FY 2016 Status Report: CIRFT Testing Data Analyses and Updated Curvature Measurements

This report provides a detailed description of FY15 test result corrections/analysis based on the FY16 Cyclic Integrated Reversible-Bending Fatigue Tester (CIRFT) test program methodology update used to evaluate the vibration integrity of spent nuclear fuel (SNF) under normal transportation conditions. The CIRFT consists of a U-frame testing setup and a real-time curvature measurement method. The three-component U-frame setup of the CIRFT has two rigid arms and linkages to a universal testing machine. The curvature of rod bending is obtained through a three-point deflection measurement method. Three linear variable differential transformers (LVDTs) are used and clamped to the side connecting plates of the U-frame to capture the deformation of the rod. The contact-based measurement, or three-LVDT-based curvature measurement system, on SNF rods has been proven to be quite reliable in CIRFT testing. However, how the LVDT head contacts the SNF rod may have a significant effect on the curvature measurement, depending on the magnitude and direction of rod curvature. It has been demonstrated that the contact/curvature issues can be corrected by using a correction on the sensor spacing. The sensor spacing defines the separation of the three LVDT probes and is a critical quantity in calculating the rod curvature once the deflections are obtained. The sensor spacing correction can be determined by using chisel-type probes. The method has been critically examined this year and has been shown to be difficult to implement in a hot cell environment, and thus cannot be implemented effectively. A correction based on the proposed equivalent gauge-length has the required flexibility and accuracy and can be appropriately used as a correction factor. The correction method based on the equivalent gauge length has been successfully demonstrated in CIRFT data analysis for the dynamic tests conducted on Limerick (LMK) (17 tests), North Anna (NA) (6 tests), and Catawba mixed oxide (MOX) (10 tests) SNF samples. These CIRFT tests were completed in FY14 and FY15. Specifically, the data sets obtained from measurement and monitoring were processed and analyzed. The fatigue life of rods has been characterized in terms of moment, curvature, and equivalent stress and strain..

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Lessons learned from CIRFT testing on SNF vibration integrity study

A cyclic integrated reversible-bending fatigue tester (CIRFT) was developed to support U.S. NRC and DOE Used Fuel Disposition Campaign studies on high burn-up (HBU) spent nuclear fuel (SNF) transportation during normal conditions of transport (NCT). Two devices were developed; the first CIRFT was successfully installed and operated in the ORNL hot-cells in September 2013. Since hot cell testing commenced several HBU SNF samples from both Zr-4 and M5 clads were investigated. The second CIRFT device was developed in February 2014, and has been used to test clad/fuel surrogate rods (stainless steel with alumina pellet inserts). The second CIRFT machine has also been used for sensor development and test sensitivity analyses, as well as loading boundary condition parameter studies. The lessons learned from CIRFT testing will be presented in this paper.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

FY 2016 Status Report: Documentation of All CIRFT Data including Hydride Reorientation Tests (Draft M2)

The first portion of this report provides a detailed description of fiscal year (FY) 2015 test result corrections and analysis updates based on FY 2016 updates to the Cyclic Integrated Reversible-Bending Fatigue Tester (CIRFT) program methodology, which is used to evaluate the vibration integrity of spent nuclear fuel (SNF) under normal conditions of transport (NCT). The CIRFT consists of a U-frame test setup and a real-time curvature measurement method. The three-component U-frame setup of the CIRFT has two rigid arms and linkages connecting to a universal testing machine. The curvature SNF rod bending is obtained through a three-point deflection measurement method. Three linear variable differential transformers (LVDTs) are clamped to the side connecting plates of the U-frame and used to capture deformation of the rod. The second portion of this report provides the latest CIRFT data, including data for the hydride reorientation test. The variations in fatigue life are provided in terms of moment, equivalent stress, curvature, and equivalent strain for the tested SNFs. The equivalent stress plot collapsed the data points from all of the SNF samples into a single zone. A detailed examination revealed that, at the same stress level, fatigue lives display a descending order as follows: H. B. Robinson Nuclear Power Station (HBR), LMK, and mixed uranium-plutonium oxide (MOX). Just looking at the strain, LMK fuel has a slightly longer fatigue life than HBR fuel, but the difference is subtle. The third portion of this report provides finite element analysis (FEA) dynamic deformation simulation of SNF assemblies . In a horizontal layout under NCT, the fuel assembly’s skeleton, which is formed by guide tubes and spacer grids, is the primary load bearing apparatus carrying and transferring vibration loads within an SNF assembly. These vibration loads include interaction forces between the SNF assembly and the canister basket walls. Therefore, the integrity of the guide tubes and spacer grids critically affects the vibration intensity of the fuel assembly during transport and must be considered when developing the multipurpose purpose canister (MPC) design for safe SNF transport.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

