Search NASA⌕ Search

SEARCH · Search NASA

Results for “CASTING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Local Modification of Cast Aluminum Alloys via the Cast-and-Print Process

Casting of aluminum alloys is a cost-effective way to mass manufacture bulk aluminum parts for automotive applications. However, the casting process requires filling of a mold, which imposes some limitations on the geometries that can be successfully cast and limits parts to be a uniform material. Therefore, we proposed that a hybrid casting plus additive manufacturing approach, Cast-and-Print, which could be used to locally modify the properties and geometry of cast parts to create difficult-to-cast, functional features. Here, we report the results of the properties of deposited materials on cast substrate, the properties of the interface of the deposited and cast material, and the application of the Cast-and-Print method to deposit rivet tabs on high-pressure die cast plates. Ultimately, the approach appears viable, but there are engineering challenges present to reliable additive processing of aluminum wires that need to be overcome for successful implementation of the technology.

42 ENGINEERING↗

Mathematical Modeling on the Influence of Casting Parameters on Initial Solidification at the Meniscus of Slab Continuous Casting

In the current study, the two-dimensional mold model was applied to investigate the influence of different casting parameters on the initial solidification at the meniscus of the continuous casting mold. The profile of the meniscus and the slag rim, and the heat flux on the hot face of the copper plate, were compared with different locations of the mold and different casting parameters. The depth of the oscillation marks and solidified meniscus through simulation was measured with different casting parameters. With the mold oscillating downward from the peak to the valley, the maximum heat flux on the hot face of the copper plate near the meniscus increased from 4.3 to 5.5 MW/m{sup 2}, the thickness of the slag rim decreased from 4.7 to 4.2 mm, and the height of the curved meniscus also decreased. With the increase of casting speed from 1.2 to 1.45 m/min, the maximum speed of the upper backflow increased from 0.6 to 0.8 m/s, and the lowest location of the meniscus at approximately 310 mm from the copper plate decreased from 22 to 12 mm below the meniscus near the nozzle, where the slag entrapment easily occurred. With the increase of the casting speed, casting superheat, and oscillation frequency, and the decrease of the water flow rate in the mold and oscillation amplitude, the thickness of the slag rim decreased. With the increase of casting speed and superheat, and the decrease of the water flow rate in the mold, oscillation frequency, and oscillation amplitude, the depth of the solidified meniscus decreased. The regression equation was fitted to estimate the depth of hooks at the subsurface of slabs.

36 MATERIALS SCIENCE↗

An Alternative Casting Technique to Improve the Creep Resistance of Cast INCONEL Alloy 740H

The increasing performance requirements of power plant designs, such as advanced-ultra supercritical (A-USC), require the use of Ni-based superalloys to replace high-strength, ferritic-martensitic steels for components subjected to temperatures above 898 K (625 °C) and for austenitic stainless steels components at temperatures above 973 K (700 °C). To date, commercial Ni-based superalloy INCONEL 740H has been shown to be appropriate for use in A-USC power plants as boiler components in a wrought product. However, large complex components in boilers as well as other casings in the turbine and valve chest require castings of a thick-wall nature. Using the alloy in its cast form would be significantly valuable in terms of range of component size, geometry and complexity. Previous investigations revealed short creep lives from cast INCONEL alloy 740H. Here in this investigation, an alternative casting route that utilized a melt procedure resulting in a fine-grain casting, and in conjunction with a computationally optimized homogenization heat treatment, not only controlled the grain size and grain boundary structure but minimized chemistry variability and segregation. A primarily equiaxed and homogenous grain size distribution was obtained from this approach with better repartition of M 23 C 6 carbides along the grain boundaries. Furthermore, better than 38 pct increase was obtained for this material in comparison to the creep life obtained from the best performing conventionally cast material. More importantly, the fine-grain homogenized (FGH) casting route resulted in the Larson–Miller plot for this material that coincided with that of wrought alloy 740. At low creep stresses (with a test still in progress), the FGH casting is resulting in higher values of the LMP than the wrought alloy.

