Search NASA⌕ Search

SEARCH · Search NASA

Results for “CIGS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Sodium-Doped Molybdenum Targets for Controllable Sodium Incorporation in CIGS Solar Cells: Preprint

The efficiency of Cu(In,Ga)Se2 (CIGS) solar cells is enhanced when Na is incorporated in the CIGS absorber layer. This work examines Na incorporation in CIGS utilizing Na-doped Mo sputtered from targets made with sodium molybdate-doped (MONA) powder. Mo:Na films with varying thicknesses were sputtered onto Mo-coated borosilicate glass (BSG) or stainless steel substrates for CIGS solar cells. Byuse of this technique, the Na content of CIGS can be varied from near-zero to higher than that obtained from a soda-lime glass (SLG) substrate. Targets and deposition conditions are described. The doped Mo films are analyzed, and the resulting devices are compared to devices fabricated on Mo-coated SLG as well as Mo-coated BSG with NaF. Completed devices utilizing MONA exceeded 15.7% efficiencywithout anti-reflective coating, which was consistently higher than devices prepared with the NaF precursor. Strategies for minimizing adhesion difficulties are presented.

14 SOLAR ENERGY↗

Stability of CIGS Solar Cells and Component Materials Evaluated by a Step-Stress Accelerated Degradation Test Method: Preprint

A step-stress accelerated degradation testing (SSADT) method was employed for the first time to evaluate the stability of CuInGaSe2 (CIGS) solar cells and device component materials in four Al-framed test structures encapsulated with an edge sealant and three kinds of backsheet or moisture barrier film for moisture ingress control. The SSADT exposure used a 15 degrees C and then a 15% relativehumidity (RH) increment step, beginning from 40 degrees C/40%RH (T/RH = 40/40) to 85 degrees C/70%RH (85/70) as of the moment. The voluminous data acquired and processed as of total DH = 3956 h with 85/70 = 704 h produced the following results. The best CIGS solar cells in sample Set-1 with a moisture-permeable TPT backsheet showed essentially identical I-V degradation trend regardless of theAl-doped ZnO (AZO) layer thickness ranging from standard 0.12 um to 0.50 um on the cells. No clear 'stepwise' feature in the I-V parameter degradation curves corresponding to the SSADT T/RH/time profile was observed. Irregularity in I-V performance degradation pattern was observed with some cells showing early degradation at low T/RH < 55/55 and some showing large Voc, FF, and efficiency degradation due to increased series Rs (ohm-cm2) at T/RH = 70/70. Results of (electrochemical) impedance spectroscopy (ECIS) analysis indicate degradation of the CIGS solar cells corresponded to increased series resistance Rs (ohm) and degraded parallel (minority carrier diffusion/recombination) resistance Rp, capacitance C, overall time constant Rp*C, and 'capacitor quality' factor (CPE-P), whic were related to the cells' p-n junction properties. Heating at 85/70 appeared to benefit the CIGS solar cells as indicated by the largely recovered CPE-P factor. Device component materials, Mo on soda lime glass (Mo/SLG), bilayer ZnO (BZO), AlNi grid contact, and CdS/CIGS/Mo/SLG in test structures with TPT showed notable to significant degradation at T/RH = 70/70. At T/RH = 85/70, substantial blistering of BZO layers on CIGS cell pieces was observed that was not seen on BZO/glass, and a CdS/CIGS sample displayed a small darkening and then flaking feature. Additionally, standard AlNi grid contact was less stable than thin Ni grid contact at T/RH = 70/70. The edge sealant and moisture-blocking films were effective to block moisture ingress, as evidenced by the good stability of most CIGS solar cells and device components at T/RH = 85/70 for 704 h, and by preservation of the initial blue color on the RH indicator strips. The SSADT experiment is ongoing to be completed at T/RH = 85/85.

14 SOLAR ENERGY↗

Cost and Potential of Monolithic CIGS Photovoltaic Modules

A bottom-up cost analysis of monolithic, glass-glass Cu(In,Ga)(Se,S)2 (CIGS) modules is presented, illuminating current cost drivers for this technology and possible pathways to reduced cost. At 14% module efficiency, for the case of U.S. manufacturing, a manufacturing cost of $0.56/WDC and a minimum sustainable price of $0.72/WDC were calculated. Potential for reduction in manufacturing costs to below $0.40/WDC in the long-term may be possible if module efficiency can be increased without significant increase in $/m2 costs. The levelized cost of energy (LCOE) in Phoenix, AZ under different conditions is assessed and compared to standard c-Si.

