Not provided.
Al-Si alloys processed by laser rapid solidification yield eutectic microstructures with ultrafine and interconnected fibers. Such fibrous structures have long been thought to bear resemblance to those formed in impurity-doped alloys upon conventional casting. Here, we show that any similarity is purely superficial. By harnessing high-throughput characterization and computer vision techniques, we perform a three-dimensional analysis of the branching behavior of the ultrafine eutectic and compare it against an impurity-modified eutectic as well as a random fractal (as a benchmark). Differences in the branching statistics point to different microstructural origins of the impurity- and quench-modified eutectic. Finally, our quantitative approach is not limited to the data presented here but can be used to extract abstract information from other volumetric datasets, without customization.
Not Available
Here, this study explores the application of friction stir processing (FSP) to enhance the material properties of Sr-modified Aural-5 alloy, with a focus on improved tensile and fatigue properties. Aural-5 is a well-known vacuum-assisted high-pressure die-cast (HPDC) Al-Si7-Mg alloy used in the automotive industry to reduce vehicle weight, enhance fuel efficiency, and lower carbon emissions. This alloy modifies its material chemistry with Sr for fine fibrous networks of eutectic silicon and manganese (Mn) to reduce die soldering. It has significantly less iron (Fe) content resulting in the elimination of detrimental needle-shaped Fe-bearing ß-phase intermetallic and improving ductility. The initial microstructure of as-received HPDC Aural-5 exhibits shrinkage porosity in the middle section, a dendritic microstructure with fibrous Al-Si eutectic colonies, a shear-band structure beneath the die-wall, large dendritic externally solidified crystals (ESCs), needle-shaped Mg 2 Si phase and significant second-phase particulates. Some of those microstructural features, such as porosity, ESCs, needle-shaped Mg 2 Si phase, and large second-phase particles, serve as initiation sites for cracks under mechanical loading, resulting in adverse effects on tensile properties, particularly ductility. FSP effectively transforms the microstructure into a wrought configuration with uniform particle distribution by eliminating porosity and disintegrating dendrites, eutectic colonies, ESCs, second-phase particles, and shear-band structures. FSP-driven microstructure modification enhances yield strength and tensile ductility by ~30% and ~35%, respectively. The fatigue life of the material in a bending mode configuration (stress ratio R = 0.1) after FSP exhibits enhancements ranging from 2.0 to 3.9 times that of the original HPDC Aural-5 alloy, depending on the applied stress level.
Steadily rising demand for glider weight reduction has driven the development of vacuum-assisted high-pressure die-cast (HPDC) Al-alloys for automotive structural components. Aural-5 is a strontium-modified HPDC alloy utilizing manganese (Mn) to reduce die soldering, eliminating detrimental needle-shaped Fe-bearing ß-phase intermetallic and improving ductility. HPDC Aural-5 contains shrinkage porosity, dendrites with Al-Si eutectic colonies, externally solidified crystals (ESCs), shear-band structure, and large second-phase particulates. Porosity, ESCs and large second-phase particles work as crack initiation sites, negatively impacting tensile properties. In this study, friction stir processing (FSP) is employed for microstructural modification of a thin-walled HPDC Aural-5 by eliminating porosity and breaking down dendrites, second-phase particles, eutectic colonies, ESCs and shear-band structures to create wrought microstructure with homogenized particle distribution. Mechanical property characterization indicates ~30% and ~35% enhancement in yield strength and ductility and associated marked effects on ~69% improvement in tear toughness according to the ASTM B871 test.
Microstructure and creep properties are studied in a eutectic AlSi10Mg alloy modified with Zr and Sc additions (Al-9.8Si-0.32Mg-0.70Zr-0.23Sc, wt%) manufactured through laser powder-bed fusion (L-PBF). Three types of Zr/Sc-bearing powders - elemental, master-alloy, and pre-alloyed - are employed in the fabrication process, with the pre-alloyed powders providing the highest incorporation of Zr and Sc in the Al matrix. Here, the as-printed alloy exhibits a fine cellular Al-Si eutectic structure which fragments and coarsens into micron-sized Si particles during aging at 300 ºC, leading to a steady drop in alloy microhardness between 0.1 and 1000 h. Coarsening of the eutectic Si phase during aging is not measurably affected by Zr and Sc in solid solution, which precipitate during aging and increases strength, compensating weakening from Si coarsening between 1 and 200 h at 300 ºC. Atom-probe analysis in the peak-aged condition (96 h/300 °C) confirms the presence of Al 3 (Sc,Zr) secondary nano-precipitates with an average radius of 1.0 nm and some Si solubility. Micron-sized grains are present throughout the alloy, with ultra-fine-grained regions at the melt pool boundaries, neither of which coarsen during long-term aging at 300 ºC. Under creep conditions at 300 °C, the Zr/Sc-bearing alloy with Al 3 (Sc,Zr) nano-precipitates exhibits power-law behavior, with a high apparent stress exponent (n a = 9) and a high threshold stress (σ th = 43 MPa), exhibiting nearly double the strength of a Zr/Sc-free AlSi10Mg control alloy (σ th = 22 MPa).
