Search NASA⌕ Search

SEARCH · Search NASA

Results for “Aqueous corrosion”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Potential-pH diagrams considering complex oxide solution phases for understanding aqueous corrosion of multi-principal element alloys

The potential-pH diagram, a graphical representation of the thermodynamically predominant reaction products in aqueous corrosion, is originally proposed for the corrosion of pure metals. The original approach only leads to stoichiometric oxides and hydroxides as the oxidation products. However, numerous experiments show that non-stoichiometric oxide scales are prevalent in the aqueous corrosion of alloys. In the present study, a room temperature potential-pH diagram considering oxide solid solutions, as a generalization of the traditional potential-pH diagram with stoichiometric oxides, is constructed for an FCC single-phase multi-principal element alloy (MPEA) based on the CALculation of PHAse Diagram method. The predominant reaction products, the ions in aqueous solution, and the cation distribution in oxides are predicted. The oxide solid solution is stabilized by the mixing free energy (or mixing entropy) and the stabilizing effect becomes more significant as the temperature increases. Consequently, solid solution oxides are stable in large regions of the potential-pH diagram and the mixing free energy mostly affects the equilibrium composition of the stable oxides, while the shape of stable regions for oxides is mostly determined by the structure of the stable oxides. Agreements are found for Ni 2+ , Fe 2+ , and Mn 2+ between the atomic emission spectroelectrochemistry measurements and thermodynamic calculations, while deviations exist for Cr 3+ and Co 2+ possibly due to surface complexation with species such as Cl - and the oxide dissolution. By incorporating the solution models of oxides, the current work presents a general and more accurate way to analyze the reaction products during aqueous corrosion of MPEAs.

Materials Science↗

A general mechanism for gel layer formation on borosilicate glass under aqueous corrosion

Mineral and glass dissolution is a scientific topic deeply investigated but incompletely understood and of a great interest for the geochemical and materials science communities. If the interfacial dissolution/reprecipitation mechanism seems to be applicable to most of silicate minerals, the debate remains open concerning glass. Here we studied two model glasses, a ternary borosilicate (CJ1) and the same glass doped with 4.1 mol% of Al2O3 (CJ2). The two glasses were altered at 90°C, pH 9, and in conditions far and close to saturation with respect to amorphous silica, to determine the initial and residual rates. Moreover, a specific experiment was conducted for a short duration with a solution highly enriched with 18O and 29Si isotopes to understand how passivating gels form. SEM, TEM and ToF-SIMS characterization, along with Monte Carlo simulations were used to understand the rate limiting reactions at play and infer the role of Al. We show that Al yields a slower matrix dissolution in dilute conditions. However, it slows down he formation and the maturation of the passivating gel and favors alteration by partial hydrolysis of Si and Al entities followed by in-situ reorganization/relaxation into a porous network. Unexpectedly, CJ1 experienced both interfacial dissolution/reprecipitation and partial hydrolysis followed by in situ reorganization of the silicate network during the course of a single experiment. This study offers a unified concept that can pave the way for the future development of a predictive kinetic model based on a detailed description of bond breaking and bond forming as a function of glass composition and alteration conditions.

Gin, Stephane↗

Network structure in alteration layer of boroaluminosilicate glass formed by aqueous corrosion

Exogenously-added LiCl has been shown to slightly accelerate the corrosion rate of a boroaluminosilicate glass called International Simple Glass (ISG) in aqueous solutions over forward- and residual-rate regimes, while KCl and CsCl impede. To understand the effect of exogenously added electrolytes on resulting hydrous species and the network structure of alteration layers, infrared spectroscopy was implemented. It was found that the fraction of molecular water relative to the surface-bound hydroxyl species is lower in the KCl and CsCl conditions compared to the LiCl and pure water conditions. An approximation for the spectral features of the thin surface films from an experimentally-obtained specular-reflectance infrared (SR-IR) spectrum was proposed; results indicate no significant difference in the Si-O bonding network of the alteration layers formed in the presence of exogenously added LiCl, KCl and CsCl. Furthermore, the observed change in corrosion rates might be linked to the relative abundance of molecular water species in the porous network, rather than the silicate bonding structure.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

PIE-Enabled Study of Aqueous Corrosion & Zr Hydriding in Cr-Coated Cladding: M3GV-23PN0101132