14 SOLAR ENERGY↗

Investigation of Some Transparent Metal Oxides as Damp Heat Protective Coating for CIGS Solar Cells: Preprint

We investigated the protective effectiveness of some transparent metal oxides (TMO) on CIGS solar cell coupons against damp heat (DH) exposure at 85oC and 85% relative humidity (RH). Sputter-deposited bilayer ZnO (BZO) with up to 0.5-um Al-doped ZnO (AZO) layer and 0.2-um bilayer InZnO were used as 'inherent' part of device structure on CdS/CIGS/Mo/SLG. Sputter-deposited 0.2-um ZnSnO and atomiclayer deposited (ALD) 0.1-um Al2O3 were used as overcoat on typical BZO/CdS/CIGS/Mo/SLG solar cells. The results were all negative -- all TMO-coated CIGS cells exhibited substantial degradation in DH. Combining the optical photographs, PL and EL imaging, SEM surface micro-morphology, coupled with XRD, I-V and QE measurements, the causes of the device degradations are attributed to hydrolyticcorrosion, flaking, micro-cracking, and delamination induced by the DH moisture. Mechanical stress and decrease in crystallinity (grain size effect) could be additional degrading factors for thicker AZO grown on CdS/CIGS.

14 SOLAR ENERGY↗

Electrical Bias as an Alternate Method for Reproducible Measurement of Copper Indium Gallium Diselenide (CIGS) Photovoltaic Modules: Preprint

Light-to-dark metastable changes in thin-film photovoltaic (PV) modules can introduce uncertainty when measuring module performance on indoor flash testing equipment. This study describes a method to stabilize module performance through forward-bias current injection rather than light exposure. Measurements of five pairs of thin-film copper indium gallium diselenide (CIGS) PV modules indicate that forward-bias exposure maintained the PV modules at a stable condition (within 1%) while the unbiased modules degraded in performance by up to 12%. It was additionally found that modules exposed to forward bias exhibited stable performance within about 3% of their long-term outdoor exposed performance. This carrier-injection method provides a way to reduce uncertainty arising from fast transients in thin-film module performance between the time a module is removed from light exposure and when it is measured indoors, effectively simulating continuous light exposure by injecting minority carriers that behave much as photocarriers do. This investigation also provides insight into the initial light-induced transients of thin-film modules upon outdoor deployment.

14 SOLAR ENERGY↗

Comparative Study of Zn(O,S) Buffer Layers and CIGS Solar Cells Fabricated by CBD, ALD, and Sputtering: Preprint

Zn(O,S) thin films were deposited by chemical bath deposition (CBD), atomic layer deposition, and sputtering. Composition of the films and band gap were measured and found to follow the trends described in the literature. CBD Zn(O,S) parameters were optimized and resulted in an 18.5% efficiency cell that did not require post annealing, light soaking, or an undoped ZnO layer. Promising resultswere obtained with sputtering. A 13% efficiency cell was obtained for a Zn(O,S) emitter layer deposited with 0.5%O2. With further optimization of process parameters and an analysis of the loss mechanisms, it should be possible to increase the efficiency.

14 SOLAR ENERGY↗

Advanced Thin Film Core Technology: CIGS Final Technical Report (FTR)

