Investigations of masers utilizing cross-relaxation
Cross relaxation processes in millimeter wave maser technology for obtaining maser amplification at higher frequencies
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Cross relaxation processes in millimeter wave maser technology for obtaining maser amplification at higher frequencies
An optical quantum thermometer with a submicron spatial resolution that is based on the physical phenomenon of optical response in the system of spin centers in silicon carbide under conditions of cross-relaxation between the optically active centers in quadruplet spin state and triplet centers, where there is anomalously strong dependence of the splitting of the fine structure on temperature, has been proposed.
Key to future spintronics and spin-based information processing technologies is the generation, manipulation, and detection of spin polarization in a solid state platform. Here, we theoretically explore an alternative route to spin injection via the use of dynamically polarized nitrogen-vacancy (NV) centers in diamond. We focus on the geometry where carriers and NV centers are confined to proximate, parallel layers and use a “trap-and-release” model to calculate the spin cross-relaxation probabilities between the charge carriers and neighboring NV centers. We identify near-unity regimes of carrier polarization depending on the NV spin state, applied magnetic field, and carrier g-factor. In particular, we find that unlike holes, electron spins are distinctively robust against spin-lattice relaxation by other, unpolarized paramagnetic centers. Further, the polarization process is only weakly dependent on the carrier hopping dynamics, which makes this approach potentially applicable over a broad range of temperatures.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
The processes that take place in the excited states of a trivalent Thulium (Tm) ion in an Yttrium Aluminum Garnet (YAG) crystal, being relevant to the use of this system for laser applications, have been the object of several studies. We have reexamined this system focusing our attention on the dynamics of Tm following its excitation in the H-3(sub 4) level. Under these conditions the system relaxes through a cross-relaxation process. H-3(sub 4) yields F-3(sub 4), H-3(sub 6) yields F-3(sub 4), whose rate depends upon both the concentration of the Tm ion and the temperature of the crystal. The excitation spectrum obtained by monitoring the 1.8 micron emission of Tm (due to the F-3(sub 4) yields H-3(sub 6) transition) indicates an increase in the contribution to this emission from the H-3(sub 4) level relative to the H-3(sub 5) level as the Tm concentration increases; this shows the increased role played by the H-3(sub 4) level in pumping the infrared emission. Correspondingly, the duration of the luminescence originating in the H-3(sub 4) level is shortened as the concentration of Tm increases. The concentration quenching of this lifetime can be fit to a model which assumes that the cross-relaxation is due to a dipole-dipole interaction; from this fit, the intrinsic Tm lifetime in the absence of cross relaxation can be derived. We have used this lifetime to calculate the rate of the cross-relaxation process. We have evaluated this rate as a function of the temperature and found it to be fastest at 77 K. We have also calculated the microscopic interaction parameters for the cross-relaxation process by using two independent experimental features: (1) the time evolution of the emission from the H-3(sub 4) level; and (2) the spectral overlap between the H-3(sub 4) yields F-3(sub 4) emission and the H-3(sub 6) yields F-3(sub 4) absorption. We have also considered the migration of excitation among the Tm ions in the F-3(sub 4) level and calculated the relevant microparameter by the use of the relevant spectral overlap. The data are consistent with the model in which the Tm ions, once excited into the H-3(sub 4) level decay by cross-relaxation to the F-3(sub 4), and then transfer rapidly their energy to other Tm ions.
The lithium yttrium silicate series of LiY 1-x Ln x SiO 4 exhibits superb chemical and optical properties, and with Ln = Ce 3+ , Sm 3+ , its spectroscopic characteristics and luminescence dynamics are investigated in the present work. Energy transfer and non-radiative relaxation dramatically influence the Ln 3+ luminescence spectra and decay dynamics, especially in the Ce 3+ -Sm 3+ co-doped phosphors. It is shown that thermal-quenching of the blue Ce 3+ luminescence is primarily due to thermal ionization in the 5d excited states rather than multi-phonon relaxation, whereas cross-relaxation arising from electric dipole-dipole interaction between adjacent Sm 3+ ions is the leading mechanism that quenches the red Sm 3+ luminescence. In the co-doped systems, Ce 3+ -Sm 3+ energy transfer in competing with the thermal quenching enhance the emission from Sm 3+ . The combined influences of concentration quenching, thermal ionization, energy transfer including cross-relaxation on the luminescence intensity of single-center and co-doped phosphors are analyzed based on the theories of ion-ion and ion-lattice interactions.
