Search NASA⌕ Search

SEARCH · Search NASA

Results for “Boride”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Dry Sliding Wear Resistance of Cobalt Boride Coatings Formed on ASTM F1537 Alloy

New results about the wear resistance of CoB-Co{sub 2}B coatings under dry sliding conditions were estimated in this work. The cobalt boride coatings were developed at the surface of the ASTM F1537 alloy by means of the powder-pack boriding process using two experimental conditions: 1223 K with 6 h of exposure and 1273 K with 10 h of exposure. Before the sliding wear tests, Vickers depth-sensing microindentation tests were conducted on the cross section of the cobalt boride coatings to estimate the distribution of hardness, Young’s modulus, and residual stresses. Otherwise, the sliding wear tests were performed on both boriding conditions and on the untreated material, using a ball-on-flat configuration comprised of an alumina ball as a counterpart with applied loads between 5 and 20 N. The wear rates of the borided ASTM F1537 alloy were ranged between 4.02 and 8.91 × 10{sup −6} mm{sup 3} N{sup −1} m{sup −1} compared with the values of the untreated material (13.90 and 15.78 × 10{sup −6} mm{sup 3} N{sup −1} m{sup −1}) for the overall set of experimental conditions; nevertheless, the influence of boriding conditions (1273 K with 10 h of exposure) tended to increase the CoB coating thickness, developing a more brittle layer that decreased the sliding wear resistance at the surface of the borided ASTM F1537 alloy. Finally, the presence of failure mechanisms on the surface of the wear tracks was analyzed for both borided ASTM F1537 alloy and untreated material.

36 MATERIALS SCIENCE↗

Single crystal studies on Co-containing {tau}-borides Co{sub 23-x}M{sub x}B{sub 6} (M=Al, Ga, Sn, Ti, V, Ir) and the boron-rich {tau}-boride Co{sub 12.3}Ir{sub 8.9}B{sub 10.5}

Single crystals of the cubic {tau}-Borides Co{sub 23-x}M{sub x}B{sub 6} (M=Al, Ga, Sn) were synthesised from the elements at temperatures between 1200 and 1500 deg. C. According to the structure refinements one (Ga, Sn: 8c) or two (Al: 4a and 8c) of the four independent metal sites show a mixed occupation Co/M resulting in the compositions Co{sub 20.9}Al{sub 2.1}B{sub 6}, Co{sub 21.9}Ga{sub 1.1}B{sub 6}, and Co{sub 21.4}Sn{sub 1.6}B{sub 6}, respectively. Melts with Indium gave access to Co{sub 23}B{sub 6} as the first binary {tau}-boride (Fm3-barm,a=10.4618(13) A, 104 refl., 14 param., R{sub 1}(F)=0.0132, wR{sub 2}(F{sup 2})=0.0210). With M=Ir mixed occupations occur for all sites and the boron content varies. The composition for the boron-poor single crystal was Co{sub 16.2}Ir{sub 6.8}B{sub 6}. A higher Ir-content enables the uptake of additional boron resulting in a composition Co{sub 12.3}Ir{sub 8.9}B{sub 10.5}. This can be explained be the substitution of metal atoms on the 8c-site by B{sub 4}-tetrahedra. A boron-rich phase was observed for the first time for a {tau}-boride of cobalt. All compositions were confirmed by EDX measurements. - Graphical Abstract: Single crystal investigations on {tau}-borides Co/M/B with M = Al, Ga, In, Sn, V, Ti, Ir explained the substitution processes. Furthermore the yielded the first binary boride, Co{sub 23}B{sub 6}, and a boron-rich Co{sub 12.3}Ir{sub 8.9}B{sub 10.5} containing B{sub 4}-tetrahedra.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Pack-boriding of Fe-Mn binary alloys: Characterization and kinetics of the boride layers

In this work, the boronizing of Fe-Mn binary alloys at 0.42, 0.76 and 0.94 wt.% Mn was carried out in a solid medium using the powder pack method. In this method, commercial Ekabor-II boron source and activator (ferro-silicon) were thoroughly mixed to form the boriding medium. The samples were boronized in an electrical resistance furnace for exposure times of 2, 4, 6 and 8 h at 1173 K under atmospheric pressure and a series of boronized samples in the temperature range 1073-1373 K for 3 h. After the furnace process, boronized samples were removed from the furnace and cooled in air. Afterwards, the boride layers generated by the pack-boronizing process were characterized by optical microscopy, scanning electron microscopy, XRD analysis, Vickers microhardness and tensile testing. The generated boride layers, showing a saw-tooth morphology, had a surface microhardness in the range 1400-1270 HV0.1. It was shown that the values of yield stresses and ultimate tensile stresses were increased as the Mn content increases in the boronized Fe-Mn binary alloys. In contrast, the values of elongations determined from the stress-strain curves were decreased. Furthermore, it was found that the calculated mean value of the activation energy of boron diffusion was close to 119 J/mol.