Chromium-coated zirconium alloy cladding is under investigation as an accident-tolerant fuel (ATF) concept to extend performance to higher burnups via improved oxidation resistance and reduced hydrogen pickup. However, hydrothermal corrosion behavior and hydrogen transport mechanisms governing in-service hydriding of these coatings remain poorly understood. In a collaborative study between Pacific Northwest National Laboratory (PNNL), Idaho National Laboratory (INL), and the University of Huddersfield, cold spray (CS) and physical vapor deposition (PVD) Cr-coated Optimized ZIRLO™ cladding samples were characterized after exposure to PWR-simulated water chemistry under both in-core (neutron irradiation) and out-of-core (aqueous-only) conditions at the MIT Research Reactor. Multi-scale characterization was performed independently at PNNL and INL to evaluate coating integrity, microstructural evolution, Cr/Zr interface chemistry, and hydride formation. Both laboratories observed a consistent divergence in hydriding behavior: out-of-core CS Cr-coated cladding exhibited elevated hydride concentrations exceeding those of uncoated cladding, whereas in-core CS samples showed substantially suppressed hydriding. In-core specimens also displayed irradiation-specific features, including nanoscale voids within the Cr coating and radiation-induced segregation clusters in the Zr substrate. CS coatings retained an interdiffusion-free Cr/Zr bond with no intermetallic layer, whereas PVD coatings exhibited inferior quality with visible cracks and pores. An automated image-based hydride quantification method systematically overestimated bulk hydrogen content relative to inert gas fusion measurements, underscoring the need for standardized sample preparation and reference standards. Interpretation of hydride nucleation and growth is complicated by the open inner-diameter of the specimens, which provides additional hydrogen pathways. The results motivate further foundational studies to support predictive models of hydrothermal corrosion and hydrogen transport in unirradiated and irradiated Cr-coated cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The effects of neutron and ionizing irradiation on the aqueous corrosion of SiC

Chemical vapor deposited (CVD) SiC and nuclear-grade SiC/SiC composite materials were exposed to light water reactor (LWR) conditions at the MIT Nuclear Reactor (MITR) here. Three sets of samples were exposed within flowing PWR-chemistry-coolant under either 1) neutron and ionizing irradiation with resulting radiolysis products, 2) radiolysis products without neutron flux, 3) loop coolant. Post-irradiation examination (PIE) exhibited an increase in corrosion from radiolysis products (particularly H 2 O 2 ), and potentially a further increase from radiation damage. For CVD SiC, regardless of exposure location, the in-situ observed corrosion rate was less than 1 µm per year, potentially within acceptable limits for LWR application.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Influence of Glycolate Anion on Aqueous Corrosion in DWPF and Downstream Facilities – SCC Testing

Glycolic acid is being evaluated as an alternate reductant in the preparation of High Level Waste for the Defense Waste Processing Facility (DWPF) at the Savannah River Site (SRS). During processing, the glycolic acid may not be completely consumed with small quantities of the glycolate anion being carried forward to waste facilities. The SRS liquid waste contractor requested an assessment of the influence of the glycolate anion on the corrosion of the materials of construction (MoC) throughout the waste processing system since this concern had not been previously evaluated. The influence of glycolic acid on the occurrence of stress corrosion cracking (SCC) had not been evaluated specifically in the previous testing. The present testing used electrochemical and coupon immersion testing to assess this influence. Additionally, the primary guidance on corrosion for operating DWPF with a formate-based flowsheet is based on testing that utilized test solutions with a small number of constituents. Recent testing used more complex solutions based on flowsheet development for DWPF. Additional electrochemical tests were also conducted to assess the influence of this difference on test results.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Measurements and mechanisms of localized aqueous corrosion in aluminum-lithium alloys

Like most heat treatable aluminum alloys, localized corrosion and stress corrosion of Al-Li-Cu alloys is strongly dependent on the nature and distribution of second phase particles. To develop a mechanistic understanding of the role of localized corrosion in the stress corrosion process, bulk samples of T(sub 1) (Al2CuLi) and a range of Al-Cu-Fe impurity phases were prepared for electrochemical experiments. Potentiodynamic polarization and galvanic couple experiments were performed in standard 0.6 M NaCl and in simulated crevice solutions to assess corrosion behavior of these particles with respect to the alpha-Al matrix. A comparison of time to failure versus applied potential using a constant load, smooth bar SCC test technique in Cl(-), Cl(-)/CrO4(2-), and Cl(-)/CO3(2-) environments shows that rapid failures are to be expected when applied potentials are more positive than the breakaway potential (E sub br) of T(sub 1) (crack tip) but less than E(sub br) of alpha-Al (crack walls). It is shown that this criterion is not satisfied in aerated Cl(-) solutions. Accordingly, SCC resistance is good. This criterion is satisfied, however, in an alkaline isolated fissure exposed to a CO2 containing atmosphere. Rapid failure induced by these fissures was recently termed preexposure embrittlement. Anodic polarization shows that the corrosion behavior of T(sub 1) is relatively unaffected in alkaline CO3(2-) environments but the alpha-Al phase is rapidly passivated. X ray diffraction of crevice walls from artificial crevices suggests that passivation of alpha-Al occurs as hydrotalcite-type compound (LiAl2(OH)6)2(+) - CO3(2-) - nH2O.

