Overview of SOFC Anode Interactions with Coal Gas Impurities

An overview of the results of SOFC anode interactions with phosphorus, arsenic, selenium, sulfur, antimony, and hydrogen chloride as single contaminants or in combinations is discussed. Tests were performed using both anode- and electrolyte-supported cells in synthetic and actual coal gas for periods greater than 1000 hours. Post-test analyses were performed to identify reaction products formed and their distribution, and compared to phases expected from thermochemical modeling. The ultimate purpose of this work is to establish maximum permissible concentrations for impurities in coal gas, to aid in the selection of appropriate coal gas clean-up technologies.

01 COAL, LIGNITE, AND PEAT↗

Degradation Mechanisms of SOFC Anodes in Coal Gas Containing Phosphorus

The interaction of phosphorus in synthetic coal gas with the nickel-based anode of solid oxide fuel cells has been investigated. Tests with both anode-supported and electrolyte-supported button cells were performed at 700 to 800oC in synthetic coal gas containing 0.5 to 10 ppm phosphorus, introduced as phosphine. Two primary modes of degradation were observed. The most obvious was the formation of a series of bulk nickel phosphide phases, of which Ni3P, Ni5P2, Ni12P5 and Ni2P were identified. Phosphorus was essentially completely captured by the anode, forming a sharp boundary between converted and unconverted anode portions. These products partially coalesced into large grains, which eventually affected electronic percolation through the anode support. Thermodynamic calculations predict that formation of the first binary nickel phosphide phase is possible at sub-parts per billion concentrations in coal gas at temperatures relevant to fuel cell operation. A second mode of degradation is attributed to surface diffusion of phosphorus to the active anode/electrolyte interface to form an adsorption layer. Direct evidence for the presence of such an adsorption layer on nickel was obtained by surface spectroscopies on fracture surfaces. Further, cell performance losses were observed well before the entire anode was converted to bulk nickel phosphide. Impedance spectroscopy revealed that these losses were primarily due to growth in electrodic resistance, whereas large ohmic increases were visible when the entire anode was converted to nickel phosphide phases. The rate of resistance growth for anode-supported cells showed a very low dependence on phosphorus concentration, attributed to phosphorus activity control within the anode by bulk nickel phosphide products.

01 COAL, LIGNITE, AND PEAT↗

Reversible Poisoning of the Nickel/Zirconia Solid Oxide Fuel Cell Anodes by Hydrogen Chloride in Coal Gas

The performance of anode-supported solid oxide fuel cells (SOFC) was evaluated in synthetic coal gas containing HCl in the temperature range 650 to 850oC. Exposure to up to 800 ppm HCl resulted in reversible poisoning of the Ni/zirconia anode by chlorine species adsorption, the magnitude of which decreased with increased temperature. Performance losses increased with the concentration of HCl to ~100 ppm, above which losses were insensitive to HCl concentration. Cell voltage had no effect on poisoning. No evidence was found for long-term degradation that can be attributed to HCl exposure. Similarly, no evidence of microstructural changes or formation of new solid phases as a result of HCl exposure was found. From thermodynamic calculations, solid nickel chloride phase formation was shown to be highly unlikely in coal gas. Further, the presence of HCl at even the highest anticipated concentrations in coal gas would minimally increase the volatility of nickel.

01 COAL, LIGNITE, AND PEAT↗

Overview of SOFC Anode Interactions with Coal Gas Impurities

An overview of the results of SOFC anode interactions with phosphorus, arsenic, selenium, sulfur, antimony, and hydrogen chloride as single contaminants or in combinations is discussed. Tests were performed using both anode- and electrolyte-supported cells in synthetic and actual coal gas for periods greater than 1000 hours. Post-test analyses were performed to identify reaction products formed and their distribution, and compared to phases expected from thermochemical modeling. The ultimate purpose of this work is to establish maximum permissible concentrations for impurities in coal gas, to aid in the selection of appropriate coal gas clean-up technologies.