36 MATERIALS SCIENCE↗

Microstructural characterization of as-fabricated monolithic plates with boron carbide, aluminum boride, and zirconium boride burnable absorbers

The use of burnable absorbers can be beneficial for nuclear reactors by extending the fuel’s operational cycle, providing additional criticality control, and flattening the power profile. In this work, three burnable absorber materials (boron carbide, aluminum boride, and zirconium boride) embedded in aluminum have been fabricated into foils and clad in AA-6061 for potential use in high performance research reactors. The as-fabricated boron-containing phases were determined using transmission electron microscopy to be AlB2, B4C, and ZrB2. TEM also revealed weak bonding at the B4C-matrix interface. SEM showed a relatively uniform spatial distribution of boron-containing phases for all the candidate materials. Higher porosity was observed in the foil containing ZrB2 in its as-rolled condition. The porosity in the ZrB2 foil was reduced by hot isostatic pressing. The size and shape distributions of the boron-containing phases were analyzed on the criteria of cross-sectional area, perimeter, roundness, circularity, and aspect ratio. A method of converting the 2D burnable absorber dispersoids seen in cross-sectional microscopy images into 3D volumes was derived using both spherical and ellipsoidal geometry models. The difference in calculated burnable absorber dispersoid average volume between the two models ranges from 20% to 100%, which could impact burnable absorber burnout rates due to differences in neutron self-shielding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Predicting the ground-state structure of sodium boride

Binary borides has been a subject of extensive research. However, the exact compositions and crystal structures of sodium borides remained controversial. Furthermore, using the ab initio variable-composition evolutionary algorithm, a new stable Na 2 B 30 with I2 1 2 1 2 1 symmetry (I2 1 2 1 2 1 –Na 2 B 30 ) is found, which is –7.38 meV / atom lower in energy than the Imma–Na 2 B 30 structure reported by experimentalists. Interestingly, the Imma–Na 2 B 30 structure is predicted to be a topological nodal line semimetal, which may result in superior electronic transport. In contrast, I2 1 2 1 2 1 –Na 2 B 30 is an ultrahard semiconductor with an unprecedented open-framework structure, whose interstitial helical boron sublattice enhances its hardness and energetic stability.

36 MATERIALS SCIENCE↗

Compressibility and strength of nanocrystalline tungsten boride under compression to 60 GPa

The compression behavior and stress state of nanocrystalline tungsten boride (WB) were investigated using radial x-ray diffraction (RXRD) in a diamond-anvil cell under non-hydrostatic compression up to 60.4 GPa. The compression properties and stress state are analyzed using lattice strain theory. Experiments were conducted at beamline X17C of the National Synchrotron Light Source. The radial x-ray diffraction data yield a bulk modulus that is qualitatively consistent with density functional theory calculations and demonstrate that WB is a highly incompressible material. A maximum differential stress, t, of about 14 GPa can be supported by nanocrystalline WB at the highest pressure. This corresponds to about 5% of the shear modulus, G, which is smaller than the values of t/G ({approx}8%-10%) observed for BC{sub 2}N, B{sub 6}O, TiB{sub 2}, and {gamma}-Si{sub 3}N{sub 4} at high pressures. Thus, while WB is highly incompressible, its strength is relatively low at high pressures compared to other hard ceramics.

