At least 19 records

Properties of Cd 0.90-x Mn x Zn 0.10 Te (x = 0.10, 0.20) crystals grown by Vertical Bridgman method

Here, in this paper, correlation between CMZT melt state and structure properties of crystals, grown by vertical Bridgman method, was investigated. The Cd 0.9-x Mn x Zn 0.1 Te crystals with various Mn composition (x = 0.1; 0.2) were grown by two-step preparation method from high purity elemental components. We have conducted series of crystal growth runs with different melt superheating degree over the alloys melting temperature. As a result, we have got the ingots with various crystalline structures and properties. It was concluded that worth crystalline structure had the bulks which were grown from the melt with lowest superheating degree. Lastly, we have determined also that band gap rose (from 1.67 at x=0.1 to 1.79 eV at x=0.2) with Mn content increasing.

36 MATERIALS SCIENCE↗

Modelling of the dynamics of HgCdTe growth by the vertical Bridgman method

The analysis of Kim and Brown (1989), which described the pseudo-steady state of the HgCdTe melt/crystal system grown by the vertical Bridgman method, is extended to the study of the transients during the crystal growth and, in particular, at the beginning of the growth. The time-dependent numerical simulations developed show the development of a diffusion layer in the melt and the direct relationship between this layer and the intensity and the pattern of convection in the melt. It is shown that the spread of the solute layer occurs on a diffusive time scale, with the initial transient to the steady-state growth rate lasting several hours for the slow growth rates that are typical of the HgCdTe growth. The simulations demonstrate all the features observed experimentally by Szofran et al. (1984).

Kim, Do H.↗

Models for convection and segregation in the growth of HgCdTe by the vertical Bridgman method

Transport processes in the vertical Bridgman growth of Hg(1-x)Cd(x)Te were investigated by numerical analysis of an idealized quasi-steady-state model of this system. The analysis was specifically directed at an explanation for the radial and axial segregation data obtained by Szofran and Lehoczky (1984) and Szofran et al. (1984) on this system, who reported, respectively, on the observations of diffusion-controlled axial segregation and on the presence of large compositional nonuniformities of CdTe across the radius of the crystal. It is shown that the data sets of these groups can be explained by the results of a detailed analysis of heat transfer, convection, and species transport which account for thermosolutal convection in the melt and for heat transfer mechanisms that dominate the HgCdTe alloy. Predictions from this analysis is applicable to the growth of other materials, because they suggest conditions for the growth of radially uniform crystals with nearly constant axial composition profiles.

Kim, Do Hyun↗

Crystal Defects in CdZnTe Crystals Grown by the Modified Low-Pressure Bridgman Method

Cadmium Zinc Telluride (CZT) is among the most promising materials for room-temperature X- and gamma-ray detectors. However, crystal defects such as Te inclusions and subgrain boundaries significantly hamper their performances. In this work, we evaluated CZT crystals grown by the modified low-pressure Bridgman technique at the IMEM Institute, Parma. We characterized the crystals by IR microscopy to identify the sizes and concentrations of the Te inclusions, along with high spatial resolution X-ray response mapping to measure the uniformity of their charge-transport properties. In addition, we employed white X-ray beam diffraction topography to analyze their crystalline structure.

36 MATERIALS SCIENCE↗

Detailed Studies of Pixelated CZT Detectors Grown with the Modified Horizontal Bridgman Method

The detector material Cadmium Zinc Telluride (CZT) achieves excellent spatial resolution and good energy resolution over a broad energy range, several keV up to some MeV. Presently, there are two main methods to grow CZT crystals, the Modified High-Pressure Bridgman (MHB) and the High-Pressure Bridgman (HPB) process. The study presented in this paper is based on MHB CZT substrates from the company Orbotech Medical Solutions Ltd. [Orbotech Medical Solutions Ltd., 10 Plaut St., Park Rabin, P.O. Box 2489, Rehovot, Israel, 76124]. Former studies have shown that high-work-function materials on the cathode side reduce the leakage current and, therefore, improve the energy resolution at lower energies. None of the studies have emphasized on the anode contact material. Therefore, we present in this paper the result of a detailed study in which for the first time the cathode material was kept constant and the anode material was varied. We used four different anode materials: Indium, Titanium, Chromium and Gold, metals with work-functions between 4.1 eV and 5.1 eV. The detector size was 2.0 x 2.0 x 0.5 cu cm with 8 x 8 pixels and a pitch of 2.46 mm. The best performance was achieved with the low-work-function materials Indium and Titanium with energy resolutions of 2.0 keV (at 59 keV) and 1.9 keV (at 122 keV) for Titanium and 2.1 keV (at 59 keV) and 2.9 keV (at 122 keV) for Indium. Taking into account the large pixel pitch of 2.46 mm, these resolutions are very competitive in comparison to those achieved with detectors made of material produced with the more expensive conventional HPB method. We present a detailed comparison of our detector response with 3D simulations. The latter comparisons allow us to determine the mobility-lifetime-products (mu tau-products) for electrons and holes. Finally, we evaluated the temperature dependency of the detector performance and ls-products. For many applications temperature dependence is important, therefore, we extended the scope of our study to temperatures as low as -30 C. There are two important results. The breakdown voltage increases with decreasing temperature, and electron mobility-lifetime-product decreases by about 30% over a range from 20 C to -30 C. The latter effect causes the energy resolution to deteriorate, but the concomitantly increasing breakdown voltage makes it possible to increase the applied bias voltage and restore the full performance

