Fluorescent aggregate structure revealed in bisphenol F epoxy thermoset

Bisphenol F (BPF) epoxy resin is a prepolymer component of thermosets used in construction of reinforced carbon fiber composites (RCFC). The fluorescence of this resin can provide information about chemical and structural alterations of the thermoset from thermal or mechanical damage. While some work has investigated the fluorescence spectra of bisphenol A epoxy resin, a structural analog of BPF, none have studied BPF. The purpose of this study is to investigate the baseline fluorescence spectra of the BPF epoxy resin for features that could be utilized for monitoring damage and structural alterations. Bisphenol F epoxy resin was found to have two emission peaks with a broad peak centered at 410 nm and a sharp peak centered at 550 nm. The broad emission peak was identified as the fluorescence from BPF epoxy monomer while the sharp emission peak was found to be from an aggregate structure present in the epoxy resin. It is hypothesized that this structure is an H-aggregate based on the emission features and structural stability of the aggregate compared to the alternative J-aggregate which was determined via density functional theory calculations. The H-aggregate was found to persist into one of the cured thermoset formulations evaluated but was lost when exposed to elevated temperatures below thermal degradation of the thermoset. This loss of aggregate structure was due to polymer network rearrangement. This new fluorescence signature can be used as an indicator of polymer network rearrangement from thermal exposure which may alter the expected material performance and precede thermal degradation.

36 MATERIALS SCIENCE↗

Regioisomer-Specific Crystallization of Diglycidyl Ether of Bisphenol F Epoxy Resin

Diglycidyl ether of bisphenol F (DGEBF) is a common industrial epoxy resin, desired for its possible replacement of the bisphenol A (BPA) analogue DGEBA due to potential health hazards of BPA. During curing, crystallization of the DGEBF resin can cause inaccurate resin-to-hardener ratios, resulting in incomplete crosslinking; therefore, understanding the crystallization of DGEBF is important for proper industrial control of the material. Here, in this work, we utilized a combination of single-crystal x-ray diffraction, Raman spectroscopy, and 1 H-NMR to investigate the crystallization of DGEBF. We observed crystallization of two DGEBF regioisomers: ortho-ortho’-DGEBF and ortho-para’-DGEBF, and report their crystal structures. Notably, para-para’-DGEBF crystallization is not observed, indicating crystallization of this regioisomer does not occur under ambient conditions. Density functional theory calculations were performed to describe the phonon modes of the ortho-ortho’- and ortho-para’-DGEBF structures, corroborating Raman signatures for the respective isomers. Using a phonon mode analysis, we identify the presence of three specific optical vibrational modes at 631.3, 344.1, and 345.6 cm -1 that are unique to the para monomer. This work offers insights into the crystallization behavior of DGEBF resins under ambient conditions and may inform potential industrial application of this material.

Neu, Jennifer [Oak Ridge National Laboratory (ORNL↗

Product specific thermal degradation kinetics of bisphenol F epoxy in inert and oxidative atmospheres using evolved gas analysis–mass spectrometry

Knowledge of the degradation kinetics for polymer materials is important for understanding thermal stability. In this study, evolved gas analysis–mass spectrometry and pyrolysis gas-chromatography-mass spectrometry were evaluated for the potential to deliver additional insight into thermal degradation kinetics of diglycidal ether of bisphenol F (DGEBF) epoxy thermoset under inert and oxidative atmospheres. Degradation products of selected precursor ions were evaluated for their uniqueness to the specific precursor using extracted ion thermographs. Unique mass peaks, solely attributed to a single reaction pathway of a specific product, were determined from extracted ion thermographs and used to determine both activation energy (E a ) and pre-exponential factors for the specific primary reaction pathways. These primary reaction pathways for DGEBF epoxy degradation were then evaluated in the context of transition state theory (TST) and related transition state enthalpies (ΔH ‡ ) and entropies (ΔS ‡ ) of activation to further elucidate the degradation process. It was determined under pyrolysis conditions, as suggested by the E a , the formation of bisphenol F monomer was the rate-limiting step toward the formation of xanthene and phenol. In contrast, under thermo-oxidative conditions, reactions involving oxygen containing species were identified as the rate-limiting step for all observed products based on the large negative ΔS ‡ calculated from TST. This work demonstrates a powerful combination of technique and theory that can provide new insight into the degradation of polymer materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Influence of temperature on accessible pyrolysis pathways of homopolymerized bisphenol A/F epoxies and copolymers