Cu(In,Ga)Se 2 (CIGS) thin-film photovoltaics are a high-efficiency and reliable technology. This project completed research in two important areas and was designed to work collaboratively with industrial partners. Task 1: Alkali Science focused on alkali post-deposition treatments (PDT). PDTs have been instrumental in the dramatic voltage improvements that have moved CIGS device efficiencies from 20% to 23.35% [1]. Based on a survey of CIGS companies at the beginning of the project, the single biggest breakthrough for the CIGS community would be a mechanistic understanding of the role of alkalis in the material system. Significant accomplishments of Task 1: Alkali Science: 1) KF post-deposition treatments were shown to improve lifetime, open-circuit voltage (VOC), and efficiency of industrial partner samples, even when done as a later step, separate from the original CIGS deposition. 2) KF boosted efficiency when incorporated at the end of the third stage of NREL CIGS growth. 3) XPS characterization of CIGS surfaces with and without PDTs led to a proposed mechanism whereby K drives structural transformation at 350 degrees C that is locked in at room temperature even after K is rinsed away. 4) Published recipes for KF and RbF PDTs. Literature to date did not provide enough detail to quickly reproduce experimental results. 5) Identified most important parameters (RbF cell temperature and lamp setpoint temperature) and set boundaries for successful RbF PDTs. The purpose of Task 2: Cell-level Reliability was to overcome the largest challenges to investor confidence and long product lifetime in CIGS-based photovoltaic products: metastability, shading-induced hot spots, and potential-induced degradation (PID). Key findings were made in each of these areas by studying CIGS reliability at the cell level: 1) Published NREL's cell-level reliability testing procedures along with challenges that were encountered while developing them. These were also distributed to the community through an MRS conference presentation. 2) Decreased metastability by adding a CdS hole-injection layer between the CIGS and Zn(O,S) in the device stack. It also improved device performance. Materials other than CdS can be used for the same purpose. 3) Reduced front-glass PID by replacing soda-lime glass with low-Na borosilicate glass. 4) Found that PID depends on leakage current and light/electrical bias. This will help labs avoid test-specific degradation. 5) Discovered that CIGS can suffer from two different types of PID with different mechanisms. Front is slower and leads to shunting ZnO. Back is faster and degrades the p-n junction. 6) Holding cells at open circuit slows PID compared to short circuit. This affects testing protocols for glass/glass modules.

14 SOLAR ENERGY↗

CIGS Technology Advancement via Fundamental Modeling of Defect/Impurity Interactions (Final Technical Report)

The primary goals of the proposed work were to provide modeling tools (and the associated insight which comes along with model development) for design and optimization of CuIn x Ga 1-x Se 2 (CIGS) and CdSeTe (CST) solar cell manufacturing processes and to establish the foundation for comprehensive end-to-end predictive modeling tools to enable optimization of thin film photovoltaic technology for performance, cost, yield, and reliability. The initial focus of efforts within this project was to develop coupled process/optical/device models for CIGS PV technology and to work with Siva Power to apply that TCAD (technology computer-aided design) system to improve the efficiency and reduce manufacturing costs for CIGS solar cells. Our approach to that end was to generate an extensive database of DFT calculations and to use those calculations via statistical thermodynamics methods and Monte Carlo simulation to develop and characterize models for the behavior of native defects as well as intentional and unintentional impurities, including the redistribution of the primary components of CIGS films. Increased effort went toward coupling those models for defect behavior and composition evolution to the performance of multicrystalline CIGS solar cells via prediction of doping level and recombination lifetime as function of manufacturing process. In the second budget period, the project pivoted to developing a similar system for the CdSeTe system, focused especially on understanding the role of Se/Te alloy concentration. Execution of the project resulted in the successful development of TCAD systems for both CIGS and CdSeTe thin film PV within the Synopsys Sentaurus framework by utilizing the Alagator interface. In the first budget period of the project, we developed quantitative models for the major components of CIGS PV and implemented them within a framework that couples process, optical, and device simulation. From the insights we have gained, we identified novel opportunities for enhancing CIGS solar cell performance and have laid the groundwork to further optimize the layer structure, composition profile, and thermal cycles for substantially improved efficiency and lower manufacturing costs. For the CIGS system, process changes to achieve greater than 1% absolute enhancement in efficiency were identified, but testing of those approaches was stymied by lack of a domestic CIGS manufacturing partner after the closure of Siva Power as well as Miasole. For CdSeTe, a fully capable TCAD system only became ready to apply near the end of the project period, so substantial opportunities remain to apply those models to enhance the leading thin film PV technology.

