conductors for high-demand applications.
Surface abrasion has been shown to introduce heavy shear stress and produce a few hundred nanometers thick altered surface layer (ASL) on Al alloys. Such ASLs exhibit microstructural changes at room temperature and different corrosion resistance than the underlying substrate. Here, we report how sample dimensions and temperature affect the deformed subsurface microstructure evolution on an abraded Al–Zn–Mg–Cu alloy using transmission electron microscopy (TEM) and atom probe tomography. The ASL microstructure evolves differently in the bulk sample than in the thin TEM specimen. In the freshly abraded ASL, the original η'/η precipitates and grain boundaries were deformed toward the abrasion direction. After 7-day natural aging of the freshly abraded bulk sample, well-defined subgrains formed locally in the ASL, and unusual Al 2 Cu (θ) and Mg x Zn y phases precipitated at the subgrain boundaries. However, during natural aging of this TEM specimen taken from the abraded and aged bulk samples, much faster changes occurred, including the continued formation of subgrains and θ particles in the entire ASL, and the diffusion of Zn atoms out of Mg x Zn y particles to form a Zn particle. On the other hand, no obvious microstructural changes occurred in the ASL during 3-month natural aging of the TEM specimen immediately taken from the freshly abraded sample. Finally, this work advances the understanding of how Al alloy microstructures respond during and following any shear deformation, and complex and unexpected effects of sample dimensions on the behavior.
Here, a CrCoNi based medium entropy alloy with small additions of Ti, Al and Nb (denoted as (CrCoNi) 93 Al 4 Ti 2 Nb) in the as-quenched condition, exhibits tensile properties comparable to those of the equiatomic CrCoNi alloy at room temperature. Dark field transmission electron microscopy (TEM), atomic resolution high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM) together with atom probe tomography (APT) show that spatially-localized long range ordering (LRO) L1 2 domains exist in this alloy. The evolution of deformation substructure with plastic deformation in this alloy was characterized using electron backscatter diffraction (EBSD), electron channeling contrast imaging (ECCI) and STEM based techniques including the recently developed weak beam dark field STEM imaging. Plastic deformation occurs by the slip of a/2<110>dislocations, which are narrowly dissociated into Shockley partial dislocations on {111} slip planes. Their dissociation distances in the (CrCoNi) 93 Al 4 Ti 2 Nb alloy are much smaller than the widths of the corresponding partials in the equiatomic CrCoNi alloy due to one or more of the minor alloying elements (Al, Ti, Nb). Dislocation slip in this alloy has a pronounced planar character. The leading dislocations in slip bands glide as pairs due to the existence of LRO domains. Multipoles were formed through the slip of dislocations with opposite signs on adjacent {111} slip planes. Those multipoles serve as building blocks for the formation of subgrain structures consisting of fine slip bands. The distances between slip bands were continuously refined during plastic deformation and dynamic refinement of slip bands plays a crucial role in strain hardening. The effects of LRO domains on planar dislocation slip, the deactivation of deformation twinning and strain hardening of this alloy are discussed.
The stability of U-Mo fuel particles embedded in an Al matrix under irradiation can be enhanced through ZrN coatings and/or heat treatment. Here, the present study investigates the irradiation behavior of fuel plates containing U-Mo fuel particles fabricated under various heat-treatment conditions and ZrN coating thicknesses. Different fission densities were also applied to each fuel plate to evaluate the effects of these variables. Results indicate that higher fission densities lead to more grain recrystallization and high burnup structure (HBS) development in the fuel particles. Heat treatment was found to mitigate the accumulation of fission gas bubbles in fuel particles at low fission densities by coarsening their grains. Fuel particles with ZrN coatings of a 1.2 μm thickness or above exhibited reduced formation of U-Mo/Al interaction layers, suggesting the existence of a critical ZrN coating thickness that minimizes the development of these layers. Fission gas bubbles were predominantly observed at grain boundaries of U-Mo fuel particles irradiated at low fission densities. Subgrain boundaries, which appeared to originate from the original grain boundaries containing fission gas bubbles or HBSs, were also observed, indicating the early stage of HBS propagation in the fuel particles.