36 MATERIALS SCIENCE↗

Deformation Behavior of Pure Copper Castings with As-Cast Surfaces for Electrical Parts

Herein, the tensile deformation behavior of pure copper castings with as-cast surfaces was investigated. It was found that small and sufficiently large uniform elongation types corresponded, respectively, to the presence or absence of a Cu-Cu{sub 2}O eutectic phase in the microstructure. Fissure defects were observed near the as-cast surfaces when the eutectic phase was present, probably leading to stress concentration. On the other hand, surface pinholes were observed when the eutectic phase was absent, and these were not prevented by directional solidification. Although the as-cast specimens (non-directionally solidified) exhibited a slightly reduced uniform elongation compared to the machined specimens in the absence of the eutectic phase, the directionally solidified as-cast samples exhibited a uniform elongation that was similar to that of the machined specimens. In addition, micropore arrays were formed along the grain boundaries inside the castings when the eutectic phase was absent, whereas almost no micropores were observed inside the directionally solidified as-cast specimens because the solidification process involved a faster cooling rate and/or higher temperature gradient. These results do not only suggest the existence of surface pinholes but also indicate that microporosity can reduce the cross-sectional area of the specimens, thus, affecting their uniform elongation.

36 MATERIALS SCIENCE↗

A New Recycled Al–Si–Mg Alloy for Sustainable Structural Die Casting Applications

The use of secondary aluminum for structural components in the automotive industry is limited by the high Fe contents in recycled alloys which often result in the formation of brittle β-Al 5 FeSi phase which reduces the ductility of aluminum castings. In this study, a new secondary Al-Si-Mg alloy with high Fe content (about 0.44 wt.%) was developed for die casting applications. Based on thermodynamic modeling, manganese was added to obtain a designed Fe-to-Mn ratio of 2 which successfully suppressed the formation of β-Al 5 FeSi phase, by forming α-Al 15 (Fe,Mn) 3 Si 2 phase with rounded or hexagonal morphology. Additionally, a fine needle-like π-Al 8 FeMg 3 Si 2 phase was also formed within the eutectic regions. The new recycled alloy showed comparable mechanical properties in as-cast and heat treated (T5 and T6) conditions to three major primary die cast alloys (≤ 0.2 wt.% Fe) with similar composition. Ductility up to 7.4% from tensile elongation was achieved in as-cast recycled alloy due to the modification and refinement of α-Al 15 (Fe,Mn) 3 Si 2 by Mn and Sr additions. Tensile elongation was further improved to 9.1% after T6 treatment as a result of dissolution of π-Al 8 FeMg 3 Si 2 phase, defragmentation of α-Al 15 (Fe,Mn) 3 Si 2 and the spheroidization of Si phase. This new alloy provides a promising path for increasing usage of recycled aluminum with high Fe content in structural die castings for automotive and other applications.

36 MATERIALS SCIENCE↗

An integrated two-dimensional modeling method for predicting ductility of thin-walled die cast magnesium

In this paper, a two-dimensional (2D) microstructure-based modeling method is developed in order to predict the ductility of a thin-walled high pressure die cast magnesium (Mg) by considering the three-dimensional (3D) thru-thickness pore distributions. For this purpose, a series of 3D synthetic microstructure-based finite element models and the corresponding 2D models are first generated with various pore volume fractions, pore size distributions and pore shapes. The input material properties for the 2D models are determined based on the 3D cubic model with a spherical pore and the generalized Neuber’s rule. Based on the resulting ductility of the 3D and 2D models, a 3D/2D ductility correlation curve is developed as a function of the characteristics/shape of the input fracture strain curve used in the 3D model. The validity of the ductility correlation curve is examined with casting samples with actual microstructures. Here, the results show that the suggested 2D modeling methodology can be used together with the ductility correlation curve in predicting the ductility of thin-walled Mg castings.