Understanding the thermal pyrolysis of epoxies and their copolymers is important for identifying structural changes resultant from thermal transients, enabling identification of failure modes of high-performance composite materials. This work expands our understanding of the thermal pyrolysis of cured epoxies and the role of temperature and composition on products, pathways, and relative rates. Numerous researchers have explored the pyrolysis of bisphenol A (BPA) epoxy. Significantly fewer have studied bisphenol F (BPF), and copolymers of BPA and BPF have been neglected. In this work, a pyrolysis gas chromatography mass spectrometer (PY-GC-MS) was used to investigate the degradation mechanism of homopolymerized BPA, BPF epoxies and their copolymers. Additionally, for polymer identification, pyrolysis >450 °C resulted in the most extensive fragmentation and is useful for material identification, though lower temperatures show different degradation product profiles that provide mechanistic insight into thermal degradation pathways. Temperature greatly influences the accessible pyrolysis pathways of BPA, revealing dual mechanisms of formation for products p-isopropylphenol and p-isopropenylphenol. For BPF at low pyrolysis temperature the p,p-bisphenol F isomer is produced at significantly lower relative abundance compared to the abundance at higher temperatures tested, but production of the other two isomers changes little with respect to temperature. This suggests the epoxy components consisting of the p,p-bisphenol F isomer have higher thermal stability. Overall, the copolymer epoxies were found to have similar degradation products in stoichiometric distributions. The major exception was the formation of the p,p-bisphenol F isomer, which shows evidence of thermal stabilizing effects from addition of BPA epoxy.

36 MATERIALS SCIENCE↗

Product-specific kinetics reveal effect of epoxy crystallization on thermoset thermal degradation

Crystallization is a common problem for epoxy resins, which are ubiquitous in industrial and commercial use. Integration of crystallized epoxy monomers into cured thermosets has been shown to alter the thermosets’ final mechanical properties. However, no studies have investigated the impact of these crystals on the thermal stability of the thermoset. Here we investigate the degradation kinetics of a bisphenol F–based epoxy thermoset with and without crystallized monomers using Product-Specific Kinetic (PSK) analysis coupled with Evolved Gas Analysis-Mass Spectrometry (EGA-MS). PSK analysis revealed significant differences in evolved product ion kinetics, suggesting changes in the degradation kinetics between thermoset configurations. Further, it was concluded that early stages of degradation are influenced most by crystal presence due to the high concentration of unreacted epoxy monomers and lower cross-linking density of the cured network. After post-cure annealing, significant changes are observed in the degradation kinetics of thermosets without crystal inclusions. Conversely, post-cure annealing procedures of crystal integrated thermosets showed little change in the thermoset degradation kinetics across all conversion extents. These findings suggest that post-cure annealing of thermosets with crystals present at the onset does not alter the cross-linking density of the polymer network enough to significantly change the degradation kinetics. We hypothesize this is because the excess monomers from the melted crystals are unable to find suitable reaction sites for complete binding into the polymer network, which has direct implications for the material properties and final thermal stability of the thermoset.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Acid external and internal environment exchange the Oreochromis niloticus tissue immune gene expression compared to the mouse macrophage polarization model

The water environment plays an important role in animal physiology. In this study, we sought to evaluate the effect of the acid environment on the Oreochromis niloticus (Nile tilapia) internal microenvironment immune response compare to the mouse macrophage model (J77A.1). The acid environment treated mouse macrophage J774A.1 model have shown that acidic treatment is able to polarize macrophages into M2-like macrophages via an increase in Ym1, Tgm2, Arg1, Fizz1, and IL-10 expression. Metabolic analysis of mouse macrophages (J774A.1) at pH 2 vs. pH 7 and pH 4 vs. pH 7 have been shown to promote the expression of intracellular acetylcholine, choline, prochlorperazine, L-leucine, and bisphenol A,2-amino-3-methylimidazo[4,5-f] quinolone metabolites in the M2-like macrophage. Immune gene expression of the O. niloticus spleen and liver treated at pH 2, 4, and 7 was shown to reduce TNF-α, IL-1 β, IL-8, and IL-12 expression compared to pH 7 treatment. Immune gene was induced in O. niloticus following culture at pH 5, 6, and 7 fresh water environment. Taken together, we found that the acid internal environment polarizes tissues into an M2 macrophage developmental microenvironment. However, if the external environment is acid, tissues are exposed to an M1 macrophage developmental microenvironment.

59 BASIC BIOLOGICAL SCIENCES↗