Buchheit, Rudolph G., Jr.↗

Measurements and mechanisms of localized aqueous corrosion in aluminum-lithium-copper alloys

Summary information is included for electrochemical aspects of stress corrosion cracking in alloy 2090 and an introduction to the work to be initiated on the new X2095 (Weldalite) alloy system. Stress corrosion cracking (SCC) was studied in both S-T and L-T orientations in alloy 2090. A constant load TTF test was performed in several environments with a potentiostatically applied potential. In the same environments the electrochemical behavior of phases found along subgrain boundaries was assessed. It was found that rapid failure due to SCC occurred when the following criteria was met: E(sub BR,T1) is less than E(sub applied) is less than E(sub Br, matrix phase). Although the L-T orientation is usually considered more resistant to SCC, failures in this orientation occurred when the stated criteria was met. This may be due to the relatively isotropic geometry of the subgrains which measure approximately 12 to 25 microns in diameters. Initial studies of alloy X2095 includes electrochemical characterization of three compositional variations each at three temperatures. The role of T(sub 1) dissolution in SCC behavior is addressed using techniques similar to those used in the research of 2090 described. SCC susceptibility is also studied using alternate immersion facilities at Reynolds Metals Corporation. Pitting is investigated in terms of stability, role of precipitate phases and constituent particles, and as initiation sites for SCC. In all research endeavors, attempts are made to link electrochemistry to microstructure. Previous work on 2090 provides a convenient basis for comparison since both alloys contain T(sub 1) precipitates but with different distributions. In 2090 T(sub 1) forms preferentially on subgrain boundaries whereas in X2095 the microstructure appears to be more homogeneous with finer T(sub 1) particles. Another point for comparison is the delta prime strengthening phase found in 2090 but absent in X2095.

Wall, Douglas↗

Stainless and carbon steel corrosion in aqueous piperazine at absorber and water wash conditions

Corrosion of carbon steel (C1010) and stainless steels (304, 316L, 430) was measured at absorber and water wash conditions at the bench scale. Corrosion rate decreases with increasing concentration of piperazine (PZ). With more than 0.003 m PZ in solution, carbon steel has acceptable corrosion performance. Corrosion of carbon steel increases with increasing partial pressure of CO2, suggesting loading is another dominant parameter. The effect is more significant for dilute PZ; therefore, untreated flue gas with high CO2 content should be avoided in the water wash. Temperature has a less significant effect than PZ concentration and loading. Carbon steel corrosion increases with increasing flow velocity at both absorber and water wash conditions

Liu, Ching-Ting↗

An Unexpected Role of H During SiC Corrosion in Water

During aqueous corrosion, atoms in the solid react chemically with oxygen, leading either to the formation of an oxide film or to the dissolution of the host material. Commonly, the first step in corrosion involves an oxygen atom from the dissociated water that reacts with the surface atoms and breaks near-surface bonds. In contrast, hydrogen on the surface often functions as a passivating species. Here, we discovered that the roles of O and H are reversed in the early corrosion stages on a Si-terminated SiC surface. O forms stable species on the surface, and chemical attack occurs by H that breaks the Si–C bonds. Here, this so-called hydrogen scission reaction is enabled by a newly discovered metastable bridging hydroxyl group that can form during water dissociation. The Si atom that is displaced from the surface during water attack subsequently forms H 2 SiO 3 , which is a known precursor to the formation of silica and silicic acid. This study suggests that the roles of H and O in oxidation need to be reconsidered.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Predicting and Controlling Corrosion (Abbreviated Final Report)

Corrosion accumulates significant replacement costs in the transportation, utility, manufacturing, and infrastructure sectors. It also underpins several of LLNL’s core missions in stockpile stewardship, defense, and energy security. Whereas most corrosion and aging models are empirically parameterized to describe well-defined conditions late in the reaction, the factors that determine the early stages of corrosion—during which mitigation could be most impactful— are poorly understood. This project addressed the critical need for new approaches to predict the kinetics of corrosion initiation based on firm physical and chemical understanding. The activities encompassed degradation of relevant metals in both hydrogen-rich and environmental corrosion scenarios. The team integrated state-of-the-art multiscale simulation, in situ characterization, and data science within three technical thrusts: hydriding of Ti alloys; aqueous corrosion of Al and Ni-Cr alloys; and degradation of additively manufactured 316L stainless steel. In each case, novel capabilities were developed to identify and track the impacts of key atomistic, compositional, and microstructural features on the metal systems. For hydriding, protocols were developed to tightly integrate multiscale models, advanced multimodal characterization, and machine learning to determine how hydrogen interacts with native passivating surface oxides and nucleates new undesired phases, shedding new light on the critical role of grain boundaries, interfaces, and atomically disordered regions. For aqueous corrosion, the project demonstrated methods to predict dissolution rates of metal surfaces in corrosive solutions, to measure and understand microstructural and grain orientation effects on corrosion susceptibility, and to investigate competing growth and dissolution kinetics of surface oxides. For additively manufactured metals, analysis using state-of-the-art microscopy techniques revealed the role of specific heterogeneities invoked during laser processing, including cellular structure, dislocations, and precipitates, on corrosion susceptibility. In addition to new capabilities and understanding, the project provided an avenue for workforce development, as well as key partnerships with stakeholders in corrosion science.