36 MATERIALS SCIENCE↗

Effects of Casting Parameters and Impurity Concentrations on As-Cast U–10Mo

This work investigates the effects of casting parameter changes on as-cast uranium-10 wt% molybdenum alloys on a 1-2kg scale. A commercial tilt-pour vacuum induction melting system was utilized to study the effects of casting atmosphere, total heating time, hold time at maximum temperature, mold temperature, and crucible type on the as-cast microstructure of U-10Mo. Ten thin plates (5.08 mm thick) and four thick plates (25.4 mm and 63.5 mm thick) were cast and analyzed for carbon, oxygen, hydrogen, and nitrogen impurities. Additionally, molybdenum content and primary dendrite length (PDL) of the microstructure was quantified. A statistical evaluation was performed to identify key carbon and oxygen relationships with operating parameters, impurities, and primary dendrite length. Additional factors investigated include: crucible material, time at maximum temperature, total heating time, and pour temperature. Zirconia crucibles reduced carbon content on average by 35%. Additionally, there was a significant statistical association between carbon and oxygen content, between oxygen content and maximum temperature hold time, between mold temperature and PDL, and between PDL, maximum temperature hold time and mold temperature.

Huber, Zachary F.↗

Cylinder block casting slab core cast geometry for sawcut entrance enhancement

An automobile vehicle engine includes multiple water jackets individually formed in a cast engine block proximate to successive ones of multiple cylinder bores. Multiple cast-in place transition regions are individually formed during a casting operation of the cast engine block at entrances to individual ones of the multiple water jackets. Individual ones of multiple sawcuts open into individual ones of the multiple cast-in place transition regions.

Petrus, Ronald John↗

The Influence of Shell Mold Composition on the As-cast Macro- and Micro-structure of Thin-Walled IN713C Superalloy Castings

In the investment casting process, the building of ceramic layers around the wax pattern is the main time-consuming stage. Increasing their number ensures sufficient mechanical properties, but also lengthens the whole process, including drying time and preheating of the mold. Four molds for casting Ni-based superalloy IN713C were strengthened by glass fibers, included in the slurry, and metal powder, of Al, Cu, Fe or Ni, in the coverage. Castings were subjected to microstructural investigations in order to find out if the new design can be promising for the manufacture of jet engine components. Bend tests revealed that the green strengths of all new molds were higher, at least 3.65 MPa, than that of the unmodified molds, 3.0 MPa. Optical microscopy revealed that the composition of a mold had a strong influence on stereological parameters of equiaxed IN713C grains. Microstructural observation and hardness measurements of castings revealed differences in the volume fraction of strengthening phases, porosity and hardness. The microstructure due to the complex chemical composition of IN713C consisted of several phases including ternary eutectics as a consequence of L → γ + Ni{sub 7}Zr{sub 2} + (Nb, Zr)C.

36 MATERIALS SCIENCE↗

Strengthening Mechanisms and Deformation Behavior of Industrially-Cast and Lab-Cast Dual-Phase High Entropy Alloy

An iron-rich high entropy alloy Al 0.65 CoCrFe 2 Ni comprising of both FCC and BCC phases was designed and fabricated using induction melting at a large industrial scale and suction casting at a small lab scale. Spinodally decomposed interdendritic regions were uniformly distributed in the industrially melted alloy, and a finer dendritic structure with smaller sized spinodal structures was observed in the alloy suction cast at lab scale. The suction cast alloy fabricated at the lab scale exhibited significantly higher compressive yield strength compared to the industrially cast alloy. The relative strengthening contributions in the alloys due to solid solution, grain boundary, dislocation interactions and interphase boundary were analyzed. Dislocation hardening was the major contributor responsible for the higher strength of the SC alloy. The deformation behavior in the alloys was examined with the help of orientation image mapping. Finally, intense slip band formation at large strains in the industrially melted alloy indicates that cold working can be an effective technique to enhance the strength of the dual-phase high entropy alloy processed at a large scale.

