Search NASASearch

SEARCH · Search NASA

Results for “Ceramic Capacitor”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

An Electron Backscatter Diffraction (EBSD)-Based Automated Tool for Ceramic Capacitor Grain Size Analysis

Ceramic capacitors continue to be recurring problem parts for NASA, despite best efforts to screen out potential defects and failures through environmental and electrical testing and nondestructive inspection techniques such as acoustic microscopy. The physical properties of ceramic capacitors necessitates thin dielectric layers capable of withstanding significant electric fields. Any defects in those ceramic layers can result in reduced insulation resistance failure modes including short circuit failures, so the quality and consistency of the dielectric material is critical. The size of the individual ceramic grains in the dielectric material is a critical parameter. However, judging “grain size” is not so simple—in a single capacitor there can be wide variation in grain sizes observed. It is theorized that by studying the grain size distributions of “known good” and “known bad” lots of capacitors, some conclusions could be drawn that would allow us to better predict to the reliability of future lots based on grain size distributions. The initial goal of this effort was to find or develop an automated tool that could inspect a capacitor and return grain size distribution results.

Robert Hodson

Ceramic Capacitor Delamination Problem

Update on ceramic capacitors issues since last years meeting. To including the story behind the issues behind the TIRS and SDO leaky capacitors.

Ceramic Capacitor

The Significance of Breakdown Voltages for Quality Assurance of Low-Voltage BME Ceramic Capacitors

Application of thin dielectric, base metal electrode (BME) ceramic capacitors for high-reliability applications requires development of testing procedures that can assure high quality and reliability of the parts. In this work, distributions of breakdown voltages (VBR) in variety of low-voltage BME multilayer ceramic capacitors (MLCCs) have been measured and analyzed. It has been shown that analysis of the distributions can indicate the proportion of defective parts in the lot and significance of the defects. Variations of the distributions after solder dip testing allow for an assessment of the robustness of capacitors to soldering-related stresses. The drawbacks of the existing screening and qualification methods to reveal defects in high-value, low-voltage MLCCs and the importance of VBR measurements are discussed. Analysis has shown that due to a larger concentration of oxygen vacancies, defect-related degradation of the insulation resistance (IR) and failures are more likely in BME compared to the precious metal electrode (PME) capacitors.

reliability

Humidity Testing of PME and BME Ceramic Capacitors with Cracks

Cracks in ceramic capacitors are one of the major causes of failures during operation of electronic systems. Humidity testing has been successfully used for many years to verify the absence of cracks and assure quality of military grade capacitors. Traditionally, only precious metal electrode (PME) capacitors were used in high reliability applications and the existing requirements for humidity testing were developed for this type of parts. With the advance of base metal electrode (BME) capacitors, there is a need for assessment of the applicability of the existing techniques for the new technology capacitors. In this work, variety of different PME and BME capacitors with introduced cracks were tested in humid environments at different voltages and temperatures. Analysis of the test results indicates differences in the behavior and failure mechanisms for BME and PME capacitors and the need for different testing conditions.

reliability

Insulation Resistance Degradation in Ni-BaTiO3 Multilayer Ceramic Capacitors

Insulation resistance (IR) degradation in NiBaTiO3 multilayer ceramic capacitors has been characterized by the measurement of both time to failure (TTF) and direct current leakage current as a function of stress time under highly accelerated life test conditions. The measured leakage current time dependence data fit well to an exponential form, and a characteristic growth time tau (sub SD) can be determined. A greater value of tau (sub SD) represents a slower IR degradation process. Oxygen vacancy migration and localization at the grain boundary region results in the reduction of the Schottky barrier height and has been found to be the main reason for IR degradation in NiBaTiO3 capacitors. The reduction of barrier height as a function oftime follows an exponential relation of phi (t ) = phi (0) e (exp -2Kt), where 13 the degradation rate constant K Koe (Ek/kT) is inversely proportional to the mean TTF (MTTF) and can be determined using an Arrhenius plot. For oxygen vacancy electromigration, a lower barrier height phi (0) will favor a slow IR degradation process, but a lower phi (0) will also promote electronic carrier conduction across the barrier and decrease the IR. As a result, a moderate barrier height phi (0) (and therefore a moderate IR value) with a longer MTTF (smaller degradation rate constant K) will result in a minimized IR degradation process and the most improved reliability in NiBaTiO3 multilayer ceramic capacitors.