FY 2016 Status Report: CIRFT Testing on Spent Nuclear Fuels and Hydride Reorientation Study

This report provides a detailed description of the Cyclic Integrated Reversible-Bending Fatigue Tester (CIRFT) testing conducted on spent nuclear fuel (SNF) rods in FY 2016, including hydride reorientation test results. Contact-based measurement, or three-LVDT-based curvature measurement, of SNF rods has proven to be quite reliable in CIRFT testing. However, how the linear variable differential transformer (LVDT) head contacts the SNF rod may have a significant effect on the curvature measurement, depending on the magnitude and direction of rod curvature. To correct such contact/curvature issues, sensor spacing, defined as the amount of separation between the three LVDT probes, is a critical measurement that can be used to calculate rod curvature once the deflections are obtained. Recently developed CIRFT data analyses procedures were integrated into FY 2016 CIRFT testing results for the curvature measurements. The variations in fatigue life are provided in terms of moment, equivalent stress, curvature, and equivalent strain for the tested SNFs. The equivalent stress plot collapsed the data points from all of the SNFs into a single zone. A detailed examination revealed that, at same stress level, fatigue lives display a descending order as follows: H. B. Robinson Nuclear Power Station (HBR), Limerick Nuclear Power Station (LMK), mixed uranium-plutonium oxide (MOX). If looking at the strain, then LMK fuel has a slightly longer fatigue life than HBR fuel, but the difference is subtle. The knee point of endurance limit in the curve of moment and curvature or equivalent quantities is more clearly defined for LMK and HBR fuels. The treatment affects the fatigue life of specimens. Both a drop of 12 in. and radial hydride treatment (RHT) have a negative impact on fatigue life. The effect of thermal annealing on MOX fuel rods was relatively small at higher amplitude but became significant at low amplitude of moment. Thermal annealing tended to extend the fatigue life of MOX fuel rod specimens. However, for HR4 testing, the thermal annealing treatment showed a negative impact on the fatigue life of the HBR rod.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

FY14 Status Report: CIRFT Testing Results on High Burnup UNF

The objective of this project is to perform a systematic study of SNF/UNF (spent nuclear fuel/or used nuclear fuel) integrity under simulated transportation environments by using hot cell testing technology developed recently at Oak Ridge National Laboratory (ORNL), CIRFT (Cyclic Integrated Reversible-Bending Fatigue Tester). Under Nuclear Regulatory Commission (NRC) sponsorship, ORNL completed four benchmarking tests, four static tests, and twelve dynamic or cycle tests on H. B. Robinson (HBR) high burn-up (HBU) fuel. With support from the US Department of Energy and the NRC, CIRFT testing has been continued. The CIRFT testing was conducted on three HBR rods (R3, R4, and R5), with two specimens failed and one specimen un-failed. The total number of cycles in the test of un-failed specimens went over 2.23 107; the test was stopped as because the specimen did not show any sign of failure. The data analysis on all the HBR SNF rods demonstrated that it is necessary to characterize the fatigue life of used fuel rods in terms of both the curvature amplitude and the maximum of absolute of curvature extremes. The latter is significant because the maxima of extremes signify the maximum of tensile stress of the outer fiber of the bending rod. So far, a large variety of hydrogen contents has been covered in the CIRFT testing on HBR rods. It has been shown that the load amplitude is the dominant factor that controls the lifetime of bending rods, but the hydrogen content also has an important effect on the lifetime attained, according to the load range tested.

fuel vibration integrity↗

CIRFT Testing of Used Nuclear Fuel Rods from the Limerick Generating Station Boiling Water Reactor (FY15 Status Report)