36 MATERIALS SCIENCE↗

The High-Temperature Mechanical Properties of EN 1.4509 Stainless Steel Cast Using Investment Casting

The high-temperature (600-900 °C) mechanical properties of EN 1.4509 stainless steel made by investment casting were studied by changing the Nb content based on this stainless steel composition standard. The results indicate that with an increase in tensile temperature, the high-temperature strength shows a downward trend and the high-temperature plasticity increases. The results also indicate that with an increase in Nb content, the high-temperature strength rises continually and the high-temperature plasticity decreases; for example, the tensile strengths at 900 °C of Steel A, Steel B and Steel C are 21, 25 and 31 MPa, respectively, and the yield strengths are 15, 20 and 22 MPa, respectively, and the elongations are 97.7, 85.3 and 73.7%, respectively. The high-temperature tensile strength of the investment casting EN 1.4509 stainless steel sample is closely related to the bulk (Ti, Nb) (C, N) and the Laves phase (Fe{sub 2}Nb) at the ferritic grain boundaries and in the ferritic grains. These are the main factors for improvement in the high-temperature strength of the tested steels; additionally, the coarse ferritic grains also play a certain role in improving the mechanical properties. The Nb content of the investment casting EN 1.4509 stainless steel can be reduced to 0.25 wt.%, and at this content, a combination of good high-temperature mechanical properties and higher room-temperature plasticity is obtained.

36 MATERIALS SCIENCE↗

Evolution of {delta}ferrite in a CF3 cast stainless steel upon neutron irradiation to 3, 5, 10, 20, and 40 dpa

The microstructural evolution of delta ferrite in a CF3 cast stainless steel irradiated to 3, 5, 10, 20, and 40 dpa with two dose rates was studied with atom probe tomography (APT) and transmission electron mi-croscopy. Spinodal decomposition and G-phase precipitates induced by neutron irradiation and thermal aging were quantified systematically. The neutron irradiation significantly enhances the spinodal decom-position in delta ferrite as both the spinodal wavelength (i.e. a characteristic repeat distance) and am-plitude (i.e. magnitude of elemental concentration fluctuation) increase after irradiation. The wavelength only varies slightly when the dose increases from 5 to 40 dpa, while the amplitude increases dramatically from 10 to 20 dpa and starts to saturate before 20 dpa. The dose rate and irradiation temperature also have a notable effect on the spinodal wavelength and amplitude. The study shows that higher dose rate promotes a larger wavelength at given irradiation doses. Regarding the G-phase precipitates, a slightly lower irradiation temperature would result in a smaller mean size of G-phase precipitates, while a lower irradiation dose rate would lead to a larger G-phase precipitates at a given temperature and dose. Over-all, the spinodal decomposition and G-phase precipitates in the delta ferrite continue to evolve with the increasing dose beyond 10 dpa. This study confirms that the formation of G-phase precipitates at the in-terdomain region between alpha and alpha-prime is facilitated by the Si and Mo atoms rejected from Fe rich alpha phase and the Ni and Mn atoms rejected from Cr rich alpha-prime phase. Neutron irradiation plays a dominant role in the ferrite instability, and the effect of prior thermal aging at 400 degrees C for 10,000 hours is negligible as the dose is 3 dpa and above.

duplex stainless steel↗

Solvent-Cast Solid Electrolyte Membranes Based on a Charged Rigid-Rod Polymer and Ionic Liquids

Solid-state electrolytes are attractive for use in electrochemical devices because they remove the need for a flammable liquid electrolyte while contributing to the structural integrity of the device. We have recently developed a class of solid electrolytes, termed molecular ionic composites (MICs), composed of ionic liquids (ILs) and a rigid-rod polyelectrolyte, poly(2,2'-disulfonyl-4,4'-benzidine terephthalamide) (PBDT). MIC materials, originally obtained through an ion-exchange process between IL and PBDT aqueous solution, possess an unprecedented combination of high ionic conductivity, high thermal stability, low flammability and widely tunable tensile storage moduli. Here we present a facile solvent casting method for preparing MIC membranes. These membranes are uniform, flexible, and tough, with tunable composition and thickness (≥ 40 μm). Unlike the previous ion-exchange method, which only allowed incorporation of hydrophilic ILs, we can now incorporate hydrophobic ILs to prepare MIC membranes for, e.g. battery electrolytes. A sodium (Na) metal symmetric cell constructed with a PBDT-Pyr 14 TFSI membrane as the solid electrolyte shows long-term stable cycling (> 500 h.) at 60 °C. Furthermore, the ability to prepare MICs using both hydrophilic and hydrophobic ILs initiates a wider range of MIC materials and broadens the array of applications accessible by MIC membranes.