08 HYDROGEN↗

Controlling the corrosion resistance of multi-principal element alloys

Multi-principal element alloys (MPEAs) offer the possibility of many degrees of freedom in the choice of alloying elements to produce either single phase solid solutions or more complex multiphase microstructures. Large ranges of material properties have been observed for MPEAs and mastery of the selection of elements and their compositions can enable novel combinations of properties not possible in traditional alloys. From the aqueous corrosion perspective, optimization of phase stability, control of heterogeneities, passive film identity and its protectiveness, as well as substrate properties such as metal-metal bond strength and activation energy associated with dissolution, can all be controlling factors governed by alloy composition and structure. These factors can mediate the electrochemical reactions controlling spontaneous corrosion. The quest for superior properties based on well-informed element choice is suggested as a path forward guiding MPEA formulations for corrosion performance. However, gaps in fundamental knowledge exist regarding (a) the specific functions of each element, (b) the behavior of elements in unusual combinations, and (c) the formation of complex protective oxides. These issues currently hold back progress in optimization of corrosion properties.

Scully, John R.↗

Corrosion of Commercial Mg–Al Alloys: AZ31B, AM60, and AZ91D

Aqueous corrosion, atmospheric corrosion, and ionic liquid dissolution studies were performed on commercial alloys AZ31B, AM60, and AZ91D and compared with previously reported results for single-phase binary Mg–Al alloys containing similar Al concentrations (αMg-2 at% Al, αMg-5 at% Al, and Mg-8 at% Al). Polarization studies in 0.6 M NaCl were used to characterize the aqueous free corrosion behavior during 20-h free immersion. Accelerated corrosion testing was performed using a rotating-disk electrode which revealed the evolution of an Al-rich mud-cracking and platelet morphology. Atmospheric droplet testing showed rapid pH increases that depended on the Al concentration in the alloy. Time-dependent contact angle measurements showed that the degree of droplet wetting increased during free corrosion by ~50° over 20 h in 0.6 M NaCl. Ionic liquid dissolution studies in 1:2 M choline chloride:urea deep eutectic solvent were performed in order to examine the current-voltage behavior of these alloys in the absence of water and hydrogen reduction. The results of these studies revealed the formation of nanowire corrosion morphologies within a honeycomb lattice structure which we attribute to selective dissolution of Mg via a two-dimensional stepflow process

25 ENERGY STORAGE↗

ISG-2: properties of the second International Simple Glass

Given the importance of glass materials to society, their durability when exposed to aqueous solutions is a critical area for research, particularly for vitrified radioactive wastes. This spurred an international team to fabricate a standardized composition based on waste immobilization glass called the International Simple Glass (ISG), which has been the subject of numerous experimental and computational studies focused on aqueous corrosion resistance. With the original batch of ISG nearly depleted, the international team designed and fabricated a standard glass material, ISG-2, where half the Ca in the original composition was replaced with Mg by mole. This paper presents information on both the ISG-2 composition and a new batch with the same nominal composition as the original ISG, designated ISG-1, including their homogeneity, their physical and thermal properties. The results of static alteration experiments are presented as well to provide a baseline for future aqueous corrosion performance investigations.

36 MATERIALS SCIENCE↗

Estimating Internal Stress of an Alteration Layer Formed on Corroded Boroaluminosilicate Glass through Spectroscopic Ellipsometry Analysis

Aqueous corrosion of glass may result in the formation of an alteration layer in the glass surface of which chemical composition and network structure are different from those of the bulk glass. Since corrosion occurs far below the glass-transition temperature, the alteration layer cannot fully relax to the new structure with the lowest possible energy. Molecular dynamics simulations suggested that such a network will contain highly strained chemical bonds, which can be manifested as a stress in the alteration layer. Common techniques to measure stress in thin films or surface layers were found inadequate for thick monolithic glass samples corroded in water. Here, we explored the use of spectroscopic ellipsometry to test the presence of internal stress in the alteration layer formed by aqueous corrosion of glass. Furthermore, a procedure for analyses of spectroscopic ellipsometry data to determine birefringence in the alteration layer was developed. Findings with the established fitting procedure suggested that a stress builds up in the corroded surface layer of a boroaluminosilicate glass if there is a change in relative humidity, pH, or electrolyte concentration of the environment to which the glass surface is exposed. A similar process may occur in other types of glass, and it may affect the surface properties of corroded glass objects.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