14 SOLAR ENERGY↗

Sodium doping of solution-processed amine-thiol based CIGS solar cells by thermal evaporation of NaCl

Poor crystallinity, high degree of porosity and rough surfaces are the main drawbacks of solution-processed CIGS absorbers resulting in lower power conversion efficiencies when compared to vacuum-based CIGS solar cells. Therefore, promoting absorber grain growth is key to further improve solution-based solar cell performance. The effect of alkali elements such as Na in CIGS absorbers is generally recognised to have beneficial effects not only on the absorber opto-electronic properties but also on the grain growth. In this work, thermal evaporation of a thin layer of NaCl prior to selenisation resulted in absorbers with significantly larger CIGS grains than previously seen with Na diffusing directly from the from soda-lime glass substrate. NaCl is non-toxic, abundant and readily available compound that has not been typically used as an evaporation source, but rather as an additive into CIGS precursor solution. The effect of Na on these solution-processed CIGS devices was primarily observed in the spectacular morphological changes leading to improved carrier collection and minority carrier lifetimes, but less on the absorber doping. Transmission electron microscopy (TEM) revealed voids forming around large CIGS grains upon NaCl addition and these had a negative effect on inter-grain carrier transport. Nonetheless, the resulting device performance doubled from 5% to 10% with addition of Na using this doping approach; however, a compromise between the optimum grain growth and optimum electronic properties had to be made. This study demonstrates a novel, simple and effective Na-doping strategy for CIGS absorbers and reveals the current limitations of the Na-doping in solution-processed atmospherically deposited cells.

14 SOLAR ENERGY↗

Manufacturing and Reliability Science for CIGS Photovoltaics

The purpose of this program was to overcome the largest challenges to investor confidence and long product lifetime in CuIn x Ga 1-x Se 2 (CIGS)-based photovoltaic products: metastability, shading-induced hot spots, and potential-induced degradation. Key findings were made in each of these areas by studying CIGS reliability at the cell level, which very few groups are currently doing. Metastability was thought to be a function of the CIGS absorber. We have challenged the state-of-the-art by showing that the metastability seen in commercial products is likely to be caused by the buffer layer. SCAPS device modeling confirmed that the buffer layer has a significant influence on metastability in CIGS devices, and also led to a processing change - the introduction of CdS islands to Zn(O,S) buffer layers - that dramatically reduced metastability in CIGS solar cells. In the reverse-bias shading task, modeling showed us that 19% solar cells are possible with thin CIGS layers of 0.5 µm. We were able to fabricate 15.2% solar cells in this project, which is the highest reported efficiency of devices in the ultra-thin class. We also discovered that the best way to dissipate less power in reverse bias was to eliminate the intrinsic ZnO layer that is often used in CIGS devices. Lower power dissipation led to devices that allowed two times the maximum power point current density in reverse without damage. Potential-induced degradation (PID) is caused by the drift of Na+ ions from the back glass to the CIGS/Mo interface, followed by diffusion into the solar cells and to the CdS region. We found that PID can be slowed by using low-conductivity borosilicate glass that contains higher K and lower Na than soda-lime glass. Based on significant progress in each of the three reliability challenges, the CIGS cell-level reliability project was very successful. We have also proved that module-level degradation mechanisms can be tested and solved at the cell level.

14 SOLAR ENERGY↗

Comprehensive characterization of CIGS absorber layers grown by one-step sputtering process

We have demonstrated that the use of a one-step sputtering process allowed for the fabrication of copper indium gallium diselenide (CIGS) thin films by RF magnetron sputtering without an additional selenization process. The CIGS thin films deposited at different substrate temperatures were synthesized on soda-lime glass (SLG) substrates using a single quaternary CIGS target. The film composition ratios of ([Cu]/[In]+[Ga]), ([Ga]/[In]+[Ga]), and ([Se]/[Cu]+[In]+[Ga]) were almost consistent with those of the sputtering target. X-ray diffraction (XRD) and Raman results showed that the crystallinity of the CIGS thin films was gradually improved as substrate temperatures increased. Transmission electron microscopy (TEM) showed that the films grown at 600 degrees C have a columnar structure with the grain size of ~100 nm. In addition, for the CIGS films grown at 600 degrees C, TEM-EDX analysis revealed that the synchronized fluctuation of the Cu and Se signals was observed in the direction of the film depth, while the In and Ga signals were constant. As a result, the CIGS solar cell made using the film showed a degraded cell efficiency of 2.5%, which might be have been caused by not only Cu-rich and Se-poor compositions but the locally unstable composition in the CIGS films fabricated by one-step sputtering.