01 COAL, LIGNITE, AND PEAT↗

Anode Interactions with Coal Gas Contaminants

This report describes efforts to characterize the interactions nickel anodes with phosphorus in coal gas using three different button cell configurations to emphasize particular degradation modes. Important parameters addressed included contaminant concentration, temperature, reaction time, fuel utilization, and current density. In addition, coupon tests in flow-through and flow-by arrangements were conducted to complement cell tests. The studies have involved extensive electrochemical testing using both dc and ac methods. Post-test analyses to determine the composition and extent of nickel modification are particularly important to understanding reactions that have occurred. This report also provides a thermodynamic assessment of contaminant reactions with nickel in a coal gas environment with regard to alteration phase formation. Contaminants addressed were phosphorus, arsenic, sulfur, selenium, and antimony. Phosphorus was found to interact strongly with nickel and result in extensive alteration phase formation, consistent with expectations based on thermodynamic properties. Even in button cell tests where the fuel utilization was low, phosphorus was found to be nearly completely captured by the nickel anode. For anode-supported cells, an important degradation mode involved loss of electronic percolation, the result of nickel phosphide formation, grain growth, and inducement of micro-fractures within the anode support. Even with excessive anode support conversion, electrochemical degradation rates were often very low. This is attributed to a “shadowing effect,” whereby a dense structure such as current leads prevent phosphorus from reacting with the nickel directly underneath. This effect maintains an electrical pathway to the active interface, and allows the cell to operate with minimal degradation until the anode is essentially completely consumed. In a planar stack, ribs on the interconnect plate would be expected to provide this conductive pathway in the event of phosphorus exposure. When phosphorus interactions proceeded to the active interface, most easily observed in tests with electrolyte-supported cells having a thin anode, the electrochemical performance decreased considerably.

01 COAL, LIGNITE, AND PEAT↗

Electrochemical, Structural and Surface Characterization of Nickel/Zirconia Solid Oxide Fuel Cell Anodes in Coal Gas Containing Antimony

The interaction of antimony with the nickel-zirconia solid oxide fuel cell (SOFC) anode has been investigated. Tests with both anode-supported and electrolyte-supported button cells were performed at 700 and 800oC in synthetic coal gas containing 10 ppb to 9 ppm antimony. Minor performance loss was observed immediately after Sb introduction to coal gas resulting in ca. 5 % power output drop. While no further degradation was observed during the following several hundred hours of testing, cells abruptly and irreversibly failed after 800-1500 hours depending on Sb concentration and test temperature. Antimony was found to interact strongly with nickel and result in extensive alteration phase formation, consistent with expectations based on thermodynamic properties. Nickel antimonide phases, NiSb and Ni5Sb2, were partially coalesced into large grains and eventually affected electronic percolation through the anode support. Initial degradation was attributed to diffusion of antimony to the active anode/electrolyte interface to form an adsorption layer.

01 COAL, LIGNITE, AND PEAT↗

Interactions of nickel/zirconia solid oxide fuel cell anodes with coal gas containing arsenic

The performance of anode-supported and electrolyte-supported solid oxide fuel cells was investigated in synthetic coal gas containing 0 to 10 ppm arsenic introduced as arsine. Arsenic was found to interact strongly with nickel in the anode, resulting in the formation of nickel-arsenic solid solution, Ni5As2 and Ni11As8, depending on temperature, arsenic concentration, and reaction time. For anode-supported cells, loss of electrical connectivity in the anode support was the principal mode of degradation, as nickel was converted to nickel arsenide phases that migrated to the surface to form large grains. Cell failure occurred well before the entire anode was converted to nickel arsenide, and followed a reciprocal square root of arsenic partial pressure dependence consistent with a diffusion-based rate-limiting step. Failure occurred more quickly with electrolyte-supported cells, which have a substantially smaller nickel inventory. For these cells, time to failure varied linearly with the reciprocal arsenic concentration in coal gas, and occurred when arsenic reached the anode/electrolyte interface. Test performed with nickel/zirconia coupons showed that arsenic was essentially completely captured in a narrow band near the fuel gas inlet.

Environmental Molecular Sciences Laboratory↗

Ni/YSZ Anode Interactions with Impurities in Coal Gas

Performance of solid oxide fuel cell (SOFC) with nickel/zirconia anodes on synthetic coal gas in the presence of low levels of phosphorus, arsenic, selenium, sulfur, hydrogen chloride, and antimony impurities were evaluated. The presence of phosphorus and arsenic led to the slow and irreversible SOFC degradation due to the formation of secondary phases with nickel, particularly close to the gas inlet. Phosphorus and antimony surface adsorption layers were identified as well. Hydrogen chloride and sulfur interactions with the nickel were limited to the surface adsorption only, whereas selenium exposure also led to the formation of nickel selenide for highly polarized cells.