The objective of this project is to perform a systematic study of spent nuclear fuel (SNF, also known as “used nuclear fuel” [UNF]) integrity under simulated transportation environments using the Cyclic Integrated Reversible-Bending Fatigue Tester (CIRFT) hot-cell testing technology developed at Oak Ridge National Laboratory (ORNL) in August 2013. Under Nuclear Regulatory Commission (NRC) sponsorship, ORNL completed four benchmark tests, four static tests, and twelve dynamic or cycle tests on H. B. Robinson (HBR) high burn-up (HBU) fuel. The clad of the HBR fuels was made of Zircaloy-4. Testing was continued in fiscal year (FY) 2014 using Department of Energy (DOE) funds. Additional CIRFT testing was conducted on three HBR rods; two specimens failed, and one specimen was tested to over 2.23 × 10 7 cycles without failing. The data analysis on all the HBR SNF rods demonstrated that it is necessary to characterize the fatigue life of the SNF rods in terms of (1) the curvature amplitude and (2) the maximum absolute of curvature extremes. The maximum extremes are significant because they signify the maximum tensile stress for the outer fiber of the bending rod. CIRFT testing has also addressed a large variation in hydrogen content on the HBR rods. While the load amplitude is the dominant factor that controls the fatigue life of bending rods, the hydrogen content also has an important effect on the lifetime attained at each load range tested. In FY 15, eleven SNF rod segments from the Limerick BWR were tested using the ORNL CIRFT equipment; one test under static conditions and ten tests under dynamic loading conditions. Under static unidirectional loading, a moment of 85 N·m was obtained at a maximum curvature of 4.0 m -1 . The specimen did not show any sign of failure during three repeated loading cycles to a similar maximum curvature. Ten cyclic tests were conducted with amplitudes varying from 15.2 to 7.1 N·m. Failure was observed in nine of the tested rod specimens. The cycles-to-failure ranged from 1.22 × 10 5 to 4.70 × 10 6 , and the amplitudes varied from 15.2 to 7.6 N·m. The measurements at the interrupts indicated a range of flexural rigidity from 30 to 50 N·m 2 . Online monitoring revealed that the flexural rigidity was slightly lower due to the higher loading, from 25 to 42 N·m 2 . Generally, no substantial change of rigidity was observed based on the online monitoring during the cyclic fatigue testing process. Overall, the decreasing trend of sample lifetime with increasing amplitude is well defined.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

ORNL Interim Progress Report on Hydride Reorientation CIRFT Tests

A systematic study of H. B. Robinson (HBR) high burnup spent nuclear fuel (SNF) vibration integrity was performed in Phase I project under simulated transportation environments, using the Cyclic Integrated Reversible-Bending Fatigue Tester (CIRFT) hot cell testing technology developed at Oak Ridge National Laboratory in 2013–14. The data analysis on the as-irradiated HBR SNF rods demonstrated that the load amplitude is the dominant factor that controls the fatigue life of bending rods. However, previous studies have shown that the hydrogen content and hydride morphology has an important effect on zirconium alloy mechanical properties. To address the effect of radial hydrides in SNF rods, in Phase II a test procedure was developed to simulate the effects of elevated temperatures, pressures, and stresses during transfer-drying operations. Pressurized and sealed fuel segments were heated to the target temperature for a preset hold time and slow-cooled at a controlled rate. The procedure was applied to both non-irradiated/prehydrided and high-burnup Zircaloy-4 fueled cladding segments using the Nuclear Regulatory Commission-recommended 400°C maximum temperature limit at various cooling rates. Before testing high-burnup cladding, four out-of-cell tests were conducted to optimize the hydride reorientation (R) test condition with pre-hydride Zircaloy-4 cladding, which has the same geometry as the high burnup fuel samples. Test HR-HBR#1 was conducted at the maximum hoop stress of 145 MPa, at a 400°C maximum temperature and a 5°C/h cooling rate. On the other hand, thermal cycling was performed for tests HR-HBR#2, HR-HBR#3, and HR-HBR#4 to generate more radial hydrides. It is clear that thermal cycling increases the ratio of the radial hydride to circumferential hydrides. The internal pressure also has a significant effect on the radial hydride morphology. This report describes a procedure and experimental results of the four out-of-cell hydride reorientation tests of hydrided Zircaloy-4 cladding, which served as a guideline to prepare in-cell hydride reorientation samples with high burnup HBR fuel segments. This report also provides the Phase II CIRFT test data for the hydride reorientation irradiated samples. The variations in fatigue life are provided in terms of moment, equivalent stress, curvature, and equivalent strain for the tested SNFs. The CIRFT results appear to indicate that hydride reoriented treatment (HRT) have a negative effect on fatigue life, in addition to hydride reorientation effect. For HR4 specimen that had no pressurization procedure applied, the thermal annealing treatment alone showed a negative impact on the fatigue life compared to the HBR rod.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