14 SOLAR ENERGY↗

Examination of Na-Doped Mo Sputtering for CIGS Devices (CRADA Final Report)

Na is an important ingredient in Cu(In,Ga)(Se,S) 2 (CIGS) photovoltaic devices, due to its ability to increase carrier density and passivate surfaces, grain boundaries, and Se vacancies. In the highest efficiency devices, Na is supplied to the growing CIGS film by diffusion through the Mo back contact from the sodalime glass substrate. This arrangement is problematic in that the Na content of the film is only indirectly controlled: deposition times, deposition temperatures, Mo morphology, and glass composition are coupled with the Na diffusion. Results in the literature show that the Mo, not the CIGS, is the primary barrier to Na diffusion. Alternatively, using a Na-free substrate or diffusion barrier, Na may be introduced by a NaF precursor deposited on top of the Mo. However, this forces a trade-off between carrier density and adhesion. If the NaF is not entirely consumed, the CIGS layer peels away from the Mo, encouraging the use of less NaF even though the best device properties tend to result from the thickest possible NaF layers. Furthermore, although early studies show that gross control of Na is sufficient to produce 12-14% small devices, the industry has reached this level and is ready to progress to higher performance. The sensitivity of NREL device efficiency (15 to 20%) to Mo morphology suggests that fine control of Na content is necessary for very high performance. This work has investigated the use of Na doped Mo (“MONA”) sputtering targets for use in preparing CIGS devices. The Mo:Na material is doped to about 3% Na by weight, implying that a 40 nm layer on top of the standard Mo contact validation of their product. contains sufficient Na to dope a 2.5 µm CIGS film. The ability to control Na doping independent of both CIGS processing conditions and adhesion is an important gain for industry and research. Manufacturers gain a route to increased manufacturability and performance, while NREL researchers gain a tightened performance distribution of devices and increased process flexibility. Our immediate partner in this work, the Climax Molybdenum Technology Center, gains validation of their product.

14 SOLAR ENERGY↗

Improvement of the CIGS solar cell performance: structure based on a ZnS buffer layer

Cu(In,Ga)Se{sub 2} (CIGS) based thin film solar cells are the most efficient thin-film solar cells today. The non-toxic and wide band-gap zinc sulphide (ZnS) is a promising material to replace the cadmium sulfide (CdS) as the buffer layer in CIGS based solar cells. In this work we present a simulation study of a CIGS based solar cell with a buffer layer of ZnS, using the simulator Silvaco-Atlas. Our primary simulation shows a 22.6% efficiency of the CIGS solar cell with the CdS buffer layer which is comparable to reported and highest experimental results. However, the simulated efficiency of the CIGS solar cell with the ZnS buffer layer as high as 23.54% was achieved. The effects of layer parameters like the thickness, the acceptor and donor densities of the CIGS absorber and ZnS buffer layers and the CBO on the photovoltaic parameters of the ZnS/CIGS solar cell are optimized in order to improve the performance of the ZnS/CIGS solar cell. The highest efficiency of 27.33% is achieved when the ZnS buffer and the CIGS absorber layers have thicknesses of 0.025 µm and 4 µm with acceptor and donor densities of 6 × 10{sup 17} cm{sup −3} and 10{sup 18} cm{sup −3}, respectively and a CBO in the range − 0.05 to 0.05 eV. The present results of simulation can help the development of the solar cells with higher conversion efficiency and low cost.

14 SOLAR ENERGY↗

Characterization of Cu(In,Ga)Se 2 (CIGS) films with varying gallium ratios

Cu(In 1-x ,Ga x )Se 2 (CIGS) absorber layers were deposited on molybdenum (Mo) coated soda-lime glass substrates with varying Ga content (described as Ga/(In+Ga) ratios) with respect to depth. As the responsible mechanisms for the limitation of the performance of the CIGS solar cells with high Ga contents are not well understood, the goal of this work was to investigate different properties of CIGS absorber films with Ga/(In+Ga) ratios varied between 0.29 and 0.41 (as determined by X-ray florescence spectroscopy (XRF)) in order to better understand the role that the Ga content has on film quality. The Ga grading in the CIGS layer has the effect causing a higher bandgap toward the surface and Mo contact while the band gap in the middle of the CIGS layer is lower. Also, a wider and larger Ga/(In+Ga) grading dip located deeper in the CIGS absorber layers tend to produce larger grains in the regions of the films that have lower Ga/(In+Ga) ratios. It was found that surface roughness decreases from 51.2 nm to 41.0 nm with increasing Ga/(In+Ga) ratios. However, the surface roughness generally decreases if the Ga grading occurs deeper in the absorber layer.