01 COAL, LIGNITE, AND PEAT↗

Multicycle study on chemical-looping combustion of simulated coal gas with a CaSO{sub 4} oxygen carrier in a fluidized bed reactor

The cyclic test of a CaSO{sub 4}-based oxygen carrier (natural anhydrite) in alternating reducing simulated coal gas and oxidizing conditions was performed at 950{degree}C in a fluidized bed reactor at atmospheric pressure. A high concentration of CO{sub 2} was obtained in the reduction. The H{sub 2} and CO conversions and CO{sub 2} yield increased initially and final decreased significantly. The release of SO{sub 2} and H{sub 2}S during the cyclic test was found to be responsible for the decrease of reactivity of a CaSO{sub 4} oxygen carrier. The oxygen carrier conversion after the reduction reaction decreased gradually in the cyclic test. Through the comparison of mass-based reaction rates as a function of mass conversion at typical cycles, it was also evident that the reactivity of a CaSO{sub 4} oxygen carrier increased for the initial cycles but finally decreased after around 15 cycles. X-ray diffraction analysis revealed that the presence and intensity of the reduction sulfur species was in accordance with the results of gas conversion. The content of CaO was higher than expected, suggesting the formation of SO{sub 2} and H{sub 2}S during the cycles. Surface morphology analysis demonstrates that the natural anhydrite particle surface varied from impervious to porous after the cyclic test. It was also observed that the small grains on the surface of the oxygen carrier sintered in the cyclic tests. Energy-dispersive spectrum analysis also demonstrated the decrease of oxygen intensity after reduction, and CaO became the main component after the 20th oxidation. Pore structure analysis suggested that the particles agglomerated or sintered in the cyclic tests. The possible method for sulfur mitigation is proposed. Finally, some basic consideration on the design criteria of a CLC system for solid fuels using a CaSO{sub 4} oxygen carrier is discussed by the references and provides direction for future work. 49 refs., 10 figs., 5 tabs.

01 COAL, LIGNITE, AND PEAT↗

Effect of temperature on reduction of CaSO{sub 4} oxygen carrier in chemical-looping combustion of simulated coal gas in a fluidized bed reactor

Chemical-looping combustion (CLC) is a promising combustion technology for gaseous and solid fuel with efficient use of energy and inherent separation of CO{sub 2}. The concept of a coal-fueled CLC system using, calcium sulfate (CaSO{sub 4}) as oxygen carrier is proposed in this study. Reduction tests of CaSO{sub 4} oxygen carrier with simulated coal gas were performed in a laboratory-scale fluidized bed reactor in the temperature range of 890-950{degree}C. A high concentration of CO{sub 2} was obtained at the initial reduction period. CaSO{sub 4} oxygen carrier exhibited high reactivity initially and decreased gradually at the late period of reduction. The sulfur release during the reduction of CaSO{sub 4} as oxygen carrier was also observed and analyzed. H{sub 2} and CO{sub 2} conversions were greatly influenced by reduction temperature. The oxygen carrier conversion and mass-based reaction rates during the reduction at typical temperatures were compared. Higher temperatures would enhance reaction rates and result in high conversion of oxygen carrier. An XRD patterns study indicated that CaS was the dominant product of reduction and the variation of relative intensity with temperature is in agreement with the solid conversion. ESEM analysis indicated that the surface structure of oxygen carrier particles changed significantly from impervious to porous after reduction. EDS analysis also demonstrated the transfer of oxygen from the oxygen carrier to the fuel gas and a certain amount of sulfur loss and CaO formation on the surface at higher temperatures. The reduction kinetics of CaSO{sub 4} oxygen carrier was explored with the shrinking unreacted-core model. The apparent kinetic parameters were obtained, and the kinetic equation well predicted the experimental data. Finally, some basic considerations on the use of CaSO{sub 4} oxygen carrier in a CLC system for solid fuels were discussed.

01 COAL, LIGNITE, AND PEAT↗

Moessbauer study at room temperature of zinc ferrite as sorbent for hot coal gas desulphurization

Abstract: The method of using Moessbauer spectroscopy at room temperature was applied to assign the iron sites in one fresh zinc ferrite sample ZF with (1:1) concentration of their component oxides and calcined at 900C as well as its sulfurization derivatives at 750C in different coal gas of composition 0.5% H{sub 2}S + 0.5% H{sub 2}; 0.5% H{sub 2}S + 10% H{sub 2}; 0.5% H{sub 2}S + 25% H{sub 2}, and 0.5% H{sub 2}S + 10% H{sub 2}O (v). The most important iron phase obtained in the sulfurized samples, was pyrrhotite, Fe1-xS that exhibit three well different ional sextets. From the peak area and the associated magnetic hyperfine fields, the average magnetic field was calculated and indicates lowering in the number of iron vacancies whereas x is close to 0.