ORNL Interim Progress Report on Static CIRFT Testing Curvature Data Update

Since the CIRFT tests reported in NUREG-7198 were generated, a number of factors that influence the recorded curvature measurement data were identified. In 2016, a data reanalysis task was undertaken to implement the lessons learned. This letter report provides the revised results of previous CIRFT tests, after implementing the following data reanalysis procedures: (A) experimental data smoothing and LVDT reset, (B) LVDT probe contact and sensor spacing correction for curvature data, and (C) LVDT probe dynamic vibration adjustment procedure development.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Sister Rod Destructive Examinations (FY23) Appendix G: CIRFT Uncertainty Calculations

This document discusses the uncertainty of measurements associated with the cyclic integrated reversible-bending fatigue tester (CIRFT) system and the resulting uncertainty in the acquired measurements and calculated information. The primary parameters measured during the CIRFT test include the deflection magnitude of the specimen, the load applied during bending, and the number of cycles to specimen gross failure. The associated primary calculated parameters are the bending radius/curvature and the bending moment. Secondary calculated parameters include specimen stress and strain amplitudes, as well as flexural rigidity. The uncertainty associated with the primary and secondary calculated parameters is investigated based on the known uncertainty in the measured parameters.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

CIRFT Data Update and Data Analyses for Spent Nuclear Fuel Vibration Reliability Study

The objective of this research is to collect experimental data on spent nuclear fuel (SNF) from pressurized water reactors (PWRs), including the H. B. Robinson Nuclear Power Station (HBR), Catawba Nuclear Station, North Anna Nuclear Power Station (NA), and the Limerick Nuclear Power Station (LMK) boiling water reactor (BWR). Data will be collected under simulated transportation environments using the cyclic integrated reversible-bending fatigue tester (CIRFT), an enabling hot-cell testing technology developed at Oak Ridge National Laboratory (ORNL). These data will be used to support ongoing SNF modeling activities and to address regulatory issues associated with SNF transport.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

CIRFT Testing of High-Burnup Used Nuclear Fuel Rods from the Pressurized Water Reactor and Boiling Water Reactor Environments (FY 2015 Status Report)

High burn-up spent nuclear fuel (SNF) cladding has a significant amount of microcracks and hydrides, which will reduce the stress intensity required for crack growth. The potential linking of microcracks during vibration loading could also reduce the fatigue threshold/incubation period significantly, accelerating fatigue failure. In addition to cladding damage, the microstructure of fuel pellets and the characteristics of the interfaces between fuel pellets and between fuel pellets and cladding are likely to be dramatically changed after high burn-up. These modifications can have a direct impact on the structural integrity and vibration response of SNF rods in transportation. As a result, vibration has been included as one of the mandatory testing conditions in the structural evaluation of packages used by the US Nuclear Regulation Commission (NRC) in transporting SNF (10 CFR §71.71). Prior to this program development, no current system is available to test the SNF and evaluate the performance of fuel rods during spent fuel transportation. The objective of this research is to develop a system that can appropriately test the response of high-burnup SNF rods in a simulated loading condition.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

CIRFT Data Update and Data Analyses for Spent Nuclear Fuel Vibration Reliability Study

The objective of this research is to collect experimental data on spent nuclear fuel (SNF) from pressurized water reactors (PWRs), including the H. B. Robinson Nuclear Power Station (HBR), Catawba Nuclear Station, North Anna Nuclear Power Station (NA), and the Limerick Nuclear Power Station (LMK) boiling water reactor (BWR).