36 MATERIALS SCIENCE↗

Ultra-fast Boriding for Improved Energy Efficiency and Reduced Emissions in Materials Processing Industries (Final Report)

High-temperature treatment processes (such as nitriding, carburizing, and boronizing) are well-established and used widely by numerous industrial sectors to achieve superior mechanical and tribological properties on all kinds of engineering components made out of ferrous materials. Unfortunately, these traditional processes are very slow and energy intensive, and they produce large amounts of CO 2 emissions and liquid/solid wastes to deal with during and after each process run. From economic and environmental points of views, it is highly desirable to develop and implement novel surface treatment technologies that are quick, cheap, clean, and energy efficient. The main objective of this project was to develop an industrial-scale ultra-fast boriding process that realizes all of these desirable attributes. The other objectives of the project were to demonstrate the superior performance, properties, and durability of borided surfaces under relevant test conditions and to transfer optimized technology to industry for large-scale practice. Major research activities included process design, modeling, product optimization, and scale-up. This project has achieved all of its stated objectives, and the industrial-scale boriding process has been successfully transferred to industry. Specifically, all of the original tasks have been completed, and the milestones have been met by scaling up from a small proof-of-concept system (which could only handle about 0.25 kg melt) to a commercial-scale boriding unit that can handle up to 4,000 kg melt. Mechanical and tribological testing of borided test samples and industrial parts has also been carried out, and their superior performance over a broad range of test conditions has been validated. With the large-scale, ultra-fast boriding process, we could achieve thick, hard, and uniform boride layers on all kinds of steel components, even after only 5 min of treatment time. We could also attain excellent uniformity in thickness over the entire exposed surfaces — even in the very sharp corners or interior sections of odd-shaped workpieces. Boriding of numerous nonferrous materials was also demonstrated, and thick boride layers (up to 300 µm in thickness) were achieved on their outer surfaces. With the use of a large-scale boriding unit at Argonne National Laboratory, our research team has successfully treated large numbers of industrial components in a batch-to-batch operation without creating any in-house gaseous emissions or producing solid and/or liquid wastes. With the use of this large unit, our team achieved surface hardness values of 15 to 45 GPa, depending on the type of metal or alloy being treated. The thick boride layers attained on steel components consisted of FeB, Fe 2 B, and Fe 3 B phases, and their hardness values ranged from 16 to 22 GPa. Layers consisting of Fe 2 B phase alone are also possible with this process, and in the case of nonferrous materials. Overall, because of the much superior property and performance improvements in treated products, much lower energy consumption, and nearly zero environmental waste and emissions, the demonstrated boriding technology may find broad applications in many cross-cutting industries. Mechanical wear, abrasion, erosion, corrosion, and scuffing are often life-limiting factors in mechanical systems that are used in manufacturing, transportation, aerospace, agricultural, earth-moving, and mining equipment; but the machine components treated by ultra-fast boriding can effectively prevent such degradations. In this project, the ultra-fast boriding was proven to be most ideal for the treatment of iron and many other ferrous alloys, like stainless steel. We have shown through our experimental studies that our method can also be used for the treatment of many nonferrous metals and alloys. In the case of superalloys and Ni 3 Al intermetallic materials, more than a 300-µm thick boride layer can be achieved with our boriding furnace within 15 to 30 min (which results in five times the hardness of the base materials). Pre-carburized steels and nonferrous alloys can also be treated by the new boriding technique. Overall, very thick (more than a quarter millimeter) and hard surface layers produced by ultra-fast boriding are expected to have a positive impact on the performance and durability of all types of machine components that are subject to corrosive, erosive, abrasive, and adhesive wear. Since the focus of our project was primarily on the large-scale boriding of ferrous materials, in this report, we will broadly cover the results from various ferrous materials that were used in our experiments. Another transformational feature of ultra-fast boriding is that it does not create any greenhouse gas emissions or solid and/or liquid wastes to deal with during or after the treatment; hence, it is an ultra-green technology (no need for expensive waste disposal and/or treatment facilities). It may eliminate the use of natural gas and other carbon-based fuels as the primary energy source in the heat treatment industry (which is the most common practice at present), thus, minimizing the CO 2 , NO x , CO, and SO x emissions that are generated in large quantities by current heat treatment practices. The main ingredient used during boriding is borax, which is a natural mineral. Our demonstrated and scaled-up technology can now be used in a wide range of manufacturing and transportation applications. It can deliver thick and uniform boride layers of more than 200 µm in steels, if needed, over the entire exposed surfaces — even in the very sharp corners or interior sections of workpieces (which are typical of gears, tools, pipes, and other components). Beneath the distinct boride layers is an equally-thick boron diffusion layer or zone, which is comparable to the diffusion zones achieved by carburizing and nitriding processes. In the cases of traditional boriding, nitriding, and/or carburizing methods, achieving such layer thickness and case depths would have taken several hours, and these surfaces would not have achieved the same levels of hardness and other desirable properties as they do with ultra-fast boriding. Some of the key stakeholders of ultra-fast boriding technology include companies that are active in heat-treatment, thermal-diffusion, and hard-coating processes; metal-forming, machining, and other manufacturing processes; and technologies related to transportation (including original equipment manufacturers for autos), mining and oil exploration, agricultural and heavy equipment. Bodycote Thermal Processing was the cost-sharing industrial partner and licensee in this project. They also provided test components and technical and commercial information pertaining to industrial components that are most suitable for ultra-fast boriding. Bodycote also coordinated some of the field tests and metallurgical examinations. Overall, ultra-fast boriding is a transformational technology that can complement, if not replace, many of the energy- and carbon-intensive surface treatment processes that are in use today, such as conventional boriding, carburizing, nitriding, carbo-nitriding, and physical and chemical vapor deposition. In our project, the developed technology was scaled-up and proven to be an ultra-green, ultra-efficient process that can drastically reduce costs, increase productivity, and improve the performance and reliability of machine components used in cross-cutting industrial applications.

