AN INITIAL ASSESSMENT OF THE CREEP-RUPTURE STRENGTHS FOR WELDMENTS WITH ALLOY 800H BASE METAL AND ALLOY 617 FILLER METAL

In Section III, Division 5 of the American Society of Mechanical Engineers Boiler and Pressure Vessel Code, Alloy 800H is qualified for elevated-temperature nuclear construction for temperatures up to 760°C (1,400°F) and a maximum service life of 300,000 hours. There are two permissible filler metals for Alloy 800H weldments specified in Division 5: ENiCrFe-2 (Alloy A) and ERNiCr-3 (Alloy 82). Low creep-rupture strengths of these weldments at the upper limits of the qualified temperatures and service lives may restrict the design envelope for elevated-temperature nuclear construction with Alloy 800H. As a result, an alternative filler metal is desired to improve the creep-rupture strengths of Alloy 800H weldments for the qualified temperatures and service lives. This work investigates an overmatched filler metal. Specifically, a weldment with Alloy 800H base metal and Alloy 617 filler metal fabricated by semiautomated gas tungsten arc welding is investigated. A scoping creep-rupture test program was conducted of cross-weld specimens at temperatures ranging from 750 to 1,000°C (1,292 to 1,832°F). Preliminary results on the creep-rupture strengths of the Alloy 800H weldment with Alloy 617 filler metal do not show significant improvement compared to the filler metals currently qualified in Division 5 for Alloy 800H weldments. Consequently, work is in progress to investigate a matching filler metal.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Continue Effort to Improve Alloy 800H Weldment

This memorandum formally documents the completion of the Level 3 milestone M3AT-22IN0604055 titled, “Continue effort to improve Alloy 800H weldment creep rupture performance,” by the transmittal of this deliverable document, entitled, “Issue memo ‘Preliminary assessment of UTP A 2133 Mn as a matching filler metal for Alloy 800H in Section III Division 5 applications.’” The deadline for this milestone is August 27, 2022. This milestone is part of the ART GCR work package AT-22IN060405, “Long-Term Very-High Temperature Reactor (VHTR) Material Qualification – INL.”

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

GCR: Development of Improved Alloy 800H Weldment

In Section III, Division 5 of the American Society of Mechanical Engineers Boiler and Pressure Vessel Code, Alloy 800H is qualified for elevated-temperature nuclear construction for temperatures up to 760°C (1400°F) and a maximum service life of 300,000 hours. There are two permissible filler metals for Alloy 800H weldments specified in Division 5: ENiCrFe-2 (Alloy A) and ERNiCr-3 (Alloy 82). Low creep-rupture strengths of these weldments at the upper limits of the qualified temperatures and service lives may restrict the design envelope for elevated-temperature nuclear construction with Alloy 800H. As a result, an alternative filler metal is desired to improve the creep-rupture strengths of Alloy 800H weldments for the qualified temperatures and service lives. This work investigates an overmatched filler metal. Specifically, a weldment with Alloy 800H base metal and Alloy 617 filler metal fabricated by semiautomated gas tungsten arc welding is investigated. A scoping creep-rupture test program was conducted of cross-weld specimens at temperatures ranging from 750 to 1000°C (1292 to 1832°F). Preliminary results on the creep-rupture strengths of the Alloy 800H weldment with an Alloy 617 filler metal do not show significant improvement compared to the filler metals currently qualified in Division 5 for Alloy 800H weldments. Consequently, work is in progress to investigate a matching filler metal, UTP A 2133 Mn.

36 MATERIALS SCIENCE↗

Assessment of UTP A 2133 Mn as a Matching Filler Metal for Alloy 800H in Section III, Division 5 Applications

Six alloys are qualified in the American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code (BPVC) for elevated-temperature nuclear components. Due to reactor design alloy restrictions and motivation to improve operational efficiency and plant lifetimes, it is necessary to maximize the usefulness of qualified alloys. One of these alloys is Alloy 800H, which is qualified for a maximum temperature of 760°C and a maximum 300,000-hour service life. However, the welding filler metals qualified to join Alloy 800H have stress rupture factors that reduce the allowable weldment strength by factors as low as 0.59 times the Alloy 800H base metal. In an effort to improve the weldment creep-rupture performance, or to increase the stress reduction factor, non-code qualified filler metals are under investigation by the Department of Energy?s Advanced Reactor Technologies program. For this investigation, UTP A 2133 Mn filler metal (Fe-Cr-Ni-Mn-Nb) was used to join 0.5 in. thick Alloy 800H plate to demonstrate passing an ASME BPVC Section IX weld qualification. The multi-pass, pulsed GTAW process showed successful weld qualification results, and additional property measurements were conducted to compare previous analyses of Alloy 82 and Alloy 617 filler metals. Future work will evaluate the cross-weld creep-rupture performance of the UTP A 2133 Mn in comparison to Alloy 82 and Alloy 617 filler metals.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Update on the Current R&D Activity in the U.S.

This presentation is to fulfil DOE commitment to GIF VHTR Materials PMB. Notched creep rupture testing: Weldment V-notch specimen test finished. 800C 60MPa, 15,716 hour rupture life. Two double V-notch specimen tests have finished. Crack growth tests: System modification was required for creep and creep-fatigue testing, Epsilon 3548COD Extensometer has been ordered, to allow load-line displacement measurements, to be paired with direct current potential drop already used to measure crack length, Sample redesigned in accordance to ASTM E2760 and E1457 to allow for both creep and creep-fatigue crack growth rate testing. Alloy 800H Weldments (1/2) and Alloy 800H Weldments (2/2), Variable Fatigue Testing, and Multi=axial Stress Relaxation. Continue work to finish 800H model, examine ?universal? constitutive model form.