Highlights: ► Lowest spin-allowed and spin-forbidden f–d transitions locate at 250 and 280 nm. ► Cross relaxation shortens lifetime of {sup 5}D{sub 3} level, while that of {sup 5}D{sub 4} are unaffected. ► Cross-relaxation can explain concentration quenching of the {sup 5}D{sub 3} emission. ► Dipole–quadrupole interaction is responsible for the non-radiative relaxation. ► Li{sub 4}SrCa(SiO{sub 4}){sub 2}:Tb{sup 3+} is thermally stable and color tunable phosphor. -- Abstract: Tb{sup 3+} ions activated Li{sub 4}SrCa(SiO{sub 4}){sub 2} phosphors were synthesized using a solid state reaction method. The phase impurity was checked by XRD. The photoluminescence (PL) excitation spectrum, emission spectra at room and high temperature, decay curves of samples with different Tb{sup 3+} ions concentration were studied in detail. Cross-relaxation and the Inokuti–Hirayama model were used to analyze the experimental results. Li{sub 4}SrCa(SiO{sub 4}){sub 2}:xTb{sup 3+} are thermally stable and color tunable phosphors.
Highlights: ► The visible quantum cutting between Tb{sup 3+} in silicate Na{sub 3}Gd{sub 0.9−x}Y{sub x}Si{sub 3}O{sub 9}:0.1Tb{sup 3+} phosphors are firstly investigated. ► Gd{sup 3+} plays an important intermediate role during the QC process and reinforces the cross relaxation efficiency. ► Na{sub 3}Gd{sub 0.9}Tb{sub 0.1}Si{sub 3}O{sub 9} has potential application for 3D-PDPs and Hg-free lamps for the total QE of 151.2%. - Abstract: The visible quantum cutting via cross-relaxation between Tb{sup 3+} ions in Na{sub 3}Gd{sub 0.9−x}Y{sub x}Si{sub 3}O{sub 9}:0.1Tb{sup 3+} phosphors are identified for the first time. It has also been found that with the increase of the ratio of Gd{sup 3+}/Y{sup 3+}, the quantum cutting efficiency increases, which indicates the Gd{sup 3+} plays an important intermediate role in energy transfer to convert vacuum ultraviolet light to visible light and reinforces the cross relaxation efficiency during the quantum cutting process. In addition, the energy transfer process from Gd{sup 3+} to Tb{sup 3+} is also investigated and discussed in terms of luminescence spectra.
Graphical abstract: The afterglow of Tb{sup 3+} is observed in CaWO{sub 4} matrix. The main emission of the afterglow is ascribed to the {sup 5}D{sub 4} {yields} {sup 7}F{sub 5} and {sup 5}D{sub 4} {yields} {sup 7}F{sub 6}. Emission due to {sup 5}D{sub 3} {yields} {sup 7}F{sub 4} and {sup 5}D{sub 3} {yields} {sup 7}F{sub 5} is weak. The cross-relaxation dominate the afterglow emission and it enhances the transition from {sup 5}D{sub 4} whereas from {sup 5}D{sub 3}. Highlights: Black-Right-Pointing-Pointer A green long afterglow is observed from Tb{sup 3+} in CaWO{sub 4} matrix. Black-Right-Pointing-Pointer Two traps which may have a strong influence on the afterglow properties are revealed by TL. Black-Right-Pointing-Pointer A mechanism model based on energy transfer from WO{sub 4}{sup 2-} group to Tb{sup 3+} followed by cross-relaxation is proposed. -- Abstract: The Tb{sup 3+} doped CaWO{sub 4} phosphors are synthesized via high temperature solid state reaction. The X-ray diffraction shows that small amount of Tb{sup 3+} does not have a significant influence on the structure of CaWO{sub 4}. A broad absorption band of the WO{sub 4}{sup 2-} group is observed from photoluminescence and the energy transfer from WO{sub 4}{sup 2-} group to Tb{sup 3+} ions induces the f-f transition. The cross-relaxation between two adjacent Tb{sup 3+} ions weakens {sup 5}D{sub 3}-{sup 7}F{sub j} transitions and enhances the {sup 5}D{sub 4}-{sup 7}F{sub j} transitions, leading to a green long afterglow of the phosphors. The thermoluminescence curves centered around 75 Degree-Sign C reveal the trap depth for afterglow generation is about 0.74-0.77 eV. The optimum Tb{sup 3+} concentration for afterglow properties is about 1%. A deep hole trap is induced when Tb{sup 3+} concentration exceeds 1% and it suppresses the thermoluminescence and the decay properties.
We present a theoretical study of the Zeeman relaxation of the magnetically trappable lowest field seeking state of MnH ({sup 7{Sigma}}) in collisions with {sup 3}He. We analyze the collisional Zeeman transition mechanism as a function of the final diatomic state and its variation as a function of an applied magnetic field. We show that as a result of this mechanism the levels with {Delta}M{sub j}>2 give negligible contributions to the Zeemam relaxation cross section. We also compare our results to the experimental cross sections obtained from the buffer-gas cooling and magnetic trapping of this molecule and investigate the dependence of the Zeeman relaxation cross section on the accuracy of the three-body interaction at ultralow energies.