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Spent nuclear fuel dynamic performance under normal conditions of transport

The objective of this project is to evaluate the spent nuclear fuel (SNF) vibration integrity under normal condition of transport. The SNF fatigue strength data has been collected from various pressurized water reactors. The CIRFT (Cyclic Integrated Reversible-Bending Fatigue Tester) has been used to simulate transportation environments. CIRFT is an enabling hot-cell testing technology developed at Oak Ridge National Laboratory (ORNL). The CIRFT consists mainly of a U-frame testing setup and a real-time curvature measurement method. The three-component U-frame setup of the CIRFT has two rigid arms and linkages to a universal testing machine. The curvature of rod bending is obtained through a three-point deflection measurement method. Three linear variable differential transformers (LVDTs) are used and clamped to the side connecting plates of the U-frame to capture the deformation of the rod. CIRFT results have provided insight into the fuel/clad system response to transportation related loads. Because of the non-homogeneous composite structure of the SNF system, finite element analyses (FEA) are needed to translate the global moment-curvature measurement into local stress-strain profiles. The detailed mechanisms of the pellet-pellet and pellet-clad interactions and the stress concentration effects at the pellet-pellet interface cannot be readily obtained directly from a CIRFT system measurement. Therefore, detailed FEA is used to understand the global test response. The major findings of CIRFT test on the high burn-up SNF are as follows: -) SNF system interface bonding plays an important role in SNF vibration performance; -) Fuel structure contributes to the SNF system stiffness; -) There are significant variations in stress and curvature of SNF systems during vibration cycles resulting from segment pellets and clad interaction, and -) SNF failure initiates at the pellet-pellet interface region and appears to be spontaneous.

42 ENGINEERING↗

Spent Nuclear Fuel Vibration Integrity Study

The objective of this research is to collect dynamic experimental data on spent nuclear fuel (SNF) under simulated transportation environments using the Cyclic Integrated Reversible-Bending Fatigue Tester (CIRFT), the hot-cell testing technology developed at Oak Ridge National Laboratory (ORNL). The collected CIRFT data will be utilized to support ongoing spent fuel modeling activities, and support SNF transportation related licensing issues. Recent testing to understand the effects of hydride reorientation on SNF vibration integrity is also being evaluated. CIRFT results have provided insight into the fuel/clad system response to transportation related loads. The major findings of CIRFT on the HBU SNF are as follows: SNF system interface bonding plays an important role in SNF vibration performance, Fuel structure contributes to the SNF system stiffness, There are significant variations in stress and curvature of SNF systems during vibration cycles resulting from segment pellets and clad interaction, and SNF failure initiates at the pellet-pellet interface region and appears to be spontaneous. Because of the non-homogeneous composite structure of the SNF system, finite element analyses (FEA) are needed to translate the global moment-curvature measurement into local stress-strain profiles. The detailed mechanisms of the pellet-pellet and pellet-clad interactions and the stress concentration effects at the pellet-pellet interface cannot be readily obtained directly from a CIRFT system measurement. Therefore, detailed FEA is used to understand the global test response, and that data will also be presented.

bending fatigue↗

Reversible Bending Fatigue Testing on Zry-4 Surrogate Rods

Testing high-burnup spent nuclear fuel (SNF) presents many challenges in areas such as specimen preparation, specimen installation, mechanical loading, load control, measurements, data acquisition, and specimen disposal because these tasks are complicated by the radioactivity of the test specimens. Research and comparison studies conducted at Oak Ridge National Laboratory (ORNL) resulted in a new concept in 2010 for a U-frame testing setup on which to perform hot-cell reversible bending fatigue testing. Subsequently, the three-dimensional finite element analysis and the engineering design of components were completed. In 2013 the ORNL team finalized the upgrade of the U-frame testing setup and the integration of the U-frame setup into a Bose dual linear motor test bench to develop a cyclic integrated reversible-bending fatigue tester (CIRFT). A final check was conducted on the CIRFT test system in August 2013, and the CIRFT was installed in the hot cell in September 2013 to evaluate both the static and dynamic mechanical response of SNF rods under simulated loads. The fatigue responses of Zircaloy-4 (Zry-4) cladding and the role of pellet pellet and pellet clad interactions are critical to SNF vibration integrity, but such data are not available due to the unavailability of an effective testing system. While the deployment of the developed CIRFT test system in a hot cell will provide the opportunity to generate the data, the use of a surrogate rod has proven quite effective in identifying the underlying deformation mechanism of an SNF composite rod under an equivalent loading condition. This paper presents the experimental results of using surrogate rods under CIRFT reversible cyclic loading. Specifically, monotonic and cyclic bending tests were conducted on surrogate rods made of a Zry-4 tube and alumina pellet inserts, both with and without an epoxy bond.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Spent Nuclear Fuel Vibration Integrity Study - 16332