01 COAL, LIGNITE, AND PEAT↗

Study on the stability of sorbents removing H{sub 2}S from hot coal gas

Mixed metal oxide containing iron with the high-sulfur capacity and reactivity is considered as one of the most favorable sorbents for desulfurization in hot gas. The stability and life of iron-based sorbents are the main challenges for the hot gas cleanup techniques. Not only the effect of gas atmosphere but also the effect of ZnO and MgO on the stability of iron-based sorbent was studied in this work. The mechanism and factors influencing sorbent stability are discussed. The results showed that the coexistence of CO and H{sub 2} result in the instability of the zinc-iron-based sorbents. The reaction of carbon deposit is the crucial step affecting the stability of sorbent for hot gas desulfurization. ZnO in the sorbent is adverse to the physical stability of the iron-based sorbents. MgO in the sorbent hardly affects the physical stability of the iron-based sorbents but improves the capacity of removing the hydrogen sulfide from hot coal gas at 773 K. 12 refs., 8 figs., 5 tabs.

01 COAL, LIGNITE, AND PEAT↗

Desulfurization behavior of iron-based sorbent with MgO and TiO{sub 2} additive in hot coal gas

The sulfidation behaviors of iron-based sorbent with MgO and MgO-TiO{sub 2} are studied under different isothermal conditions from 623 to 873 K in a fixed bed reactor. The results of sorbents sulfidation experiments indicate that the sorbents with MgO and TiO{sub 2} additives are more attractive than those without additives for desulfurization of hot coal gas. The sulfur capacity (16.17, 18.45, and 19.68 g S/100 g sorbent) of M1F, M3F, and M5F sorbent containing 1, 3, and 5% MgO, respectively, is obviously bigger than that (15.02 g S/100 g sorbent) of M0F without additive. The feasible sulfidation temperature range for M3F sorbent is 773-873 K. The M3F sorbent is optimally regenerated at the temperature of 873 K, under the gas containing 2% oxygen, 15% steam and N{sub 2}, in the space velocity of 2500 h{sup -1}. The sorbent regenerated is also well performed in the second sulfidation (the effective sulfur capacities of 17.98 g S/100 g sorbents and the efficiency of removal sulfur of 99%). The capacity to remove sulfur decreases with steam content increasing in feeding gas from 0 to 10%, but it can restrain the formation of carbon and iron carbide. The addition of TiO{sub 2} in sorbent can shift the optimal sulfidation temperature lower. The iron-based sorbent with 3% MgO and 10% TiO{sub 2} (MFT) is active to the deep removal of H{sub 2}S and COS, especially in the temperature range of 673-723 K. The sulfur removal capacity of MFT sorbent is 21.60 g S/100 g sorbent. 16 refs., 12 figs., 8 tabs.

01 COAL, LIGNITE, AND PEAT↗

Interactions of Alumina-Based and Magnesia-Based Refractories with Iron Melts and Slags: A Review

A novel flash ironmaking technology (FIT) based on the direct reduction of iron ore concentrate with a reductant gas (such as hydrogen, natural gas, coal gas, or a combination thereof) in a flash furnace is being developed at the University of Utah. This technology which is undergoing large-scale laboratory testing aims at overcoming the limitations of blast furnace ironmaking by bypassing the problematic pelletization/sintering and cokemaking steps.[1–5] Refractory selection is expected to play an important step in the development of FIT and its proposed scale-up. For nominating an appropriate refractory for the FIT, understanding the interactions of candidate refractories with iron/iron oxide and slags under H{sub 2}/CO/CO{sub 2}/H{sub 2}O environments is necessary. This work is undertaken to review the existing literature on the interactions of important refractories with iron melts and relevant slags with an emphasis on two of the most commonly used refractories in ironmaking and steelmaking applications: the alumina-based refractories (used widely in blast furnace operations) and the magnesia-based refractories (used extensively in primary as well as secondary steelmaking). First, a comprehensive review on the interactions of alumina-based refractories with iron melts and slags has been done. Next the existing literature on the interactions of magnesia-based refractories with iron melts and relevant slags has been reviewed. Summaries have been included after each section and sub-section along with comments and critical insights from the authors. Finally, in the concluding remarks the differences in operating conditions between existing iron and steelmaking practices and the novel FIT have been highlighted. On the basis of these differences, it has been argued that the results and conclusions available from previous studies on refractory–metal–slag interactions are of little significance to flash ironmaking. Thus, there exists a need to carry out laboratory experiments for evaluating refractory performance in flash ironmaking under conditions relevant to the current process (FIT).

36 MATERIALS SCIENCE↗