The energy transfer processes in Tm,Ho:YAG lasers were investigated in spectral studies and measurements of the temporal response to pulsed excitation. These processes include the population of the 3H4 pump band of Tm, cross-relaxation in Tm, the transfer of energy from Tm to Ho, and various loss mechanisms. It was found that the Tm cross-relaxation is due to a dipole-dipole interaction between Tm ions and that the rate of this process is a function of temperature and ion concentration.
Graphical abstract: - Highlights: • In 60ZnCl{sub 2}–20KCl–20BaCl{sub 2}–xTbCl{sub 3} glasses, no energy transfer occurred for 0 < x ≤ 0.34. • For 0.34 < x ≤ 1.25, the cross relaxation, ({sup 5}D{sub 3} → {sup 5}D{sub 4}) → ({sup 7}F{sub 0} ← {sup 7}F{sub 6}) occurred between Tb{sup 3+} ions. • For 0 < x ≤ 0.34, the 72% of excited electrons were radiatively relaxed by the {sup 5}D{sub 3} → {sup 7}F{sub J} transitions. • The lifetime of the {sup 5}D{sub 3} initial level was long and 1.1 ms. - Abstract: 60ZnCl{sub 2}–20KCl–20BaCl{sub 2}–xTbCl{sub 3} glasses (x = 0.10, 0.25, 0.50, 0.75, 1.00, and 1.25) were prepared by melt-quenching method, and Tb{sup 3+} fluorescence properties were investigated under 355 nm excitation. Regardless of x values, the electrons that were relaxed from the {sup 5}D{sub 3} to {sup 5}D{sub 4} level of Tb{sup 3+} ions by the multiphonon relaxation, were repressed to 28% of all the excited electrons because the ZnCl{sub 2}-based glass had much lower phonon energy than oxide glasses. For 0 < x ≤ 0.34, the cross relaxation, ({sup 5}D{sub 3} → {sup 5}D{sub 4}) → ({sup 7}F{sub 0} ← {sup 7}F{sub 6}), was repressed, and consequently 72% and 28% of all the excited electrons were radiatively relaxed by the {sup 5}D{sub 3} → {sup 7}F{sub J} (J = 6, 5, 4, 3, and 2) and {sup 5}D{sub 4} → {sup 7}F{sub J} (J = 6, 5, 4, and 3) transitions, respectively. The lifetimes of the {sup 5}D{sub 3} and {sup 5}D{sub 4} initial levels were obtained to be 1.1 and 2.1 ms, respectively.
The primary excited state decay and energy transfer processes in singly Tm{sup 3+}-doped TeO{sub 2}:ZnO:Bi{sub 2}O{sub 3}:GeO{sub 2} (TZBG) glass relating to the {sup 3}F{sub 4}{yields}{sup 3}H{sub 6}{approx}1.85 {mu}m laser transition have been investigated in detail using time-resolved fluorescence spectroscopy. Selective laser excitation of the {sup 3}H{sub 4} manifold at 794 nm, the {sup 3}H{sub 5} manifold at 1220 nm, and {sup 3}F{sub 4} manifold at 1760 nm has established that the {sup 3}H{sub 5} manifold is entirely quenched by multiphonon relaxation in tellurite glass. The luminescence from the {sup 3}H{sub 4} manifold with an emission peak at 1465 nm suffers strong suppression due to cross relaxation that populates the {sup 3}F{sub 4} level with a near quadratic dependence on the Tm{sup 3+} concentration. The {sup 3}F{sub 4} lifetime becomes longer as the Tm{sup 3+} concentration increases due to energy migration and decreases to 2.92 ms when [Tm{sup 3+}] = 4 mol. % as a result of quasi-resonant energy transfer to free OH{sup -} radicals present in the glass at concentrations between 1 x 10{sup 18} cm{sup -3} and 2 x 10{sup 18} cm{sup -3}. Judd-Ofelt theory in conjunction with absorption measurements were used to obtain the radiative lifetimes and branching ratios of the energy levels located below 25 000 cm{sup -1}. The spectroscopic parameters, the cross relaxation and Tm{sup 3+}({sup 3}F{sub 4}) {yields} OH{sup -} energy transfer rates were used in a numerical model for laser transitions emitting at 2335 nm and 1865 nm.