reliability

Evaluation of Case Size 0603 BME Ceramic Capacitors

High volumetric efficiency of commercial base metal electrode (BME) ceramic capacitors allows for a substantial reduction of weight and sizes of the parts compared to currently used military grade precious metal electrode (PME) capacitors. Insertion of BME capacitors in space applications requires a thorough analysis of their performance and reliability. In this work, six types of cases size 0603 BME capacitors from three vendors have been evaluated. Three types of multilayer ceramic capacitors (MLCCs) were designed for automotive industry and three types for general purposes. Leakage currents in the capacitors have been measured in a wide range of voltages and temperatures, and measurements of breakdown voltages (VBR) have been used to assess the proportion and severity of defects in the parts. The effect of soldering-related thermal shock stresses was evaluated by analysis of distributions of VBR for parts in 'as is' condition and after terminal solder dip testing at 350 C. Highly Accelerated Life Testing (HALT) at different temperatures was used to assess the activation energy of degradation of leakage currents and predict behavior of the parts at life test and normal operating conditions. To address issues related to rework and manual soldering, capacitors were soldered onto different substrates at different soldering conditions. The results show that contrary to a common assumption that large-size capacitors are mostly vulnerable to soldering stresses, cracking in small size capacitors does happen unless special measures are taken during assembly processes.

testing

Insulation Resistance Degradation in Ni-BaTiO3 Multilayer Ceramic Capacitors

Insulation resistance (IR) degradation in Ni-BaTiO3 multilayer ceramic capacitors has been characterized by the measurement of both time to failure and direct-current (DC) leakage current as a function of stress time under highly accelerated life test conditions. The measured leakage current-time dependence data fit well to an exponential form, and a characteristic growth time SD can be determined. A greater value of tau(sub SD) represents a slower IR degradation process. Oxygen vacancy migration and localization at the grain boundary region results in the reduction of the Schottky barrier height and has been found to be the main reason for IR degradation in Ni-BaTiO3 capacitors. The reduction of barrier height as a function of time follows an exponential relation of phi (𝑡)=phi (0)e(exp -2Κt), where the degradation rate constant 𝐾=𝐾o𝑒(𝐸𝑘/𝑘𝑇) is inversely proportional to the mean time to failure (MTTF) and can be determined using an Arrhenius plot. For oxygen vacancy electromigration, a lower barrier height phi(0) will favor a slow IR degradation process, but a lower phi(0) will also promote electronic carrier conduction across the barrier and decrease the insulation resistance. As a result, a moderate barrier height phi(0) (and therefore a moderate IR value) with a longer MTTF (smaller degradation rate constant 𝐾) will result in a minimized IR degradation process and the most improved reliability in Ni-BaTiO3 multilayer ceramic capacitors.

dielectric degradation

Insulation Resistance and Leakage Currents in Low-Voltage Ceramic Capacitors with Cracks

Measurement of insulation resistance (IR) in multilayer ceramic capacitors (MLCCs) is considered a screening technique that ensures the dielectric is defect-free. This work analyzes the effectiveness of this technique for revealing cracks in ceramic capacitors. It is shown that absorption currents prevail over the intrinsic leakage currents during standard IR measurements at room temperature. Absorption currents, and consequently IR, have a weak temperature dependence, increase linearly with voltage (before saturation), and are not sensitive to the presence of mechanical defects. In contrary, intrinsic leakage currents increase super-linearly with voltage and exponentially with temperature (activation energy is in the range from 0.6 eV to 1.1 eV). Leakage currents associated with the presence of cracks have a weaker dependence on temperature and voltage compared to the intrinsic leakage currents. For this reason, intrinsic leakage currents prevail at high temperatures and voltages, thus masking the presence of defects.

testing

Insulation Resistance and Leakage Currents in Low-Voltage Ceramic Capacitors with Cracks