25 ENERGY STORAGE↗

Casting and Characterization of U-50Zr

Uranium alloyed with 50 wt% zirconium (U-50Zr) is a proposed light water reactor (LWR) nuclear fuel by Lightbridge Corporation (LTBR). The proposed method for making the U-50Zr alloy is to arc-melt master alloys and then remelt in a vacuum induction melter (VIM) to consolidate the material and cast into an intermediate shape. After casting, the material will eventually need to be formed into a desired fuel shape. The work discussed in this report resulted from a joint effort between Ltbr and Pacific Northwest National Laboratory (PNN) to investigate a 500g – 1kg scale casting process to produce the U-50Zr alloy in the desired δ-UZr 2 phase and characterize the impurities and microstructure that result from the casting process. Master alloys were fabricated in an arc melter, then five castings were carried out in a VIM with multiple inert coating and crucible materials to find an appropriate combination. Both ZrO 2 and graphite crucibles were used and different combinations of Y 2 O 3 , CaZrO 3 , and TiC to identify which would contain the molten metal with the least reaction. On each casting, the C, O, N, H impurities were analyzed as well as the phase by x-ray diffraction and microstructure. Of the five castings, two resulted in majority of δ-UZr 2 phase-pure material and had impurity levels within acceptable ranges. The two most successful castings utilized a graphite crucible with a TiC undercoating and a Y 2 O 3 overcoat. The O and N levels were below 1000 ppm and the C content was variable but did not result in measurable carbide formation. The highest success casting resulted in an average of 282 ppm C, 567 ppm O, 217 ppm N and 79 ppm H. This casting's crucible and inert coating material was repeated with slightly different casting parameters and resulted in higher C numbers but similar phase identification. The differences between each casting are discussed and recommendations are made for future experiments to better decide on a casting process to go forward with.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Enhancing isotope mixing in U-10Mo downblend castings with electromagnetic stirring

Uranium alloyed with 10 wt percent molybdenum (U-10Mo) is the proposed fuel for use in the United States’ high-performance research reactors. The U-10Mo fuel is fabricated by a two-step casting process that downblends highly enriched uranium with depleted uranium (DU) and/or natural uranium (NU) and subsequently alloys the resulting high-assay low-enriched uranium (HALEU) with Mo. Currently, a two-step casting process is needed to meet the ingots’ U-235 enrichment homogeneity specifications. This work demonstrates the ability to provide more homogeneous U-235 distributions during downblend casting by using zirconia for crucibles rather than graphite. When graphite is used as a crucible, the electromagnetic field produced by the induction heater couples directly with the graphite. Zirconia is nonconducting in this study, and therefore does not couple with the field. The induction field couples directly with the metal, and causes electromagnetic stirring (EMS) in the molten metal pool. Eight downblend casting experiments were carried out in this work. Four were performed with zirconia crucibles and four with graphite crucibles. The U-235 enrichment was measured at nine discrete points in each casting using laser ablation multi-collector inductively coupled mass spectrometry (LA-MC-ICP-MS). The enrichment homogeneity was approximately eight times better in zirconia crucible castings than in graphite crucible castings as measured by the plate enrichment range and enrichment coefficient of variation. The results show a single casting step could be used to meet USHPRR enrichment specifications if electromagnetic stirring is present during casting. A related investigation was carried out to determine whether it is appropriate to measure enrichment on as-cast ingots or whether heat treated specimens should be used to accurately characterize enrichment. The results show that the as-cast microstructure plays a significant role in enrichment homogeneity. It is recommended that all enrichment measurements be done after the homogenization heat treatment typical of U-10Mo processing.

36 MATERIALS SCIENCE↗