Erdemir, Ali↗

High-throughput studies of novel magnetic materials in borides

Borides are a versatile material family with various properties for valuable applications. Conventional magnetism, such as ferromagnetism and antiferromagnetism in borides, have been extensively studied. However, research on unconventional magnetism in borides where quantum effects are dominant is scarce. Here, we implement a high-throughput workflow combining first-principles calculations, materials prediction, and magnetic properties calculations to discover novel magnetism and magnetic materials in borides. Successfully applying the workflow, we report three families of novel magnetic borides, including two families of borides exhibiting quantum magnetism. One is a family of dimerized quantum magnets among YCrB 4 -type borides, which provides a rare platform for studying the spin-gap quantum critical point. The other is a family of altermagnets among FeMo2B 2 -type borides, extending the magnetic orderings exhibited by borides beyond conventional ferromagnetism and antiferromagnetism. We also predict a family of magnetic laminate transition metal borides, known as the MAB phases, in the AlFe 2 B 2 -type family, which provide pure-phase or alloying candidates for studying magnetocaloric materials and the associated magnetic transitions. The workflow is expected to be used in further studies of novel magnetism and magnetic materials.

36 MATERIALS SCIENCE↗

Investigation of the fracture mechanics of boride composites

Fracture energies of WC-6Co, Boride 5 (ZrB2+SiC), Boride 8(ZrB2+SiC+C) and Boride 8-M2(ZrB2+SiC+C) were measured by slow bend and impact tests of notched charpy bars. Cobalt bonded tungsten carbide exhibited impact energies of 0.76 ft-lb or 73.9 in-lb/square inch. Boride 5 and the Boride 8 exhibit impact energies one third and one quarter of that observed for WC-6Co comparing favorably with measurements for SiC and Si3N4. Slow bend-notched bar-fracture energies for WC-6Co were near 2.6 in-lb/square inch or 1/20 the impact energies. Slow bend energies for Boride 8-M2, Boride 8 and Boride 5 were 58%, 42% and 25% of the value observed for WC-6Co. Fractograph showed differences for WC-6Co where slow bend testing resulted in smooth transgranular cleavage while samples broken by impact exhibited intergranular failures. By contrast the boride fractures showed no distinction based on testing method. Fabrication studies were conducted to effect alteration of the boride composites by alloying and introduction of graphite cloth.

Kaufman, L.↗

Fracture Toughness of Thick Boride Layers Estimated by the Cross-Sectioned Scratch Test

New results about the fracture toughness (K{sub c}) of thick boride layers estimated by the cross-sectioned scratch test are presented in this study. The FeB-Fe{sub 2}B layers developed at the surface of borided AISI 1018 and AISI 1045 steels and the Fe{sub 2}B layer formed on the borided AISI 1045 steel exposed to a diffusion annealing process (DAP) were used for this purpose. The cross-sectioned scratch tests were performed with a Vickers diamond stylus drawn across the thick boride layer under a constant load to produce a half-cone-shaped fracture near to the top surface of the borided steels. The height of the half-cone-shaped fracture as a function of the cross-sectioned scratch loads was used to determine the fracture toughness of the FeB and Fe{sub 2}B layers. The results showed a fracture resistance of ∼2.8 MPa√m for the FeB layer formed at the surface of borided AISI 1045 steel. Likewise, the effect of the DAP on the surface of the borided AISI 1045 steel promoted the formation of an exclusively Fe{sub 2}B layer, with an increase in the fracture toughness of the whole boride layer around 5 MPa√m. Finally, the principle of the technique can be used to minimize the influence of the anisotropic properties on the fracture toughness along the depth of boride layers.