Jung, I.↗

High-temperature treatment of In-doped CZT crystals grown by the high-pressure Bridgman method

We evaluated the effect of high-temperature treatment of Cd0.9Zn0.1Te:In single crystals using Hall-effect measurements, medium- and high-temperature annealing under various deviations from stoichiometry, and infra-red (IR) transmission microscopy Annealing at ~730 K sharply increased the electrical conductivity (by ~1-2 orders-of-magnitude). Plots of the temperature- and cadmium-pressure dependences of the electrical conductivity, carrier concentration, and mobility were obtained. Treating previously annealed Cd-samples under a Te overpressure at 1070 K allowed us to restore their resistance to its initial high values. The main difference in comparing this material with CdTe was its lowered electron density. We explained our results within the framework of Kröger’s theory of quasi-chemical reactions between point defects in solids.

60 APPLIED LIFE SCIENCES↗

Growth of new materials for solid state laser applications. The growth of ZnGeP2 by the vertical Bridgman method

This is the final technical report on the cooperative NASA program 'Growth of New Materials for Solid State Laser Applications,' covering the period from 9-1-86 through 3-31-91. The first two and one half years of the program, from 9-1-86 through 3-31-89, was devoted to the development of new eye-safe laser sources. Single crystal fibers of rare earth doped and co-doped YAG were grown by the laser-heated pedestal growth method, characterized for their structural properties and supplied to NASA/Langley for spectroscopic evaluation. From 4-1-89 though 3-31-91, research focused on the growth of zinc germanium phosphide for nonlinear optical applications in the IR. The vertical Bridgman growth process was evaluated as a means to achieve better control over the short wavelength optical absorption in this material that adversely affects 2 micron-pumped optical parametric oscillators.

Feigelson, R. S.↗

Growth experiment of narrow band-gap semiconductor PbSnTe single crystals in space (M-1)

An experiment on crystal growth of Pb(1-x)Sn(x)Te in microgravity is planned. This material is an alloy of the compound semiconductors PbTe and SnTe. It is a promising material for infrared diode lasers and detectors in the wavelength region between 6 and 30 micron. Since the electrical properties of Pb(1-x)Sn(x)Te depend greatly on the Pb/Sn ratio and crystalline defects as well as impurity concentration, homogeneous, defect-free, high-quality crystals are anticipated. Although many growth methods, such as the pulling method, the Bridgman method, the vapor growth method, etc., have been applied to the growth of Pb(1-x)Sn(x)Te, large, homogeneous, low-defect-density crystals have not yet been grown on Earth. The unsuccessful results were caused by buoyancy-driven convection in the fluids induced by the specific gravity difference between heated and cooled fluids on Earth. A crystal is grown by cooling the melt from one end of the ampoule. In crystal growth from the melt, about 30 percent of the SnTe in the melt is rejected at the solid-liquid interface during solidification. On Earth, the rejected SnTe is completely mixed with the remaining melt by convection in the melt. Therefore, SnTe concentration in the melt, and accordingly in the crystal, increases as the crystal grows. In the microgravity environment, buoyancy-driven convection is suppressed because the specific gravity difference is negligible. In that case, the rejected SnTe remains at the solid-liquid interface and its concentration increases only at the interface. If the growth rate is higher than the PbTe-SnTe interdiffusion rate, the amount of SnTe which diffuses from the interface into the melt increases as SnTe piles up at the interface, and finally it balances the amount of rejected SnTe during solidification, resulting in steady-state SnTe transportation at the interface. By using this principle, compositionally homogeneous crystals can be grown. Furthermore, low-defect-density crystals will be grown in microgravity, because convection causes crystalline defects by mising hot and cold fluids and generating temperature fluctuations in them.