Measurement of insulation resistance (IR) in multilayer ceramic capacitors (MLCCs) is considered a screening technique that ensures the dielectric is defect-free. This work analyzes the effectiveness of this technique for revealing cracks in ceramic capacitors. It is shown that absorption currents prevail over the intrinsic leakage currents during standard IR measurements at room temperature. Absorption currents, and consequently IR, have a weak temperature dependence, increase linearly with voltage (before saturation), and are not sensitive to the presence of mechanical defects. In contrary, intrinsic leakage currents increase super-linearly with voltage and exponentially with temperature (activation energy is in the range from 0.6 eV to 1.1 eV). Leakage currents associated with the presence of cracks have a weaker dependence on temperature and voltage compared to the intrinsic leakage currents. For this reason, intrinsic leakage currents prevail at high temperatures and voltages, thus masking the presence of defects.

dielectric polarization

A General Reliability Model for Ni-BaTiO3-Based Multilayer Ceramic Capacitors

The evaluation of multilayer ceramic capacitors (MLCCs) with Ni electrode and BaTiO3 dielectric material for potential space project applications requires an in-depth understanding of their reliability. A general reliability model for Ni-BaTiO3 MLCC is developed and discussed. The model consists of three parts: a statistical distribution; an acceleration function that describes how a capacitor's reliability life responds to the external stresses, and an empirical function that defines contribution of the structural and constructional characteristics of a multilayer capacitor device, such as the number of dielectric layers N, dielectric thickness d, average grain size, and capacitor chip size A. Application examples are also discussed based on the proposed reliability model for Ni-BaTiO3 MLCCs.

statistical modeling

A Reliability Model for Ni-BaTiO3-Based (BME) Ceramic Capacitors

The evaluation of multilayer ceramic capacitors (MLCCs) with base-metal electrodes (BMEs) for potential NASA space project applications requires an in-depth understanding of their reliability. The reliability of an MLCC is defined as the ability of the dielectric material to retain its insulating properties under stated environmental and operational conditions for a specified period of time t. In this presentation, a general mathematic expression of a reliability model for a BME MLCC is developed and discussed. The reliability model consists of three parts: (1) a statistical distribution that describes the individual variation of properties in a test group of samples (Weibull, log normal, normal, etc.), (2) an acceleration function that describes how a capacitors reliability responds to external stresses such as applied voltage and temperature (All units in the test group should follow the same acceleration function if they share the same failure mode, independent of individual units), and (3) the effect and contribution of the structural and constructional characteristics of a multilayer capacitor device, such as the number of dielectric layers N, dielectric thickness d, average grain size r, and capacitor chip size S. In general, a two-parameter Weibull statistical distribution model is used in the description of a BME capacitors reliability as a function of time. The acceleration function that relates a capacitors reliability to external stresses is dependent on the failure mode. Two failure modes have been identified in BME MLCCs: catastrophic and slow degradation. A catastrophic failure is characterized by a time-accelerating increase in leakage current that is mainly due to existing processing defects (voids, cracks, delamination, etc.), or the extrinsic defects. A slow degradation failure is characterized by a near-linear increase in leakage current against the stress time; this is caused by the electromigration of oxygen vacancies (intrinsic defects). The two identified failure modes follow different acceleration functions. Catastrophic failures follow the traditional power-law relationship to the applied voltage. Slow degradation failures fit well to an exponential law relationship to the applied electrical field. Finally, the impact of capacitor structure on the reliability of BME capacitors is discussed with respect to the number of dielectric layers in an MLCC unit, the number of BaTiO3 grains per dielectric layer, and the chip size of the capacitor device.

reliability

Unstable insulation resistance in ceramic capacitors

The effects of low and varying values of insulation resistance (IR) and their significance in the cause of failure in ceramic capacitors were investigated. Two specific instances involving hardware failure involving ceramic capacitors were examined. It is shown that monolithic, multilayer ceramic capacitors may exhibit low and unstable IR at low voltages, or exhibit no voltage. Other significant results are reported.

Holladay, A. M.