36 MATERIALS SCIENCE↗

An alternative method of gas boriding applied to the formation of borocarburized layer

The borocarburized layers were produced by tandem diffusion processes: carburizing followed by boriding. An alternative method of gas boriding was proposed. Two-stage gas boronizing in N{sub 2}-H{sub 2}-BCl{sub 3} atmosphere was applied to the formation of iron borides on a carburized substrate. This process consisted in two stages, which were alternately repeated: saturation by boron and diffusion annealing. The microstructure and microhardness of produced layer were compared to those-obtained in case of continuous gas boriding in H{sub 2}-BCl{sub 3} atmosphere, earlier used. The first objective of two-stage boronizing, consisting in acceleration of boron diffusion, has been efficiently implemented. Despite the lower temperature and shorter duration of boronizing, about 1.5 times larger iron borides' zone has been formed on carburized steel. Second objective, the absolute elimination of brittle FeB phase, has failed. However, the amount of FeB phase has been considerably limited. Longer diffusion annealing should provide the boride layer with single-phase microstructure, without FeB phase. - Highlights: Black-Right-Pointing-Pointer Alternative method of gas boriding in H{sub 2}-N{sub 2}-BCl{sub 3} atmosphere was proposed. Black-Right-Pointing-Pointer The process consisted in two stages: saturation by boron and diffusion annealing. Black-Right-Pointing-Pointer These stages of short duration were alternately repeated. Black-Right-Pointing-Pointer The acceleration of boron diffusion was efficiently implemented. Black-Right-Pointing-Pointer The amount of FeB phase in the boride zone was limited.

36 MATERIALS SCIENCE↗

Boride-based Ceramic Super-high Temperature Thermocouples in Harsh Environments (Final Scientific/Technical Report)

An electromotive force (emf) can be generated along a temperature gradient between the cold end and hot end of a thermoelectric material, termed the Seebeck effect. Based on the Seebeck effect, metallic alloys have been extensively employed to detect temperatures for centuries, named thermocouples. However, commercially available thermocouple alloys suffer from limitations, such as oxidation, chemical degradation, and poor long-term stability under high-temperature harsh environments. This DOE-funded project aimed to develop high-temperature, chemically tolerant thermocouples suitable for operation in extreme environments relevant to semiconducting thermoelectric materials. The research focused on boride-based semiconducting thermoelectric compounds as candidates for next-generation thermocouples with enhanced oxidation resistance, chemical stability, and thermal robustness under conditions representative of charcoal-fired electricity facilities. During the funded years, boride materials were synthesized using an arc-plasma technique under ambient air and argon atmospheres, enabling scalable and cost-effective production compared with conventional boride fabrication methods. The synthesized borides were processed into nanostructured powders, followed by consolidation into dense bulk materials using a spark plasma sintering (SPS) bottom-up approach. Comprehensive characterization was performed, including microstructural analysis, electrical transport measurements, and optical and thermal property evaluation. Both p-type and n-type boride electric legs were fabricated and integrated into boride-based thermocouples. The thermal and irradiation stabilities of the boride nanomaterials and bulk thermoelectric materials were systematically evaluated to assess suitability for long-term operation in harsh environments. Additionally, 12 students were broadly hands-on trained spanning the full research workflow, including word processing and technical editing (e.g., LATEX for manuscript and poster preparation), data collection and analysis (using Python and related libraries and hardware interfaces), sample preparation (including arc-plasma synthesis and spark plasma sintering), and advanced characterization techniques (such as X-ray diffraction, UV–vis spectroscopy, electron microscopy, differential thermal analysis (DTA), and Seebeck coefficient measurements, etc). Overall, this project demonstrated the feasibility of boride-based thermoelectric materials as durable high-temperature thermocouples, providing a promising pathway toward robust temperature sensing technologies aligned with DOE energy infrastructure and extreme-environment monitoring needs.

20 FOSSIL-FUELED POWER PLANTS↗