Corrosion behavior of cast Al-Cu-Mn-Zr (ACMZ) and RR350 alloys was compared to a cast 319 alloy in 3.5 wt.% NaCl. After 168 h immersion, ACMZ and RR350 alloys suffered from preferential attack adjacent to intermetallic particles decorated at grain boundaries while the attack in 319 occurred in eutectic Al-Si dendritic boundaries. Electrochemical data allowed semiquantitative comparison of alloy resistance to corrosion initiation, and ACMZ type alloys, including RR350 and three alloys with higher Cu, were considered more resistant than 319 due to the absence of deleterious Si particles. In case of 319, such Si particles presumably drove higher micro-galvanic influence to initiate and sustain Al corrosion. With lower susceptibility to corrosion initiation, ACMZ alloys should exhibit higher or at minimum similar resistance compared to cast 319.
Two A356 aluminum alloys (Al-Si-Mg), one with 0.09 wt.% Fe and one with 0.91 wt.% Fe, were cast in a graphite mold with the simultaneous application of local ultrasonic intensification to refine the as-cast microstructure. Ultrasonication during casting transformed the morphology of primary Al grains from dendritic (~140-290 microns in size) to globular (~33-36 microns in size). The alloy with high Fe exhibited globular grains at distances up to 45 mm away from the ultrasound probe, while the alloy with low Fe exhibited globular grains at distances only up to 6 mm away from the ultrasound probe. Near the location of the ultrasound probe (< 2 mm away), a second non-dendritic microstructural morphology was observed with fine aluminum grains (~9-25 microns in size). This unique fine-grained morphology has not been previously reported, contains a greater concentration of Si relative to the globular microstructure, and may be a large, fully eutectic region. Ultrasonication during casting also transformed the morphology of the ß-Al 5 FeSi phase particles (which are deleterious to the strength and ductility of the alloy) in the high Fe alloy from needle-like to rectangular, which could enable the greater use of secondary Al alloys. Thermodynamic simulations conducted to calculate the solidification paths of the two alloys studied predict that the ß-Al 5 FeSi phase begins to form earlier in the alloy with high Fe. Finally, data suggest that the ß-Al 5 FeSi phase (which is more abundant in alloys with high Fe content) may enhance ultrasonically-induced grain refinement.
Heterostructured materials comprised of relatively soft/hard disparate phases typically exhibit composite strengthening but lack plastic deformability at ambient temperatures. However, heterostructured systems comprised of nanoscale phases can simultaneously enhance yield strength and strain hardening, thereby promoting uniform distribution of plastic flow. In this review, the atomic-scale deformation mechanisms in model systems of eutectic alloys, Al-Al 2 Cu and Al-Si, refined to nanoscales via laser rapid solidification are discussed, and compared with literature on multi-component (high entropy) eutectics such as Ni-Al-Fe-based with Cr and/or Co additions. The nano-lamellar Al-Al 2 Cu structures exhibit unit defect mechanisms not reported in monolithic Al 2 Cu intermetallic: localized shear on {0 1 1} and shear-induced faults on {1 2 1} planes, constrained by closely-spaced dislocation arrays in Al confined by Al/Al 2 Cu interfaces. The unexpected plasticity mechanisms are enabled by slip continuity in nanoscale Al-Al 2 Cu eutectics associated with the orientation relationship and interface habit planes. In nano-fibrous Al-Si eutectic, tensile ductility at strength approaching 600 MPa is observed resulting from dislocation plasticity in the nano-Al channels and cracking in Si nanofibers. Molecular dynamics simulations show that Al dislocations easily cross-slip (screw) or climb (edge) along Al-Si interfaces, making slip transmission difficult. The propagation of nano-cracks is suppressed by surrounding strain hardening Al, retaining good ductility of the sample, in spite of lack of direct slip transmission. Finally, the critical unit mechanisms of slip transmission and interface-enabled plasticity observed in nanoscale eutectic binary systems can also explain the strength-ductility relationship in multi-component eutectics and homogeneously distributed plastic flow with increasing microstructural heterogeneity.
