Calculated heats of formation and combustion of boron compounds (boron, hydrogen, carbon, silicon)
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
In vitro studies using boron-labeled antibodies and elemental boron as neutron target in therapy for tumors and cancer
The relationship between emission properties and sample composition is studied for lanthanum-boron compounds. Specifically, the La-B system is considered between 1400 and 2100 K and between LaB(4.24) and LaB(29.2) to determine the phase relationship, chemical activity of the compounds, vapor composition, and vaporization rate. The results indicate that: (1) a blue-colored phase near LaB(9) exists between a purple-colored LaB(6) and elemental boron, (2) vaporization is sufficiently more rapid than diffusion so that great compositional differences exist between the surface and the interior, (3) an activation energy lowers the boron vaporization rate from LaB(6), and (4) a steady-state surface composition between LaB(6.04) and LaB(6.07) exists for freely vaporizing materials as a function of interior composition, purity, and temperature. It is noted that the ultimate life of a thermionic diode is governed by electrode vaporization rate whereas efficiency is governed by the electrode work function.
Thermostability and heat sink capacity of diborane, pentaborane, and ethyl decaborane fuels for jet aircraft
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Boron-arsenic and boron-phosphorus films have been grown on Si sapphire and silicon-on-sapphire (SOS) by pyrolyzing Group 3 alkyls of boron, i.e., trimethylborane (TMB) and triethylborane (TEB), in the presence of AsH3 and PH3, respectively, in an H2 atmosphere. No evidence for reaction between the alkyls and the hydrides on mixing at room temperature was found. However, the films were predominantly amorphous. The film growth rate was found to depend on the concentration of alkyl boron compound and was essentially constant when TEB and AsH3 were pyrolyzed over the temperature range 550 C to 900 C. The films were found to contain mainly carbon impurities (the amount varying with growth temperature), some oxygen, and were highly stressed and bowed on Si substrates, with some crazing evident in thin (2 micron) B-P and thick (5 micron) B-As films. The carbon level was generally higher in films grown using TEB as the boron source. Films grown from PH3 and TMB showed a higher carbon content than those grown from AsH3 and TMB. Based on their B/As and B/P ratios, films with nominal compositions B sub12-16 As2 and B sub1.1-1.3 P were grown using TMB as the boron source.
A silicon carbide powder of a 5-micron grain size is mixed with 0.15 to 0.60 wt% mixture of a boron compound, i.e., boric acid, boron carbide (B4C), silicon boride (SiB4 or SiB6), aluminum boride, etc., and an aluminum compound, i.e., aluminum, aluminum oxide, aluminum hydroxide, aluminum carbide, etc., or aluminum boride (AlB2) alone, in such a proportion that the boron/aluminum atomic ratio in the sintered body becomes 0.05 to 0.25 wt% and 0.05 to 0.40 wt%, respectively, together with a carbonaceous additive to supply enough carbon to convert oxygen accompanying raw materials and additives into carbon monoxide.
The MOCVD growth of B-As and B-P films on Si, sapphire, and Si-on-sapphire substrates is described; in this process, trimethylborane (TMB) or triethylborane (TEB) is pyrolyzed in the presence of AsH3 or PH3 in an H2 atmosphere. The procedures employed are outlined, and the results are presented in graphs, tables, and micrographs. It is found that the growth rate of the primarily amorphous films is dependent on the TMB or TEB concentration but approximately constant for TEB and AsH3 at 550-900 C. The nominal compositions of films grown using TMB are given as B(12-16)As2 and B(1-1.3)P. Carbon impurities and significant stress, bowing, and crazing are observed in the films grown on Si substrates, with the highest carbon content in the films grown from TMB and PH3.
Explore the source record for details and available documents.
Absorption bands and localized vibrational modes of silicon doped with boron compounds containing phosphorus, arsenic, antimony, or lithium
Addition of boron compound to lower burning rate of solid propellant binder is reported. Chemical reactions involved in propellant binder modification are described. Advantages of method for lowering burning rate are analyzed.
Fiber burnout process yields low densities. Low density attained by process of sacrificial burnout. Graphite or carbon fibers mixed into slurry of silica, alumina, and boron-compound fibers in amounts ranging from 25 to 75 percent of total fiber content by weight. Mixture formed into blocks and dried. Blocks placed in kiln and heated to 1,600 degrees F(870 degrees C) for several hours. Graphite or carbon fibers slowly oxidize away, leaving voids and reducing block density. Finally, blocks heated to 2,350 degrees F (1,290 degrees C) for 90 minutes to bond remaining ceramic fibers together. Developed for use on Space Shuttle and other spacecraft, rigid insulation machined to requisite shape and bonded in place.
Addition of small amount of soluble, organic boron compound to matrix precursor of carbon-fiber/carbon-matrix (carbon/carbon) composite increases strength and toughness of composite. Compound catalyzes graphitization of matrix, giving rise to greater degree of graphitization at lower processing temperature. Technique used to advantage in carbon/carbon materials requiring lower temperature processing, such as those with inhibited matrices or materials sensitive to changes in fiber properties.
A Silicon carbide-silicon matrix composite having improved oxidation resistance at high temperatures in dry or water-containing environments is provided. A method is given for sealing matrix cracks in situ in melt infiltrated silicon carbide-silicon matrix composites. The composite cracks are sealed by the addition of various additives, such as boron compounds, into the melt infiltrated silicon carbide-silicon matrix.
A Silicon carbide-silicon matrix composite having improved oxidation resistance at high temperatures in dry or water-containing environments is provided. A method is given for sealing matrix cracks in situ in melt infiltrated silicon carbide-silicon matrix composites. The composite cracks are sealed by the addition of various additives, such as boron compounds, into the melt infiltrated silicon carbide-silicon matrix.
Modern aspects and developments in chemistry of fluorine and fluorinated compounds
Small additions of boron were shown to improve the room temperature ductility of the intermetallic compound Ni3Al. Boron is believed to segregate to the gain boundaries and strengthen them, allowing the inheret ductility of the grains to be achieved. The present study was undertaken to see if boron has a similar effect on the low temperature tensile properties of the equiatomic intermetallic compound FeAl. A binary alloy without boron is compared with an alloy containing 0.78 at % B (0.2 wt %) B, by tensile testing over the temperature range of 300 K to 640 K. Both alloys were processed by powder metallurgy. Results showed that 0.78 at % B addition to FeAl does indeed change the room temperature fracture mode from intergranular to transgranular, suggesting a strengthening of grain boundaries. The alloy containing boron is, however, still brittle at room temperature. A slight decrease in the ductile to brittle transition temperature is, nevertheless, observed. In addition a significant increase in strength of the alloy is observed with boron addition.