The objective of this research is to collect dynamic experimental data on spent nuclear fuel (SNF) under simulated transportation environments using the Cyclic Integrated Reversible-Bending Fatigue Tester (CIRFT), the hot-cell testing technology developed at Oak Ridge National Laboratory (ORNL). The collected CIRFT data will be utilized to support ongoing spent fuel modeling activities, and support SNF transportation related licensing issues. Recent testing to understand the effects of hydride reorientation on SNF vibration integrity is also being evaluated. CIRFT results have provided insight into the fuel/clad system response to transportation related loads. The major findings of CIRFT on the HBU SNF are as follows: - SNF system interface bonding plays an important role in SNF vibration performance, - Fuel structure contributes to the SNF system stiffness, - There are significant variations in stress and curvature of SNF systems during vibration cycles resulting from segment pellets and clad interaction, and - SNF failure initiates at the pellet-pellet interface region and appears to be spontaneous. Because of the non-homogeneous composite structure of the SNF system, finite element analyses (FEA) are needed to translate the global moment-curvature measurement into local stress-strain profiles. The detailed mechanisms of the pellet-pellet and pellet-clad interactions and the stress concentration effects at the pellet-pellet interface cannot be readily obtained directly from a CIRFT system measurement. Therefore, detailed FEA is used to understand the global test response, and that data will also be presented. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

BWR Spent Nuclear Fuel Interfacial Bonding Efficiency Study

The objective of this project is to perform a systematic study of spent nuclear fuel (SNF, also known as “used nuclear fuel” [UNF]) integrity under simulated transportation environments using the Cyclic Integrated Reversible-Bending Fatigue Tester (CIRFT) hot-cell testing technology developed at Oak Ridge National Laboratory (ORNL) in August 2013. Under Nuclear Regulatory Commission (NRC) sponsorship, ORNL completed four benchmark tests, four static tests, and twelve dynamic or cycle tests on H. B. Robinson (HBR) high burn-up (HBU) fuel. The clad of the HBR fuels was made of Zircaloy-4. Testing was continued in fiscal year (FY) 2014 using Department of Energy (DOE) funds. Additional CIRFT testing was conducted on three HBR rods; two specimens failed, and one specimen was tested to over 2.23 × 10 7 cycles without failing. The data analysis on all the HBR SNF rods demonstrated that it is necessary to characterize the fatigue life of the SNF rods in terms of (1) the curvature amplitude and (2) the maximum absolute of curvature extremes. The maximum extremes are significant because they signify the maximum tensile stress for the outer fiber of the bending rod. CIRFT testing has also addressed a large variation in hydrogen content on the HBR rods. While the load amplitude is the dominant factor that controls the fatigue life of bending rods, the hydrogen content also has an important effect on the lifetime attained at each load range tested. In FY 15, eleven SNF rod segments from the Limerick BWR were tested using the ORNL CIRFT equipment; one test under static conditions and ten tests under dynamic loading conditions. Under static unidirectional loading, a moment of 85 N·m was obtained at a maximum curvature of 4.0 m -1 . The specimen did not show any sign of failure during three repeated loading cycles to a similar maximum curvature. Ten cyclic tests were conducted with amplitudes varying from 15.2 to 7.1 N·m. Failure was observed in nine of the tested rod specimens. The cycles-to-failure ranged from 1.22 × 10 5 to 4.70 × 10 6 , and the amplitudes varied from 15.2 to 7.6 N·m. The measurements at the interrupts indicated a range of flexural rigidity from 30 to 50 N·m 2 . Online monitoring revealed that the flexural rigidity was slightly lower due to the higher loading, from 25 to 42 N·m 2 . Generally, no substantial change of rigidity was observed based on the online monitoring during the cyclic fatigue testing process. Overall, the decreasing trend of sample lifetime with increasing amplitude is well defined.

interface bonding efficiency↗