Laser surface remelting of aluminum alloys has emerged as a promising technique to enhance mechanical properties through refined microstructures. This process involves rapid cooling rates ranging from 10 3 to 10 8 °C/s, which increase solid solubility within aluminum alloys, shifting their eutectic composition to a larger value of silicon content. Consequently, the resulting microstructure combines a strengthened aluminum matrix with silicon fibers. This study focuses on the laser scanning of Al-Si aluminum alloy to reduce the size of aluminum matrix spacings and transform fibrous silicon particles from micrometer to nanometer dimensions. Analysis revealed that the eutectic structure contained 17.55% silicon by weight, surpassing the equilibrium eutectic composition of 12.6% silicon. Microstructure dimensions within the molten zones, termed ‘melt pools’, were extensively examined using Scanning Electron Microscopy (SEM) at intervals of approximately 20 μm from the surface. A notable increase in hardness, exceeding 50% compared to the base plate, was observed in the melt pool regions. Thus, it is exemplified that laser surface remelting introduces a novel strengthening mechanism in the alloy. Moreover, this study develops an in situ method for predicting melt pool properties and dimensions. A predictive model is proposed, correlating energy density and spectral signals emitted during laser remelting with mechanical properties and melt pool dimensions. This method significantly reduces characterization time from days to seconds, offering a streamlined approach for future studies in additive manufacturing.
The presence and morphology of Fe-containing intermetallic phases affect the mechanical properties of aluminum alloys, especially in secondary Al–Si-based cast alloys. Although strontium (Sr) addition of 50 to 500 ppm is known to refine the needle-type eutectic silicon structure, the influence of Sr on the formation of Fe-intermetallic phases remains unclear. The present work investigates the combined additions of Sr and Mn to Al–9Si–0.6Fe–0.35Mg (All compositions are in wt pct except otherwise stated.) alloys on the formation of Fe-intermetallic phases at different solidification rates from ~ 1.5 to ~ 60 °C/s. Long and branched-type AlFeSi phase with size ranging from 50 to 120 µm are more common when solidified at the rate of 1.5 °C/s regardless of Sr and Mn additions. However, at the fast solidification rate of 60 °C/s, a 60 ppm Sr addition significantly reduced the average length of needle-shaped AlFeSi phase to less than 3 to 5 µm. Thermodynamic simulations have been performed using CALculation of PHAse Diagrams (CALPHAD) models to predict the formation of various phases and their possible interactions during solidification. The results indicated that the combination of a high solidification rate and about 60 ppm of Sr is beneficial to refining the δ-Al 3 FeSi 2 phase in Al–Si–Mg alloys containing 0.6 pctFe. As a result, this unexpected finding of Fe-intermetallic refinement by low Sr addition (~60 ppm) provides an important guide in designing secondary alloys for sustainable casting applications.
Iron (Fe) has been considered a major impurity since it is detrimental to the mechanical properties of many cast aluminum alloys due to the formation of Fe-containing brittle intermetallic phases. Fe is found naturally as an impurity in bauxite ore, resulting in Fe contamination of aluminum alloys with increasing contamination from current recycling practices. The Al–Ce–Fe system was investigated using CALPHAD (CALculation of PHAse Diagrams) modeling and experimental casting techniques. It was found that additions of Fe to the Al–Ce system are beneficial to the strength (slightly) and ductility (significantly) of the ternary alloys, which is attributed to the formation of fine metastable Al 8 CeFe 2 phase with aggregate morphology and equilibrium Al 10 CeFe 2 phase, suppressing coarse proeutectic Al 11 Ce 3 phase in near-eutectic Al–Ce alloys. Heat treatment study showed that the metastable Al 8 CeFe 2 phase transforms to predicted equilibrium Al 10 CeFe 2 phase at 500 °C, with essentially no intermetallic or grain coarsening; thus, the alloy displayed excellent property retention. The Al–Ce–Fe alloy system offers opportunities for sustainable, recyclable alloy development using low-cost Fe and low-cost cerium (a byproduct of rare-earth extraction).
Laser Surface Remelting (LSR) was applied to arc-melted Al-20Si-0.2Sr, Al-20Si-0.2Ce, and Al-20Si hypereutectic alloys to refine microstructures. Experiments revealed that microstructures in the melt pool varied from fully eutectic to a mixture of Al dendrites and inter-dendritic eutectic. We calculated cooling rates using the Eagar-Tsai model and correlated cooling rates with characteristic microstructures, revealing that a cooling rate on the order of 104 K/s could lead to maximized fully eutectic microstructure morphology. Due to rapid solidification, the Si composition in the LSR eutectic was measured at 18.2 wt.%, higher than the equilibrium eutectic composition of 12.6 wt.%Si. Compared to Al-20Si, Ce addition had no significant effect on the volume fraction of the fully eutectic structure but refined Si fibers to approximately 30 nm in diameter. Sr addition did not further refine the diameter of eutectic Si fibers compared to Al-20Si but increased the volume fraction of the fully eutectic microstructure morphology. The refinement ratio (φ) of the Si fiber diameter from the bottom of the melt pool to the surface for the three alloys was similar, at around 28%. The established correlation between the cooling rate and the size and morphology of the microstructure within the melt pool will enable tailoring of the microstructure in laser-processed as well as deposited alloys for high strength and plasticity.