Visible quantum cutting (QC) through downconversion was observed upon 4f{sup 8}-4f{sup 7}5d{sup 1} excitation of Tb{sup 3+} in both BaGdB{sub 9}O{sub 16} and Ca{sub 8}MgGd(PO{sub 4}){sub 7} compounds. The QC involves a cross relaxation process between two neighboring Tb{sup 3+}. Modified and new QC models are proposed based on the QC mechanisms in Gd{sup 3+}-Tb{sup 3+} system. Two calculation equations for the cross relaxation efficiency are suggested according to the energy transfer theory and spectral results. By studying the spectral characteristics of Tb{sup 3+} in hosts from fluoride to oxide, it indicates that the visible QC in Gd{sup 3+}-Tb{sup 3+} system may occur mainly depending on the structural features of phosphors, rather than the phonon energies of matrixes. All of the above conclusions have meaning of guidance for investigating other phosphors with QC phenomenon.
The paper compares the cross-relaxation, energy transfer and loss processes in Tm- and Ho-doped YAG and YLF as a function of temperature, Tm concentration, and excitation power. Significant differences in the behavior of Tm and Tm,Ho in YAG and YLF crystals were found. The cross-relaxation rates of Tm(6 pct) are faster in YLF (about 5 microsec) than YAG (about 10 microsec). The energy transfer rates between Tm and Ho are faster in YLF than YAG. The time it takes for the maximum intensity of 1.7-micron emission to drop 10 percent is 25 microsec for YLF:Tm(6 pct),Ho(0.6 pct) and 65 microsec YAG:Tm(6 pct),Ho(0.5 pct). The losses occurring with increasing pump power for 2.1-micron emission of the above samples are 30 percent less in YLF than YAG. These qualitative differences point to YLF as a valuable 2-micron laser host material.
Highlights: • The upconversion emission of Ho{sup 3+} ions was tuned from green to red. • The upconversion mechanism of Ho{sup 3+} ions was discussed based on emission spectrum. • The conversion efficiency between Ho{sup 3+} and Ce{sup 3+} were studied and calculated. - Abstract: The red upconversion emission of lanthanide-doped fluoride nanocrystals have great potential applications in color display and anticounterfeiting applications, especially for biological imaging and biomedical. In this work, a significant enhancement of red upconversion emission of Ho{sup 3+} ions was successfully obtained in the cubic phase NaLuF{sub 4} nanocrystals through codoping Ce{sup 3+} ions under NIR 980 nm excitation. The ratio of red-to-green emission of Ho{sup 3+} ions was enhanced about 10-fold, which is due to two efficient cross relaxation processes derived from Ho{sup 3+} and Ce{sup 3+} ions promoted the red emission and quenched the green emission. The upconversion emission and luminescent colors of NaLuF{sub 4}: Yb{sup 3+}/Ho{sup 3+} nanocrystals were carefully investigated by a confocal microscopy setup. The possible upconversion emission mechanism and conversion efficiency of cross relaxation between Ho{sup 3+} and Ce{sup 3+} ions were discussed in detail. The current study suggests that strong red emission of NaLuF{sub 4}: Yb{sup 3+}/Ho{sup 3+}/Ce{sup 3+} nanomaterials can be used for color display and anticounterfeiting techniques.
Highlights: • Borate glasses with Sm3+ ions were synthesized by melt quenching technique. • Under 402 nm excitation Borate glasses show reddish orange luminescence. • Energy transfer through cross-relaxation leads to fall in decay time of Sm3+ ions. • I-H model confirms energy transfer between Sm3+ ions as dipole-dipole in nature. • 1 mol% Sm3+ ions in these glasses are apt for red photonic device applications. - Abstract: This work describes mainly the optical absorption, photoluminescence (PL) and decay spectral properties of Sm{sup 3+} ions doped borate glasses to understand their possible usage in tricolor w-LEDs and lasers.The XRD spectrum recorded for an un-doped glass confirms glassy nature of the as prepared glass. The Judd-Ofelt (J-O) intensity parameters evaluated from experimental oscillator strengths were used in estimating the various radiative parameters. Under 402 nm excitation, the PL spectra exhibit intense emission at 600 nm for which the decay spectral profiles were recorded.The decay profiles are converting from single exponential to non-exponential with increase in Sm{sup 3+} ion concentration ensuing decrease in experimental lifetimes which may be attributed to the efficient energy transfer through cross-relaxation process. The non-exponential decay curves fitted to I-H model reveals the interaction between the Sm{sup 3+} ions as dipole-dipole in nature. From the evaluated emission cross-sections, quantum efficiency, branching ratios and CIE co-ordinates, it is concluded that 1 mol% Sm{sup 3+} ions in these glasses are aptly suitable to fabricate reddish-orange luminescent devices.