Yamada, Tomoaki↗

Charge transport properties in CdZnTe detectors grown by the vertical Bridgman technique

Presently, a great amount of effort is being devoted to the development of CdTe and CdZnTe (CZT) detectors for a large variety of applications such as medical, industrial, and space research. We present the spectroscopic properties of some CZT crystals grown by the standard vertical Bridgman method and by the boron oxide encapsulated vertical Bridgman method, which has been recently implemented at IMEM-CNR (Parma, Italy). In this technique, the crystal is grown in an open quartz crucible fully encapsulated by a thin layer of liquid boron oxide. This method prevents contact between the crystal and the crucible, thereby allowing larger single grains with a lower dislocation density to be obtained. Several mono-electrode detectors were realized, with each having two planar gold contacts. The samples are characterized by an active area of about 7 mm x 7 mm and thicknesses ranging from 1 to 2 mm. The charge transport properties of the detectors have been studied by mobility-lifetime ({mu} x {tau}) product measurements, carried out at the European Synchrotron Radiation Facility (Grenoble, France) in the planar transverse field configuration, where the impinging beam direction is orthogonal to the collecting electric field. We have performed several fine scans between the electrodes with a beam spot of 10 {mu}m x 10 {mu}m at various energies from 60 to 400 keV. In this work, we present the test results in terms of the ({mu} x {tau}) product of both charge carriers.

36 MATERIALS SCIENCE↗

Bridgman growth of large-aperture yttrium calcium oxyborate crystal

Highlights: ► YCOB is a novel non-linear optical crystal possessing good thermal, mechanical and nonlinear optical properties. ► Large size crystal growth is key technology question for YCOB crystal. ► YCOB crystals 3 in. in diameter were grown with modified vertical Bridgman method. ► It is a more effective growth method to obtain large size and high quality YCOB crystal. -- Abstract: Large-aperture yttrium calcium oxyborate YCa{sub 4}O(BO{sub 3}){sub 3} (YCOB) crystals with 3 in. in diameter were grown with modified vertical Bridgman method, and the large crystal plate (63 mm × 68 mm × 20 mm) was harvested for high-average power frequency conversion system. The crack, facet growth and spiral growth can be effectively controlled in the as-grown crystal, and Bridgman method displays more effective in obtain large size and high quality YCOB crystal plate than Czochralski technique.

36 MATERIALS SCIENCE↗

Passive particle dosimetry

Present methods of dosimetry are reviewed with emphasis on the processes using silver chloride crystals for ionizing particle dosimetry. Differences between the ability of various crystals to record ionizing particle paths are directly related to impurities in the range of a few ppm (parts per million). To understand the roles of these impurities in the process, a method for consistent production of high purity silver chloride, and silver bromide was developed which yields silver halides with detectable impurity content less than 1 ppm. This high purity silver chloride was used in growing crystals with controlled doping. Crystals were grown by both the Czochalski method and the Bridgman method, and the Bridgman grown crystals were used for the experiments discussed. The distribution coefficients of ten divalent cations were determined for the Bridgman crystals. The best dosimeters were made with silver chloride crystals containing 5 to 10 ppm of lead; other impurities tested did not produce proper dosimeters.

Childs, C. B.↗

Growth of Bi doped cadmium zinc telluride single crystals by Bridgman oscillation method and its structural, optical, and electrical analyses

The II-VI compound semiconductor cadmium zinc telluride (CZT) is very useful for room temperature radiation detection applications. In the present research, we have successfully grown Bi doped CZT single crystals with two different zinc concentrations (8 and 14 at. %) by the Bridgman oscillation method, in which one experiment has been carried out with a platinum (Pt) tube as the ampoule support. Pt also acts as a cold finger and reduces the growth velocity and enhances crystalline perfection. The grown single crystals have been studied with different analysis methods. The stoichiometry was confirmed by energy dispersive by x-ray and inductively coupled plasma mass spectroscopy analyses and it was found there is no incorporation of impurities in the grown crystal. The presence of Cd and Te vacancies was determined by cathodoluminescence studies. Electrical properties were assessed by I-V analysis and indicated higher resistive value (8.53x10{sup 8} {Omega} cm) for the crystal grown with higher zinc concentration (with Cd excess) compare to the other (3.71x10{sup 5} {Omega} cm).

36 MATERIALS SCIENCE↗

ZnTeO{sub 3} crystal growth by a modified Bridgman technique

Highlights: • ZnTeO{sub 3} single crystals were grown for the first time by a modified Bridgman method. • The growth is still possible in a system that lacks congruent melting. • A growth is best when melt is exposed to a steeper axial thermal gradient. • Optical and electrical properties were investigated for the grown crystals. - Abstract: Zinc Tellurite (ZnTeO{sub 3}) crystals were grown for the first time using a modified Bridgman method with a 2.5 kHz radio frequency (RF) furnace. Single crystal growth of ZnTeO{sub 3} was hindered by many complicating factors, such as the evaporation of TeO{sub 2} above 700 °C and the formation of more than one phase during crystal growth. While there were several successful runs that produced ZnTeO{sub 3} single crystals, it was found that large (≥10 cm{sup 3}) single ZnTeO{sub 3} crystals resulted when the crucible was exposed to a steeper vertical thermal gradient and when the temperature of the melt was raised to at least 860 °C. The results of powder X-ray diffraction (XRD) patterns were in accordance with the X-ray powder diffraction file (PDF) for ZnTeO{sub 3}. Some optical, electrical and structural properties of ZnTeO{sub 3} single crystals were reported in this paper.

36 MATERIALS SCIENCE↗