Absorption Voltages and Insulation Resistance in Ceramic Capacitors with Cracks

Time dependence of absorption voltages (Vabs) in different types of low-voltage X5R and X7R ceramic capacitors was monitored for a maximum duration of hundred hours after polarization. To evaluate the effect of mechanical defects on Vabs, cracks in the dielectric were introduced either mechanically or by thermal shock. The maximum absorption voltage, time to roll-off, and the rate of voltage decrease are shown to depend on the crack-related leakage currents and insulation resistance in the parts. A simple model that is based on the Dow equivalent circuit for capacitors with absorption has been developed to assess the insulation resistance of capacitors. Standard measurements of the insulation resistance, contrary to the measurements based on Vabs, are not sensitive to the presence of mechanical defects and fail to reveal capacitors with cracks. Index Terms: Ceramic capacitor, insulation resistance, dielectric absorption, cracking.

cracking

Guidelines for Selection, Screening and Qualification of Low-Voltage Commercial Multilayer Ceramic Capacitors for Space Programs

This document has been developed in the course of NASA Electronic Parts and Packaging (NEPP) program and is not an official endorsement of the insertion of commercial capacitors in space programs or an established set of requirements for their testing. The purpose of this document is to suggest possible ways for selection, screening, and qualification of commercial capacitors for NASA projects and open discussions in the parts engineering community related to the use of COTS ceramic capacitors. This guideline is applicable to commercial surface mount chip, simple parallel plate design, multi-layer ceramic capacitors (MLCCs) rated to voltages of 100V and less. Parts with different design, e.g. low inductance ceramic capacitors (LICA), land grid array (LGA) etc., might need additional testing and tailoring of the requirements described in this document. Although the focus of this document is on commercial MLCCs, many procedures discussed below would be beneficial for military-grade capacitors

Teverovsky, Alexander A.

Ni-BaTiO3-Based Base-Metal Electrode (BME) Ceramic Capacitors for Space Applications

A multi-layer ceramic capacitor (MLCC) is a high-temperature (1350C typical) co-fired ceramic monolithic that is composed of many layers of alternately stacked oxide-based dielectric and internal metal electrodes. To make the dielectric layers insulating and the metal electrode layers conducting, only highly oxidation-resistant precious metals, such as platinum, palladium, and silver, can be used for the co-firing of insulating MLCCs in a regular air atmosphere. MLCCs made with precious metals as internal electrodes and terminations are called precious-metal electrode (PME) capacitors. Currently, all military and space-level applications only address the use of PME capacitors.

Ceramic Capacitors

Cracking Problems in Low-Voltage Chip Ceramic Capacitors

Cracking remains the major reason of failures in multilayer ceramic capacitors (MLCCs) used in in space electronics. Due to a tight quality control of space-grade components, the probability that as manufactured capacitors have cracks is relatively low, and cracking is often occurs during assembly, handling and the following testing of the systems. Majority of capacitors with cracks are revealed during the integration and testing period, but although extremely rarely, defective parts remain undetected and result in failures during the mission. This situation is aggravated by manual soldering and rework that are often used during low volume production of circuit boards for space. Although failures of MLCCs are often attributed to the post-manufacturing stresses, in many cases they are due to a combination of certain deviations in the manufacturing processes that result in hidden defects in the parts and excessive stresses during assembly and use. This report gives an overview of design, manufacturing and testing processes of MLCCs focusing on elements related to cracking problems. The existing and new screening and qualification procedures and techniques are briefly described and assessed by their effectiveness in revealing cracks. The capability of different test methods to simulate stresses resulting in cracking, mechanisms of failures in capacitors with cracks, and possible methods of selecting the most robust to manual soldering stresses capacitors are discussed.

testing

A Thermal Runaway Failure Model for Low-Voltage BME Ceramic Capacitors with Defects

Reliability of base metal electrode (BME) multilayer ceramic capacitors (MLCCs) that until recently were used mostly in commercial applications, have been improved substantially by using new materials and processes. Currently, the inception of intrinsic wear-out failures in high quality capacitors became much greater than the mission duration in most high-reliability applications. However, in capacitors with defects degradation processes might accelerate substantially and cause infant mortality failures. In this work, a physical model that relates the presence of defects to reduction of breakdown voltages and decreasing times to failure has been suggested. The effect of the defect size has been analyzed using a thermal runaway model of failures. Adequacy of highly accelerated life testing (HALT) to predict reliability at normal operating conditions and limitations of voltage acceleration are considered. The applicability of the model to BME capacitors with cracks is discussed and validated experimentally.

reliability